The strong photoluminescence (PL) of SiOx:H prepared by plasma enhanced chemical vapor deposition has been systematically studied in conjunction with infrared and micro-Raman spectra. We have found that each PL spectrum is comprised of two Gaussian components, a main band and a shoulder. The main band might originate from amorphous silicon clusters embedded in die SiOx network, and its redshift with annealing temperature is due to expansion of the silicon clusters. The shoulder remains at about 835 nm in spite of the annealing temperature and possibly comes from luminescent defect centers. The enhanced PL spectra after 1170 degrees C annealing are attributed to the quantum confinement effects of nanocrystalline silicon embedded in the SiO2 matrix. (C) 1998 American Institute of Physics.
Resumo:
The microstructure, hydrogen bonding configurations and hydrogen content of high quality and stable hydrogenated amorphous silicon (a-Si:H) films prepared by a simple ''uninterrupted growth/annealing" plasma enhanced chemical vapor deposition technique have been investigated by Raman scattering and infrared absorption spectroscopy. The high stability a-Si:H films contain small amounts of a microcrystalline phase and not less hydrogen (10-16 at. %), particularly, the clustered phase hydrogen, Besides, the hydrogen distribution is very inhomogeneous. Some of these results are substantially distinct from those of conventional device-quality n-Si:H film or stable cr-Si:H films prepared by the other techniques examined to date. The stability of n-Si:H films appears to have no direct correlation with the hydrogen content or the clustered phase hydrogen concentration. The ideal n-Si:H network with high stability and low defect density is perhaps not homogeneous. (C) 1998 American Institute of Physics.
Resumo:
We use nuclear reaction analysis to study hydrogen in unintentionally doped GaN, and high-concentration hydrogen, nearly 10(21) cm(-3), is detected. Accordingly, a broad but intense infrared absorption zone with a peak at 2962 cm(-1) is reported, which is tentatively assigned to the stretch mode of NH: Ga complex. The complex is assumed to be one candidate answering for background electrons in unintentionally doped GaN. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
High-quality GaN epilayers have been grown by gas source molecular beam epitaxy using ammonia as the nitrogen source. During the growth, the growth rate is up to 1.2 mu m/h and can be varied from 0.3 to 1.2 mu m. The unintentional n-type doping as low as 7x10(17) cm(-3) was obtained at room temperature. Low-temperature photoluminescence spectrum was dominated by near-edge emission without deep-level related luminescence, indicative of high-quality epilayers. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
GaN epilayers on sapphire (0001) substrates were grown by the gas source molecular beam epitaxy (GSMBE) method using ammonia (NH,) gas as the nitrogen source. Properties of gallium nitride (GaN) epilayers grown under various growth conditions were investigated. The growth rate is up to 0.6 mu m/h in our experiments. Cathodoluminescence, photoluminescence and Hall measurements were used to characterize the films. It was shown that the growth parameters have a significant influence on the GaN properties. The yellow luminescence was enhanced at higher growth temperature. And a blue emission which maybe related to defects or impurity was observed. Although the emission at 3.31 eV can be suppressed by a low-temperature buffer layer, a high-quality GaN epilayer can be obtained without the buffer layer. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
We use a polarizer to investigate quantum-well infrared absorption, and report experimental results as follows. The intrasubband transition was observed in GaAs/AlxGa1-xAs multiple quantum wells (MQWs) when the incident infrared radiation (IR) is polarized parallel to the MQW plane. According to the selection rule, an intrasubband transition is forbidden. Up to now, most studies have only observed the intersubband transition between two states with opposite parity. However, our experiment shows not only the intersubband transitions, but also the intrasubband transitions. In our study, we also found that for light doping in the well (4x10(18) cm(-3)), the intrasubband transition occurs only in the lowest subband, while for the heavy doping (8x10(18) cm(-3)), such a transition occurs not only in the lowest subband, but also in the first excited one, because of the electron subband filling. Further experimental results show a linear dependence of the intrasubband transition frequency on the root of the well doping density. These data are in good agreement with our numerical results. Thus we strongly suggest that such a transition can be attributed to plasma oscillation. Conversely, when the incident IR is polarized perpendicular to the MQW plane, intersubband-transition-induced signals appear, while the intrasubband-transition-induced spectra disappear for both light and heavy well dopings. A depolarization blueshift was also taken into account to evaluate the intersubband transition spectra at different well dopings. Furthermore, we performed a deep-level transient spectroscopy (DLTS) measurement to determine the subband energies at different well dopings. A good agreement between DLTS, infrared absorption, and numerical calculation was obtained. In our experiment, two important phenomena are noteworthy: (1) The polarized absorbance is one order of magnitude higher than the unpolarized spectra. This puzzling result is well explained in detail. (2) When the IR, polarized perpendicular to the well plane, normally irradiates the 45 degrees-beveled edge of the samples, we only observed intersubband transition spectra. However, the intrasubband transition signals caused by the in-plane electric-field component are significantly absent. The reason is that such in-plane electric-field components can cancel each other out everywhere during the light propagating in the samples. The spectral widths of bound-to-bound and bound-to-continuum transitions were also discussed, and quantitatively compared to the relaxation time tau, which is deduced from the electron mobility. The relaxation times deduced from spectral widths of bound-to-bound and bound-to-continuum transitions are also discussed, and quantitatively compared to the relaxation time deduced from electron mobility. [S0163-1829(98)01912-2].
Resumo:
We have examined photoluminescence (PL), IR absorption and Raman spectra of a series of hydrogenated amorphous silicon oxide (a-SiOx:H, (0 < x < 2)) films fabricated by plasma enhanced chemical vapor deposition (PECVD). Two strong luminescence bands were observed at room temperature, one is a broad envelope comprising a main peak around 670 nm and a shoulder at 835 nm, and the other, peaked around 850 nm; is found only after being annealed up to 1170 degrees C in N-2 environment. In conjunction with IR and Raman spectra, the origins of the two luminescent bands and their annealing behaviors are discussed on the basis of quantum confinement effects.
Resumo:
Raman scattering, photoluminescence (PL), and nuclear reaction analysis (MA) have been employed to investigate the effects of rapid thermal annealing (RTA) on GaN films grown on sapphire (0001) substrates by gas-source molecular-beam epitaxy, The Raman spectra showed the presence of the E-2 (high) mode of GaN and shift of this mode from 572 to 568 cm(-1) caused by annealing. The results showed that RTA has a significant effect on the strain relaxation caused by the lattice and thermal expansion misfit between the GaN epilayer and the substrate. The PL peak exhibited a blueshift in its energy position and a decrease in the full width at half maximum after annealing, indicating an improvement in the optical quality of the film. Furthermore, a green luminescence appeared after annealing and increased in intensity with increasing annealing time. This effect was attributed to H concentration variation in the GaN film, which was measured by NRA. A high H concentration exists in as-grown GaN, which can neutralize the deep level, and the H-bonded complex dissociates during RTA, This leads to the appearance of a luminescent peak in the PL spectrum. (C) 1998 American Institute of Physics.
Resumo:
The effect of rapid thermal annealing (RTA) in a Nz ambient up to 900 degrees C has been investigated for GaN films grown on sapphire(0 0 0 1) substrates. Raman spectra, X-ray diffractometry and Hall-effect studies were performed for this purpose. The Raman spectra show the presence of the E-2 (high) mode and a shift in the wave number of this mode with respect to the annealing processing. This result suggests the presence and relaxation of residual stress due to thermal expansion misfit in the films which are confirmed by X-ray measurements and the structure quality of GaN epilayer was improved. Furthermore, the electron mobility increased at room temperature with respect to decrease of background electron concentration after RTA. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
The low frequency (<13 MHz) dielectric response and its light-induced change in undoped a-Si:H were investigated in detail. The dielectric constant epsilon (the real part) in this range decreases with illumination time: following a stretched exponential law similar to that found for other light-induced changes. The saturation relative change was about 0.1-0.2 % for the measured samples. The change is fading away either after repeated illumination-annealing training or by aging at room temperature. The present results indicate some rearrangement of the whole Si network caused by light soaking.
Resumo:
The structural characteristics of gallium nitride (GaN) films grown on sapphire(0001) substrates by gas source molecular beam epitaxy (GSMBE) have been investigated using high-resolution synchrotron irradiation X-ray diffraction and cathodoluminescence with a variable energy electron beam. Besides the well-known GaN hexagonal structure, a small portion of cubic phase GaN was observed. The X-ray measurements provide an essential means for the structural identification of the GaN layers. Arising from the variable penetration depth of the electron beam in the cathodoluminescence measurements, it was found that the fraction of the GaN cubic-phase typically increased as the probing depth was increased. The results suggest that the GaN cubic phase is mostly located near the interface between the substrate and GaN layer due to the initial nucleation.
Resumo:
A parallel optical communication subsystem based on a 12 channels parallel optical transmitter module and a 12 channels parallel optical receiver module can be used as a 10Gbps STM-64 or an OC-192 optical transponder. The bit error rate of this parallel optical communication subsystem is about 0 under the test by SDH optical transport tester during three hours and eighteen minutes.
Resumo:
Tandem amorphous silicon solar cells have attracted extensive interest because of better performance than single junction counterpart. As n/p junctions play an important role in the current transportation of tandem solar cells, it is important to design and fabricate good n/p junctions.The properties of the n/p junction of amorphous silicon (a-Si) were studied. We investigate the effect of interposing a nanocrystalline p(+) layer between n (top cell) and p (bottom cell) layers of a tandem solar cell. The crystalline volume fraction, the band gap, the conductivity and the grain size of the nanocrystalline silicon (nc-Si) p(+) layer could be modulated by changing the deposition parameters.Current transport in a-Si based n/p ("tunnel") junctions was investigated by current-voltage measurements. The voltage dependence on the resistance (V/J) of the tandem cells was examined to see if n/p junction was ohmic contact. To study the affection of different doping concentration to the properties of the nc-Si p(+) layers which varied the properties of the tunnel junctions, three nc-Si p(+) film samples were grown, measured and analyzed.
Resumo:
Hybrid composites composed of zinc phthalocyanine embedded in silicon matrixes have attracted attention because of the potential for solar energy conversion. We produce hybrid composites by thermal evaporation for the plithalocyanine and PECVD (Plasma Enhanced Chemical Vapor Deposition) for the silicon matrix. Deposition of ZnPc/a-Si(amorphous silicon) composites was achieved in a sequential manner. The compound films were characterized by optical transmittance spectra and photoconductivity measurement. The optical transmittance measurements were carried out in the visible region (500 - 800 nm). Compared to pure silicon film, the photosensitivity of compound functional films was enhanced by one order of magnitude. This demonstrates the Si sensitized by adding ZnPc.