929 resultados para prism-waveguide coupler


Relevância:

40.00% 40.00%

Publicador:

Resumo:

The field of surface polariton physics really took off with the prism coupling techniques developed by Kretschmann and Raether, and by Otto. This article reports on the construction and operation of a rotatable, in vacuo, variable temperature, Otto coupler with a coupling gap that can be varied by remote control. The specific design attributes of the system offer additional advantages to those of standard Otto systems of (i) temperature variation (ambient to 85 K), and (ii) the use of a valuable, additional reference point, namely the gap-independent reflectance at the Brewster angle at any given, fixed temperature. The instrument is placed firmly in a historical context of developments in the field. The efficacy of the coupler is demonstrated by sample attenuated total reflectance results on films of platinum, niobium, and yttrium barium copper oxide and on aluminum/gallium arsenide (Al/GaAs) Schottky diode structures. (C) 2000 American Institute of Physics. [S0034-6748(00)02411-4].

Relevância:

40.00% 40.00%

Publicador:

Resumo:

One dimensional magnetic photonic crystals (1D-MPC) are promising structures for integrated optical isolator applications. Rare earth substituted garnet thin films with proper Faraday rotation are required to fabricate planar 1D-MPCs. In this thesis, flat-top response 1D-MPC was proposed and spectral responses and Faraday rotation were modeled. Bismuth substituted iron garnet films were fabricated by RF magnetron sputtering and structures, compositions, birefringence and magnetooptical properties were studied. Double layer structures for single mode propagation were also fabricated by sputtering for the first time. Multilayer stacks with multiple defects (phase shift) composed of Ce-YIG and GGG quarter-wave plates were simulated by the transfer matrix method. The transmission and Faraday rotation characteristics were theoretically studied. It is found that flat-top response, with 100% transmission and near 45o rotation is achievable by adjusting the inter-defect spacing, for film structures as thin as 30 to 35 μm. This is better than 3-fold reduction in length compared to the best Ce-YIG films for comparable rotations, thus allows a considerable reduction in size in manufactured optical isolators. Transmission bands as wide as 7nm were predicted, which is considerable improvement over 2 defects structure. Effect of repetition number and ratio factor on transmission and Faraday rotation ripple factors for the case of 3 and 4 defects structure has been discussed. Diffraction across the structure corresponds to a longer optical path length. Thus the use of guided optics is required to minimize the insertion losses in integrated devices. This part is discussed in chapter 2 in this thesis. Bismuth substituted iron garnet thin films were prepared by RF magnetron sputtering. We investigated or measured the deposition parameters optimization, crystallinity, surface morphologies, composition, magnetic and magnetooptical properties. A very high crystalline quality garnet film with smooth surface has been heteroepitaxially grown on (111) GGG substrate for films less than 1μm. Dual layer structures with two distinct XRD peaks (within a single sputtered film) start to develop when films exceed this thickness. The development of dual layer structure was explained by compositional gradient across film thickness, rather than strain gradient proposed by other authors. Lower DC self bias or higher substrate temperature is found to help to delay the appearance of the 2nd layer. The deposited films show in-plane magnetization, which is advantageous for waveguide devices application. Propagation losses of fabricated waveguides can be decreased by annealing in an oxygen atmosphere from 25dB/cm to 10dB/cm. The Faraday rotation at λ=1.55μm were also measured for the waveguides. FR is small (10° for a 3mm long waveguide), due to the presence of linear birefringence. This part is covered in chapter 4. We also investigated the elimination of linear birefringence by thickness tuning method for our sputtered films. We examined the compressively and tensilely strained films and analyze the photoelastic response of the sputter deposited garnet films. It has been found that the net birefringence can be eliminated under planar compressive strain conditions by sputtering. Bi-layer GGG on garnet thin film yields a reduced birefringence. Temperature control during the sputter deposition of GGG cover layer is critical and strongly influences the magnetization and birefringence level in the waveguide. High temperature deposition lowers the magnetization and increases the linear birefringence in the garnet films. Double layer single mode structures fabricated by sputtering were also studied. The double layer, which shows an in-plane magnetization, has an increased RMS roughness upon upper layer deposition. The single mode characteristic was confirmed by prism coupler measurement. This part is discussed in chapter 5.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The results of theoretical investigations of two-channel waveguide modulator based on Surface Wave (SW) propagation are presented. The structure studied consists of two n-type semiconductor waveguide channels separated from each other by a dielectric gap and coated by a metal. The SW propagates at the semiconductor-metal interface across an external magnetic field which is parallel to the interface. An external dc voltage is applied to the metal surface of one channel to provide a small phase shift between two propagating modes. In a coupled mode approximation, two possible regimes of operation of the structure, namely as a directional coupler and as an electro-optical modulator, are considered. Our results suggest new applications in millimeter and submillimeter wave solid-state electronics and integrated optics.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Low loss index enhanced planar waveguides in Nd3+-doped silicate glass were fabricated by 3.0 MeV C+ ion implantation. The enhancement of the refractive index confined the light propagating in the waveguide. The prism-coupling method was used to measure dark modes in the waveguide. The effective refractive indices of the waveguide were obtained based on the dark modes. The moving fiber method was applied to measure the waveguide propagation loss. Loss measured in non-annealed samples is about 0.6 dB/cm. And the waveguide mode optical near-field output at 633 nm was presented. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nd:silicate glass was implanted at room temperature by 6.0 MeV C3+ ions with a dose of 2.0 x 10(15) ions cm(-2). A waveguide with thickness of about 6.3 mu m was formed. The prism-coupling method was used to observe the dark modes of the waveguide at 633 nm and 1539 nm, respectively. There are three dark modes at 633 nm, of which one is the enhanced-index mode. The propagation loss of the enhanced-index mode in the waveguide measured at 633 nm is 0.42 dB cm(-1) after annealing at 217 degrees C for 35 min. The reflectivity calculation method was applied to simulate the refractive index profiles in the waveguide. The mode optical near-field output at 633 nm was presented.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A photonic wire-based directional coupler based on SOI was fabricated by e-beam lithography (EBL) and the inductively coupled plasma (ICP) etching method. The size of the sub-micron waveguide is 0.34 mu m x 0.34 mu m, and the length in the coupling region and the separation between the two parallel waveguides are 410 and 0.8 mu m, respectively. The measurement results are in good agreement with the results simulated by 3D finite-difference time-domain method. The transmission power from two output ports changed reciprocally with about 23 nm wavelength spacing between the coupled and direct ports. The extinction ratio of the device was between 5 and 10 dB, and the insertion loss of the device in the wavelength range 1520-1610 nm was between 22 and 24 dB, which included an about 18.4 +/- 0.4 dB coupling loss between the taper fibers and the polished sides of the device. (c) 2008 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A 3-dB multimode interference optical coupler based on rib waveguides with trapezoidal cross section was designed and fabricated on silicon-on-insulator wafer. Potassium hydroxide (KOH) anisotropic chemical etching of silicon was used to fabricate the waveguides to obtain smooth interface. A modified finite-difference beam propagation method was used to simulate the multimode rib waveguide with slope interfaces. The rms roughness of etching interface is as small as 1.49 nm. The propagation loss of the waveguide is 1.3 dB/cm at wavelength of 1.55 mum. The fabricated 3-dB coupler has a good uniformity of 0.2 dB.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

SOI (silicon-on-insulator) is a new material with a lot of important performances such as large index difference, low transmission loss. Fabrication processes for SOI based optoelectronic devices are compatible with conventional IC processes. Having the potential of OEIC monolithic integration, SOI based optoelectronic devices have shown many good characteristics and become more and more attractive recently. In this paper, the recent progresses of SOI waveguide devices in our research group are presented. By highly effective numerical simulation, the single mode conditions for SOI rib waveguides with rectangular and trapezoidal cross-section were accurately investigated. Using both chemical anisotropic wet etching and plasma dry etching techniques, SOI single mode rib waveguide, MMI coupler, VOA (variable optical attenuator), 2X2 thermal-optical switch were successfully designed and fabricated. Based on these, 4X4 and 8X8 SOI optical waveguide integrated switch matrixes are demonstrated for the first time.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Size tolerance of a 4X4 general interference tapered multimode interference (MMI) coupler in a silicon-on-insulator (SOI) structure is investigated by means of a 2-D finite difference beam propagation method (2D-FDBPM), together with an effective refractive index method (EIM). The results show that the tapered multimode interference coupler exhibits relatively larger size tolerance when light is launched from the edgeport than from midport, though it has much better output power uniformity when light is launched from midport. Besides that, it can reduce the device length greatly. The 4X4 general interference tapered MMI coupler has a slightly larger size tolerance compared with a conventional straight multimode interference coupler. (C) 2003 Society of Photo-Optical Instrumentation Engineers.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

MMI coupler with large cross section has low coupling loss between the device and fiber. However, large chip area is required. Recently proposed N x N tapered MMI coupler shows a substantial reduction in device geometry. No such kind of devices with N > 2 has yet been realized up to now. The authors have demonstrated a 4 x 4 parabolically tapered MMI coupler with large cross section that can match the SM fiber in silicon-on-insulator (SOI) technology. The device exhibits a minimum uniformity of 0.36 dB and excess loss of 3.7 dB, It represents a key component for realization of MMI-based silicon integrated optical circuit technology.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Characteristics of microring/racetrack resonators, in submicron SOI rib waveguides, have been investigated. The effects of waveguide dimensions, coupler design, roughness, and oxide cladding are considered. Moreover, guided mode, loss and dispersion of such waveguides are analyzed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Oxidizing thick porous silicon layer into silicon dioxide is a timesaving and low-cost process for producing thick silicon dioxide layer used in silicon-based optical waveguide devices. The solution of H2O2 is proposed to post-treat thick porous silicon (PS) films. The prepared PS layer as the cathode is applied about 10 mA/cm(2) current in mixture of ethanol, HF, and H2O2 solutions, in order to improve the stability and the smoothness of the surface. With the low-temperature dry-O-2 pre-oxidizations and high-temperature wet O-2 oxidizations process, a high-quality SiO2 30 mu m thickness layer that fit for the optical waveguide device was prepared. The SEM images show significant improved smoothness on the surface of oxidized PS thick films, the SiO2 film has a stable and uniformity reflex index that measured by the prism coupler, the uniformity of the reflex index in different place of the wafer is about 0.0003.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A silicon-on-insulator based channel-shifted multimode interference coupler is designed and fabricated. A two dimensional beam propagation method is used to analyze the dependence of coupler′s performances on the width and length of the multimode waveguide. The device fabricated has a power shift ratio of 73 and an excess loss of about 2.2 dB. An enhancement of fabrication accuracies could further improve the coupler performances.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Here, we demonstrate that efficient nano-optical couplers can be developed using closely spaced gap plasmon waveguides in the form of two parallel nano-sized rectangular slots in a thin metal film or membrane. Using the rigorous numerical finite-difference and finite element algorithms, we investigate the physical mechanisms of coupling between two neighboring gap plasmon waveguides and determine typical coupling lengths for different structural parameters of the coupler. Special attention is focused onto the analysis of the effect of such major coupler parameters, such as thickness of the metal film/membrane, slot width, and separation between the plasmonic waveguides. Detailed physical interpretation of the obtained unusual dependencies of the coupling length on slot width and film thickness is presented based upon the energy consideration. The obtained results will be important for the optimization and experimental development of plasmonic sub-wavelength compact directional couplers and other nano-optical devices for integrated nanophotonics.