81 resultados para Particle-size
Resumo:
This work presents a spray-dryer designed to oxalate-niobate precursors and suitable for the production of Niobium Carbide. The dryer was intended to produce powders of controlled particle size. First, the precursor is dissolved in water to produce a solution of known concentration and then it is atomized on the spray-dryer to produce the powder. This equipment consists of a 304 stainless steel chamber, 0.48 m x 1.9 m (diameter x length), with a conical shape at the lower portion, which is assembled on a vertical platform. The chamber is heated by three 4 kW electrical resistances. In this process, drying air is heated as it flows inside a serpentine surrounding the chamber, in contrary to more traditional processes in which the hot drying air is used to heat the component. The air enters the chamber at the same temperature of the chamber, thus avoiding adherence of particles on the internal surface. The low speed flow is concurrent, directed from the top to the bottom portion of the chamber. Powders are deposited on a 0.4 m diameter tray, which separates the cylindrical portion from the conical portion of the chamber. The humid air is discharged though a plug placed underneath the collecting tray. A factorial experimental planning was prepared to study the influence of five parameters (concentration, input flow, operation temperature, drying air flow and spray air flow) on the characteristics of the powders produced. Particle size distribution and shape were measured by laser granulometry and scanning electronic microscopy. Then, the powders are submitted to reaction in a CH4 / H2 atmosphere to compare the characteristics of spray-dried powders with powders synthetizided by conventional methods
Resumo:
This work aims at studying the influence of the concentration of calcite, its grain size and sintering temperature to obtain porous coating formulations that meet the design specifications. The experiments involved the physical-chemical and mineralogical caracterization of the raw materials, and mechanical tests on specimens dried and sintered, performing a planning mixture and factorial experiment, using the response surface methodology. The ceramic bodies studied were prepared by dry process, characterized, placed in conformity by uniaxial pressing and sintered at temperatures of 940 º C, 1000ºC, 1060ºC, 1120°C and 1180°C using a fast-firing cycle. The crystalline phases formed during sintering at temperatures under study, revealed the presence of anorthite and wolastonite, and quartz-phase remaining. These phases were mainly responsible for the physical and mechanical properties of the sintered especimens. The results shown that as increases the participation of carbonate in the composition of ceramic bodies there is an increase of water absorption and a slight reduction in linear shrinkage for all sintering temperatures. As for the mechanical strength it was observed that it tended to decrease for sintering at temperatures between 940 ° C and 1060 ° C and to increase for sintering at temperatures above 1060 ° C occurring with greater intensity for compositions with higher content of calcite. The resistence decreased with increasing participation of quartz in all sintering temperatures. The decrease in grain size of calcite caused a slight increase in water absorption for formulation with the same concentration of carbonate, remaining virtually unchanged the results of linear shrinkage and mechanical strength. In conclusion, porous ceramic coating (BIII) can be obtained using high concentrations of calcite and keeping the properties required in technical standards and that the particle size of calcite can be used as tuning parameter for the properties of ceramic products.
Resumo:
The municipal district of Equador-RN is located in an area of great amounts of ores, being your main economical activity the extraction and the kaolin improvement. The main originating from environmental problem that activity is the amount of generated residue, about 70% of the extracted kaolin. The residues are simply piled up in lands of the improvement companies, occupying like this a large area and causing impact in the existent flora. When dry, the residues transform powdered and for the action of the wind, they disperse, polluting the air. Being like this, the present work has as objective evaluates the incorporation of the great residue, originating from of the kaolin improvement, in partial substitution of all the employed aggregates in a conventional mixture of asphalt concrete, which was used in the paving of BR101/RN061 - passage between Ponta Negra and Ares. That evaluation was accomplished in three stages. The first refers to the evaluation of the physical, thermal and mineralogical characteristics of the residue with the intention of to classify it and to define your application as aggregate (small and great). The second refers to the physical characterization of the aggregates and of the asphalt material used in the conventional mixture. And the third, to the evaluation of the mixtures containing residue, which were elaborated starting from the conventional mixture with the gradual incorporation of the residue, from 5 to 40%, in substitution to the part of the conventional aggregates, in way to obtain similar particle size curves the one of the conventional mixture. That evaluation was accomplished through the comparison between the volumetric composition, the mechanical behavior and the susceptibility to the humidity of the mixtures containing residue with the one of the conventional mixture, and with the one of the DNIT specifications. The results show that the great residue originating from of the kaolin improvement has grains of the most varied size, being like this, it can substitute part of all the conventional aggregates and of the filler in an asphalt mixture. Besides, your mineralogical composition presented the same present minerals in the composition of conventional aggregates used in paving. The results evaluation of the volumetric composition of the mixtures containing residue indicates that it can use up to 30% of residue in substitution to the conventional aggregates. The evaluation of the mechanical behavior of those mixtures indicates that the residue increment in the studied mixtures caused an increase of the stability and a reduction of the resistance to the traction. The values obtained in the resistance to the traction meet below the minimum value specified by DNIT, but close to the value obtained in the conventional mixture. When taking in consideration the susceptibility of the same ones to the humidity, the results indicate that she can use up to 25% of residue
Resumo:
Eutrophication is a growing process present in the water sources located in the northeast of Brazil. Among the main consequences of these changes in trophic levels of a water source, stands out adding complexity to the treatment to achieve water standards. By these considerations, this study aimed to define, on a laboratory scale, products and operational conditions to be applied in the processing steps using raw water from Gargalheiras dam, RN, Brazil. The dam mentioned shows a high number of cyanobacteria, with a concentration of cells / ml higher than that established by Decree No. 518/04 MS. The same source was also considered by the state environmental agency in 2009 as hypereutrophic. The static tests developed in this research simulated direct filtration (laboratory filters) and pre-oxidation with chlorine and powdered activated carbon adsorption. The research included the evaluation of the coagulants aluminum hydrochloride (HCA) and alum (SA). The development of the research investigated the conditions for rapid mixing, the dosages of coagulants and pHs of coagulation by the drawing of diagrams. The interference of filtration rate and particle size of filtering means were evaluated as samples and the time of contact were tested with chlorine and activated carbon. By the results of the characterization of the raw water source it was possible to identify the presence of a high pH (7.34). The true color was significant (29 uH) in relation to the apparent color and turbidity (66 uH and 13.60 NTU), reflecting in the measurement of organic matter: MON (8.41 mg.L-1) and Abs254 (0.065 cm-1). The optimization of quick mix set time of 17", the speed gradient of 700 s-1 in the coagulation with HCA and the time of 20" with speed gradient of 800 s-1 for SA. The smaller particle sizes of sand filtering means helped the treatment and the variation in filtration rate did not affect significantly the efficiency of the process. The evaluation of the processing steps found adjustment in standard color and turbidity of the Decree nº 518/04 MS, taking in consideration the average values found in raw water. In the treatment using the HCA for direct filtration the palatable pattern based on the apparent color can be achieved with a dose of 25 mg L-1. With the addition of pre-oxidation step, the standard result was achieved with a reduced dose for 12 mgHCA.L-1. The turbidity standard for water was obtained by direct filtration when the dose exceeds 25 mg L-1 of HCA. With pre-oxidation step there is the possibility of reducing the dose to 20 mg L-1.The addition of CAP adsorption, promoted drinking water for both parameters, with even lower dosage, 13 mg L-1 of HCA. With coagulation using SA removal required for the parameter of apparent color it was achieved with pre-oxidation and 22 mgSA.L-1. Despite the satisfactory results of treatment with the alum, it was not possible to provide water with turbidity less than 1.00 NTU even with the use of all stages of treatment
Resumo:
A technological alternative for the correct disposal of tires is the use in the construction of embankment with soil and shredded tires. The use of waste tires in tropical soils requires prior knowledge of the properties and limitations of these materials. In this work, the results of an experimental program was devised to characterize the behavior of mixtures of waste tires and a lateritic soil. The residue used in this study is classified as tire buffings with an average size of 1.4 mm. The laboratory program included testing of particle size analysis, Atterberg limits, compaction, direct shear tests, permeability and confined compression tests with pure soil, pure tire and the mixtures. Proportions of 0% (pure soil), 10%, 20%, 40%, 50 % and 100% (pure tire) by weight were used. For the confining stress levels used in the study, the presence of tire residue provided a considerable increase in shear strength of the mixture. The maximum shear strength was obtained for a residue content of 40% by weight. Permeability tests on samples of waste under a confining stress of 100 kPa showed that the permeability increases significantly with increasing residue content until a residue content of 20%. The increase in permeability after that value showed to be negligible. Confined compression tests showed that the soil mixed with tire residue becomes more compressible than the pure soil. The secant constrained modulus (Msec) for the same vertical stress decreases with increasing percentage of residue.
Resumo:
The sludge generated in stabilization ponds can be designed for various purposes, among them we mention agricultural use, recovery of degraded areas and civil construction. The choice of these alternatives should be made based on qualitative and quantitative characteristics of the sludge. In this context, this study characterized the digested sludge from an anaerobic lagoon in Cidade do Natal/RN, which deals exclusively with residues of depleted septic tanks and pits. The sludge showed levels of macro and micronutrients that confirm its potential for agriculture, with 139.49 g.kg -1 organic matter, 15.40 g.kg-1 nitrogen and metal concentrations below those required by Resolution No. 375/06 of CONAMA, besides the absence of fecal coliform and less than 0.15 viable helminthes eggs/g, on average. The particle size distribution showed that most of the particles have a diameter similar to the sand, allowing the replacement of this input, for example. Analysis of the leachate and of the sludge solubilized classified as non-inert and non-hazardous according to NBR 10.004/04. The volume produced in three years of operation by the pond was 1903.50m³, equivalent to approximately 400 kg of dry sludge. Overall, the concentrations of the parameters were similar to literature, although none of them addresses sludge anaerobic pond treating sewer from septic tanks and pits.The sludgepresents technical feasibility to various types of use, however the cost of dewatering and especially with transport can derail it. It needs to be made a more thorough study of the costs to prove its economic viability
Resumo:
It was synthesized different Ni1-xMgxFe2O4 (0,2 ≤ x ≤ 0,7) compositions by use of citrate precursor method. Initially, the precursory citrates of iron, nickel and magnesium were mixed and homogenized. The stoichiometric compositions were calcined from 350°C to 1200°C at ambient atmosphere or in argon atmosphere. The calcined powders were characterized by XRD, TGA/DTG, FTIR, magnetic measures and reflectivity using the wave guide method. I was observed pure magnetic phase formation between 350°C and 500°C, with formation of ferrite and hematite after 600°C at ambient atmosphere. The calcined powder at argon atmosphere formed pure ferromagnetic phase at 1100°C and 1200°C. The Rietveld analyses calculated the cations level occupation and the crystallite size. The analyses obtained nanometric crystals (11-66 nm), that at 900°C/3h presents micrometric sizes (0,45 - 0,70 Om). The better magnetization results were 54 Am2/Kg for x= 0,2 composition, calcined at 350°C/3h and 30 min, and 55,6 Am2/Kg for x= 0,2 1200°C, calcined in argon. The hysteresis shows characteristics of soft magnetic material. Two magnetization processes were considered, superparamagnetism at low temperature and the magnetic domains formation at high temperatures. The materials presented absorption less or equal the 50 % in ranges specific frequency. As for the 2,0 and 3,0 thickness (in 11,0 - 11,8 GHz), the reflectivity of the x= 0,3, 0,5 and 0,4 compositions, all calcined at 900°C/3h showed agreement with MS and O. Various factors contribute for the final radiation absortion effect, such as, the particle size, the magnetization and the polymer characteristics in the MARE composition. The samples that presented better magnetization does not obtaining high radiation absorption. It is not clear the interrelaction between the magnetization and the radiation absorption in the strip of frequencies studied (8,2 - 12,4 GHz)
Resumo:
In this work, expanded perlite, a mineral clay, consisting of SiO2 and Al2O3 in the proportions of 72.1 and 18.5%, respectively, was used as an adsorbent for oil in its pure expanded form as well as hydrofobized with linseed oil. Thermogravimetry (TG), Derivative Thermogravimetry (DTG) and Differential Thermal Analysis (DTA) were used to study the thermal behavior and quantify the percent adsorption of perlite in differents processes comparing the results with the ones obtained using Gravimetric Analysis. In the process of hydrophobization with linseed oil granulometric fractions > 20, 20-32 and 32-60 mesh were used and adsorption tests with crude oil were performed in triplicate at room temperature. The results obtained by TG/DTG in dynamic atmosphere of air showed mass losses in a single step for the expanded perlite with pure adsorbed oil, indicating that the adsorption of oil was limited and that the particle size did not in this process. Linseed oil has performed well as an agent of hydrophobized perlite (32 to 60 mesh) indicating a maximum percentage of 59.9% and 68.6% the linseed with a fraction range from considering the data obtained by thermogravimetry and Gravimetry, respectively. The adsorption of oil in the expanded perlite and hydrofobized pure perlite with linseed oil did not produce good results, characterizing an increase of 0.5 to 4.6% in pure perlite and 3.3% in hydrofobized perlite with granulometric 32 to 60 mesh
Resumo:
Chitosan nanoparticles have been used in several systems for the controlled release of drugs. The aim of this study was to obtain and characterize chitosan nanoparticles prepared by the method of coacervation / precipitation using sodium sulfate at different concentrations as the crosslinking agent. The characterization was done using zeta potential and small angle Xray scattering, SAXS. The dispersions of chitosan were obtained at pH 1 and pH = 3. The results of zeta potential at pH = 1 ranged from +64.8 to +29.27 mV and for pH = 3 they varied from +72.4 to +23.48 mV, indicating that the chain of chitosan is positively charged in acidic pH and the behavior of nanoparticles in terms of surface charge was independent of pH. However, the results indicated a dependence of particle size in relation to pH. This difference in behavior was explained by the influence of enthalpic and entropic components
Resumo:
Produced water has lately aroused interest due to their high degree of salinity, suspended oil particles, chemicals added in various manufacturing processes, heavy metals and radioactivity sometimes. Along with oil and due to its high volume production, water production is one of the pollutants of most concern in the process of oil extraction. PAHs due to their ubiquity and their characteristics carcinogenic or mutagenic and teratogenic even have attracted the attention of every scientific society. Formed from the incomplete combustion of organic matter may be natural or anthropogenic. Some materials have been researched with the goal of cleaning up environmental matrices that may be contaminated by hydrocarbons. Among these materials researched various clays have been employed, of which highlights the vermiculite. The family of phyllosilicates, vermiculite for its potential and its high hydrophobic surface area has been a tool widely used in the decontamination of water in processes of oil spills. However, when it loses its capacity expanded hydrophobic having the necessity of using a hidrofobizante to make it organophilic. Among the numerous hidrofobizantes researched and used the linseed oil was the pioneer. In this study sought to evaluate the capacity of removal of PAHs using the vermiculite hydrofobized with linseed oil and wax also, for it was made use of the 24 full factorial design as the main tool for the experiments. We also evaluated the clay grain size (-20 +48 and -48 +80 #), the percentage of hidrofobizante applied (5 and 10%) and salinity of the water produced synthesized in our laboratory (35,000 and 55,000 ppm). The molecular fluorescence spectroscopy due to its sensitivity and speed was used to verify the adsorption capacity of clay, as well as gas chromatography served as an auxiliary technique to identify and quantify the PAHs in solution. In order to characterize the vermiculite was made use of X-ray fluorescence and X-ray diffraction. The infrared and thermogravimetry were essential to note hydrophobization and the amount of coating of clay. According to the fluorescence analysis showed that the test 12 was the best result in about 98% adsorption of fluorescent compounds, however the high salinity, the smallest particle size, the highest percentage of hidrofobizante and the use of linseed oil showed greater efficiency in the removal capacity of these hydrocarbons, in accordance with the trend followed by the analysis of the major factors of the factorial design. To verify the adsorption capacity of clay using a fixed volume of water produced synthetically, used as the test base 12, at their respective levels and factors. Thus, it was observed that after adding about 1 ½ liters of water solution produced synthetically, about 300 times its volume in mass, the vermiculite was able to adsorb 80% of fluorescent species present in solution
Resumo:
Cutting fluids are lubricants used in metal-mechanical industries. Their complex composition varies according to the type of operation carried out, also depending on the metals under treatment or investigation. Due to the high amount of mineral oil produced in Northeastern Brazil, we have detected the need to better use this class of material. In this work, two novel formulations have been tested, both based on naphthenic mineral oil and additives, such as: an emulsifying agent (A), an anticorrosion agent (B), a biocide (C) and an antifoam agent (D). Each formulation was prepared by mixing the additives in the mineral oil at a 700-rpm stirring velocity for 10 min, at 25°C, employing a 24 factorial planning. The formulations were characterized by means of density, total acid number (TAN), viscosity, flash point and anticorrosion activity. In a subsequent study, oil-in-water emulsions were prepared from these novel formulations. The emulsions were analyzed in terms of stability, corrosion degree, percentage of foam formation, conductivity, accelerated stability and particle size. The samples were appropriately labeled, and, in special, two of them were selected for featuring emulsion properties which were closer to those of the standards chosen as references (commercial cutting oils). Investigations were undertaken on the ability of NaCl and CaCl2 to destabilize the emulsions, at concentrations of 2%, 5% and 10%, at an 800-rpm stirring velocity for 5 min and temperatures of 25º, 40º, 50º and 60ºC. The recovered oils were chemically altered by reincorporating the same additives used in the original formulations, followed by preparation of emulsions with the same concentrations as those of the initial ones. The purpose was to assess the possibility of reusing the recovered oil. The effluents generated during the emulsion destabilization step were characterized via turbidity index, contents of oil and grease, pH, and contents of anions and cations, observing compliance with the parameters established by the current environmental legislation (Brazil s CONAMA 357/05 resolution). It could be concluded that the formulations presented excellent physicochemical properties as compared to commercial cutting fluids, showing that the quality of the newly-prepared fluids is superior to that of the formulations available in the market, enabling technically and environmentally-safe applications
Resumo:
In this research the removal of light and heavy oil from disintegrated limestone was investigated with use of microemulsions. These chemical systems were composed by surfactant, cosurfactant, oil phase and aqueous phase. In the studied systems, three points in the water -rich microemulsion region of the phase diagrams were used in oil removal experiments. These microemulsion systems were characterized to evaluate the influence of particle size, surface tension, density and viscosity in micellar stability and to understand how the physical properties can influence the oil recovery process. The limestone rock sample was characterized by thermogravimetry, BET area, scanning electron microscopy and X-ray fluorescence. After preparation, the rock was placed in contact with light and heavy oil solutions to allow oil adsorption. The removal tests were performed to evaluate the influence of contact time (1 minute, 30 minutes, 60 minutes and 120 minutes), the concentration of active matter (20, 30 and 40 %), different cosurfactants and different oil phases. For the heavy oil, the best result was on SME 1, with 20 % of active matter, 1 minute of contact time, with efficiency of 93,33 %. For the light oil, also the SME 1, with 20 % of active matter, 120 minutes of contact time, with 62,38 % of efficiency. From the obtained results, it was possible to conclude that microemulsions can be considered as efficient chemical systems for oil removal from limestone formations
Resumo:
Materials consisting of perovskite-type oxides (ABO3) have been developed in this work for applications in fuel cell cathodes of solid oxide type (SOFC). These ceramic materials are widely studied for this type of application because they have excellent electrical properties, conductivity and electrocatalytic. The oxides LaMnO3, LaFeO3, LaFe0.2Mn0.8O3 e La0.5Fe0.5MnO3 were synthesized by the method of microwave assisted combustion and after sintering at 800°C in order to obtain the desired phases. The powders were characterized by thermogravimetry (TG), X-ray diffraction (XRD), X-ray fluorescence (XRF), scanning electron microscopy (SEM) and voltammetric analysis (cyclic voltammetry and polarization curves). The results obtained by XRF technique showed that the microwave synthesis method was effective in obtaining doping oxides with values near stoichiometric. In general, powders were obtained with particle size less than 0.5 μm, having a porous structure and uniform particle size distribution. The particles showed spherical form, irregular and crowded of varying sizes, according to the analysis of SEM. The behavior of the oxides opposite the thermal stability was monitored by thermogravimetric curves (TG), which showed low weight loss values for all samples, especially those of manganese had its structure. By means of Xray diffraction of the samples sintered at 800°C was possible to observe the formation of powders having high levels of crystallinity. Furthermore, undesirable phases such as La2O3 and MnOx were not identified in the diffractograms. These phases block the transport of oxygen ions in the electrode/electrolyte interface, affecting the electrochemical activity of the system. The voltammetric analysis of the electrocatalysts LF-800, LM-800, LF2M8-800 e L5F5M-800 revealed that these materials are excellent electrical conductors, because it increased the passage of electrical current of the working electrode significantly. Best performance for the oxygen reduction reaction was observed with iron-rich structures, considering that the materials obtained have characteristics suitable for use in fuel cell cathodes of solid oxide type
Resumo:
The environmental impact due to the improper disposal of metal-bearing industrial effluents imposes the need of wastewater treatment, since heavy metals are nonbiodegradable and hazardous substances that may cause undesirable effects to humans and the environment. The use of microemulsion systems for the extraction of metal ions from wastewaters is effective when it occurs in a Winsor II (WII) domain, where a microemulsion phase is in equilibrium with an aqueous phase in excess. However, the microemulsion phase formed in this system has a higher amount of active matter when compared to a WIII system (microemulsion in equilibrium with aqueous and oil phases both in excess). This was the reason to develop a comparative study to evaluate the efficiency of two-phases and three-phases microemulsion systems (WII and WIII) in the extraction of Cu+2 and Ni+2 from aqueous solutions. The systems were composed by: saponified coconut oil (SCO) as surfactant, n-Butanol as cosurfactant, kerosene as oil phase, and synthetic solutions of CuSO4.5H2O and NiSO4.6H2O, with 2 wt.% NaCl, as aqueous phase. Pseudoternary phase diagrams were obtained and the systems were characterized by using surface tension measurements, particle size determination and scanning electron microscopy (SEM). The concentrations of metal ions before and after extraction were determined by atomic absorption spectrometry. The extraction study of Cu+2 and Ni+2 in the WIII domain contributed to a better understanding of microemulsion extraction, elucidating the various behaviors presented in the literature for these systems. Furthermore, since WIII systems presented high extraction efficiencies, similar to the ones presented by Winsor II systems, they represented an economic and technological advantage in heavy metal extraction due to a small amount of surfactant and cosurfactant used in the process and also due to the formation of a reduced volume of aqueous phase, with high concentration of metal. Considering the reextraction process, it was observed that WIII system is more effective because it is performed in the oil phase, unlike reextraction in WII, which is performed in the aqueous phase. The presence of the metalsurfactant complex in the oil phase makes possible to regenerate only the surfactant present in the organic phase, and not all the surfactant in the process, as in WII system. This fact allows the reuse of the microemulsion phase in a new extraction process, reducing the costs with surfactant regeneration
Resumo:
Chitosan is a biopolymer derived from the shells of crustaceans, biodegradable, inexpensive and renewable with important physical and chemical properties. Moreover, the different modifications possible in its chemical structure generate new properties, making it an attractive polysaccharide owing to its range of potential applications. Polymers have been used in oil production operations. However, growing concern over environmental constraints has prompted oil industry to search for environmentally sustainable materials. As such, this study sought to obtain chitosan derivatives grafted with hydrophilic (poly(ethylene glycol), mPEG) and/or hydrophobic groups (n-dodecyl) via a simple (one-pot) method and evaluate their physicochemical properties as a function of varying pH using rheology, small-angle Xray scattering (SAXS), dynamic light scattering (DLS) and zeta potential. The chitosan derivatives were prepared using reductive alkylation under mild reaction conditions and the chemical structure of the polymers was characterized by nuclear magnetic resonance (1H NMR) and CHN elemental analysis. Considering a constant mPEG/Chitosan molar ratio on modification of chitosan, the solubility of the polymer across a wide pH range (acidic, neutral and basic) could only be improved when some of the amino groups were submitted to reacetylation using the one-pot method. Under these conditions, solubility is maintained even with the simultaneous insertion of n-dodecyl. On the other hand, the solubility of derivatives obtained only through mPEG incorporation using the traditional methodology, or with the ndodecyl group, was similar to that of its precursor. The hydrophilic group promoted decreased viscosity of the polymer solutions at 10 g/L in acid medium. However, at basic pH, both viscosity and thermal stability increased, as well as exhibited a pronounced pseudoplastic behavior, suggesting strong intermolecular associations in the alkaline medium. The SAXS results showed a polyelectrolyte behavior with the decrease in pH for the polymer systems. DLS analyses revealed that although the dilute polymer solutions at 1 g/L and pH 3 exhibited a high density of protonated amino groups along the polymer chain, the high degree of charge contributed significantly to aggregation, promoting increased particle size with the decrease in pH. Furthermore, the hydrophobic group also contributed to increasing the size of aggregates in solution at pH 3, whereas the hydrophilic group helped reduce their size across the entire pH range. Nevertheless, the nature of aggregation was dependent on the pH of the medium. Zeta potential results indicated that its values do not depend solely on the surface charge of the particle, but are also dependent on the net charge of the medium. In this study, water soluble associative polymers exhibit properties that can be of great interest in the petroleum industry