Resumo:
This paper deals with the use of Stem theory as applied to a clay-water electrolyte system, which is more realistic to understand the force system at micro level man the Gouy-Chapman theory. The influence of the Stern layer on potential-distance relationship has been presented quantitatively for certain specified clay-water systems and the results are compared with the Gouy-Chapman model. A detailed parametric study concerning the number of adsorption spots on the clay platelet, the thickness of the Stern layer, specific adsorption potential and the value of dielectric constant of the pore fluid in the Stern layer, was carried out. This study investigates that the potential obtained at any distance using the Stern theory is higher than that obtained by the Gouy-Chapman theory. The hydrated size of the ion is found to have a significant influence on the potential-distance relationship for a given clay, pore fluid characteristics and valence of the exchangeable ion.
Resumo:
Glass composites of strontium tetraborate, SrB4O7 (SBO) with bismuth vanadate, Bi2VO5.5 (BiV) of the composition (1-x) SBO-x BN (0 less than or equal to x less than or equal to 0.75), have been synthesized. X-ray powder diffraction and electron microscopy indicate as-quenched composites to be amorphous and the annealed samples showed the presence of nanometer sized particles of BN dispersed in the glassy matrix of SBO. The dielectric constant of these composites increases with increase in the volume fraction of BiV, at 300 K. The measured dielectric constant of the composite very nearly obeys the Maxwell's relationship. Optical transmission studies confirm a steady shirt in the optical absorption edge towards longer wavelengths with increase in x
Resumo:
Lead Zirconate (PbZrO3) thin films were deposited by pulsed laser ablation method. Pseudocubic (110) oriented in-situ films were grown at low pressure. The field enforced anti-ferroelectric (AFE) to ferroelectric (FE) phase transformation behaviour was investigated by means of a modified Sawyer Tower circuit as well as capacitance versus applied voltage measurements. The maximum polarisation obtained was 36 mu C cm(-2) and the critical field to induce ferroelectric state and to reverse the antiferroelectric slates were 65 and 90 kV cm(-1) respectively. The dielectric properties were investigated as a function of frequency and temperature. The dielectric constant of the AFE lead zirconate thin him was 190 at 100 kHz which is more than the bulk ceramic value (120) with a dissipation factor of less than 0.07. The polarisation switching kinetics of the antiferroelectric PbZrO3 thin films showed that the switching time to be around 275 ns between antipolar state to polar states. (C) 1999 Elsevier Science S.A. All rights reserved.
Electrical characterization of Ba(Zr0.1Ti0.9)O-3 thin films grown by pulsed laser ablation technique
Resumo:
In situ annealed thin films of ferroelectric Ba(Zr0.1Ti0.9)O-3 were deposited on platinum substrates by pulsed laser ablation technique. The as grown films were polycrystalline in nature without the evidence of any secondary phases. The polarization hysteresis loop confirmed the ferroelectricity, which was also cross-checked with the capacitance-voltage characteristics. The remnant polarization was about 5.9 muC cm(-2) at room temperature and the coercive field was 45 kV. There was a slight asymmetry in the hysteresis for different polarities, which was thought to be due to the work function differences of different electrodes. The dielectric constant was about 452 and was found to exhibit low frequency dispersion that increased with frequency, This was related to the space-charge polarization. The complex impedance was plotted and this exhibited a semicircular trace, and indicated an equivalent parallel R - C circuit within the sample. This was attributed to the grain response. The DC leakage current-voltage plot was consistent with the space-charge limited conduction theory, but showed some deviation, which was explained by assuming a Poole-Frenkel type conduction to be superimposed on to the usual space-charge controlled current. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
The reversible and irreversible components of the total polarization in a thin film of SrBi2(Ta-0.5,Nb-0.5)(2)O-9 were calculated. The C-V loop was integrated to obtain the reversible part of the total polarization. The reversible polarization was only 20% of the total polarization and showed almost no hysteresis. However, the dielectric constant due to the total polarization was almost the same as that for the reversible polarization in the saturation region of the large signal P-E hysteresis loop. The reversible part was subtracted from the total polarization to calculate the irreversible counterpart of it. The irreversible polarization showed a near-square shaped hysteresis loop, while the reversible polarization was obeying the Rayleigh law. The small signal hysteresis was simulated from the parameters obtained from the Rayleigh-curve fit with the experimental curve and then it was compared with the result obtained from direct measurement with small amplitude. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Relaxor properties of polycrystalline 0.7Pb(Mg1/3Nb2/3)O-3-0.3PbTiO(3) (PMN-PT) thin films were studied in terms of the diffuse nature of phase transition along with the frequency dispersion of temperature (T-m) at which the dielectric constant exhibits maximum value. Existence of remnant polarization (P-r) above the phase transition temperature, which is a characteristic property of typical relaxor ferroelectric has also been observed in the present case. The films exhibited a gradual decrease of remnant polarization with increase of temperature. Among the different models of relaxor ferroelectric, Vogel-Fulcher model has been found to be suitable to describe the frequency dispersion of T-m in this case. Freezing of dipole moment with decrease of temperature was thought to be the origin of the temperature dependence of dielectric dispersion.
Resumo:
Single crystals of a recent ferroelectric material, glycine phosphite were grown from aqueous solution employing the techniques of slow cooling and controlled evaporation. Powder X-ray diffraction studies as well as thermal analysis were carried out on the grown crystals. The morphology of the crystal has been determined using contact and optical goniometry. The mechanical hardness of the crystal was evaluated by Vickers indentation method. Thickness dependence of the dielectric properties has been investigated and the results can be interpreted in terms of a surface layer of lower dielectric constant.
Resumo:
Zinc oxide (ZnO) thin films have been prepared on silicon substrates by sol-gel spin coating technique with spinning speed of 3,000 rpm. The films were annealed at different temperatures from 200 to 500 A degrees C and found that ZnO films exhibit different nanostructures at different annealing temperatures. The X-ray diffraction (XRD) results showed that the ZnO films convert from amorphous to polycrystalline phase after annealing at 400 A degrees C. The metal oxide semiconductor (MOS) capacitors were fabricated using ZnO films deposited on pre-cleaned silicon (100) substrates and electrical properties such as current versus voltage (I-V) and capacitance versus voltage (C-V) characteristics were studied. The electrical resistivity decreased with increasing annealing temperature. The oxide capacitance was measured at different annealing temperatures and different signal frequencies. The dielectric constant and the loss factor (tan delta) were increased with increase of annealing temperature.
Resumo:
This article presents the analysis of ultra wide band (UWB) filler designed using a symmetrical three parallel coupled line resonator in low temperature co-fired ceramic (LTCC) medium: The ground plane with an aperture incorporated in it improves the coupling. Based on circuit models, the designed UWB filter has been analyzed, and the results have been confirmed by experiments. The filter has been realized with Dupont LTCC tape DuPont 951 (that has dielectric constant of 7.8). Maximum insertion loss of the experimental filter is 1.5 dB. The group variation over the pass band of the filter is within 0.2 us. Dimensions of the experimental LTCC filter are 20 x 10 x 0.72 mm. (C) 2011 Wiley Periodicals, Inc. Microwave Opt Technol Lett 53:2580-2583,2011; View this article online at wileyonlinelibrary.com. DOI 10.1002/mop.26311
Resumo:
Performance improvement of a micromachined patch antenna operating at 30 GHz with a capacitively coupled feed arrangement is presented here. Such antennas are useful for monolithic integration with active components. Specifically, micromachining can be employed to achieve a low dielectric constant region under the patch which causes (i) the suppression of surface waves and hence the increase in radiation efficiency and (ii) increase in the bandwidth. The performance of such a patch antenna can be significantly improved by selecting a coupled feed arrangement. We have optimized the dimensions and location of the capacitive feeding strip to get the maximum improvement in bandwidth. Since this is a totally planar arrangement, and does not involve any stacked structures, this antenna is easy to fabricate using standard microfabrication techniques. The antenna element thus designed has a -10 dB bandwidth of 1600 MHz
Resumo:
Bi-layered Aurivillius compounds prove to be efficient candidates of nonvolatile memories. SrBi2Nb2O9 thin films were deposited by excimer laser ablation at low substrate temperature (400 °C) followed by an ex situ annealing at 750 °C. The polarization hysteresis behavior was confirmed by variation of polarization with the external applied electric field and also verified with capacitance versus voltage characteristics. The measured values of spontaneous and remnant polarizations were, respectively, 9 and 6 μC/cm2 with a coercive field of 90 kV/cm. The measured dielectric constant and dissipation factors at 100 kHz were 220 and 0.02, respectively. The frequency analysis of dielectric and ac conduction properties showed a distribution of relaxation times due to the presence of multiple grain boundaries in the films. The values of activation energies from the dissipation factor and grain interior resistance were found to be 0.9 and 1.3 eV, respectively. The deviation in these values was attributed to the energetic conditions of the grain boundaries and bulk grains. The macroscopic relaxation phenomenon is controlled by the higher resistive component in a film, such as grain boundaries at lower temperatures, which was highlighted in the present article in close relation to interior grain relaxation and conduction properties.
Resumo:
Polycrystalline films of SrBi2Nb2O9 were grown using pulsed-laser ablation. The ferroelectric properties were achieved by low-temperature deposition followed by a subsequent annealing process. The lower switching voltage was obtained by lowering the thickness, which did not affect the insulating nature of the films. The hysteresis results showed an excellent square-shaped loop with results (Pr = 6 μC/cm2, Ec = 100 kV/cm) in good agreement with earlier reports. The films also exhibited a dielectric constant of 250 and a dissipation factor of 0.02. The transport studies indicated an ohmic behavior, while higher voltages induced a bulk space charge.
Resumo:
The effect of Mg doping in ZnO is investigated through structural, electrical, and optical properties. Zn1−xMgxO (0<×<0.3) thin films were deposited on Si (100) and corning glass substrates using multimagnetron sputtering. Investigations on the structural properties of the films revealed that the increase in Mg concentration resulted in phase evolution from hexagonal to cubic phase. The temperature dependent study of dielectric constant at different frequencies exhibited a dielectric anomaly at 110 °C. The Zn0.7Mg0.3O thin films exhibited a well-defined polarization hysteresis loop with a remnant polarization of 0.2 μC/cm2 and coercive field of 8 kV/cm at room temperature. An increase in the band gap with an increase in Mg content was observed in the range of 3.3–3.8 eV for x = 0–0.3. The average transmittance of the films was higher than 90% in the wavelength region λ = 400–900 nm.
Resumo:
Novel ferroelectric bismuth vanadate, Bi2VO5.5 (BVO), thin films have been grown between lattice matched metallic LaNiO3 (LNO) layers deposited on SrTiO3 (STO) by the pulsed laser deposition technique. LNO/BVO/LNO/STO and Au/BVO/LNO/STO trilayer structures exhibited c‐oriented (001) growth of BVO. LNO has been found to be a good metallic electrode with sheet resistance ∼20 Ω in addition to aiding c‐axis oriented BVO growth. The dielectric constant, ϵr of LNO/BVO/LNO/STO, at 300 K was about 12. However, when an Au electrode was used on top of BVO/LNO/STO film, it showed a significant improvement in the dielectric constant (ϵr=123). The ferroelectric properties of BVO thin films have been confirmed by hysteresis behavior with a remnant polarization, Pr=4.6×10−8 C/cm2 and coercive field, Ec=23 kV/cm at 300 K.
Resumo:
Structural and electrical properties of Eu2O3 films grown on Si(100) in 500–600 °C temperature range by low pressure metalorganic chemical vapor deposition are reported. As-grown films also possess the impurity Eu1−xO phase, which has been removed upon annealing in O2 ambient. Film’s morphology comprises uniform spherical mounds (40–60 nm). Electrical properties of the films, as examined by capacitance-voltage measurements, exhibit fixed oxide charges in the range of −1.5×1011 to −6.0×1010 cm−2 and dielectric constant in the range of 8–23. Annealing has resulted in drastic improvement of their electrical properties. Effect of oxygen nonstoichiometry on the film’s property is briefly discussed.