Konecranes Corporation manufactures huge steel structures in 16 factories worldwide, in which the environment and quality varies. The company has a desire to achieve the same weld quality in each factory, regardless of the manufacturing place. The main subject of this master’s thesis was to develop the present box girder crane welding process, submerged arc welding and especially the fillet welding. Throughput time and manufacturing costs can be decreased by welding the full penetration fillet weld without a bevel, changing present groove types for more appropriate ones and by achieving the desired weld quality on the first time. Welding experiments of longitudinal fillet welding were made according to the present challenges, which the manufacturing process is facing. In longitudinal fillet welding tests the main focus was to achieve full penetration fillet weld for 6, 8 and 10 millimeters thick web plates with single and twin wire submerged arc welding. Full penetration was achieved with all the material thicknesses, both with single and twin wire submerged arc welding processes. The main problem concerning the weld was undercutting and shape of the weld bead. The question about insufficiency of presently used power sources with twin wire was risen up during testing, due to the thicknesses that require high welding current. Bigger power source is required when box girders are welded nonstop, if twin wire is used. For single wire process the penetration was achieved with significantly less amperage than with twin wire.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In ship and offshore terminal construction, welded cross sections are thick and the number of welds very high. Consequently, there are two aspects of great importance; cost and heat input. Reduction in the welding operation time decreases the costs of the work force and avoids excessive heat, preventing distortion and other weld defects. The need to increase productivity while using a single wire in the GMAW process has led to the use of a high current and voltage to improve the melting rate. Unfortunately, this also increases the heat input. Innovative GMAW processes, mostly implemented for sheet plate sections, have shown significant reduction in heat input (Q), low distortion and increase in welding speed. The aim of this study is to investigate adaptive pulsed GMAW processes and assess relevant applications in the high power range, considering possible benefits when welding thicker sections and high yield strength steel. The study experimentally tests the usability of adaptive welding processes and evaluates their effects on weld properties, penetration and shapes of the weld bead.The study first briefly reviews adaptive GMAW to evaluate different approaches and their applications and to identify benefits in adaptive pulsed. Experiments are then performed using Synergic Pulsed GMAW, WiseFusionTM and Synergic GMAW processes to weld a T-joint in a horizontal position (PB). The air gap between the parts ranges from 0 to 2.5 mm. The base materials are structural steel grade S355MC and filler material G3Si1. The experiment investigates heat input, mechanical properties and microstructure of the welded joint. Analysis of the literature reveals that different approaches have been suggested using advanced digital power sources with accurate waveform, current, voltage, and feedback control. In addition, studies have clearly indicated the efficiency of lower energy welding processes. Interest in the high power range is growing and a number of different approaches have been suggested. The welding experiments in this study reveal a significant reduction of heat input and a weld microstructure with the presence of acicular ferrite (AF) beneficial for resistance to crack propagation. The WiseFusion bead had higher dilution, due to the weld bead shape, and low defects. Adaptive pulse GMAW processes can be a favoured choice when welding structures with many welded joints. The total heat reduction mitigates residual stresses and the bead shape allows a higher amperage limit. The stability of the arc during the process is virtually spatter free and allows an increase in welding speed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Tämän tutkimuksen tavoitteena oli nykyisin tuotantokäytössä olevan rullaoikaisukoneen automatisointi ja uuden oikaisukonekokonaisuuden mitoitus tulevaisuuden materiaaliominaisuuksien perusteella. Automatisoinnilla on tarkoitus nykyisessä käytössä helpottaa nauhahitsaajan työtä ja lähitulevaisuudessa optimoida romutustarvetta kelojen keula- ja häntäalueilla. Uuden oikaisukonekokonaisuuden osalta työssä on määritetty rullaoikaisukoneen rullakoot, rullien keskiöetäisyys, vaadittava moottoriteho ja rullien tuennan tarve sekä erillisen hilseenmurskaimen/rullavenytysoikaisukoneen tarve peittauslinjan toiminnassa. Rullaoikaisukoneen asetusarvojen laskeminen toteutettiin ympyräkaarimenetelmää ja seurantatutkimusta käyttäen. Ensimmäisen ylärullan asetteluarvot on laskettu suorilla kaavasovelluksilla. Toisen ylärullan kohdalla oli tarpeellista tehdä laajempaa seurantatutkimusta, jotta löydettiin sellainen tapa, jolla myös sen arvot saataisiin riippuvaiseksi ensimmäisen ylärullan asetteluarvoista ja ympyränkaarimenetelmästä. Uutta oikaisukonekokonaisuutta varten suoritettujen laskelmien perusteella rullaoikaisukoneen telakokoa ja keskiöetäisyyttä on pienennettävä, moottoritehoa on kasvatettava ja työrullien tuentaa on parannettava verrattuna nykyiseen tuotantokoneeseen. Esioikaisukonetyyppisen rullaoikaisukoneen rajoittuneesta oikaisutuloksesta ja tietyillä kelalaaduilla esiintyvä erittäin luja wüstiittihilse puoltaa vahvasti erillisen hilseenmurskaimen lisäämistä peittauslinjan konekantaan.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Hitsauksen tuottavuuteen vaikuttavat hitsausmäärä, käytetyt prosessit ja laatu. Työn teoriaosuudessa tutustutaan hitsauksen tuottavuuteen sekä suunnittelullisesta että valmistuksellisesta näkökulmasta. Hitsauksen laadulliset asiat, kuten laatustandardit ja vaatimukset käydään läpi keskittyen standardin SFS-EN ISO 3834 kattaviin laatuvaatimuksiin. Rikkomaton ja rikkova aineenkoetus ja yleisimmät hitsausvirheet esitetään yleisellä tasolla. Hitsausprosesseista esitetään MIG/MAG- ja MAG-täytelankahitsauksen sekä pulssihitsauksen perusteet. Tässä diplomityössä tutkitaan pulssihitsauksen soveltuvuutta sähkögeneraattorin staattoripaketin eripariliitoksen hitsaukseen ja kykyä parantaa sekä tuottavuutta että laatua. Tutkimus perustuu koehitsauksiin ja niiden perusteella tehtyihin johtopäätöksiin. Lisäksi pohditaan sisätuulettimien hitsauksen kehittämistä ja annetaan kehitysehdotus valmistusprosessista. Koehitsauksien perusteella pulssihitsaus on hyvä prosessiparannus staattoripakettien hitsaukseen. Kohdistettu valokaari ja alhaisempi lämmöntuonti verrattuna perinteiseen MAG-hitsaukseen sekä hitsauksen yksinkertaisuus tuovat etuja eripariliitoksen hitsauksen laatuun. Kustannuslaskelmien myötä hitsausprosessin muutoksen odotetaan tuovan kustannussäästöjä. Hitsauslaadun parantuessa ja jälkityöstön määrän vähentyessä hitsausprosessin muutos on kannattava.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Työssä tutkittiin Ruukki Oyj:n suorasammutetusta S960QC-teräksestä valmistetun kuormaakantavan levyjen ristiliitoksen pienahitsien lujuutta, muodonmuutoskykyä ja vaurioitumismekanismia laajaan kokeelliseen aineistoon perustuen. Tärkeimpänä muuttujana koematriisissa olivat eri MAG-hitsausprosessit. Perinteisen kuumakaarihitsauksen vertailukohteena oli Kemppi Oy:n uusi adaptiivinen valokaaren pituutta säätävä WiseFusion-hitsaustoiminto kuuma- ja pulssikaarihitsauksessa. Näiden kolmen hitsausprosessin rinnalla varioitiin erisuuruisia a-mittoja, eri hitsauslisäaineita ja hitsin erikylkisyyttä. Lisäksi juuritunkeuman estämisen vaikutusta hitsien käyttäytymiseen tutkittiin täydentävällä koesarjalla, jossa tunkeuman muodostuminen estettiin levyjen väliin asetetulla volframilevyllä. Työn perimmäisenä tavoitteena oli selvittää syy aiemmassa tutkimuksessa havaitulle pienahitsien vaurioitumiselle leikkautumalla sularajaa pitkin. Sularajan suhteellista pituutta saadaan kasvatettua estämällä hitsin juuritunkeuma ja absoluuttista pituutta saadaan lisää kateettipoikkeaman avulla. Lisäksi tutkimuksessa oli tarkoitus tuoda esille suurlujuusteräksisen liitoksen eri mitoituslähtökohdat (mm. lämmöntuonnin kontrollointi). Tämän vuoksi hitsausparametrit mitattiin jännitteen ja virran hetkellisiin arvoihin perustuen, jolloin kuuma- ja pulssikaarihitsauksen laskennalliset hitsaustehot ovat vertailukelpoisia. Koehitseistä valmistettiin hieet hitsien tarkan geometrian määrittämiseksi ja liitoksen mekaaniset ominaisuudet tutkittiin vetokokeella. Tulosten perusteella sularajavaurio aktivoituu pulssikaarella hitsatuissa koekappaleissa. Tämä aiheutunee pulssi- ja kuumakaarihitsauksen sularajan mikrorakenteiden eroavaisuudesta. Sularajavaurio näyttää huonontavan hitsien muodonmuutoskykyä, mutta jatkokokeita tuloksen verifioimiseksi on tehtävä. S960QC-teräkselle ominaisen pehmenneen vyöhykkeen vaurio ei aktivoitunut, vaikka Ruukin antamat jäähtymisaikasuositukset ylitettiin reilusti.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Tässä tutkimuksessa selvitetään ilman hitsauslisäainetta tapahtuvan laser–TIG–hybridihitsausprosessin soveltuvuus 6 mm ja 8 mm paksujen päittäisliitettyjen S355 K2 ja Laser 355 MC rakenneterästen hitsaukseen. Hitsien tarkastelussa huomio kiinnitetään hitsausnopeuteen, hitsien tunkeumaan, liittämistehokkuuteen, hitsien kovuuteen ja hitsausliitoksen ulkonäköön. Muita tutkittavia asioita ovat laser-TIG-hybridihitsattujen levyjen muodonmuutokset ja suuresta hitsausnopeudesta sekä pienestä t8/5 jäähtymisajasta johtuvat mahdolliset kylmähalkeamat. Laser-TIG-hybridihitsejä verrataan robotti-MAG- ja käsin MAG-hitseihin sekä kaarihitsausstandardin SFS-EN ISO 5817 hitsiluokkien mukaisiin raja-arvoihin. Laser-TIG-hybridihitsausprosessissa TIG-valokaari mahdollistaa tasaisen ja lähes roiskeettoman hitsin ja lasersäde aikaansaa syvän tunkeuman sekä tasalaatuisen juurihitsin. Laser-TIG-hybridihitsausprosessilla 6 mm paksut S355 K2 rakenneteräslevyt on mahdollista hitsata levyn yhdeltä puolelta kerralla valmiiksi. Paksummat 8 mm levyt voidaan hitsata levyn yhdeltä tai molemmilta puolilta suoritettavalla laser-TIG-hybridihitsauksella. Laser-TIG-hybridihitsausprosessilla hitsatut hitsit ovat hyvin siistejä ja lähes roiskeettomia. Verrattaessa laser-TIG-hybridihitsausprosessia muihin hitsausprosesseihin sen voidaan todeta olevan erittäin kilpailukykyinen 6 mm paksujen päittäisliitettyjen rakenneterästen hitsaamisessa, mutta se soveltuu myös 8 mm paksujen rakenneterästen hitsaamiseen. Tutkitut hitsit täyttävät kaarihitsausstandardin SFS-EN ISO 5817 B- ja D-hitsiluokkien mukaiset raja-arvot. Vertailukokeet 6 mm paksulla S355 rakenneteräksellä osoittavat, että yhdeltä puolelta suoritettavan laser-TIG-hybridihitsauksen hitsausnopeus on robotti-MAG-hitsaukseen verrattuna yli nelinkertainen ja MAG-käsinhitsaukseen verrattuna yli viisinkertainen. Laser-TIG-hybridihitsauksessa liittämistehokkuus on noin viisinkertainen robotti-MAGhitsaukseen verrattuna. Molemmilta puolilta suoritettavalla laser-TIG-hybridihitsauksella voidaan 8 mm paksulla S355 rakenneteräksellä saavuttaa noin kolminkertainen hitsausnopeus ja liittämistehokkuus robotti-MAG-hitsaukseen verrattuna. Laser-TIG-hybridihitsauksessa TIG-kaaren tuoman lisälämmön ansiosta suurillakin hitsausnopeuksilla (1 m/min) voidaan saavuttaa edulliset kovuusarvot. Kovuusmittausten tulosten perusteella 6 mm ja 8 mm paksujen S355 K2 ja Laser 355 MC rakenneterästen hitsit eivät ylittäneet kaarihitsausstandardin määrittelemää 350 HV kovuuden enimmäisrajaa. Laser-TIG-hybridihitsauksen edullisesta lämmöntuonnista johtuen levyjen pituus- ja poikittaissuuntaiset muodonmuutokset ovat noin 80 prosenttia pienemmät kuin käsin suoritettavassa MAG-hitsauksessa. Laser-TIG-hybridihitsausprosessilla käytetään I-railoa, mutta robotti-MAG- ja käsin MAG-hitsausprosesseilla joudutaan käyttämään V-railoa, jolloin lämmöntuonti ja siitä johtuvat muodonmuutokset ovat suuremmat. Korkea liittämistehokkuus ja edullinen lämmöntuonti merkitsevät vähäisempiä muodonmuutoksia ja siten merkittäviä säästöjä työ-, materiaali- ja energiakustannuksissa. 8 mm ja sitä paksummilla S355 rakenneteräksillä levyn yhdeltä puolelta suoritettava päittäisliitoksen hitsaaminen on laser-TIG hybridihitsauksella haastavaa, koska yli 200 A:n TIG-kaarivirralla suuri metallisula aiheuttaa avaimenreiän sulkeutumisen ja avaimenreiän alaosaan muodostuu kaasukuplia. Tästä voidaan tehdä sellainen johtopäätös, että päittäisliitettävien levyjen ilmarakoa pitäisi kasvattaa niin suureksi, että avaimenreiän sulavirtaus ei pääse estymään. Yli 0,25 mm:n ilmarako edellyttää lasersäteen vaaputusta tai säteen halkaisijan kasvattamista. Ilmaraon kasvattaminen edellyttää myös lisäaineen käyttöä. Tutkimustulosten perusteella laser-TIG-hybridihitsausprosessilla voidaan saavuttaa merkittäviä etuja ja kustannussäästöjä, joten sen hyödyntämistä kannattaa harkita 8 mm ja sitä ohuempien päittäisliitettävien tuotteiden konepaja- ja tehdastuotannossa. Laser-TIGhybridihitsausprosessi soveltuu esimerkiksi seuraavien tuotteiden hitsaamiseen: päittäisliitettävät levyt, palkit, koneenosat, putket, säiliöt ja erilaiset pyörähdyskappaleet.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Joining processes and techniques need to meet the trend of new applications and the development of new materials. The application in connection with thick and thin plates in industrial fields is wide and the joining technology is in very urgent need. The laser-TIG hybrid welding technology can play the respective advantages of both of them. One major advantage of the hybrid laser-TIG welding technology is its efficient use of laser energy. Additionally, it can develop into a high and new advanced welding technology and become a hot spot in both the application and research area. This thesis investigated laser –TIG hybrid welding with the aim of enlightening the reader on its advantages, disadvantages and future areas of improvement. The main objective is to investigate laser-TIG hybrid on the welding of various metals (steels, magnesium, aluminium etc.). In addition, it elaborates on various possible combinations on hybrid laser-TIG welding technology and their benefits. The possibility of using laser-TIG hybrid in welding of thick materials was investigated. The method applied in carrying out this research is by using literature review. The results showed that hybrid laser-TIG is applicable to almost all weldable metals. Also it proves to be effective in welding refractive metals. The possibility of welding with or without filler materials is of economic advantage especially in welding of materials with no filler material. Thick plate’s hybrid laser-TIG welding is showing great prospects although it normally finds its used in welding thin materials in the range of 0.4 to 0.8 mm. The findings show that laser-TIG hybrid welding can be a versatile welding process and therefore will be increasingly used industrially due to its numerous advantages and the development of new TIG arc that enhances its capabilities.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

At present, permanent magnet synchronous generators (PMSGs) are of great interest. Since they do not have electrical excitation losses, the highly efficient, lightweight and compact PMSGs equipped with damper windings work perfectly when connected to a network. However, in island operation, the generator (or parallel generators) alone is responsible for the building up of the network and maintaining its voltage and reactive power level. Thus, in island operation, a PMSG faces very tight constraints, which are difficult to meet, because the flux produced by the permanent magnets (PMs) is constant and the voltage of the generator cannot be controlled. Traditional electrically excited synchronous generators (EESGs) can easily meet these constraints, because the field winding current is controllable. The main drawback of the conventional EESG is the relatively high excitation loss. This doctoral thesis presents a study of an alternative solution termed as a hybrid excitation synchronous generator (HESG). HESGs are a special class of electrical machines, where the total rotor current linkage is produced by the simultaneous action of two different excitation sources: the electrical and permanent magnet (PM) excitation. An overview of the existing HESGs is given. Several HESGs are introduced and compared with the conventional EESG from technical and economic points of view. In the study, the armature-reaction-compensated permanent magnet synchronous generator with alternated current linkages (ARC-PMSG with ACL) showed a better performance than the other options. Therefore, this machine type is studied in more detail. An electromagnetic design and a thermal analysis are presented. To verify the operation principle and the electromagnetic design, a down-sized prototype of 69 kVA apparent power was built. The experimental results are demonstrated and compared with the predicted ones. A prerequisite for an ARC-PMSG with ACL is an even number of pole pairs (p = 2, 4, 6, …) in the machine. Naturally, the HESG technology is not limited to even-pole-pair machines. However, the analysis of machines with p = 3, 5, 7, … becomes more complicated, especially if analytical tools are used, and is outside the scope of this thesis. The contribution of this study is to propose a solution where an ARC-PMSG replaces an EESG in electrical power generation while meeting all the requirements set for generators given for instance by ship classification societies, particularly as regards island operation. The maximum power level when applying the technology studied here is mainly limited by the economy of the machine. The larger the machine is, the smaller is the efficiency benefit. However, it seems that machines up to ten megawatts of power could benefit from the technology. However, in low-power applications, for instance in the 500 kW range, the efficiency increase can be significant.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Tässä diplomityössä kehitettiin yksitoimisten puristussylinterien valmistusta Rautessa. Sylinterien valmistuksessa haastavin vaihe on sylinteriputken ja pohjan välinen hitsaus. Hitsauksen avuksi suunniteltiin sylinterin sisäpuolinen juuritukilaite. Hitsauskokeita suoritettiin hitsin pohjan jauhekaarihitsaukselle ja MAG-hitsaukselle. Juuritukilaitteen toimivuutta testattiin koehitsauksilla. Puristussylinterien materiaali on S355J2-terästä, jonka ainevahvuus on 20 – 60 mm. Paksujen rakenneterästen hitsauksessa täytyy ottaa huomioon hitsausliitoksen mekaanisten ominaisuuksien muuttuminen sekä eri halkeamien synty. Hitsauksen laatuun ja laadunhallintaan voidaan vaikuttaa monien eri tekijöiden avulla. Hitsausohjeen avulla, ja muut laatutekijät huomioiden, voidaan hitseille asetetut laatukriteerit täyttää. Juurituen käyttö nopeuttaa puristussylinterien hitsausta vähintään 50 %. Jauhekaarihitsaus kuparista juuritukea vasten synnyttää vaikeasti poistettavan kuonan juuren puolelle. Perinteinen MAG-hitsaus kuparista juuritukea vasten sisältää liian monta muuttujaa, mikä tekee siitä epäluotettavan pohjapalon hitsaukseen. Työssä suunnitellun juuritukilaitteen käyttö tuotannossa vaatii lisää hitsauskokeita.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Tuulivoima on Euroopassa nopeimmin kasvava energian tuotantomuoto. Tuulivoimateollisuuden arvioidaan kasvavan Suomessa huomattavasti lähivuosien aikana ennakoidun syöttötariffipäätöksen myötä, jolloin kilpailu alalla tulee kasvamaan. Tavoitteena oli kehittää tuulivoimalan tornin valmistusta Levator Oy:ssä hitsaustuotantoa tehostamalla ja tuotannon ohjattavuutta parantamalla. Kehitystyöhön kuului toisen hitsauslinjan käyttöönoton suunnittelu ja ohjeiston laatiminen työnjohdolle. Toisen hitsauslinjan käyttöönoton suunnittelun tarkoituksena oli suunnitella muutokset nykyiseen tuotantoon uuden linjan käyttöönoton mahdollistamiseksi. Suunnittelu aloitettiin valitsemalla hitsausprosessit, jonka jälkeen suunniteltiin laitetarpeet työvaihe-analyysien pohjalta. Tuotantolayout muutettiin nykyisestä funktionaalisesta tuotannosta tuotantosoluista koostuvaksi tuotantolinjaksi, jolloin materiaalien virtautus parani huomattavasti. Tuotannon ohjaustavaksi valittiin kapeikko-ohjaus. Ohjeiston laatimisen tarkoituksena oli kerätä ja dokumentoida kaikki tuotannossa tarvittava tieto. Ohjeiston sisältää laadunohjaus, materiaalivirtojen ohjaus ja työnohjaus osiot, joiden tarkoituksena on helpottaa työnjohtamista. Ohjeisto määrittelee yhtenäiset tuotannon toimintatavat, jolloin tuotannon ohjattavuus helpottuu. Tavoitteet täyttyivät, kun toisen tuotantolinjan käyttöönoton vaatimat muutokset aloitettiin suunnitelmien mukaisesti syyskuussa 2009. Ohjeiston sisältö saatiin määriteltyä ja eri osioiden pilotit saatiin valmiiksi joulukuun aikana. Tuotannon ohjattavuus kehittyi huomattavasti ja samalla tuottavuus parani merkittävästi.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The Arctic region becoming very active area of the industrial developments since it may contain approximately 15-25% of the hydrocarbon and other valuable natural resources which are in great demand nowadays. Harsh operation conditions make the Arctic region difficult to access due to low temperatures which can drop below -50 °C in winter and various additional loads. As a result, newer and modified metallic materials are implemented which can cause certain problems in welding them properly. Steel is still the most widely used material in the Arctic regions due to high mechanical properties, cheapness and manufacturability. Moreover, with recent steel manufacturing development it is possible to make up to 1100 MPa yield strength microalloyed high strength steel which can be operated at temperatures -60 °C possessing reasonable weldability, ductility and suitable impact toughness which is the most crucial property for the Arctic usability. For many years, the arc welding was the most dominant joining method of the metallic materials. Recently, other joining methods are successfully implemented into welding manufacturing due to growing industrial demands and one of them is the laser-arc hybrid welding. The laser-arc hybrid welding successfully combines the advantages and eliminates the disadvantages of the both joining methods therefore produce less distortions, reduce the need of edge preparation, generates narrower heat-affected zone, and increase welding speed or productivity significantly. Moreover, due to easy implementation of the filler wire, accordingly the mechanical properties of the joints can be manipulated in order to produce suitable quality. Moreover, with laser-arc hybrid welding it is possible to achieve matching weld metal compared to the base material even with the low alloying welding wires without excessive softening of the HAZ in the high strength steels. As a result, the laser-arc welding methods can be the most desired and dominating welding technology nowadays, and which is already operating in automotive and shipbuilding industries with a great success. However, in the future it can be extended to offshore, pipe-laying, and heavy equipment industries for arctic environment. CO2 and Nd:YAG laser sources in combination with gas metal arc source have been used widely in the past two decades. Recently, the fiber laser sources offered high power outputs with excellent beam quality, very high electrical efficiency, low maintenance expenses, and higher mobility due to fiber optics. As a result, fiber laser-arc hybrid process offers even more extended advantages and applications. However, the information about fiber or disk laser-arc hybrid welding is very limited. The objectives of the Master’s thesis are concentrated on the study of fiber laser-MAG hybrid welding parameters in order to understand resulting mechanical properties and quality of the welds. In this work only ferrous materials are reviewed. The qualitative methodological approach has been used to achieve the objectives. This study demonstrates that laser-arc hybrid welding is suitable for welding of many types, thicknesses and strength of steels with acceptable mechanical properties along very high productivity. New developments of the fiber laser-arc hybrid process offers extended capabilities over CO2 laser combined with the arc. This work can be used as guideline in hybrid welding technology with comprehensive study the effect of welding parameter on joint quality.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The iron and steelmaking industry is among the major contributors to the anthropogenic emissions of carbon dioxide in the world. The rising levels of CO2 in the atmosphere and the global concern about the greenhouse effect and climate change have brought about considerable investigations on how to reduce the energy intensity and CO2 emissions of this industrial sector. In this thesis the problem is tackled by mathematical modeling and optimization using three different approaches. The possibility to use biomass in the integrated steel plant, particularly as an auxiliary reductant in the blast furnace, is investigated. By pre-processing the biomass its heating value and carbon content can be increased at the same time as the oxygen content is decreased. As the compression strength of the preprocessed biomass is lower than that of coke, it is not suitable for replacing a major part of the coke in the blast furnace burden. Therefore the biomass is assumed to be injected at the tuyere level of the blast furnace. Carbon capture and storage is, nowadays, mostly associated with power plants but it can also be used to reduce the CO2 emissions of an integrated steel plant. In the case of a blast furnace, the effect of CCS can be further increased by recycling the carbon dioxide stripped top gas back into the process. However, this affects the economy of the integrated steel plant, as the amount of top gases available, e.g., for power and heat production is decreased. High quality raw materials are a prerequisite for smooth blast furnace operation. High quality coal is especially needed to produce coke with sufficient properties to ensure proper gas permeability and smooth burden descent. Lower quality coals as well as natural gas, which some countries have in great volumes, can be utilized with various direct and smelting reduction processes. The DRI produced with a direct reduction process can be utilized as a feed material for blast furnace, basic oxygen furnace or electric arc furnace. The liquid hot metal from a smelting reduction process can in turn be used in basic oxygen furnace or electric arc furnace. The unit sizes and investment costs of an alternative ironmaking process are also lower than those of a blast furnace. In this study, the economy of an integrated steel plant is investigated by simulation and optimization. The studied system consists of linearly described unit processes from coke plant to steel making units, with a more detailed thermodynamical model of the blast furnace. The results from the blast furnace operation with biomass injection revealed the importance of proper pre-processing of the raw biomass as the composition of the biomass as well as the heating value and the yield are all affected by the pyrolysis temperature. As for recycling of CO2 stripped blast furnace top gas, substantial reductions in the emission rates are achieved if the stripped CO2 can be stored. However, the optimal recycling degree together with other operation conditions is heavily dependent on the cost structure of CO2 emissions and stripping/storage. The economical feasibility related to the use of DRI in the blast furnace depends on the price ratio between the DRI pellets and the BF pellets. The high amount of energy needed in the rotary hearth furnace to reduce the iron ore leads to increased CO2 emissions.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This thesis studies quality, productivity and economy in welding manufacturing in West African states such as Ghana, Nigeria and Cameroon. The study consists of two parts: the first part, which forms the theoretical background, reviews relevant literature concerning the metal and welding industries, and measurement of welding quality, productivity and economy. The second part, which is the empirical part, aims to identify activities in the metal manufacturing industries where welding is extensively used and to determine the extent of welding quality, productivity and economy measurements in companies operating in the metal manufacturing industries. Additionally, the thesis aims to identify challenges that companies face and to assess the feasibility of creating a network to address these issues. The research methods used in the empirical part are the case study (qualitative) method and the survey (quantitative) method. However, the case study method was used to elicit information from companies in Ghana, while the survey method was used to elicit information from companies in Nigeria and Cameroon. The study considers important areas that contribute to creating awareness and understanding of the current situation of the welding industry in West Africa. These areas include the metal manufacturing industrial sector, metal products manufactured, metal production and manufacturing systems deployed, welding quality, productivity and economy measurement systems utilized, equipment and materials on the markets, general challenges facing companies in welding operations, welding technology programs and research in local universities, and SWOT analysis of the various West African states. The notable findings indicate that majority of the companies operate in the constructionindustrial sector. Also, majority of the companies are project manufacturing oriented, thus provide services to customers operating in the growing industries such as the oil and gas, mining, food and the energy industry. In addition, only few companies are certified under standards such as ISO 9001, ISO 3834, and OHSAS 18001. More so, majority of the companies employ manual welding technique, and shielded metal arc welding (SMAW) as the commonly used welding process. Finally, welder salary is about € 300 / month as of June 2013 and the average operations turnover of medium to large companies is about € 5 million / year as at 2012. Based on analysis of the results of the study, it is noted that while welding activities are growing, the availability of cheap labor, the need for company and welder qualification and certification, and the need to manufacture innovative products through developmental projects (transfer of welding expertise and technology) remain as untapped opportunities in the welding industry in the West African states. The study serves as a solid platform for further research and concludes with several recommendations for development of the West African welding industry.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Viime vuosien aikana tapahtunut nikkelin hinnan nouseminen on vaikuttanut austeniittis-ferriittisten ruostumattomien terästen, ns. duplex -terästen kehittämiseen. Niukkaseosteisemmissa lean duplex -teräksissä seostetun nikkelin määrää on vähennetty ja sitä on korvattu typellä ja mangaanilla. Nämä muutokset ko. terästen seostuksessa aiheuttavat haasteita hitsaukselle, erityisesti austeniitti-ferriitti -suhteen säilyttämisessä, sekä sitä kautta iskusitkeyden ja korroosio-ominaisuuksien säilyttämiselle. Suurempi typen osuus myös lisää teräksen hitsisulan viskositeettia, mikä heikentää juuripalkojen hitsauksessa tunkeumaa. Tässsä diplomityössä on tutkittu keinoja helpottaa paksujen (yli 20 mm) lean duplex -teräslevyjen hitsausta käytännön näkökulmasta, sekä parantaa hitsattujen levyjen iskusitkeyttä. Hitsauskokeilla löydettiin hitsausta helpottavia menetelmiä ja kokeista saatiin karsimalla valikoitua hitsausarvot, joilla pystytään hitsaamaan painelaitedirektiivin mukaisesti hyväksyttäviä hitsejä lean duplex -laatuihin LDX2101 ja UR2202.