Resumo:

温度梯度法(TGT)生长的Al2O3晶体因石墨发热体在高温时的挥发和原料中过渡性金属离子的存在,晶体在不同部位呈现不同颜色,一般上部为浅红色,尾部为浅黄绿色,将TGT法生长的Al2O3晶体(Ф110×80mm^3)依次经过高温氧化气氛、高温还原气氛脱碳、去色退火实验,即“两步法”退火实验,晶体变成无色、透明,经测试,Al2O3晶体的完整性、光学透过率和光学均匀性均有显著提高。

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Sapphire crystals, 140 mm in diameter and 90 turn in height, have been grown by temperature gradient techniques (TGT). The growth direction of the boule was fixed by means of Lane X-ray diffraction. A prominent 204 nm absorption band in TGT-Al2O3. which does not appear in single crystals grown by Czochralski method has been studied. Analysis further substantiates the F-center model of this band. Two relatively weaker bands absorbing at 232 nm and 254 nm were ascribed to F+ centers. F-type centers concentration was determined using Smakula's equation. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A 120TW/36fs laser system based on Ti:sapphire chirped-pulse amplification (CPA) has been successfully established in our lab. The final four pass Ti:sapphire amplifier pumped by an energetic single-shot Nd:YAG-Nd:glass laser was designed and optimized. With 24J/8ns pump energy at 532 nm, 300 mJ/220 ps chirped pulse was amplified to 5.98 J in this amplifier, and a total saturated gain of similar to 20 was achieved. The focused intensity of compressed beam could reach to 10(20) W/cm(2) with the M-2 of similar to 2.0. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conical emission is investigated for Ti:sapphire femtosecond laser pulses propagating in water. The colored rings can be observed in the forward direction due to the constructive and destructive interference of transverse wavevector, which are induced by the spatio-temporal gradient of the free-electron density. With increasing input laser energy, due to filamentation and pulse splitting induced by the plasma created by multiphoton excitation of electrons from the valence band to the conduction band, the on-axis spectrum of the conical emission is widely broadened and strongly modulated with respect to input laser spectrum, and finally remains fairly constant at higher laser energy due to intensity clamping in the filaments.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have developed a two-stage Ti:sapphire amplifier system which can produce 17-TW/23-fs pulses at a repetition rate 10 MHz. A birefringent plate is used in the regenerative amplifier to alleviate gain narrowing, while an all-reflective cylindrical-mirror-based pulse stretcher and an acousto-optic programmable dispersive filter (AOPDF) are used to compensate for the higher order dispersion of the system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

New parasitic lasing suppression techniques are developed and high gain amplification is demonstrated in a petawatt level Ti:sapphire amplifier based on the chirped pulse amplification (CPA) scheme. Cladding the large aperture Ti: sapphire with refractive-index matched liquid doped with absorber suppresses the transverse lasing. The acousto-optic programmable dispersive filter (AOPDF) is used to realize side-lobe suppression in the temporal profile of the compressed pulse. The 800 nm laser output with peak power of 0.89 PW and pulse width of 29.0 fs is demonstrated. (c) 2007 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The interference patterns produced by Gaussian-shaped broad-bandwidth femtosecond pulsed laser sources are derived. The interference pattern contains both spatial and temporal properties of laser beam. Interference intensity dependent on the bandwidth of femtosecond laser are given. We demonstrate experimentally both the spatial and the temporal coherence properties of a Ti:sapphire femtosecond pulse laser, as well as its power spectrum by using a pinhole pair.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Porous SiO2 antireflective (AR) coatings are prepared from the colloidal silica solution modified with methyltriethoxysilane (MTES) based on the sol-gel route. The viscosity of modified silica suspensions changes but their stability keeps when MTES is introduced. The refractive indices of modified coatings vary little after bake treatment from 100 to 150 Celsius. The modified silica coatings on Ti:sapphire crystal, owning good homogeneity, display prominent antireflective effect within the laser output waveband (750-850 nm) of Ti:sapphire lasers, with average transmission above 98.6%, and own laser induced damage thresholds (LIDTs) of more than 2.2 J/cm2 at 800 nm with the pulse duration of 300 ps.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this letter, we present an all solid-state, injection-seeded Ti:sapphire laser. The laser is pumped by a laser diode pumped frequency-doubled Nd:YAG laser, and injection-seeded by an external cavity laser diode with the wavelength between 770 and 780 nm. The single longitude mode and the doubling efficiency of the laser are obtained after injection seeding. The experimental setup and relative results are reported. It is a good candidate laser source for mobile differential absorption lidar (DIAL) system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By employing a continuous-wave (CW) Ti:sapphire tunable laser as a pumping source and a Cr4+:YAG single crystal as the saturable absorber (SA), a passively Q-switched Nd:YAG ceramic laser has been demonstrated at room temperature. With an absorbed pumping power of 541 mW at 808 nm, an average output power of 61 mW at 1064 nm has been obtained with 3.5 mu J pulse energy, 15 ns pulse width and 18.18 kHz repetition rate, and the corresponding slope-efficiency is 15%. The relationships between the pulse width, repetition rate, average output power, pulse energy, and peak power on the absorbed pumping power for different initial transmission of the Cr4+:YAG SA are discussed separately. The Nd:YAG ceramic is one of the most promising laser materials for compact, efficient, all-solid-state pulsed lasers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High-quality 2at%-doped Yb:CaF2 and Yb,Na:CaF2 single crystals with diameter of 76mm were grown by the temperature gradient technique. For the first time, distribution coefficients (KO) of Yb in the two crystals were determined to be 1.07 and 0.91, respectively, by measuring the Yb concentrations at the growth starting position in the as-grown boules. Absorption and emission spectra of the two different crystals were measured at room temperature. Experimental results show that Na+ ions codoping with Yb3+ as charge compensators make Yb3+ ions in CaF2 lattice to be a quasi-single-center system, and greatly suppress the deoxidization of Yb3+ to Yb2+ (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The annealing effects of sapphire substrate on the quality of epitaxial ZnO films grown by metalorganic chemical vapor deposition (MOCVD) were studied. The atomic steps formed on (0 0 0 1) sapphire (alpha-Al2O3) substrate surface by annealing at high temperature was analyzed by atomic force microscopy (AFM). The annealing effects of sapphire substrate on the ZnO films were examined by X-ray diffraction (XRD), AFM and photoluminescence (PL) measurements. Experimental results indicate that the film quality is strongly affected by annealing treatment of the sapphire substrate surface., The optimum annealing temperature of sapphire substrates is given. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

gamma-LiAlO2 layers with a highly preferred (1 0 0) orientation were prepared by vapor transport equilibration (VTE) technique on (0 0 0 1) sapphire substrate. Microststructure of the gamma-LiAlO2 layers was studied by XRD and SEM. In the temperature range from 750 to 1100 degrees C, the residual stress in the gamma-LiAlO2 layers varied from tensile to compressive with the increase of VTE temperature, and the critical point of the change between tensile and compressive stress is around 975 degrees C. (c) 2005 Elsevier B.V. All rights reserved.