Resumo:
Synthesis of 2-amino-1,3,4-oxadiazole derivatives of N-Cbz(benzyloxycarbonyl)/Boc-protected amino/peptide acids under sonication is described. The conditions involved in the present protocol are simple, mild, and racemization free. The utility of 2-amino group in the substituted oxadiazoles for the incorporation of peptide and ureido bonds to obtain hybrid peptidomimetics is also delineated. The 2-amino-1,3,4-oxadiazole 3b was obtained as a single crystal, and its molecular structure has been confirmed through X-ray crystallographic study.
Resumo:
Two shape-persistent covalent cages (CC1(r) and CC2(r)) have been devised from triphenyl amine-based trialdehydes and cyclohexane diamine building blocks utilizing the dynamic imine chemistry followed by imine bond reduction. The cage compounds have been characterized by several spectroscopic techniques which suggest that CC1(r) and CC2(r) are 2+3] and 8+12] self-assembled architectures, respectively. These state-of-the-art molecules have a porous interior and stable aromatic backbone with multiple palladium binding sites to engineer the controlled synthesis and stabilization of ultrafine palladium nanoparticles (PdNPs). As-synthesized cage-embedded PdNPs have been characterized by transmission electron microscopy (TEM), scanning electron microscopy (SEM), and powder X-ray diffraction (PXRD). Inductively coupled plasma optical emission spectrometry reveals that Pd@CC1(r) and Pd@CC2(r) have 40 and 25 wt% palladium loading, respectively. On the basis of TEM analysis, it has been estimated that as small as similar to 1.8 nm PdNPs could be stabilized inside the CC1(r), while larger CC2(r) could stabilize similar to 3.7 nm NPs. In contrast, reduction of palladium salts in the absence of the cages form structure less agglomerates. The well-dispersed cage-embedded NPs exhibit efficient catalytic performance in the cyanation of aryl halides under heterogeneous, additive-free condition. Moreover, these materials have excellent stability and recyclability without any agglomeration of PdNPs after several cycles.
Resumo:
Sn4+-doped In2O3 (ITO) is a benchmark transparent conducting oxide material. We prepared ligand-free but colloidal ITO (8nm, 10% Sn4+) nanocrystals (NCs) by using a post-synthesis surface-modification reaction. (CH3)(3)OBF4 removes the native oleylamine ligand from NC surfaces to give ligand-free, positively charged NCs that form a colloidal dispersion in polar solvents. Both oleylamine-capped and ligand-free ITO NCs exhibit intense absorption peaks, due to localized surface plasmon resonance (LSPR) at around =1950nm. Compared with oleylamine-capped NCs, the electrical resistivity of ligand-free ITO NCs is lower by an order of magnitude (approximate to 35mcm(-1)). Resistivity over a wide range of temperatures can be consistently described as a composite of metallic ITO grains embedded in an insulating matrix by using a simple equivalent circuit, which provides an insight into the conduction mechanism in these systems.
Resumo:
Two-dimensional ZnO nanowall networks were grown on ZnO-coated silicon by thermal evaporation at low temperature without catalysts or additives. All of the results from scanning electronic spectroscope, X-ray diffraction and Raman scattering confirmed that the ZnO nanowalls were vertically aligned and c-axis oriented. The room-temperature photoluminescence spectra showed a dominated UV peak at 378 nm, and a much suppressed orange emission centered at similar to 590 nm. This demonstrates fairly good crystal quality and optical properties of the product. A possible three-step, zinc vapor-controlled process was proposed to explain the growth of well-aligned ZnO nanowall networks. The pre-coated ZnO template layer plays a key role during the synthesis process, which guides the growth direction of the synthesized products. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
"Click" chemistry has become an efficient avenue to unimolecular polymeric nanoparticles through the self-crosslinking of individual polymer chains containing appropriate functional groups. Herein we report the synthesis of ultra-small (7 nm in size) polymethyl methacrylate (PMMA) nanoparticles (NPs) by the "metal-free" cross-linking of PMMA-precursor chains prepared by reversible addition-fragmentation chain transfer (RAFT) polymerization containing beta-ketoester functional groups. Intramolecular collapse was performed by the one-pot reaction of beta-ketoester moieties with alkyl diamines in tetrahydrofurane at r.t. (i.e., by enamine formation). The collapsing process was followed by size exclusion chromatography and by nuclear magnetic resonance spectroscopy. The size of the resulting PMMA-NPs was determined by dynamic light scattering. Enamine "click" chemistry increases the synthetic toolbox for the efficient synthesis of metal-free, ultra-small polymeric NPs.
Resumo:
The synthesis and direct observation of 1,1-di-tert-butyldiazene (16) at -127°C is described. The absorption spectrum of a red solution of 1,1-diazene 16 reveals a structured absorption band with λ max at 506 run (Me_2O, -125°C). The vibrational spacing in S_1 is about 1200 cm^(-1). The excited state of 16 emits weakly with a single maximum at 715 run observed in the fluorescence spectrum (Me_2O:CD_2Cl_2, -196°C). The proton NMR spectrum of 16 occurs as a singlet at 1.41 ppm. Monitoring this NMR absorption at -94^0 ± 2°C shows that 1,1-diazene 16 decomposes with a first-order rate of 1.8 x 10^(-3) sec(-1) to form isobutane, isobutylene and hexarnethylethane. This rate is 10^8 and 10^(34) times faster than the thermal decomposition of the corresponding cis and trans 1,2-di-tert-butyldiazene isomers. The free energy of activation for decomposition of 1,1-diazene 16 is found to be 12.5 ± 0.2 kcal/mol at -94°C which is much lower than the values of 19.1 and 19.4 kcal/lmole calculated at -94°C for N-(2,2,6,6- tetramethylpiperidyl)nitrene (3) and N-(2,2,5,5- tetrarnethylpyrrolidyl)nitrene (4), respectively. This difference between 16 and the cyclic-1,1-diazenes 3 and 4 can be attributed to a large steric interaction between the tert-butyl groups in 1,1-diazene 16.
In order to investigate the nature of the singlet-triplet gap in 1,1-diazenes, 2,5-di-tert-butyl-N-pyrrolynitrene (22) was generated but was found to be too reactive towards dimerization to be persistent. In the presence of dimethylsulfoxide, however, N-pyrrolynitrene (22) can be trapped as N-(2,5-di-tert-butyl- N'-pyrrolyl)dimethylsulfoxirnine (38). N-(2,5-di-tert-butyl-N'-pyrrolyl)dimethylsulfoximine (38-d^6) exchanges with free dimethylsulfoxide at 50°C in solution, presumably by generation and retrapping of pyrrolynitrene 22.
Resumo:
Part I: Synthesis of L-Amino Acid Oxidase by a Serine- or Glycine-Requiring Strain of Neurospora
Wild-type cultures of Neurospora crassa growing on minimal medium contain low levels of L-amino acid oxidase, tyrosinase, and nicotinarnide adenine dinucleotide glycohydrase (NADase). The enzymes are derepressed by starvation and by a number of other conditions which are inhibitory to growth. L-amino acid oxidase is, in addition, induced by growth on amino acids. A mutant which produces large quantities of both L-amino acid oxidase and NADase when growing on minimal medium was investigated. Constitutive synthesis of L-amino acid oxidase was shown to be inherited as a single gene, called P110, which is separable from constitutive synthesis of NADase. P110 maps near the centromere on linkage group IV.
L-amino acid oxidase produced constitutively by P110 was partially purified and compared to partially purified L-amino acid oxidase produced by derepressed wild-type cultures. The enzymes are identical with respect to thermostability and molecular weight as judged by gel filtration.
The mutant P110 was shown to be an incompletely blocked auxotroph which requires serine or glycine. None of the enzymes involved in the synthesis of serine from 3-phosphoglyceric acid or glyceric acid was found to be deficient in the mutant, however. An investigation of the free intracellular amino acid pools of P110 indicated that the mutant is deficient in serine, glycine, and alanine, and accumulates threonine and homoserine.
The relationship between the amino acid requirement of P110 and its synthesis of L-amino acid oxidase is discussed.
Part II: Studies Concerning Multiple Electrophoretic Forms of Tyrosinase in Neurospora
Supernumerary bands shown by some crude tyrosinase preparations in paper electrophoresis were investigated. Genetic analysis indicated that the location of the extra bands is determined by the particular T allele present. The presence of supernumerary bands varies with the method used to derepress tyrosinase production, and with the duration of derepression. The extra bands are unstable and may convert to the major electrophoretic band, suggesting that they result from modification of a single protein. Attempts to isolate the supernumerary bands by continuous flow paper electrophoresis or density gradient zonal electrophoresis were unsuccessful.
Resumo:
This dissertation is divided into three parts.
The first section is concerned with protein synthesis in cellfree systems from reticulocytes. The sub-cellular reticulocyte fractions, reagents, etc. have been examined for the presence of traces of ribonuclease, using. an assay based upon the loss of infectivity of RNA fran bacteriophage MS2. This assay is sensitive to 5 x 10-7 γ RNase/ml. In addition, the loss of synthetic capacity of an 80S ribosome on dissociation has been studied, and can be attributed to loss of messenger RNA when the monomer is separated into subunits. The presence of ribonuclease has been shown to be a major cause of polyribosome disintegration during cell-free protein synthesis.
The second section concerns the changes in ribosomes and polyribosomes which occur during the maturation of a reticulocyte into an erythrocyte. With increasing age, the cells lose a large proportion of the ribonucleoprotein, but the percentage of ribosomes present as polyribosomes is only slightly altered. The loss of hemoglobin synthesis on maturation is probably due to both the loss of total ribosomes and to the lessened specific activity of the polyribosomes.
The third section contains analytical ultracentrifugation data on 80S ribosomes, polyribosomes, and ribosomal RNA from reticulocytes. The 60s and 40s subunits, obtained by dissociation of the 80s particle with inorganic pyrophosphate, were also studied. The RNA from reticulocyte ribosomes has been examined under a variety of denaturing conditions, including dimethyl sulfoxide treatment, formaldehyde reaction and thermal denaturation. From these studies we can conclude that the 28S and 16S RNA's are single polynucleotide chains and are not made up of smaller RNA subunits hydrogen-bonded together.
Resumo:
Enzyme-catalyzed production of biodiesel is the object of extensive research due to the global shortage of fossil fuels and increased environmental concerns. Herein we report the preparation and main characteristics of a novel biocatalyst consisting of Cross-Linked Enzyme Aggregates (CLEAs) of Candida antarctica lipase B (CALB) which are covalently bound to magnetic nanoparticles, and tackle its use for the synthesis of biodiesel from non-edible vegetable and waste frying oils. For this purpose, insolubilized CALB was covalently cross-linked to magnetic nanoparticles of magnetite which the surface was functionalized with –NH2 groups. The resulting biocatalyst combines the relevant catalytic properties of CLEAs (as great stability and feasibility for their reutilization) and the magnetic character, and thus the final product (mCLEAs) are superparamagnetic particles of a robust catalyst which is more stable than the free enzyme, easily recoverable from the reaction medium and reusable for new catalytic cycles. We have studied the main properties of this biocatalyst and we have assessed its utility to catalyze transesterification reactions to obtain biodiesel from non-edible vegetable oils including unrefined soybean, jatropha and cameline, as well as waste frying oil. Using 1% mCLEAs (w/w of oil) conversions near 80% were routinely obtained at 30°C after 24 h of reaction, this value rising to 92% after 72 h. Moreover, the magnetic biocatalyst can be easily recovered from the reaction mixture and reused for at least ten consecutive cycles of 24 h without apparent loss of activity. The obtained results suggest that mCLEAs prepared from CALB can become a powerful biocatalyst for application at industrial scale with better performance than those currently available.
Resumo:
Two kinds of nickel(II) and copper(II) P-diketone complexes derived from thenoyltrifluoroacetone ligand with blue-violet light absorption were synthesized by reacting free ligand and different metal(II) ions in sodium methoxide solution. Their structures were postulated based on elemental analysis, ESI-MS, FT-IR spectra and UV-vis electronic absorption spectra. Smooth films on K9 glass substrates were prepared using the spin-coating method. Their solubility in organic solvents, absorption properties of thin film and thermal stability of these complexes were evaluated. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
A catalyst-free synthesis of ZnO nanostructures using platinum microheaters under ambient environmental conditions has been developed. Different types of ZnO nanostructures are synthesized from the oxidization of Zn thin film by local heating. The characterization of two shapes of Pt microheaters is investigated and the relationship between the applied power for heat generation and ZnO nanostructure synthesis is investigated by local heating experiments under ambient conditions. Based on the developed heating approach, synthesis area, location, and morphologies of ZnO nanostructures can be controlled through the deposited thickness of Zn layer and applied heating voltages. Furthermore, a connected multiple-structure (Zn-ZnO-Zn) layer is synthesized using combinative multimicroheaters. © 2002-2012 IEEE.
Resumo:
We investigate how to tailor the structural, crystallographic and optical properties of GaAs nanowires. Nanowires were grown by Au nanoparticle-catalyzed metalorganic chemical vapor deposition. A high arsine flow rate, that is, a high ratio of group V to group III precursors, imparts significant advantages. It dramatically reduces planar crystallographic defects and reduces intrinsic carbon dopant incorporation. Increasing V/III ratio further, however, instigates nanowire kinking and increases nanowire tapering. By choosing an intermediate V/III ratio we achieve uniform, vertically aligned GaAs nanowires, free of planar crystallographic defects, with excellent optical properties and high purity. These findings will greatly assist the development of future GaAs nanowire-based electronic and optoelectronic devices, and are expected to be more broadly relevant to the rational synthesis of other III-V nanowires. © 2008 WILEY-VCH Verlag GmbH & Co. KGaA.
Resumo:
Two-dimensional ZnO nanowall networks were grown on ZnO-coated silicon by thermal evaporation at low temperature without catalysts or additives. All of the results from scanning electronic spectroscope, X-ray diffraction and Raman scattering confirmed that the ZnO nanowalls were vertically aligned and c-axis oriented. The room-temperature photoluminescence spectra showed a dominated UV peak at 378 nm, and a much suppressed orange emission centered at similar to 590 nm. This demonstrates fairly good crystal quality and optical properties of the product. A possible three-step, zinc vapor-controlled process was proposed to explain the growth of well-aligned ZnO nanowall networks. The pre-coated ZnO template layer plays a key role during the synthesis process, which guides the growth direction of the synthesized products. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
High quality n-type CdS nanobelts (NBs) were synthesized via an in situ indium doping chemical vapor deposition method and fabricated into field effect transistors (FETs). The electron concentrations and mobilities of these CdS NBs are around (1.0x10(16)-3.0x10(17))/cm(3) and 100-350 cm(2)/V s, respectively. An on-off ratio greater than 10(8) and a subthreshold swing as small as 65 mV/decade are obtained at room temperature, which give the best performance of CdS nanowire/nanobelt FETs reported so far. n-type CdS NB/p(+)-Si heterojunction light emitting diodes were fabricated. Their electroluminescence spectra are dominated by an intense sharp band-edge emission and free from deep-level defect emissions. (c) 2006 American Institute of Physics.
Resumo:
Arrays of vertically well-aligned ZnO nanorod-nanowall junctions have been synthesized on an undoped ZnO-coated silicon substrate by a carbothermal reduction and vapour phase transport method. X-ray diffraction (XRD) and scanning electron microscopy (SEM) show that the nanostructures are well-oriented with the c-axis perpendicular to the substrate. The room temperature photoluminescence (PL) spectrum of the as-prepared ZnO nanostructure reveals a dominant near-band-edge (NBE) emission peak and a weak deep level (DL) emission, which demonstrates its good optical properties. Temperature-dependent PL spectra show that both the intensity of NBE and DL emissions increased with decreasing temperature. The NBE emission at 3.27 eV is identified to originate from the radiative free exciton recombination. The possible growth mechanism of ZnO nanorod-nanowall junctions is also proposed.