199 resultados para LANTHANUM SILICATES


Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this study, a bioactive zirconia-toughened alumina (ZTA) composite was developed for orthopedic applications. This composite was obtained by slip casting of suspension powder mixtures.Biomimetic processes were used to grow a bone-like apatite layer on composite substrates using sodium silicate solution as a nucleating agent and simulated body fluids. The composites, with or without coating, were characterized by diffuse reflectance infrared Fourier transform (DRIFT) spectroscopy and scanning electron microscopy (SEM) with energy dispersion spectroscopy (EDS), and their apparent density was determined by the Archimedes method. The composites obtained by this process possessed the expected stiffness and dimensions and their density values were similar to those of the composite's theoretical density (98.8%TD). The morphology of the hydroxyapatite formed on the composite surface was homogeneous and composed of small globules, characterizing a carbonated hydroxyapatite. The results of the tests indicated that the method employed to produce the composite and its coating was efficient under the conditions of this study. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Er3+ -containing gallium-lanthanum oxysulfide glasses have been prepared from Ga2O3 and La2S3 in a sulfur/argon reactive atmosphere. The samples have been characterized by absorption and emission spectroscopy and IR emission kinetics. Er3+ electronic transition intensities have been analyzed in the light of the Judd-Ofelt formalism, and quantum efficiencies evaluated for the Er3+ emission at 1.5 and 2.7 mum. The results so obtained suggest that these glasses display favorable properties concerning IR optical applications. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this work, Eu(III) and Eu(II) doped gadolinium silicates has been obtained as compact tubes starting from spherical gadolinium hydroxide carbonate using the pores of silica matrix as support and its surface as reagent. Eu(III) doped gadolinium silicate with hexagonal phase shows an interesting visible shifted charge transfer band when compared to disilicate with orthorhombic phase that was also obtained. Eu(II) gadolinium silicate has been prepared using CO atmosphere presenting an intense blue emission. The divalent europium system shows a potential application as an UV-blue converter. The samples were characterized by scanning electron microscopy (SEM), X-ray powder diffractometry (XRD) and photoluminescence spectroscopy. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The electronic structure of Pb1-xLaxTiO3 (PLT) compounds for x ranging from 0 to 30 at. % of La is investigated by means of soft x-ray absorption near edge structure (XANES) at the Ti L-3,L-2 and O K edges. The greatest modification in the structure of the Ti 2p XANES spectra of the PLT compounds is observed in the region of the high energy peak of the L-3 edge (e(g) states), which exhibits a splitting in the undoped sample. As the amount of lanthanum increases, this splitting becomes less pronounced. This modification is interpreted as a decrease in the degree of disorder of titanium atoms, which is correlated to the substitution of Pb by La atoms. The structural changes observed at the low energy peaks of the O K-edge XANES spectra of the PLT compounds may be interpreted in terms of hybridization between O 2p, Ti 3d, and Pb 6p orbitals. A decrease in the degree of hybridization observed as Pb atoms are replaced by La atoms may be related to the differences in the ferroelectric properties observed between x=0.0 and x=0.30 compounds. (c) 2006 American Institute of Physics.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The surface corrosion process associated with the hydrolysis of fluorozirconate glass, Z-BLAN (53ZrF(4), 20BaF(2), 20NaF, 4LaF(2), 3AlF(3)), and the corrosion protection efficiency of a nanocrystalline transparent SnO2 layer were investigated by X-ray photoelectron spectroscopy. The tin oxide film was deposited by the sol-gel dip-coating process in the presence of Tiron(R) as particle surface modifier agent. The chemical bonding structure and composition of the surface region of coated and non-coated ZBLAN were studied before water contact and after different immersion periods (5-30 min). In contrast to the effects occurring for non-coated glass, where the surface undergoes a rapid selective dissolution of the most soluble species inducing the formation of a new surface phase consisting of stable zirconium oxyfluoride, barium fluoride and lanthanum fluoride species, the results for the SnO2-coated glass showed that the hydrolytic attack induces a filling of the film nanopores by dissolved glass material and the formation of tin oxylluoride and zirconium oxyfluoride species. This process results in a modified film, which acts as a hermetic diffusion barrier protecting efficiently the glass surface. (C) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Eu3+ and Tm3+ doped lanthanum fluoride and lanthanum oxyfluoride are obtained from Eu3+, Tm3+ containing lanthanum fluoracetate solutions. The nature of the crystal phase obtained could be controlled by the temperature of heat treatment. Spectral characteristics of Eu3+ doped crystal phases were sufficiently different to allow utilization of Eu3+ as structural probes. Tm3+ emission at the technologically important spectral region of 1450nm could be observed for the fluoride and oxyfluoride crystal phases. The large bandwidth obtained (around 120nm) suggests potential applications in optical amplification. SiO2-LaF3-LaOF composite materials were also prepared. It is observed that for heat treatments above 800degreesC, fluorine loss, probably in the form of SiF4 hinder the observation of Tm3+ emission. Eu3+ spectroscopic characteristics clearly show the evolution of a fluoride like environment to an amorphous oxide one as the temperature of heat treatment increased. Thin films obtained by dip-coating on V-SiO2 substrates and treated at 300degreesC, 500degreesC and 800degreesC display guided modes in the visible and infrared regions. Optical characteristics (refractive index and films thickness) were obtained at 543.5, 632.8 and 1550nm. Attenuation as low as 1.8dB/cm was measured at 632.8nm. (C) 2004 Published by Elsevier B.V.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Crack-free polycrystalline PLZT (Pb,a)(Zr,Ti)O-3 thin films with the perovskite structure were prepared by dir-coating using the Pechinis process. Lead acetate, hydrated lanthanum carbonate, zirconium n-propoxide and titanium isopropoxide were used as raw materials. The viscosity of the solution was adjusted in the range of 20 to 56 cP and the films were deposited by a dip-coating process on silicon (100) as substrate. Solutions with ionic concentration of 0.1 and 0.2 M were used. Thin film deposition was accomplished by dipping the substrates in the solution with control of withdrawal speed from 5 to 20 mm/min. The thin films were thermally treated in two steps: at 300 degreesC amid 650 degreesC. The influence of withdrawal speed. viscosity, heating rate and ionic concentration on the morphology of PLZT thin film was discussed. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Pb1-XLaXTiO3 thin films, (X = 0.0; 13 and 0.27 mol%) were prepared by the polymeric precursor method. Thin films were deposited on Pt/Ti/SiO2/Si (1 1 1), Si (1 0 0) and glass substrates by spin coating, and annealed in the 200-300degreesC range in an O-2 atmosphere. X-ray diffraction, scanning electron microscopy and atomic force microscopy were used for the microstructural characterization of the thin films. Photoluminescence (PL) at room temperature has been observed in thin films of (PbLa)TiO3. The films deposited on Pt/Ti/SiO2/Si substrates present PL intensity greater than those deposited on glass and silicon substrates. The intensity of PL in these thin films was found to be dependent on the thermal treatment and lanthanum molar concentration. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The broadband inter-configurational (4f(1)5d(1)-->4f(2)) emission of Pr(3+) doped in lanthanum orthophosphate (LaPO(4)) and in calcium pyrophosphate (Ca(2)P(2)O(7)) has been investigated under plasma excitation. The synthesis by spray pyrolysis at moderate temperature followed by a controlled annealing proves to be a very efficient way to produce good quality UVC emitting phosphor Ca(1.92)Pr(0.04)Na(0.04)P(2)O(7) (alpha phase). The emission of this phosphor in the wavelength range 200-350 nm has been measured with a prototype device, which can be employed for anti-microbial testing. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The observation that mice with a selective ablation of the androgen receptor (AR) in Sertoli cells (SC) (SCARKO mice) display a complete block in meiosis supports the contention that SC play a pivotal role in the control of germ cell development by androgens. To delineate the physiological and molecular mechanism responsible for this control, we compared tubular development in pubertal SCARKO mice and littermate controls. Particular attention was paid to differences in SC maturation, SC barrier formation and cytoskeletal organization and to the molecular mediators potentially involved. Functional analysis of SC barrier development by hypertonic perfusion and lanthanum permeation techniques and immunohistochemical analysis of junction formation showed that SCARKO mice still attempt to produce a barrier separating basal and adluminal compartment but that barrier formation is delayed and defective. Defective barrier formation was accompanied by disturbances in SC nuclear maturation (immature shape, absence of prominent, tripartite nucleoli) and SC polarization (aberrant positioning of SC nuclei and cytoskeletal elements such as vimentin). Quantitative RT-PCR was used to study the transcript levels of genes potentially related to the described phenomena between day 8 and 35. Differences in the expression of SC genes known to play a role in junction formation could be shown from day 8 for Cldn11, from day 15 for Cldn3 and Espn, from day 20 for Cdh2 and Jam3 and from day 35 for ZO-1. Marked differences were also noted in the transcript levels of several genes that are also related to cell adhesion and cytoskeletal dynamics but that have not yet been studied in SC (Actn3, Ank3, Anxa9, Scin, Emb, Mpzl2). It is concluded that absence of a functional AR in SC impedes the remodeling of testicular tubules expected at the onset of spermatogenesis and interferes with the creation of the specific environment needed for germ cell development.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In the present investigation some spectroscopic properties of several lanthanide squarate hydrates are reported. The Raman spectra show the same distinctive Jahn-Teller intensity pattern for non-totally symmetric modes, as previously observed for the free anion. In the case of the terbium salt, the Tb3+ emission is very intense even at room temperature, revealing an efficient excitation via the ligand electronic levels. The Tb3+ dilution in Gd3+ or La3+ hosts increases this excitation efficiency without any appreciable variation in the 5D4 excited-state lifetime. However, the Eu3+ emission is very weak, with excited states located above the 5D2 level (ca. 21 550 cm-1) being completely quenched at room temperature. At lower temperatures higher-lying levels are not so efficiently quenched. The broad band observed in the UV excitation spectra of Eu3+ and Tb3+ is easily assigned to an intra-ligand transition leading to ligand-to-lanthanide ion energy transfer processes. As observed for Tb3+, Eu3+ dilution in Gd3+ or La3+ hosts also increases the relative emission intensity mediated by the ligand, without variation in the 5D0 excited-state lifetime. The Eu3+ 5D0 excitation spectra show vibronic structures that can be interpreted on the basis of the data available from the vibrational spectra. An increase in the vibronic intensities is observed as the lanthanide concentration is increased. © 1994.