557 resultados para SIO2-FILMS
Resumo:
The effect of Mg doping in ZnO is investigated through structural, electrical, and optical properties. Zn1−xMgxO (0<×<0.3) thin films were deposited on Si (100) and corning glass substrates using multimagnetron sputtering. Investigations on the structural properties of the films revealed that the increase in Mg concentration resulted in phase evolution from hexagonal to cubic phase. The temperature dependent study of dielectric constant at different frequencies exhibited a dielectric anomaly at 110 °C. The Zn0.7Mg0.3O thin films exhibited a well-defined polarization hysteresis loop with a remnant polarization of 0.2 μC/cm2 and coercive field of 8 kV/cm at room temperature. An increase in the band gap with an increase in Mg content was observed in the range of 3.3–3.8 eV for x = 0–0.3. The average transmittance of the films was higher than 90% in the wavelength region λ = 400–900 nm.
Resumo:
We present a systematic study to explore the effect of important process variables on the composition and structure of niobium nitride thin films synthesized by Reactive Pulsed Laser Deposition (RPLD) technique through ablation of high purity niobium target in the presence of low pressure nitrogen gas. Secondary Ion Mass Spectrometry has been used in a unique way to study and fix gas pressure, substrate temperature and laser fluence, in order to obtain optimized conditions for one variable in single experimental run. The x-ray diffraction and electron microscopic characterization have been complemented by proton elastic backscattering spectroscopy and x-ray photoelectron spectroscopy to understand the incorporation of oxygen and associated non-stoichiometry in the metal to nitrogen ratio. The present study demonstrates that RPLD can be used for obtaining thin film architectures using non-equilibrium processing. Finally the optimized NbN thin films were characterized for their hardness using nano-indentation technique and found to be similar to 30 GPa at the deposition pressure of 8 Pa. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The effect of deposition temperature on residual stress evolution with temperature in Ti-rich NiTi films deposited on silicon substrates was studied. Ti-rich NiTi films were deposited on 3? Si (100) substrates by DC magnetron sputtering at three deposition temperatures (300, 350 and 400 degrees C) with subsequent annealing in vacuum at their respective deposition temperatures for 4 h. The initial value of residual stress was found to be the highest for the film deposited and annealed at 400 degrees C and the lowest for the film deposited and annealed at 300 degrees C. All the three films were found to be amorphous in the as-deposited and annealed conditions. The nature of the stress response with temperature on heating in the first cycle (room temperature to 450 degrees C) was similar for all three films although the spike in tensile stress, which occurs at similar to 330 degrees C, was significantly higher in the film deposited and annealed at 300 degrees C. All the films were also found to undergo partial crystallisation on heating up to 450 degrees C and this resulted in decrease in the stress values around 5560 degrees C in the cooling cycle. The stress response with temperature in the second thermal cycle (room temperature to 450 degrees C and back), which is reflective of the intrinsic film behaviour, was found to be similar in all cases and the elastic modulus determined from the stress response was also more or less identical. The three deposition temperatures were also not found to have a significant effect on the transformation characteristics of these films such as transformation start and finish temperatures, recovery stress and hysteresis.
Resumo:
The compositional evolution in sputter deposited LiCoO2 thin films is influenced by process parameters involved during deposition. The electrochemical performance of these films strongly depends on their microstructure, preferential orientation and stoichiometry. The transport process of sputtered Li and Co atoms from the LiCoO2 target to the substrate, through Ar plasma in a planar magnetron configuration, was investigated based on the Monte Carlo technique. The effect of sputtering gas pressure and the substrate-target distance (dst) on Li/Co ratio, as well as, energy and angular distribution of sputtered atoms on the substrate were examined. Stable Li/Co ratios have been obtained at 5 Pa pressure and dst in the range 5−11 cm. The kinetic energy and incident angular distribution of Li and Co atoms reaching the substrate have been found to be dependent on sputtering pressure. Simulations were extended to predict compositional variations in films prepared at various process conditions. These results were compared with the composition of films determined experimentally using x-ray photoelectron spectroscopy (XPS). Li/Co ratio calculated using XPS was in moderate agreement with that of the simulated value. The measured film thickness followed the same trend as predicted by simulation. These studies are shown to be useful in understanding the complexities in multicomponent sputtering.
Resumo:
Optical parameters of chalcogenide glass multilayers with 12–15 nm modulation lengths prepared by thermal evaporation can be changed by laser irradiation. Photoluminescence (PL) studies were carried out on such nonirradiated and irradiated multilayered samples of a-Se/As2S3 (sublayer thickness of a-Se is 4–5 nm for one set of samples and 1–2 nm for the other set. However As2S3 sublayer thickness is 11–12 nm for both sets of samples.) PL intensity can be increased by several orders of magnitude by reducing the Se well layer (lower band gap) thickness and can be further increased by irradiating the samples with appropriate wavelengths in the range of the absorption edge. The broadening of luminescence bands takes place either with a decrease in Se layer thickness or with irradiation. The former is due to the change in interface roughness and defects because of the enhanced structural disorder while the latter is due to photoinduced interdiffusion. The photoinduced interdiffusion creates defects at the interface between Se and As2S3 by forming an As–Se–S solid solution. From the deconvoluted PL spectrum, it is shown that the peak PL intensity, full width half maximum, and the PL quantum efficiency of particular defects giving rise to PL, can be tuned by changing the sublayer thickness or by interdiffusion.
Resumo:
Novel ferroelectric bismuth vanadate, Bi2VO5.5 (BVO), thin films have been grown between lattice matched metallic LaNiO3 (LNO) layers deposited on SrTiO3 (STO) by the pulsed laser deposition technique. LNO/BVO/LNO/STO and Au/BVO/LNO/STO trilayer structures exhibited c‐oriented (001) growth of BVO. LNO has been found to be a good metallic electrode with sheet resistance ∼20 Ω in addition to aiding c‐axis oriented BVO growth. The dielectric constant, ϵr of LNO/BVO/LNO/STO, at 300 K was about 12. However, when an Au electrode was used on top of BVO/LNO/STO film, it showed a significant improvement in the dielectric constant (ϵr=123). The ferroelectric properties of BVO thin films have been confirmed by hysteresis behavior with a remnant polarization, Pr=4.6×10−8 C/cm2 and coercive field, Ec=23 kV/cm at 300 K.
Resumo:
Substrate temperature and ion bombardment during deposition have been observed to modify significantly the optical and structural properties of dielectric thin films. Single‐layer films of CeO2 have been deposited by electron beam evaporation with simultaneous oxygen‐ion bombardment using a Kaufman broad beam ion source and maintaining the substrates at elevated temperature. A systematic study has been made on the influence of (a) substrate temperature in the range ambient to 300 °C, (b) ion energy in the range 300–700 eV, and (c) ion current density 100–220 μA/cm2 on optical properties such as refractive index, extinction coefficient, inhomogeneity, packing density, and structural properties. The refractive index increased with in increase in substrate temperature: ion energy up to 600 eV and ion current density. Homogeneous, absorption free and high index (2.48) films have been obtained at 600 eV, 220 μA/cm2 and at substrate temperature of 300 °C. The packing density of the films was observed to be unity for the same deposition conditions. Substrate temperature with simultaneous ion bombardment modified the structure of the films from highly ordered to fine grain structure.
Resumo:
Ferroelectric superlattice structures consisting of alternating layers of BaTiO3 and SrTiO3 with variable interlayer thickness were grown on Pt (111)/TiO2/SiO2/Si (100) substrates by pulsed laser deposition. The presence of superlattice reflections in the x-ray diffraction pattern clearly showed the superlattice behavior of the fabricated structures over a range of 6.4–20 nm individual layer thicknesses. Depth profile conducted by secondary ion mass spectrometry analysis showed a periodic concentration of Ba and Sr throughout the film. Polarization hysteresis and the capacitance-voltage characteristics of these films show clear size dependent ferroelectric characteristics. The spontaneous (Ps) and remnant (Pr) polarizations increase gradually with decreasing periodicity, reach a maximum at a finite thickness and then decrease. The competition between the size effect and long-range ferroelectric interaction is suggested as a possible reason for this phenomenon. The temperature dependence of Ps and Pr shows a single ferroelectric phase transition, and the Curie temperature is estimated to be about 316 K. The curve shows that the ferroelectric superlattice tends to form an artificial material, responding as a single structure with an averaged behavior of both the parent systems.
Resumo:
Structural and electrical properties of Eu2O3 films grown on Si(100) in 500–600 °C temperature range by low pressure metalorganic chemical vapor deposition are reported. As-grown films also possess the impurity Eu1−xO phase, which has been removed upon annealing in O2 ambient. Film’s morphology comprises uniform spherical mounds (40–60 nm). Electrical properties of the films, as examined by capacitance-voltage measurements, exhibit fixed oxide charges in the range of −1.5×1011 to −6.0×1010 cm−2 and dielectric constant in the range of 8–23. Annealing has resulted in drastic improvement of their electrical properties. Effect of oxygen nonstoichiometry on the film’s property is briefly discussed.
Resumo:
Barium zirconium titanate [Ba(Zr0.05Ti0.95)O3, BZT] thin films were prepared by pulsed laser ablation technique and dc leakage current conduction behavior was extensively studied. The dc leakage behavior study is essential, as it leads to degradation of the data storage devices. The current-voltage (I-V) of the thin films showed an Ohmic behavior for the electric field strength lower than 7.5 MV/m. Nonlinearity in the current density-voltage (J-V) behavior has been observed at an electric field above 7.5 MV/m. Different conduction mechanisms have been thought to be responsible for the overall I-V characteristics of BZT thin films. The J-V behavior of BZT thin films was found to follow Lampert’s theory of space charge limited conduction similar to what is observed in an insulator with charge trapping moiety. The Ohmic and trap filled limited regions have been explicitly observed in the J-V curves, where the saturation prevailed after a voltage of 6.5 V referring the onset of a trap-free square region. Two different activation energy values of 1.155 and 0.325 eV corresponding to two different regions have been observed in the Arrhenius plot, which was attributed to two different types of trap levels present in the film, namely, deep and shallow traps.
Resumo:
The composition, structural, electrical, and optical properties of as-grown and heat treated tin-mono-sulfide (SnS) ultra-thin films have been studied. The ultra-thin SnS films were prepared on glass substrates by thermal resistive evaporation technique. All the SnS films contained nanocrystallites and exhibited p-type conductivity with a low Hall-mobility, <50 cm(2)/Vs. All these films are highly tin rich in nature and exhibited orthorhombic crystal structure. As compared to other films, the SnS films annealed at 300 degrees C showed a low electrical resistivity of similar to 36 Omega cm with an optical band gap of similar to 1.98 eV. The observed electrical and optical properties of all the films are discussed based on their composition and structural parameters. These nanocrystalline ultra-thin SnS films could be expected as a buffer layer for the development of tandem solar cell devices due to their low-resistivity and high absorbability with an optimum band gap. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Thin films of Ti62.5Si37.5 composition were deposited by the pulsed-laser ablation technique on single-crystal Nad substrates at room temperature and on ′single-crystal′ superalloy substrates at elevated temperatures. Both vapour and liquid droplets generated by pulsed-laser ablation of the target become quenched on the substrate. Amorphization had taken place in the process of quenching of vapour-plasma as well as small liquid droplets on NaCl substrates at room temperature. In addition to the formation of Ti5Si3, a metastable fcc phase (a 0 = 0.433 nm) also forms in micron-sized large droplets as well as in the medium-sized submicron droplets. The same metastable fcc phase nucleates during deposition from the vapour state at 500°C and at 600°C on a superalloy substrate as well as during crystallization of the amorphous phase. The evolution of the metastable fcc phase in the Ti-Si system during non-equilibrium processing is reported for the first time.
Resumo:
The gamma-phase poly (vinylidene fluoride) (PVDF) films are usually prepared using dimethyl sulfoxide (DMSO) solvent, regardless of preparation temperature. Here we report the crystallization of both alpha and gamma-phase PVDF films by varying preparation temperature using DMSO solvent. The gamma-phase PVDF films were annealed at 70, 90, 110, 130 and 160 degrees C for five hours. The changes in the phase contents in the PVDF at different annealing conditions have been described. When thin films were annealed at 90 degrees C for 5 h, maximum percentage of beta-phase appears in PVDF thin films. The gamma-phase PVDF films completely converted to alpha-phase when they were annealed at 160 degrees C for 5 h. From X-ray diffraction (XRD), Fourier transform infrared spectrum (FTIR), differential scanning calorimetry (DSC) and Raman studies, it is confirmed that the PVDF thin films, cast from solution and annealed at 90 degrees C for 5 h, have maximum percentage of beta-phase. The beta-phase PVDF shows a remnant polarization of 4.9 mu C/cm(2) at 1400 kV/cm at 1 Hz.
Resumo:
Abstract | A growing interest in the research of chalcogenide glasses can be currently witnessed, which to a large extent is caused by newly opened fields of applications for these materials. Applications in the field of micro- and opto-electronics, xerography and lithography, acousto-optic and memory switching devices and detectors for medical imaging seem to be most remarkable. Accordingly, photo induced phenomena in chalcogenide glasses are attracting much interest. These phenomena can be found both in uniform thin films as well as multilayered films. Among amorphous multilayers, chalcogenide multilayers are attractive because of the potential it has for tailoring the optical properties. I will be presenting some basic idea of photoinduced effects followed by the diffusion mechanisms of Se, Sb and Bi in to As2S3 films.
Resumo:
Amorphous silicon carbide (a-Si(1-x)C(x)) films were deposited on silicon (100) and quartz substrates by pulsed DC reactive magnetron sputtering of silicon in methane (CH(4))-Argon (Ar) atmosphere. The influence of substrate temperature and target power on the composition, carbon bonding configuration, band gap, refractive index and hardness of a-SiC films has been investigated. Increase in substrate temperature results in slightly decreasing the carbon concentration in the films but favors silicon-carbon (Si-C) bonding. Also lower target powers were favorable towards Si-C bonding. X-ray photoelectron spectroscopy (XPS) results agree with the Fourier Transform Infrared (FTIR), UV-vis spectroscopy results. Increase in substrate temperature resulted in increased hardness of the thin films from 13 to 17 GPa and the corresponding bandgap varied from 2.1 to 1.8 eV. (C) 2011 Elsevier B.V. All rights reserved.