50 resultados para Joint Angular Velocity
Resumo:
The Iowa Department of Education collects information on joint enrollment in Iowa’s 15 community colleges. Jointly enrolled students are high school students enrolled in community college credit coursework. Most jointly enrolled students enroll through Senior Year Plus programs such as PSEO (Postsecondary Enrollment Options) and concurrent enrollment. Others enroll independently by paying tuition or enrolling in courses delivered through contractual agreements that do not meet the definition of concurrent enrollment. For more information about Senior Year Plus programs, please refer to the department’s website. This report consists of fiscal year and trend data on joint enrollment including headcount enrollment, credit hours, student demographics, and enrollment by program type and offering arrangement. All data included in this report is taken from the Community College Management Information System (MIS) and confirmed by each college, unless otherwise noted.
Resumo:
Audit report on the Iowa Water Pollution Control Works Financing Program and the Iowa Drinking Water Facilities Financing Program, joint programs of the Iowa Finance Authority and the Iowa Department of Natural Resources for the year ended June 30, 2012
Resumo:
This report summarizes joint enrollment in Iowa's community colleges. Jointly enrolled students are high school students enrolled in community college credit coursework. This report contains fiscal year data for the state's 15 community colleges reported through the Community College Management Information System (MIS) and confirmed by each college.
Resumo:
Longitudinal joint quality control/assurance is essential to the successful performance of asphalt pavements and it has received considerable amount of attention in recent years. The purpose of the study is to evaluate the level of compaction at the longitudinal joint and determine the effect of segregation on the longitudinal joint performance. Five paving projects with the use of traditional butt joint, infrared joint heater, edge restraint by milling and modified butt joint with the hot pinch longitudinal joint construction techniques were selected in this study. For each project, field density and permeability tests were made and cores from the pavement were obtained for in-lab permeability, air void and indirect tensile strength. Asphalt content and gradations were also obtained to determine the joint segregation. In general, this study finds that the minimum required joint density should be around 90.0% of the theoretical maximum density based on the AASHTO T166 method. The restrained-edge by milling and butt joint with the infrared heat treatment construction methods both create the joint density higher than this 90.0% limit. Traditional butt joint exhibits lower density and higher permeability than the criterion. In addition, all of the projects appear to have segregation at the longitudinal joint except for the edge-restraint by milling method.
Resumo:
Experiments with early entry light sawing of Portland cement concrete (PCC) contraction joints began in Iowa in 1989. Since that time, changes in early sawing equipment have occurred as well as changes in specifications for sawing. The option to use early sawing for transverse contraction joints was specified in 1992. A problem happening occasionally with early sawing was the break out of some of the concrete around the end of the joint as the saw blade approached the edge of the slab. To prevent this, it was proposed that the sawing would terminate approximately 1/2" to 3/4" before the edge of the slab, creating a "short joint". This procedure would also leave a concrete "dam" to prevent the run-out and waste of the hot liquid joint sealant onto the shoulder. It would also eliminate the need for the labor and material for applying a duct tape dam at the open ends of each sawed joint to stop hot liquid sealant run-out Agreements were made with the contractor to apply the "short joint" technique for 1 day of paving. The evaluation and results are compared with an adjoining control section. The research found no negative aspects from sawing the "short joint". Three specific findings were noted. They are the following: 1) No joint end "blow-out" spalls of concrete occurred. 2) The need for the duct tape dam to stop liquid sealant overflow was eliminated. 3) Joint end corner spalls appear to be caused mainly by construction shouldering operations equipment. The "short joint" sawing technique can be routinely applied to early entry sawed transverse contraction joints with expectations of only positive results.
Resumo:
Most pavement contraction joint seals in Iowa, in general, have been performing in less than a satisfactory manner. The effective life of the seals, in maintaining a watertight joint, has been only from two to five years. In search of improvements, research was proposed to evaluate preformed neoprene joint seals. The performance of those seals was to be compared mainly with the hot poured rubberized asphalt sealants and cold applied silicone sealants or other sealants commonly used at the time this research began. Joint designs and methods of sawing were also investigated. All evaluations were done in new portland cement concrete (PCC) pavements. Three projects were initially selected and each included a research section of joint sealing. Some additional sites were later added for evaluation. Several joint sealants were evaluated at each research site. The various sites included high, medium and low levels of traffic. Evaluations were done over a five-year period. Neoprene joint seals provided better performance than hot or cold field formed joints.
Resumo:
Audit report on the Iowa Water Pollution Control Works Financing Program and the Iowa Drinking Water Facilities Financing Program, joint programs of the Iowa Finance Authority and the Iowa Department of Natural Resources for the year ended June 30, 2013
Resumo:
Premature failure of concrete pavement contraction joint seals is an ongoing and costly problem for the Iowa Department of Transportation. Several joint seal test sections consisting of variations in sawing methods, joint cleaning techniques, sealant installation, and sealant types have been established over the past few years. Laboratory analysis and field inspections were done as a part of the tests, and core samples were taken for laboratory adhesion pull tests. Such methods often cover specifically small areas and may not expose hidden failures. Some tests are also labor-intensive and destructive, especially that of coring. An innovative, nondestructive, broad coverage joint seal tester that yields quick results has been designed and developed for evaluation of pavement joint seal performance. The Iowa vacuum joint seal tester (IA-VAC) applies a low vacuum above a joint seal that has been spray-covered with a foaming water solution. Any unsealed area or leak that exists along the joint will become quickly and clearly visible by the development of bubbles at the leak point. By analyzing the results from the IA-VAC tests, information on the number and types of leaks can be obtained; such information will help identify the source of the problem and direct efforts toward a solution.
Resumo:
The joint between two lanes of asphalt pavement is often the first area of a roadway which shows signs of deterioration and requires maintenance. As the final lift of hot asphalt is being placed in a construction project, it is being forced p against the adjoining lane of cold asphalt, forming the longitudinal joint. The mating of the two lanes, to form a high quality seal, is often not fully successful and later results in premature stripping or raveling as water enters the unsealed joint. The application of a hot poured rubberized asphaltic joint sealant along the joint face in the final stage of construction should help to form a watertight joint seal. A new product, especially formulated for the longitudinal joint in asphalt pavements was proposed to improve joint sealing. The following describes the experimental application of the new product, Crafco, PN 34524.
Resumo:
Over the years, the Iowa Department of Transportation has established an outstanding network of connector highways across the state of Iowa. Construction and paving of these primary roadways has essentially been completed. Unfortunately, many of these primary highway pavements are reaching their design life and are in need of rehabilitation. The emphasis, therefore, has shifted from the construction of new highways to the maintenance and rehabilitation of existing highways. The Iowa DOT in recent years has become more concerned with preventing the ingress of surface water into the pavement structure. Crack sealing is receiving greater emphasis. Specifications have been modified to require improved low modulus crack and joint sealing materials.
Resumo:
The objective of this research was to evaluate the performance of portland cement concrete pavement contraction joints utilizing a variety of sealants and joint preparations and to identify an effective sealant system. The variables evaluated were: (1) sealant material; (2) joint preparation; (3) size of saw cut (sealant reservoir); and (4) the use of backing material. This progress report contains project results to date.
Resumo:
Blowing and drifting of snow is a major concern for transportation efficiency and road safety in regions where their development is common. One common way to mitigate snow drift on roadways is to install plastic snow fences. Correct design of snow fences is critical for road safety and maintaining the roads open during winter in the US Midwest and other states affected by large snow events during the winter season and to maintain costs related to accumulation of snow on the roads and repair of roads to minimum levels. Of critical importance for road safety is the protection against snow drifting in regions with narrow rights of way, where standard fences cannot be deployed at the recommended distance from the road. Designing snow fences requires sound engineering judgment and a thorough evaluation of the potential for snow blowing and drifting at the construction site. The evaluation includes site-specific design parameters typically obtained with semi-empirical relations characterizing the local transport conditions. Among the critical parameters involved in fence design and assessment of their post-construction efficiency is the quantification of the snow accumulation at fence sites. The present study proposes a joint experimental and numerical approach to monitor snow deposits around snow fences, quantitatively estimate snow deposits in the field, asses the efficiency and improve the design of snow fences. Snow deposit profiles were mapped using GPS based real-time kinematic surveys (RTK) conducted at the monitored field site during and after snow storms. The monitored site allowed testing different snow fence designs under close to identical conditions over four winter seasons. The study also discusses the detailed monitoring system and analysis of weather forecast and meteorological conditions at the monitored sites. A main goal of the present study was to assess the performance of lightweight plastic snow fences with a lower porosity than the typical 50% porosity used in standard designs of such fences. The field data collected during the first winter was used to identify the best design for snow fences with a porosity of 50%. Flow fields obtained from numerical simulations showed that the fence design that worked the best during the first winter induced the formation of an elongated area of small velocity magnitude close to the ground. This information was used to identify other candidates for optimum design of fences with a lower porosity. Two of the designs with a fence porosity of 30% that were found to perform well based on results of numerical simulations were tested in the field during the second winter along with the best performing design for fences with a porosity of 50%. Field data showed that the length of the snow deposit away from the fence was reduced by about 30% for the two proposed lower-porosity (30%) fence designs compared to the best design identified for fences with a porosity of 50%. Moreover, one of the lower-porosity designs tested in the field showed no significant snow deposition within the bottom gap region beneath the fence. Thus, a major outcome of this study is to recommend using plastic snow fences with a porosity of 30%. It is expected that this lower-porosity design will continue to work well for even more severe snow events or for successive snow events occurring during the same winter. The approach advocated in the present study allowed making general recommendations for optimizing the design of lower-porosity plastic snow fences. This approach can be extended to improve the design of other types of snow fences. Some preliminary work for living snow fences is also discussed. Another major contribution of this study is to propose, develop protocols and test a novel technique based on close range photogrammetry (CRP) to quantify the snow deposits trapped snow fences. As image data can be acquired continuously, the time evolution of the volume of snow retained by a snow fence during a storm or during a whole winter season can, in principle, be obtained. Moreover, CRP is a non-intrusive method that eliminates the need to perform man-made measurements during the storms, which are difficult and sometimes dangerous to perform. Presently, there is lots of empiricism in the design of snow fences due to lack of data on fence storage capacity on how snow deposits change with the fence design and snow storm characteristics and in the estimation of the main parameters used by the state DOTs to design snow fences at a given site. The availability of such information from CRP measurements should provide critical data for the evaluation of the performance of a certain snow fence design that is tested by the IDOT. As part of the present study, the novel CRP method is tested at several sites. The present study also discusses some attempts and preliminary work to determine the snow relocation coefficient which is one of the main variables that has to be estimated by IDOT engineers when using the standard snow fence design software (Snow Drift Profiler, Tabler, 2006). Our analysis showed that standard empirical formulas did not produce reasonable values when applied at the Iowa test sites monitored as part of the present study and that simple methods to estimate this variable are not reliable. The present study makes recommendations for the development of a new methodology based on Large Scale Particle Image Velocimetry that can directly measure the snow drift fluxes and the amount of snow relocated by the fence.
Resumo:
Audit report on the Iowa Water Pollution Control Works Financing Program and the Iowa Drinking Water Facilities Financing Program, joint programs of the Iowa Finance Authority and the Iowa Department of Natural Resources, for the year ended June 30, 2014
Resumo:
Iowa's first portland cement concrete pavement was constructed in 1904 in the City of LeMars. A portion of that pavement served traffic until 1974 at which time it was resurfaced. The first rural Iowa pee pavement (16' wide, 6" to 7" thick) was constructed under the direction of the Iowa State Highway Commission in 1913. Some of Iowa's early pavements had transverse joints at 25-foot spacings. At that time, joint spacings across the nation ranged from 24 to 100 ft. There have been many changes in joint design over the years with some pavements being constructed without transverse joints. Joint spacing on Iowa primary pavements has generally remained around 20 feet with this spacing having been adopted as an Iowa standard in 1954. Until 1978 it was common to specify a 40-foot joint spacing on secondary pavements. The performance of the pavements with joint spacings greater than 20 feet, and in some cases no contraction joints, generated a 1955 research project on joint spacing. This project was 16 miles long containing sections without contraction joints and sections with joints sawed at intervals of 20, 50 and 80 feet. Approximately half of the sawed joints were left unsealed. The results of this research supported the 20-foot spacing, but were inconclusive regarding the benefits of sealing. One of the desired characteristics of joint sealing material is that it should act as a moisture barrier and prevent the intrusion of surface water. It was generally accepted from past experience that the hot poured type joint seals did not provide this effective moisture barrier.
Resumo:
Concern about premature joint sealant failures occurring in portland cement concrete (PCC) pavements gave impetus to initiating this research project. Eight sealants, including three silicone sealants, were evaluated and tested in the lab as well as incorporated in approximately 700 joints in the field and evaluated over a six-year period. The preliminary data show that among the silicone sealants, Dow Corning 888 rated the highest. However, this was rated third overall behind the W. R. Meadows cold-applied Sof Seal and Crafco #231 hot pour sealants. The W. R. Meadows and Crafco sealants cost approximately 30 percent and 50 percent less to furnish and place than the Dow Corning product. All joint sealants will continue to be evaluated.