6 resultados para molar mass
em ArchiMeD - Elektronische Publikationen der Universität Mainz - Alemanha
Resumo:
Flory-Huggins interaction parameters and thermal diffusion coefficients were measured for aqueous biopolymer solutions. Dextran (a water soluble polysaccharide) and bovine serum albumin (BSA, a water soluble protein) were used for this study. The former polymer is representative for chain macromolecules and the latter is for globular macromolecules. The interaction parameters for the systems water/dextran and water/BSA were determined as a function of composition by means of vapor pressure measurements, using a combination of headspace sampling and gas chromatography (HS-GC). A new theoretical approach, accounting for chain connectivity and conformational variability, describes the observed dependencies quantitatively for the system water/dextran and qualitatively for the system water/BSA. The phase diagrams of the ternary systems water/methanol/dextran and water/dextran/BSA were determined via cloud point measurements and modeled by means of the direct minimization of the Gibbs energy using the information on the binary subsystems as input parameters. The thermal diffusion of dextran was studied for aqueous solutions in the temperature range 15 < T < 55 oC. The effects of the addition of urea were also studied. In the absence of urea, the Soret coefficient ST changes its sign as T is varied; it is positive for T > 45.0 oC, but negative for T < 45.0 oC. The positive sign of ST means that the dextran molecules migrate towards the cold side of the fluid; this behavior is typical for polymer solutions. While a negative sign indicates the macromolecules move toward the hot side; this behavior has so far not been observed with any other binary aqueous polymer solutions. The addition of urea to the aqueous solution of dextran increases ST and reduces the inversion temperature. For 2 M urea, the change in the sign of ST is observed at T = 29.7 oC. At higher temperature ST is always positive in the studied temperature range. To rationalize these observations it is assumed that the addition of urea opens hydrogen bonds, similar to that induced by an increase in temperature. For a future extension of the thermodynamic studies to the effects of poly-dispersity, dextran was fractionated by means of a recently developed technique called Continuous Spin Fractionation (CSF). The solvent/precipitant/polymer system used for the thermodynamic studies served as the basis for the fractionation of dextran The starting polymer had a weight average molar mass Mw = 11.1 kg/mol and a molecular non-uniformity U= Mw / Mn -1= 1.0. Seventy grams of dextran were fractionated using water as the solvent and methanol as the precipitant. Five fractionation steps yielded four samples with Mw values between 4.36 and 18.2 kg/mol and U values ranging from 0.28 to 0.48.
Resumo:
An einer Vielzahl biogener Polyelektrolyte, wie z.B. den Nukleinsäuren DNA und RNA sowie Proteinen, ist die Ausbildung von Strukturhierarchien durch Selbstorganisation von Strukturelementen zu beobachten. Dabei wird das Strukturbildungsverhalten durch eine Kopplung von Wechselwirkungen auf verschiedenen Längenskalen, den kurzreichweitigen ausgeschlossenen Volumen und den langreichweitigen elektrostatischen Wechselwirkungen (Coulomb-Wechselwirkungen), die wiederum durch eine Vielzahl mikroskopische Parameter (z.B. Konformation) beeinflusst werden, bestimmt. Durch diese Komplexität ist es nicht möglich, den für die Strukturbildung hochgeladener Systeme bedeutsamen Beitrag der elektrostatischen Wechselwirkungen isoliert zu betrachten. Aus diesem Grund werden zur Aufklärung von Wechselwirkungs- und Strukturbildungsmechanismen vereinfachte Modell-Systeme herangezogen. Eine Möglichkeit besteht in der Verwendung synthetischer, kettensteifer Polyelektrolyte. Im Rahmen dieser Arbeit wurde das Aggregationsverhalten wässriger Lösungen dodecylsubstituierter Poly(para-phenylen)sulfonate (PPPS) sowie die Beeinflussung der Strukturbildung durch verschiedene Parameter charakterisiert. Als Einflussparameter wurden einerseits die Gegenion-Spezies und andererseits die Temperatur- und Konzentrations-Abhängigkeit untersucht. Hierzu wurden wässrige Lösungen der freien Säuren der PPPS mit Molekulargewichten zwischen MW = 18 kg/mol bis 58 kg/mol mittels Licht-, Röntgen- und Neutronenstreuung sowie durch Licht-, Polarisations-, Transmissionselektronen- und Rasterkraftmikroskopie in einem Konzentrationsbereich von 0,0008 < c < 1,1 g/L untersucht.
Resumo:
In this thesis, we investigated the evaporation of sessile microdroplets on different solid substrates. Three major aspects were studied: the influence of surface hydrophilicity and heterogeneity on the evaporation dynamics for an insoluble solid substrate, the influence of external process parameters and intrinsic material properties on microstructuring of soluble polymer substrates and the influence of an increased area to volume ratio in a microfluidic capillary, when evaporation is hindered. In the first part, the evaporation dynamics of pure sessile water drops on smooth self-assembled monolayers (SAMs) of thiols or disulfides on gold on mica was studied. With increasing surface hydrophilicity the drop stayed pinned longer. Thus, the total evaporation time of a given initial drop volume was shorter, since the drop surface, through which the evaporation occurs, stays longer large. Usually, for a single drop the volume decreased linearly with t1.5, t being the evaporation time, for a diffusion-controlled evaporation process. However, when we measured the total evaporation time, ttot, for multiple droplets with different initial volumes, V0, we found a scaling of the form V0 = attotb. The more hydrophilic the substrate was, the more showed the scaling exponent a tendency to an increased value up to 1.6. This can be attributed to an increasing evaporation rate through a thin water layer in the vicinity of the drop. Under the assumption of a constant temperature at the substrate surface a cooling of the droplet and thus a decreased evaporation rate could be excluded as a reason for the different scaling exponent by simulations performed by F. Schönfeld at the IMM, Mainz. In contrast, for a hairy surface, made of dialkyldisulfide SAMs with different chain lengths and a 1:1 mixture of hydrophilic and hydrophobic end groups (hydroxy versus methyl group), the scaling exponent was found to be ~ 1.4. It increased to ~ 1.5 with increasing hydrophilicity. A reason for this observation can only be speculated: in the case of longer hydrophobic alkyl chains the formation of an air layer between substrate and surface might be favorable. Thus, the heat transport to the substrate might be reduced, leading to a stronger cooling and thus decreased evaporation rate. In the second part, the microstructuring of polystyrene surfaces by drops of toluene, a good solvent, was investigated. For this a novel deposition technique was developed, with which the drop can be deposited with a syringe. The polymer substrate is lying on a motorized table, which picks up the pendant drop by an upward motion until a liquid bridge is formed. A consecutive downward motion of the table after a variable delay, i.e. the contact time between drop and polymer, leads to the deposition of the droplet, which can evaporate. The resulting microstructure is investigated in dependence of the processes parameters, i.e. the approach and the retraction speed of the substrate and the delay between them, and in dependence of the intrinsic material properties, i.e. the molar mass and the type of the polymer/solvent system. The principal equivalence with the microstructuring by the ink-jet technique was demonstrated. For a high approach and retraction speed of 9 mm/s and no delay between them, a concave microtopology was observed. In agreement with the literature, this can be explained by a flow of solvent and the dissolved polymer to the rim of the pinned droplet, where polymer is accumulated. This effect is analogue to the well-known formation of ring-like stains after the evaporation of coffee drops (coffee-stain effect). With decreasing retraction speed down to 10 µm/s the resulting surface topology changes from concave to convex. This can be explained with the increasing dissolution of polymer into the solvent drop prior to the evaporation. If the polymer concentration is high enough, gelation occurs instead of a flow to the rim and the shape of the convex droplet is received. With increasing delay time from below 0 ms to 1s the depth of the concave microwells decreases from 4.6 µm to 3.2 µm. However, a convex surface topology could not be obtained, since for longer delay times the polymer sticks to the tip of the syringe. Thus, by changing the delay time a fine-tuning of the concave structure is accomplished, while by changing the retraction speed a principal change of the microtopolgy can be achieved. We attribute this to an additional flow inside the liquid bridge, which enhanced polymer dissolution. Even if the pendant drop is evaporating about 30 µm above the polymer surface without any contact (non-contact mode), concave structures were observed. Rim heights as high as 33 µm could be generated for exposure times of 20 min. The concave structure exclusively lay above the flat polymer surface outside the structure even after drying. This shows that toluene is taken up permanently. The increasing rim height, rh, with increasing exposure time to the solvent vapor obeys a diffusion law of rh = rh0 tn, with n in the range of 0.46 ~ 0.65. This hints at a non-Fickian swelling process. A detailed analysis showed that the rim height of the concave structure is modulated, unlike for the drop deposition. This is due to the local stress relaxation, which was initiated by the increasing toluene concentration in the extruded polymer surface. By altering the intrinsic material parameters i.e. the polymer molar mass and the polymer/solvent combination, several types of microstructures could be formed. With increasing molar mass from 20.9 kDa to 1.44 MDa the resulting microstructure changed from convex, to a structure with a dimple in the center, to concave, to finally an irregular structure. This observation can be explained if one assumes that the microstructuring is dominated by two opposing effects, a decreasing solubility with increasing polymer molar mass, but an increasing surface tension gradient leading to instabilities of Marangoni-type. Thus, a polymer with a low molar mass close or below the entanglement limit is subject to a high dissolution rate, which leads to fast gelation compared to the evaporation rate. This way a coffee-rim like effect is eliminated early and a convex structure results. For high molar masses the low dissolution rate and the low polymer diffusion might lead to increased surface tension gradients and a typical local pile-up of polymer is found. For intermediate polymer masses around 200 kDa, the dissolution and evaporation rate are comparable and the typical concave microtopology is found. This interpretation was supported by a quantitative estimation of the diffusion coefficient and the evaporation rate. For a different polymer/solvent system, polyethylmethacrylate (PEMA)/ethylacetate (EA), exclusively concave structures were found. Following the statements above this can be interpreted with a lower dissolution rate. At low molar masses the concentration of PEMA in EA most likely never reaches the gelation point. Thus, a concave instead of a convex structure occurs. At the end of this section, the optically properties of such microstructures for a potential application as microlenses are studied with laser scanning confocal microscopy. In the third part, the droplet was confined into a glass microcapillary to avoid evaporation. Since here, due to an increased area to volume ratio, the surface properties of the liquid and the solid walls became important, the influence of the surface hydrophilicity of the wall on the interfacial tension between two immiscible liquid slugs was investigated. For this a novel method for measuring the interfacial tension between the two liquids within the capillary was developed. This technique was demonstrated by measuring the interfacial tensions between slugs of pure water and standard solvents. For toluene, n-hexane and chloroform 36.2, 50.9 and 34.2 mN/m were measured at 20°C, which is in a good agreement with data from the literature. For a slug of hexane in contact with a slug of pure water containing ethanol in a concentration range between 0 and 70 (v/v %), a difference of up to 6 mN/m was found, when compared to commercial ring tensiometry. This discrepancy is still under debate.
Resumo:
From a physical-chemical point of view, it is challenging to form complexes with polyelectrolytes, consisting of only molecule of the largest component, i.e. the component with the highest number of charges. In this study, complexes are formed with DNA because of its potential applications as an artificial vector for gene delivery. The aim of this work is to prepare complexes in aqueous solutions as well as in organic solvents containing only one DNA molecule. For this purpose, the topology, equilibrium and conformation of complexes between a supercoiled DNA pUC19 (2686 base pairs) and spermine containing hydrophilic and/or hydrophobic moieties or a polylysine with a hydrophilic block are determined by means of dynamic (DLS) and static light scattering (SLS), atomic force microscopy (AFM), and circular dichroism (CD) spectroscopy. It is demonstrated that all of these complexes consisted of only one molecule of the polyanion. Only the polylysine-b-polyethylene glycol copolymer satisfied the conditions: 1) 100% neutralization of DNA charges and with a small excess of the cation (lower than 30%) and 2) form stable complexes at every charge ratio. rnDNA complex formation is also investigated in organic solvents. Precipitation is induced by neutralizing the charge of the supercoiled DNA pUC19 with the surfactants dodecyltrimethylammonium bromide (DTAB) and tetradecyltrimethylammonium bromide (TTAB). After isolation and drying of the solids, the complexes are dissolved in organic solvents. DNA-TTA complexes are only soluble in methanol and DNA-DTA in DMF. The complexes again consisted of only one DNA molecule. The final topology of the complexes is different in methanol than in DMF. In the former case, DNA seems to be compacted whereas in the latter case, the DNA-DTA complexes seem to have an expanded conformation. Upon complex formation with polycations in organic solvents (with polyvilylpyridine brush (b-PVP) in methanol and with a protected polylysine in DMF), DNA aggregates and precipitates. rnDNA is linearized with an enzyme (SmaI) to investigate the influence of the initial topology of the polyanion on the final conformation of the complexes in organic solvents. Two main differences are evidenced: 1. Complexes in organic solvents formed with linear DNA have in general a more expanded conformation and a higher tendency to aggregate. 2. If a polycation, i.e. the b-PVP, is added to the linear DNA-TTA complexes in methanol, complexes with the polycation are formed at a higher charge ratio. In DMF, the addition of the same b-PVP and of b-PLL did not lead to the formation of complexes.rn
Resumo:
The most important property controlling the physicochemical behaviour of polyelectrolytes and their applicability in different fields is the charge density on the macromolecular chain. A polyelectrolyte molecule in solution may have an effective charge density which is smaller than the actual charge density determined from its chemical structure. In the present work an attempt has been made to quantitatively determine this effective charge density of a model polyelectrolyte by using light scattering techniques. Flexible linear polyelectrolytes with a Poly(2-Vinylpyridine) (2-PVP) backbone are used in the present study. The polyelectrolytes are synthesized by quaternizing the pyridine groups of 2-PVP by ethyl bromide to different quaternization degrees. The effect of the molar mass, degree of quaternization and solvent polarity on the effective charge is studied. The results show that the effective charge does not vary much with the polymer molar mass or the degree of quaternization. But a significant increase in the effective charge is observed when the solvent polarity is increased. The results do not obey the counterion condensation theory proposed by Manning. Based on the very low effective charges determined in this study, a new mechanism for the counterion condensation phenomena from a specific polyelectrolyte-counterion interaction is proposed
Resumo:
In this thesis cholesteric films made of liquid crystalline cellulose derivatives with improved optical properties were prepared. The choice of the solvent, hydrogen bond influencing additives, the synthetic realization of a very high degree of substitution on the cellulosic polymer and the use of mechanical stirring at the upper concentration limit of the liquid crystalline range were the basis for an improved alignment of the applied cellulose tricarbamates. In combination with a tuned substrate treatment and film preparation method, cholesteric films were obtained, with optical properties that were theoretically predicted and only known from low molecular weight liquid crystals so far. Subsequent polymerization allowed a permanent fixing of the alignment and the fabrication of free standing and insensitive films.rnThe incorporation of inorganic nanorods into the cholesteric host material was mediated with tailored block copolymers, available via controlled radical polymerization methods. In addition to the shape match between the rodlike mesogens of the host and the nanorods it was possible to increase the miscibility of both materials. Nevertheless, the size of the nanorods, in comparison to the mesogens, in these densely packed liquid crystalline phases as well as their long equilibration times were the reasons for phase separation. Nanorods are, in principle, valuable substitutes for organics, but their utilization in cellulosic CLC was not to be combined with a high quality alignment of the cholesteric structure.rnA swelling process of polymerized films in a dye solution or dissolving dyes in non-polymerized CLC was used for incorporation of the organic chromophores. With the first method the CLC could be aligned and polymerized without any disturbance due to dye molecules. The optical properties of dye and CLC were matched, with regard to mirrorless lasing devices. The dye was optically excited and laser emission supported by the cholesteric cavity was obtained. The polarization and wavelength of the emitted radiation as well as its bandwidth, the obtained interference pattern and threshold behavior of the emission proofed the feedback mechanism that was not believed to be realizable in liquid crystalline polymers. rnUtilization of a microfluidic co-flow injection device enabled us to transfer the properties of cellulosic CLC from the planar film shape to spherical micrometer sized particles. The pure material yielded particles with distorted mesogen alignment similar to films prepared by capillary flow. Dilution of the CLC with a solvent that migrated into the carrier phase during particle preparation provided the basis for particles with well ordered areas. rnAlthough cellulose derivatives were known for their liquid crystalline behavior for decades and synthesized in mass production, their application as feedback material was affected by bad optical properties. In comparison to low molar mass compounds, the low degree of order in the CLC phase was the cause. With the improved material, defined lasing emission was shown and characterized. Derivatives of cellulose are desirable materials, because, as a renewable resource, they are available in large amounts for a low price and need only simple derivatization reactions. The fabrication of CLC films with tunable lasing emission, for which this thesis can provide a starting point, is in good agreement with today's requirements of modern technology and its miniaturization.rn