695 resultados para LOCALIZED CORROSION
Resumo:
Research is described that sought to understand how senior managers within regional contracting firms conceptualize and enact competitiveness. Existing formal discourses of construction competitiveness include the discourse of 'best practice' and the various theories of competitiveness as routinely mobilized within the academic literature. Such discourses consistently underplay the influence of contextual factors in shaping how competitiveness is enacted. An alternative discourse of competitiveness is outlined based on the concepts of localized learning and embeddedness. Two case studies of regional construction firms provide new insights into the emergent discourses of construction competitiveness. The empirical findings resonate strongly with the concepts of localized learning and embeddedness. The case studies illustrate the importance of de-centralized structures which enable multiple business units to become embedded within localized markets. A significant degree of autonomy is essential to facilitate localized entrepreneurial behaviour. In essence, sustained competitiveness was found to depend upon the extent to which de-centralized business units enact ongoing processes of localized learning. Once local business units have become embedded within localized markets the essential challenge is how to encourage continued entrepreneurial behaviour while maintaining a degree of centralized control and coordination. Of key importance is the recognition that the capabilities that make companies competitive transcend organizational boundaries such that they become situated within complex networks of relational ties.
Resumo:
16S rRNA gene sequencing was used to identify a sulfate-reducing bacterium (SRB) from a Danish North Sea oilfield water injection system. This species was cultivated, purified and subsequently identified as being >97% similar to Desulfovibrio gracilis. Like some other Desulfovibrio species this SRB, strain OP102, could reduce nitrate as an electron acceptor and produce ammonia in the absence of sulfate. In addition, in the presence of sulfate, when nitrate was dosed at 100 mg/l it was again reduced by the bacterium, with some ammonium production. Therefore, this mechanism could be important in oilfield systems where nitrate is applied to prevent sulfide generation by SRB which leads to reservoir souring. In static tests the influence of this Desulfovibrio on corrosion was assessed using carbon steel coupons, in the presence of sulfate and in the presence of sulfate with 100 mg/l nitrate. Corrosion rates were less than 1.5 mpy when coupons were incubated in the same water, with sulfate and with nitrate. Furthermore, the occurrence of pitting corrosion was fairly low under all circumstances.
Resumo:
A series of bimetallic ruthenium complexes [{Ru(dppe)Cp*}2(μ-C≡CArC≡C)] featuring diethynylaromatic bridging ligands (Ar = 1,4-phenylene, 1,4-naphthylene, 9,10-anthrylene) have been prepared and some representative molecular structures determined. A combination of UV–vis–NIR and IR spectroelectrochemical methods and density functional theory (DFT) have been used to demonstrate that one-electron oxidation of compounds [{Ru(dppe)Cp*}2(μ-C≡CArC≡C)](HC≡CArC≡CH = 1,4-diethynylbenzene; 1,4-diethynyl-2,5-dimethoxybenzene; 1,4-diethynylnaphthalene; 9,10-diethynylanthracene) yields solutions containing radical cations that exhibit characteristics of both oxidation of the diethynylaromatic portion of the bridge, and a mixed-valence state. The simultaneous population of bridge-oxidized and mixed-valence states is likely related to a number of factors, including orientation of the plane of the aromatic portion of the bridging ligand with respect to the metal d-orbitals of appropriate π-symmetry.
Resumo:
The electronic properties of four divinylanthracene-bridged diruthenium carbonyl complexes [{RuCl(CO)(PMe3)3}2(μ[BOND]CH[DOUBLE BOND]CHArCH[DOUBLE BOND]CH)] (Ar=9,10-anthracene (1), 1,5-anthracene (2), 2,6-anthracene (3), 1,8-anthracene (4)) obtained by molecular spectroscopic methods (IR, UV/Vis/near-IR, and EPR spectroscopy) and DFT calculations are reported. IR spectroelectrochemical studies have revealed that these complexes are first oxidized at the noninnocent bridging ligand, which is in line with the very small ν(C[TRIPLE BOND]O) wavenumber shift that accompanies this process and also supported by DFT calculations. Because of poor conjugation in complex 1, except oxidized 1+, the electronic absorption spectra of complexes 2+, 3+, and 4+ all display the characteristic near-IR band envelopes that have been deconvoluted into three Gaussian sub-bands. Two of the sub-bands belong mainly to metal-to-ligand charge-transfer (MLCT) transitions according to results from time-dependent DFT calculations. EPR spectroscopy of chemically generated 1+–4+ proves largely ligand-centered spin density, again in accordance with IR spectra and DFT calculations results.
Resumo:
Water soluble anionic and cationic bis-triazine ligands are able to suppress (mask) the extraction of corrosion and fission products such as Ni(II) and Pd(II) that are found in PUREX raffinates. Thus it is possible to separate these elements from the minor actinide Am(III). Although some masking agents have previously been developed that retard the extraction of Pd(II), this is the first time a masking agent has been developed for Ni(II).
Resumo:
This article argues that two movements in constant interplay operate within the historical trajectory of the Spanish language: the localization that becomes globalized and the globalization that becomes localized. Equally, this article illustrates how, at the same time that Spanish is expanding in the world, new idiosyncratic and localized forms of the language are emerging. This article deals with the issues of standardization and language ideology, language contact, and redefinition of identities. The article focuses on three geographic loci: Spain, where Spanish opposes Catalan, Basque, and Galician; the United States, where migrants' Spanish dialects converge and confront English and each other; and finally, Latin America, where Spanish is in contact with Portuguese, indigenous, and Afro-Hispanic languages. The concepts that structure the discussion explain both language expansion and contraction as well as the conflict and constant negotiation between a language's standardized forms and its regional and social varieties.
Resumo:
Spatial and temporal fluctuations in the concentration field from an ensemble of continuous point-source releases in a regular building array are analyzed from data generated by direct numerical simulations. The release is of a passive scalar under conditions of neutral stability. Results are related to the underlying flow structure by contrasting data for an imposed wind direction of 0 deg and 45 deg relative to the buildings. Furthermore, the effects of distance from the source and vicinity to the plume centreline on the spatial and temporal variability are documented. The general picture that emerges is that this particular geometry splits the flow domain into segments (e.g. “streets” and “intersections”) in each of which the air is, to a first approximation, well mixed. Notable exceptions to this general rule include regions close to the source, near the plume edge, and in unobstructed channels when the flow is aligned. In the oblique (45 deg) case the strongly three-dimensional nature of the flow enhances mixing of a scalar within the canopy leading to reduced temporal and spatial concentration fluctuations within the plume core. These fluctuations are in general larger for the parallel flow (0 deg) case, especially so in the long unobstructed channels. Due to the more complex flow structure in the canyon-type streets behind buildings, fluctuations are lower than in the open channels, though still substantially larger than for oblique flow. These results are relevant to the formulation of simple models for dispersion in urban areas and to the quantification of the uncertainties in their predictions.
Resumo:
The biocompatibility of commercially pure (cp) titanium stems from its chemical stability within an organism, due to a fine film of impermeable titanium oxide covering the metal surface, which guarantees its resistance to corrosion. Despite its biocompatible characteristic, this material does not promote the formation of a hydroxyapatite layer, therefore, many research groups have sought to alter the material`s surface, introducing modifications that might influence corrosion resistance. The electrochemical behavior of cp Ti, with hydroxyapatite coating and without hydroxyapatite coating, commonly used in implant materials, was investigated using an artificial saliva solution at 25 degrees C and pH=7.4. In the conditions of the study it was observed that the hydroxyapatite layer influences the properties of corrosion resistance. This study of the behavior of cp Ti with and without hydroxyapatite coating, in naturally aerated artificial saliva solution at 25 degrees C, was based on open circuit potential measurements and potentiodynamic polarization curves. At approximately 1x10(-6) A/cm(2) the potential for cp Ti with and without hydroxyapatite coating begins to increase at a faster rate, but at -74mV (SCE) for coated cp Ti and at 180mV (SCE) for uncoated cp Ti the increase in potential begins to slow. This behavior, characterized by a partial stabilization of current density, indicates that in those potential ranges a protective passive film is formed.
Resumo:
Aim The microbial profile of localized aggressive periodontitis (LAgP) has not yet been determined. Therefore, the aim of this study was to evaluate the subgingival microbial composition of LAgP. Material and Methods One hundred and twenty subjects with LAgP (n=15), generalized aggressive periodontitis (GAgP, n=25), chronic periodontitis (ChP, n=30) or periodontal health (PH, n=50) underwent clinical and microbiological assessment. Nine subgingival plaque samples were collected from each subject and analysed for their content of 38 bacterial species using checkerboard DNA-DNA hybridization. Results Red complex and some orange complex species are the most numerous and prevalent periodontal pathogens in LAgP. The proportions of Aggregatibacter actinomycetemcomitans were elevated in shallow and intermediate pockets of LAgP subjects in comparison with those with GAgP or ChP, but not in deep sites. This species also showed a negative correlation with age and with the proportions of red complex pathogens. The host-compatible Actinomyces species were reduced in LAgP. Conclusion A. actinomycetemcomitans seems to be associated with the onset of LAgP, and Porphyromonas gingivalis, Tannerella forsythia, Treponema denticola, Campylobacter gracilis, Eubacterium nodatum and Prevotella intermedia play an important role in disease progression. Successful treatment of LAgP would involve a reduction in these pathogens and an increase in the Actinomyces species.
Continuity of the dynamics in a localized large diffusion problem with nonlinear boundary conditions
Resumo:
This paper is concerned with singular perturbations in parabolic problems subjected to nonlinear Neumann boundary conditions. We consider the case for which the diffusion coefficient blows up in a subregion Omega(0) which is interior to the physical domain Omega subset of R(n). We prove, under natural assumptions, that the associated attractors behave continuously as the diffusion coefficient blows up locally uniformly in Omega(0) and converges uniformly to a continuous and positive function in Omega(1) = (Omega) over bar\Omega(0). (C) 2009 Elsevier Inc. All rights reserved.
Resumo:
In this paper we study the continuity of asymptotics of semilinear parabolic problems of the form u(t) - div(p(x)del u) + lambda u =f(u) in a bounded smooth domain ohm subset of R `` with Dirichlet boundary conditions when the diffusion coefficient p becomes large in a subregion ohm(0) which is interior to the physical domain ohm. We prove, under suitable assumptions, that the family of attractors behave upper and lower semicontinuously as the diffusion blows up in ohm(0). (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
The corrosion resistance of Ti and Ti-6Al-4V was investigated through electrochemical impedance spectroscopy, EIS, potentiodynamic polarisation curves and UV-Vis spectrophotometry. The tests were done in Hank solution at 25 degrees C and 37 degrees C. The EIS measurements were done at the open circuit potential at specific immersion times. An increase of the resistance as a function of the immersion time was observed, for Ti (at 25 degrees C and 37 degrees C), and for Ti-6Al-4V (at 25 degrees C), which was interpreted as the formation and growth of a passive film on the metallic surfaces. (C) 2009 Elsevier Ltd. All rights reserved.
Resumo:
This paper presents a study of AISI 1040 steel corrosion in aqueous electrolyte of acetic acid buffer containing 3.1 and 31 x 10(-3) mol dm(-3) of Na(2)S in both the presence and absence of 3.5 wt.% NaCl. This investigation of steel corrosion was carried out using potential polarization, and open-circuit and in situ optical microscopy. The morphological analysis and classification of types of surface corrosion damage by digital image processing reveals grain boundary corrosion and shows a non-uniform sulfide film growth, which occurs preferentially over pearlitic grains through successive formation and dissolution of the film. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
Fuel distribution uses 304 stainless steel containers for the storage of biofuels, however there are few reports in the literature about the corrosive aspects this. steel in biodiesel. The objective of this research is to study the corrosive behavior of 304 austenitic stainless steel in the presence of biodiesel, unwashed and washed, with aqueous solutions of citric, oxalic, acetic and ascorbic acids 0,01 mol L(-1), and compare with results obtained for the copper (ASTM D130). The employedtechniques were: atomic absorption spectrometry (AAS) and optical microscopy (OM). The results of EA A showed a low rate of corrosion for the stainless steel, the alloys elements studied were Cr, Ni and Fe, the highest rate was observed for the chrome, 1.78 ppm / day in biodiesel with or without washing. The OM of the 304 steel, when compared with that of copper has a low corrosion rate in the 304 steel/biodiesel system. Not with standing, this demonstrates that not only the 304 steel, but also the copper corrodes in biodiesel