179 resultados para NI-CU ALLOYS


Relevância:

40.00% 40.00%

Publicador:

Resumo:

The identification, characterization and stability range of the phases present in a series of Cu-Al alloys, with Al content from 11.0 to 15.0 wt.%, were studied by Differential Thermal Analysis (DTA), Optical Microscopy (OM), Scanning Electron Microscopy (SEM), Transmission Electron Microscopy (TEM), Selected Area Electron Diffraction (SAED), Auger Electron Spectroscopy (AES), Energy Dispersive X-Ray Spectroscopy (EDX) and X-Ray Diffraction (XRD). In some alloys and in a temperature range from 790 degrees C to 850 degrees C the presence of black spots exhibiting regular shapes and an homogeneous distribution was noticed through metallographic microscopy. Data from TEM and AES indicate that these spots are made of two monocrystalline phases having different Al contents and a crystallographic orientation relationship. (C) 1998 Elsevier B.V. S.A. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Titanium alloys are among the most important and frequently used class of biomaterials. In addition to biocompatibility, it is important that an implant material present satisfactory mechanical properties that allow long term use in the body. To improve such properties, different heat treatments are used, as well as doping with oxygen. The presence of interstitial oxygen in the crystal lattice causes deformation, increases the hardness, and causes modifications in anelasticity, thereby decreasing the elastic modulus. In this study, an alloy was prepared by arc melting precursor metals, heat and mechanically treated, and doped with oxygen, resulting in samples with different processing conditions. In each condition, the alloy was characterised in terms of amount of oxygen, X-ray diffraction, and optical microscopy. In addition, properties of the alloy, such as hardness and elastic modulus, were analysed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper reports on the phase transformation during the preparation of Ni-25Nb, Ni-25Ta, Ni-20Nb-5Ta and Ni-15Nb-10Ta (at-%) powders by high-energy ball milling from elemental powders. The milling process was performed in a planetary ball milling using stainless steel balls and vials, rotary speed of 300rpm, and a ball-to-powder of 10:1. To minimize contamination and spontaneous ignition the powders were handled under argon atmosphere in a glove box. The milled powders were characterized by means of X-ray diffraction techniques. Results indicated that the Ni atoms were preferentially dissolved into the Nb (and/or Ta) lattice at the initial milling times, which contributed to change the relative intensity on the diffraction peaks. After the dissolution of Nb (and/or Ta) into the Ni lattice, the Ni peaks were moved to the direction of lower diffraction angles in Ni-25Nb, Ni-25Ta, Ni-20Nb-5Ta, Ni-15Nb-10Ta powders, indicating that the mechanical alloying was achieved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Objectives. This study was undertaken to evaluate the shear bond strength of four materials used as aesthetic material bonded to Ni-Cr alloy.Methods. Sixty-eight alloy discs were prepared and divided equally into four groups, and received four treatments for veneering: conventional feldspathic porcelain (Noritake EX-3) and three light-cured prosthodontic composite resins (Artglass, Solidex and Targis). The aesthetic materials were applied after metal structure conditioning in accordance with the manufacturers' recommendations. The specimens were stored in distilled water at 37 degreesC for 7 days. A universal testing machine was used to measure the shear bond strength of the specimens at a cross head speed of 0.5 mm/min. Fractured specimens were examined by using both optical and scanning electron microscope.Results. The analysis of variance and Tukey's test showed that the strongest mean shear bond was obtained with Noritake EX-3 (mean shear bond strength 42.90 +/- 7.82 MPa). For composites, the highest mean shear bond strength was observed for Targis (12.30 +/- 1.57 MPa); followed by Solidex (11.94 +/- 1.04 MPa) and Artglass (10.04 +/- 0.75 MPa). Optical analysis of the fractured surf aces indicated that for Targis and Noritake EX-3 all failures were a mixture of both cohesive and adhesive patterns. As for Artglass and Solidex, the fractures were mainly adhesive in nature.Conclusions. The Solidex system was equivalent to the Targis system in bond strength and exhibited greater strength than the Artglass system. The porcelain fused-to-metal showed considerably higher shear bond strength than the three metal-resin bonding techniques. (C) 2003 Elsevier B.V. Ltd. Ali rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The electrochemical behavior in 0.5 M H2SO4 at 25 degreesC of a Cu-Al(9.3 wt%)-Ag(4.7 wt%) alloy submitted to different heat treatments and an annealed Cu- Al(9.7 wt%)-Ag(34.2 wt%) were studied by means of open circuit potential (E-mix) measurements, potentiodynamic polarizations and cyclic voltammetry. SEM and EDX microanalysis were used to examine the changes caused by the electrochemical perturbations. The steady state potentials observed for the studied samples were correlated in terms of the phases present in the alloys surface. The resulting E/I potentiodynamic profiles were explained in terms of the potentiodynamic behavior of pure copper and pure silver. The presence of aluminum decreased the extent of copper oxidation. In the apparent Tafel potential region, two anodic Tafel slopes were obtained: 40 mV dec(-1) in the low potential region and 130 mV dec(-1) in the high potential region, which were related with the electrochemical processes involving copper oxidation. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The influence of additions of 2, 4, 6, 8, 10 and 12 wt.% Ag in the isothermal aging kinetics of the Cu-8 wt.% Al alloy was studied using microhardness measurements, differential scanning calorimetry, optical and scanning electron microscopy and X-ray diffractometry. The results indicate that the presence of silver is responsible for the shift of the equilibrium concentration to higher Al contents, allowing the formation of the gamma(1) phase (Al4Cu9) in this alloy. For Ag additions up to 6% the dominant kinetic process is Ag precipitation and for additions from 8 to 12% Ag the nucleation of the perlitic phase dominates. (C) 2003 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The effect of 4 mass% Ag addition on the thermal behavior of the Cu-9 mass% Al alloy was studied using differential scanning calorimetry (DSC), optical microscopy (OM), scanning electron microscopy (SEM), energy dispersive X-ray analysis (EDX) and X-ray diffractometry (XRD). The results showed that the presence of silver causes (Cu)-alpha+(alpha+gamma1)-->(Cu)-alpha+beta transformation to occur in two stages. In the first one, part of the produced beta phase combines with the precipitated Ag to give a silver-rich phase and in the second one the transformation is completed. The formation of this silver-rich phase seems to be enhanced at very low cooling rates.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The effect of Ag additions on the reverse martensitic transformation in the Cu-10 mass% Al alloy was studied using differential thermal analysis (DTA), optical (OM) and scanning electron microscopies (SEM) and X-ray diffractometry. The results indicated that Ag additions to the Cu-10 mass% Al alloy shift the equilibrium concentration to higher Al contents, allow to obtain both beta(1)' and beta' martensitic phases in equilibrium and that Ag precipitation is a process associated with the perlitic phase formation.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Thermal analysis and compression tests at room temperature have been carried out for Cu-10 wt.% Al and Cu-10 wt.% Al-10 wt.% Ag alloys samples. The results indicate that the decomposition reaction of the (beta(1)) parent phase is decreased suppressed and a martensite stabilization effect can be induced by Ag addition. The Cu-Al-Ag alloy shows some degree of shape memory capacity. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The non-occurrence of the beta' -> (alpha+ gamma(1)) decomposition reaction in the Cu-9 wt.% Al-6 wt.% Ag alloy, on ageing between 200 and 450 degrees C, is discussed considering the influence of Ag on point defects redistribution and energy difference between martensite and the ordered parent phase. (c) 2005 Elsevier B.V All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The influence of 4 wt.%Ag addition on the isothermal decomposition kinetics of the beta' phase in the Cu-9wt.%Al alloy was studied by microhardness measurements, optical and scanning electron microscopy (SEM), energy dispersive X-ray (EDX) analysis, and X-ray diffractometry. The results showed that the presence of Ag decreases the beta' --> (alpha + gamma(1)) decomposition reaction rate in the Cu-9%Al-4%Ag alloy, an effect that may be associated to the gamma(1) phase which catalyses the Ag precipitation, making it faster than the decomposition reaction, and thus, stabilizing the martensitic phase. (C) 2003 Elsevier B.V. All rights reserved.