668 resultados para sputtering
Resumo:
Thin films of Y--Ba--Cu--O have been prepared by conventional methods of RF sputtering. The films exhibit superconducting onset temperatures as high as 91K, midpoint at 80K and a zero resistance state at 35K. Critical current measurements implied critical current densities of the order of 31 A/cm exp 2 . An attempt has been made to establish the role of substrate and various deposition parameters. 7 ref.--AA.
Resumo:
This paper deals with the reactive sputtering of titanium in an argon and oxygen mixture. The variation in cathode potential as a function of oxygen partial pressure has been explained in terms of cathode poisoning effects. The titania films deposited during this process have been studied for their structural and optical characteristics. The effect of substrate temperature (from 25 to 400 °C) and annealing (from 250 to 700 °C) on the packing density, refractive index, extinction coefficient, and crystallinity has been investigated. The refractive index varied from 2.24 to 2.46 and extinction coefficient from 2.6 × 10-3 to 10.4× 10-3 at 500 nm as the substrate temperature increased from 25 to 400 °C. The refractive index increased from 2.19 to 2.35 and extinction coefficient changed from 3.2× 10-3 to 11.6 × 10-3 at 500 nm as the annealing temperature was increased from 250 to 700 °C. Anatase and rutile phases have been observed in the films deposited at 400 °C substrate temperature and annealed at 300 °C. The changes in the optical constants at higher substrate temperature have been attributed to an increase in packing density, oxygen content, and crystallinity of the films.
Resumo:
Studies of ZrO2 films prepared by d.c. reactive magnetron sputtering are described. The effects of substrate temperature on the packing density, refractive index, extinction coefficient and crystallinity phase have been investigated in the temperature range 25–450 °C. The refractive index varied from 1.84 to 1.95 and extinction coefficient from 2 × 10−3 to 9.6 × 10−3. This was explained on the basis of an increase in packing density from 0.686 to 0.813. The change in packing density has been attributed to a decrease in the oxygen condensation at higher temperatures. Annealing results in a decrease in refractive index and increase in extinction coefficient. The films deposited at 150 °C showed a monoclinic phase which transforms to a tetragonal phase at higher substrate temperatures.
Resumo:
The characteristics of the high pressure oxygen-sputtering plasma in the pressure range 0.8–2.4 mbar have been studied using the Langmuir probe technique. The variation in plasma parameters such as positive ion density, electron density, mean electron energy and floating potential with pressure and temperature has been investigated. It has been observed that the positive ion density increases at high substrate temperatures whereas the negative ion density decreases. The study of the variation in mean electron energy and floating potential also indicated the possibility that the number of negative ions is less when the substrates are at elevated temperatures. Since the negative ions are supposed to cause re-sputtering and make the films off-stoichiometric, the reduction in the negative ion density as observed at elevated substrate temperatures is better suited for depositing stoichiometric YBa2Cu3O7−δ superconducting thin films.
Resumo:
Utilising Jones' method associated with the Wiener-Hopf technique, explicit solutions are obtained for the temperature distributions on the surface of a cylindrical rod without an insulated core as well as that inside a cylindrical rod with an insulated inner core when the rod, in either of the two cases, is allowed to enter, with a uniform speed, into two different layers of fluid with different cooling abilities. Simple expressions are derived for the values of the sputtering temperatures of the rod at the points of entry into the respective layers, assuming the upper layer of the fluid to be of finite depth and the lower of infinite extent. Both the problems are solved through a three-part Wiener-Hopf problem of special type and the numerical results under certain special circumstances are obtained and presented in tabular forms.
Resumo:
Niobium pentoxide thin films have been deposited on silicon and platinum-coated silicon substrates by reactive magnetron sputtering. The as-deposited films were amorphous and showed good electrical properties in terms of a dielectric permittivity of about 30, and leakage current density of 10(-6) A cm(-2) al a field of 120 kV cm(-1). A rapid thermal annealing process at 800 degrees C further increased the dielectric constant to 90 and increased the leakage current density to 5 x 10(-6) A cm(-2). The current-voltage characteristics observed at low and high fields suggested a combination of phenomena at different regimes of applied electric field. The capacitance-voltage characteristics performed in the metal-insulator-semiconductor configuration indicated good electronic interfaces with a nominal trap density of 4.5 x 10(12) cm(-2) eV(-1), which is consistent with the behavior observed with conventional dielectrics such as SiO2 on silicon surfaces.
Resumo:
The kinetics of the processes in facing targets sputtering of multicomponent oxide films is presented. The novel configuration of the process exhibits an enhanced ionization efficiency. Discharge diagnostics performed using optical emission spectroscopy revealed strong dependence of plasma parameters on process conditions. Numerical simulation based on thermalization and diffusion of sputtered atoms has been performed to estimate the transport efficiency in off-axis mode. Composition, structure and epitaxial quality of YBa2Cu3O7-x films prepared was found to be strongly dependent on atomic flux ratios (of Cu/Y and Ba/Y) arriving at the substrate, resputtering effect and phase stability of YBa2Cu3O7-x These studies have been shown to be useful in understanding the complex processes that occur in sputtering of multicomponent films. (C) 1999 Elsevier Science S.A. All rights reserved.
Resumo:
The optimisation is reported on the design of unbalanced magnetron (UBM) sputtering cathodes. For the study, a planar circular cathode backed by a double-coil electromagnet (compatible for a 100 mm diameter target) was developed. The variation of the structure and strength of the magnetic field in front of the target was investigated for different current combinations in the electromagnetic coils, and its effect on the sputtering process was analysed. The observations on the magnetic field geometry revealed some interesting features, such as the balancing point of the fields along the axis (null-point), and the zero axial region over the target surface (B-z = 0 ring). The positions of both could be controlled by adjusting the ratio of the electric current in the coils. The magnetic field null-point could be used as a reference for the region of homogeneous film growth. The B-z = 0 ring was the location where the glow discharge concentrated (or where the maximum target erosion occurred). The diameter of the ring determined the area covered by the discharge and thus the sputtering efficiency. The optimum substrate position can be fixed according to the position of the null-point and optimisation of sputtering can be achieved by adjusting the diameter of the B-z = 0 ring. The results of this study should be helpful in the designing of an ideal UBM using permanent magnets as well as electromagnets. (C) 1999 Elsevier Science Ltd. All rights reserved.
Resumo:
Titanium dioxide (TiO(2)) films have been deposited on glass and p-silicon (1 0 0) substrates by DC magnetron sputtering technique to investigate their structural, electrical and optical properties. The surface composition of the TiO(2) films has been analyzed by X-ray photoelectron spectroscopy. The TiO(2) films formed on unbiased substrates were amorphous. Application of negative bias voltage to the substrate transformed the amorphous TiO(2) into polycrystalline as confirmed by Raman spectroscopic studies. Thin film capacitors with configuration of Al/TiO(2)/p-Si have been fabricated. The leakage current density of unbiased films was 1 x10(-6) A/cm(2) at a gate bias voltage of 1.5 V and it was decreased to 1.41 x 10(-7) A/cm(2) with the increase of substrate bias voltage to -150 V owing to the increase in thickness of interfacial layer of SiO(2). Dielectric properties and AC electrical conductivity of the films were studied at various frequencies for unbiased and biased at -150 V. The capacitance at 1 MHz for unbiased films was 2.42 x 10(-10) F and it increased to 5.8 x 10(-10) F in the films formed at substrate bias voltage of -150 V. Dielectric constant of TiO(2) films were calculated from capacitance-voltage measurements at 1 MHz frequency. The dielectric constant of unbiased films was 6.2 while those formed at -150 V it increased to 19. The optical band gap of the films decreased from 3.50 to 3.42 eV with the increase of substrate bias voltage from 0 to -150 V. (C) 2011 Elsevier B. V. All rights reserved.
Resumo:
Zn1−xMgxO (x = 0.3) thin films have been fabricated on Pt/TiO2/SiO2/Si substrates using multimagnetron sputtering technique. The films with wurtzite structure showed a (002) preferred orientation. Ferroelectricity in Zn1−xMgxO films was established from the temperature dependent dielectric constant and the polarization hysteresis loop. The temperature dependent study of dielectric constant at different frequencies exhibited a dielectric anomaly at 110 °C. The resistivity versus temperature characteristics showed an anomalous increase in the vicinity of the dielectric transition temperature. The Zn1−xMgxO thin films exhibit well-defined polarization hysteresis loop, with a remanent polarization of 0.2 μC/cm2 and coercive field of 8 kV/cm at room temperature.
Resumo:
Titanium-carbon (Ti-C) thin films of different compositions were prepared by a combination of pulsed DC (for Ti target) and normal DC (for graphite target) magnetron co-sputtering on oxidized silicon and fused quartz substrates. At 33.7 at.% of C content, pure hcp Ti transforms into fcc-TiC with a preferential orientation of (2 2 0) along with (1 1 1) and (2 0 0). A clear transformation in the preferential orientation from (2 2 0) to (1 1 1) has been observed when the C content was increased to 56 at.%. At 62.5 at.% of C, TiC precipitates in an amorphous carbon matrix whereas further increase in C leads to X-ray amorphous films. The cross-sectional scanning electron microscope images reveal that the films with low carbon content consists of columnar grains, whereas, randomly oriented grains are in an amorphous carbon matrix at higher carbon content. A dramatic variation was observed in the mechanical properties such as hardness, H, from 30 to 1 GPa and in modulus, E, from 255 to 25 GPa with varying carbon content in the films. Resistance to plastic deformation parameter was observed as 0.417 for films containing 62.5 at.% of C. Nanoscratch test reveals that the films are highly scratch resistant with a coefficient of friction ranging from 0.15 to 0.04. (C) 2012 Elsevier B.V. All rights reserved.