996 resultados para semiconductor epitaxial layers
Resumo:
Indicator inks, previously shown to be capable of rapidly assessing photocatalytic activity via a novel photo-reductive mechanism, were simply applied via an aerosol spray onto commercially available pieces of Activ (TM) self-cleaning glass. Ink layers could be applied with high evenness of spread, with as little deviation as 5% upon UV-visible spectroscopic assessment of 25 equally distributed positions over a 10 cm x 10 cm glass cut. The inks were comprised of either a resazurin (Rz) or dichloroindophenol (DCIP) redox dye with a glycerol sacrificial electron donor in an aqueous hydroxyethyl cellulose (HEC) polymer media. The photo-reduction reaction under UVA light of a single spot was monitored by UV-vis spectroscopy and digital images attained from a flat-bed scanner in tandem for both inks. The photo-reduction of Rz ink underwent a two-step kinetic process, whereby the blue redox dye was initially reduced to a pink intermediate resorufin (Rf) and subsequently reduced to a bleached form of the dye. In contrast, a simple one-step kinetic process was observed for the reduction of the light blue redox dye DCIP to its bleached intermediates. Changes in red-green-blue colour extracted from digital images of the inks were inversely proportional to the changes seen at corresponding wavelengths via UV-visible absorption spectroscopy and wholly indicative of the reaction kinetics. The photocatalytic activity areas of cuts of Activ (TM) glass, 10 cm x 10 cm in size, were assessed using both Rz and DCIP indicator inks evenly sprayed over the films: firstly using UVA lamp light to activate the underlying Activ (TM) film (1.75 mW cm(-2)) and secondly under solar conditions (2.06 +/- 0.14 mW cm(-2)). The photo-reduction reactions were monitored solely by flat-bed digital scanning. Red-green-blue values of a generated 14 x 14 grid (196 positions) that covered the entire area of each film image were extracted using a Custom-built program entitled RGB Extractor(C). A homogenous degradation over the 196 positions analysed for both Rz (Red colour deviation = 19% UVA, 8% Solar: Green colour deviation = 17% UVA, 12% Solar) and DCIP (Red colour deviation = 22% UVA, 16% Solar) inks was seen in both UVA and solar experiments, demonstrating the consistency of the self-cleaning titania layer on Activ (TM). The method presented provides a good solution for the high-throughput photocatalytic screening of a number of homogenous photocatalytically active materials simultaneously or numerous positions on a single film; both useful in assessing the homogeneity of a film or determining the best combination of reaction components to produce the optimum performance photocatalytic film. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Novel diode test structures have been manufactured to characterize long-range dopant diffusion in tungsten silicide layers. A tungsten silicide to p-type silicon contact has been characterized as a Schottky barrier rectifying contact with a silicide work function of 4.8 eV. Long-range diffusion of boron for an anneal at 900 °C for 30 min has been shown to alter this contact to become ohmic. Long-range diffusion of phosphorus with a similar anneal alters the contact to become a bipolar n-p diode. Bipolar diode action is demonstrated experimentally for anneal schedules of 30 min at 900 °C, indicating long-range diffusion of phosphorus (~38 µm), SIMS analysis shows dopant redistribution is adversely affected by segregation to the silicide/oxide interface. The concept of conduit diffusion has been demonstrated experimentally for application in advanced bipolar transistor technology. © 2009 IEEE.
Resumo:
The properties of the combinatorial frequency generation and wave scattering by periodic stacks of nonlinear passive semiconductor layers are explored. It is demonstrated that the nonlinearity in passive weakly nonlinear semiconductor medium has the resistive nature associated with the dynamics of carriers. The features of the combinatorial frequency generation and the effects of the pump wave scattering and parameters of the constituent semiconductor layers on the efficiency of the frequency mixing are discussed and illustrated by the examples. © 2013 IEICE.
Resumo:
Epitaxial BaTiO3 films and epitaxial BaTiO3/SrTiO3 multilayers were grown by pulsed laser deposition on vicinal surfaces of (001)-oriented Nb-doped SrTiO3 (SrTiO3:Nb) single-crystal substrates. Atomic force microscopy was used to investigate the surface topography of the deposited films. The morphology of the films, of the BaTiO3/SrTiO3 interfaces, and of the column boundaries was investigated by cross-sectional high-resolution transmission electron microscopy. Measurements of the dielectric properties were performed by comparing BaTiO3 films and BaTiO3/SrTiO3 multilayers of different numbers of individual layers, but equal overall thickness. The dielectric loss saturates for a thickness above 300 nm and linearly decreases with decreasing film thickness below a thickness of 75 nm. At the same thickness of 75 nm, the thickness dependence of the dielectric constant also exhibits a change in the linear slope both for BaTiO3 films and BaTiO3/SrTiO3 multilayers. This behaviour is explained by the change observed in the grain morphology at a thickness of 75 nm. For the thickness dependence of the dielectric constant, two phenomenological models are considered, viz. a 'series-capacitor' model and a 'dead-layer' model.
Resumo:
The formation of epitaxial BaTiO3/SrTiO3 multilayers; is studied in terms of the growth mechanism by investigating surface morphologies, crystalline orientations, microstructures, and structures of the interfaces, as well as by determining the dielectric properties. Under specific conditions, the epitaxial BaTiO3 films follow a layer-then-island (Stranski-Krastanov) mechanism on SrTiO3 (001)-oriented substrates. In view of actual efforts made to grow epitaxial superlattices involving very thin individual layers of BaTiO3 and/or SrTiO3, we have determined that the BaTiO3 films Of up to 6,nm thickness do not show any defects and have a sharp BaTiO3-on-SrTiO3 interface. On the contrary, SrTiO3-on-BaTiO3 interfaces within multilayers are rough, probably due to the different growth mechanisms of the two different materials, or due to a difference in the morphological stability of the growth surfaces caused by different surface energies of BaTiO3 and SrTiO3 and by different mobilities of the Ba and Sr atoms reaching the SrTi3 and BaTiO3 layers, respectively.
Resumo:
Epitaxial thin films Of various bismuth-layered perovskites SrBi(2)Ta(2)O(9), Bi(4)Ti(3)O(12), BaBi(4)Ti(4)O(15), and Ba(2)Bi(4)Ti(5)O(18) were deposited by pulsed laser deposition onto epitaxial conducting LaNiO(3) or SrRuO(3) electrodes on single crystalline SrTiO(3) substrates with different crystallographic orientations or on top of epitaxial buffer layers on (100) silicon. The conductive perovskite electrodes and the epitaxial ferroelectric films are strongly influenced by the nature of the substrate, and bismuth-layered perovskite ferroelectric films with mixed (100), (110)- and (001)-orientations as well as with uniform (001)-, (116)- and (103)- orientations have been obtained. Structure and morphology investigations performed by X-ray diffraction analysis, scanning probe microscopy, and transmission electron microscopy reveal the different epitaxial relationships between films and substrates. A clear correlation of the crystallographic orientation of the epitaxial films with their ferroelectric properties is illustrated by macroscopic and microscopic measurements of epitaxial bismuth-layered perovskite thin films of different crystallographic orientations.
Resumo:
Epitaxial BaTiO3 films and BaTiO3/SrTiO3 multilayers were grown by pulsed laser deposition (PLD) on (001)-oriented Nb-doped SrTiO3 (SrTiO3:Nb) substrates. Measurements of the dielectric properties were performed comparing BaTiO3 films and BaTiO3/SrTiO3 multilayers of different number of individual layers, but equal overall thickness. The dielectric loss saturates for a thickness above 300 nm, and linearly decreases with decreasing film thickness below a thickness of 75 nm, and it is independent on the number of multilayers, pointing to some interface effect. The thickness dependence of the dielectric constant of BaTiO3 films and BaTiO3/SrTiO3 multilayers; exhibits a change in the linear slope at a thickness of 75 nm. This behavior is explained by the change observed in the morphology at a thickness of 75 nm. In order to explain the thickness dependence of the dielectric constant, two approaches are considered in this paper, viz. a "series capacitor" model and a "dead layer" model.
Resumo:
Cu2ZnSnSe4 (CZTSe) is a p-type semiconductor with a high absorption coefficient, 104 to 105 cm-1, and is being seen as a possible replacement for Cu(In,Ga)Se2 in thin film solar cells. Yet, there are some fundamental properties of CZTSe that are not well known, one of them is its band gap. In order to resolve its correct value it is necessary to improve the growth conditions to ensure that single phase crystalline thin films are obtained. One of the problems encountered when growing CZTSe is the loss of Sn through evaporation of SnSe. Stoichiometric films are then difficult to obtain and usually there are other phases present. One possible way to overcome this problem is to increase the pressure of growth of CZTSe. This can be done by introducing an atmosphere of an inert gas like Ar or N2. In this work we report the results of morphological, structural and optical studies of the properties of CZTSe thin films grown by selenization of DC magnetron sputtered metallic layers under different Ar pressures. The films are analysed by SEM/EDS, Raman scattering and XRD.
Resumo:
There is an increasing demand for renewable energies due to the limited availability of fossil and nuclear fuels and due to growing environmental problems. Photovoltaic (PV) energy conversion has the potential to contribute significantly to the electrical energy generation in the future. Currently, the cost for photovoltaic systems is one of the main obstacles preventing production and application on a large scale. The photovoltaic research is now focused on the development of materials that will allow mass production without compromising on the conversion efficiencies. Among important selection criteria of PV material and in particular for thin films, are a suitable band gap, high absorption coefficient and reproducible deposition processes capable of large-volume and low cost production. The chalcopyrite semiconductor thin films such as Copper indium selenide and Copper indium sulphide are the materials that are being intensively investigated for lowering the cost of solar cells. Conversion efficiencies of 19 % have been reported for laboratory scale solar cell based on CuInSe2 and its alloys. The main objective of this thesis work is to optimise the growth conditions of materials suitable for the fabrication of solar cell, employing cost effective techniques. A typical heterojunction thin film solar cell consists of an absorber layer, buffer layer and transparent conducting contacts. The most appropriate techniques have been used for depositing these different layers, viz; chemical bath deposition for the window layer, flash evaporation and two-stage process for the absorber layer, and RF magnetron sputtering for the transparent conducting layer. Low cost experimental setups were fabricated for selenisation and sulphurisation experiments, and the magnetron gun for the RF sputtering was indigenously fabricated. The films thus grown were characterised using different tools. A powder X-ray diffractometer was used to analyse the crystalline nature of the films. The energy dispersive X-ray analysis (EDX) and scanning electron microscopy i (SEM) were used for evaluating the composition and morphology of the films. Optical properties were investigated using the UV-Vis-NIR spectrophotometer by recording the transmission/absorption spectra. The electrical properties were studied using the two probe and four probe electrical measurements. Nature of conductivity of the films was determined by thermoprobe and thermopower measurements. The deposition conditions and the process parameters were optimised based on these characterisations.
Resumo:
The scope of this work is the fundamental growth, tailoring and characterization of self-organized indium arsenide quantum dots (QDs) and their exploitation as active region for diode lasers emitting in the 1.55 µm range. This wavelength regime is especially interesting for long-haul telecommunications as optical fibers made from silica glass have the lowest optical absorption. Molecular Beam Epitaxy is utilized as fabrication technique for the quantum dots and laser structures. The results presented in this thesis depict the first experimental work for which this reactor was used at the University of Kassel. Most research in the field of self-organized quantum dots has been conducted in the InAs/GaAs material system. It can be seen as the model system of self-organized quantum dots, but is not suitable for the targeted emission wavelength. Light emission from this system at 1.55 µm is hard to accomplish. To stay as close as possible to existing processing technology, the In(AlGa)As/InP (100) material system is deployed. Depending on the epitaxial growth technique and growth parameters this system has the drawback of producing a wide range of nano species besides quantum dots. Best known are the elongated quantum dashes (QDash). Such structures are preferentially formed, if InAs is deposited on InP. This is related to the low lattice-mismatch of 3.2 %, which is less than half of the value in the InAs/GaAs system. The task of creating round-shaped and uniform QDs is rendered more complex considering exchange effects of arsenic and phosphorus as well as anisotropic effects on the surface that do not need to be dealt with in the InAs/GaAs case. While QDash structures haven been studied fundamentally as well as in laser structures, they do not represent the theoretical ideal case of a zero-dimensional material. Creating round-shaped quantum dots on the InP(100) substrate remains a challenging task. Details of the self-organization process are still unknown and the formation of the QDs is not fully understood yet. In the course of the experimental work a novel growth concept was discovered and analyzed that eases the fabrication of QDs. It is based on different crystal growth and ad-atom diffusion processes under supply of different modifications of the arsenic atmosphere in the MBE reactor. The reactor is equipped with special valved cracking effusion cells for arsenic and phosphorus. It represents an all-solid source configuration that does not rely on toxic gas supply. The cracking effusion cell are able to create different species of arsenic and phosphorus. This constitutes the basis of the growth concept. With this method round-shaped QD ensembles with superior optical properties and record-low photoluminescence linewidth were achieved. By systematically varying the growth parameters and working out a detailed analysis of the experimental data a range of parameter values, for which the formation of QDs is favored, was found. A qualitative explanation of the formation characteristics based on the surface migration of In ad-atoms is developed. Such tailored QDs are finally implemented as active region in a self-designed diode laser structure. A basic characterization of the static and temperature-dependent properties was carried out. The QD lasers exceed a reference quantum well laser in terms of inversion conditions and temperature-dependent characteristics. Pulsed output powers of several hundred milli watt were measured at room temperature. In particular, the lasers feature a high modal gain that even allowed cw-emission at room temperature of a processed ridge wave guide device as short as 340 µm with output powers of 17 mW. Modulation experiments performed at the Israel Institute of Technology (Technion) showed a complex behavior of the QDs in the laser cavity. Despite the fact that the laser structure is not fully optimized for a high-speed device, data transmission capabilities of 15 Gb/s combined with low noise were achieved. To the best of the author`s knowledge, this renders the lasers the fastest QD devices operating at 1.55 µm. The thesis starts with an introductory chapter that pronounces the advantages of optical fiber communication in general. Chapter 2 will introduce the fundamental knowledge that is necessary to understand the importance of the active region`s dimensions for the performance of a diode laser. The novel growth concept and its experimental analysis are presented in chapter 3. Chapter 4 finally contains the work on diode lasers.
Resumo:
Ultrathin bimetallic layers create unusual magnetic and surface chemical effects through the modification of electronic structure brought on by low dimensionality, polymorphism, reduced screening, and epitaxial strain. Previous studies have related valence and core-level shifts to surface reactivity through the d-band model of Hammer and Nørskov, and in heteroepitaxial films this band position is determined by competing effects of coordination, strain, and hybridization of substrate and overlayer states. In this study we employ the epitaxially matched Pd on Re{0001} system to grow films with no lateral strain. We use a recent advancement in low-energy electron diffraction to expand the data range sufficiently for a reliable determination of the growth sequence and out-of-plane surface relaxation as a function of film thickness. The results are supported by scanning tunneling microscopy and X-ray photoemission spectroscopy, which show that the growth is layer-by-layer with significant core-level shifts due to changes in film structure, morphology, and bonding.
Resumo:
This paper reports a direct observation of an interesting split of the (022)(022) four-beam secondary peak into two (022) and (022) three-beam peaks, in a synchrotron radiation Renninger scan (phi-scan), as an evidence of the layer tetragonal distortion in two InGaP/GaAs (001) epitaxial structures with different thicknesses. The thickness, composition, (a perpendicular to) perpendicular lattice parameter, and (01) in-plane lattice parameter of the two epitaxial ternary layers were obtained from rocking curves (omega-scan) as well as from the simulation of the (022)(022) split, and then, it allowed for the determination of the perpendicular and parallel (in-plane) strains. Furthermore, (022)(022) omega:phi mappings were measured in order to exhibit the multiple diffraction condition of this four-beam case with their split measurement.
Resumo:
Semiconductor magnetic quantum dots are very promising structures, with novel properties that find multiple applications in spintronic devices. EuTe is a wide gap semiconductor with NaCl structure, and strong magnetic moments S=7/2 at the half filled 4f(7) electronic levels. On the other hand, SnTe is a narrow gap semiconductor with the same crystal structure and 4% lattice mismatch with EuTe. In this work, we investigate the molecular beam epitaxial growth of EuTe on SnTe after the critical thickness for island formation is surpassed, as a previous step to the growth of organized magnetic quantum dots. The topology and strain state of EuTe islands were studied as a function of growth temperature and EuTe nominal layer thickness. Reflection high energy electron diffraction (RHEED) was used in-situ to monitor surface morphology and strain state. RHEED results were complemented and enriched with atomic force microscopy and grazing incidence X-ray diffraction measurements made at the XRD2 beamline of the Brazilian Synchrotron. EuTe islands of increasing height and diameter are obtained when the EuTe nominal thickness increases, with higher aspect ratio for the islands grown at lower temperatures. As the islands grow, a relaxation toward the EuTe bulk lattice parameter was observed. The relaxation process was partially reverted by the growth of the SnTe cap layer, vital to protect the EuTe islands from oxidation. A simple model is outlined to describe the distortions caused by the EuTe islands on the SnTe buffer and cap layers. The SnTe cap layers formed interesting plateau structures with easily controlled wall height, that could find applications as a template for future nanostructures growth. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Spin polarization is a key characteristic in developing spintronic devices. Diluted magnetic heterostructures (DMH), where subsequent layers of conventional and diluted magnetic semiconductors (DMS) are alternate, are one of the possible ways to obtain it. Si being the basis of modern electronics, Si or other group-IV DMH can be used to build spintronic devices directly integrated with conventional ones. In this work we study the physical properties and the spin-polarization effects of p-type DMH based in group-IV semiconductors (Si, Ge, SiGe, and SiC), by performing self-consistent (k) over right arrow . (p) over right arrow calculations in the local spin density approximation. We show that high spin polarization can be maintained in these structures below certain values of the carrier concentrations. Full spin polarization is attained in the low carrier concentration regime for carrier concentrations in the DMS layer up to similar to 2.0 x 10(19) cm(-3) for Si and up to similar to 6.0 x 10(19) cm(-3) for SiC. Partial, but still important spin polarization can be achieved for all studied group-IV DMH, with the exception of Ge for carrier concentrations up to 6.0 x 10(19) cm(-3). The role played by the effective masses and the energy splitting of the spin-orbit split-off hole bands is also discussed throughout the paper.