155 resultados para Phosphorus-doped Silicon

em Chinese Academy of Sciences Institutional Repositories Grid Portal


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Boron-doped ( B-doped) silicon nanowires have been successfully synthesized by plasma-enhanced chemical vapor deposition (PECVD) at 440degreesC using silane as the Si source, diborane( B2H6) as the dopant gas and An as the catalyst. It is desirable to extend this technique to the growth of silicon nanowire pn junctions because PECVD enables immense chemical reactivity.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Exciton-mediated energy transfer model in Er-doped silicon was presented. The emission intensity is related to optically active Er concentration, lifetime of excited Er3+ ion and spontaneous emission. The thermal quenching of the Er luminescence in Si is caused by thermal ionization of Er-bound exciton complex and nonradiative energy back-transfer processes, which correspond to the activation energy of 6.6 and 47.4 meV, respectively. Er doping in silicon introduces donor states, a large enhancement in the electrical activation of Er (up to two orders of magnitude) is obtained by co-implanting Er with O. It appears that the donor states are the gateway to the optically active Er. (C) 2000 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel method, based on an infrared absorption and neutron irradiation technique, has been developed for the determination of interstitial oxygen in heavily boron-doped silicon. The new procedure utilizes fast neutron irradiated silicon wafer specimens. On fast neutron irradiation, the free carriers of high concentration in silicon can be trapped by the irradiated defects and the resistivity increased. The resulting calibration curve for the measurement of interstitial oxygen in boron-doped silicon has been established on the basis of the annealing behaviour of irradiated boron-doped CZ silicon.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

It was determined that oxygen concentration in heavily Sb-doped silicon was about 40% lower than that in the lightly doped Czochralski grown silicon and decreased with increasing content of Sb by means of coincident elastic recoil detection analysis. Through thermodynamic calculation, the oxygen loss by evaporation from the free surface of melt is only due to the formation of SiO, and Sb2O3 evaporation can be neglected. The basic reason for oxygen concentration reduction in heavily Sb-doped CZSi was that oxygen solubility decreased when element Sb with larger radius doped degenerately into silicon crystal. (C) 1999 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Boron-doped (B-doped) silicon nanowires (SiNWS) have been prepared and characterized by Raman scattering and photoluminescence (PL). B-doped SiNWS were grown by plasma enhanced chemical vapor deposition (PECVD), using diborane (B2H6) as the dopant gas. Raman spectra show a band at 480cm(-1),which is attributed to amorphous silicon. Photoluminescence at room temperature exhibits three distinct emission peaks at 1.34ev, 1.42ev, 1.47ev. Possible reason for these is suggested.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

It is well known that the value of room-temperature conductivity sigma(RT) of boron-doped silicon films is one order lower than that of phosphorus-doped silicon films, when they are deposited in an identical plasma-enhanced chemical vapour deposition system. We use surface acoustic wave and secondary-ion mass spectrometry techniques to measure the concentration of total and electrically active boron atoms. It is shown that only 0.7% of the total amount of incorporated boron is electrically active. This is evidence that hydrogen atoms can passivate substitutional B-Si bonds by forming the neutral B-H-Si complex. By irradiating the boron-doped samples with a low-energy electron beam, the neutral B-H-Si complex converts into electrically active B-Si bonds and the conductivity can be increased by about one order of magnitude, up to the same level as that of phosphorus-doped samples.

Relevância:

100.00% 100.00%

Publicador:

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A new technique is reported for the rapid determination of interstitial oxygen in heavily Sb-doped silicon. This technique includes wafer thinning and low-temperature 10 K infrared measurement on highly thinned wafers. The fine structure of the interstitial oxygen absorption band around 1136 cm(-1) is obtained. Our results show that this method efficiently reduces free-carrier absorption interference, allowing a high reliability of measurement, and can be used at resistivities down to 1 x 10(-2) Omega cm for heavily Sb-doped silicon.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Er-doped silicon-rich silicon nitride (SRN) films were deposited on silicon substrate by an RF magnetron reaction sputtering system. After high temperature annealing, the films show intense photoluminescence in both the visible and infrared regions. Besides broad-band luminescence centered at 780 nm which originates from silicon nanocrystals, resolved peaks due to transitions from all high energy levels up to ~2H_(11/2) to the ground state of Er~(3+) are observed. Raman spectra and HRTEM measurements have been performed to investigate the structure of the films, and possible excitation processes are discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Boron-doped hydrogenated silicon films with different gaseous doping ratios (B_2H_6/SiH_4) were deposited in a plasma-enhanced chemical vapor deposition (PECVD) system. The microstructure of the films was investigated by atomic force microscopy (AFM) and Raman scattering spectroscopy. The electrical properties of the films were characterized by their room temperature electrical conductivity (σ) and the activation energy (E_a). The results show that with an increasing gaseous doping ratio, the silicon films transfer from a microcrystalline to an amorphous phase, and corresponding changes in the electrical properties were observed. The thin boron-doped silicon layers were fabricated as recombination layers in tunnel junctions. The measurements of the Ⅰ-Ⅴ characteristics and the transparency spectra of the junctions indicate that the best gaseous doping ratio of the recombination layer is 0.04, and the film deposited under that condition is amorphous silicon with a small amount of crystallites embedded in it. The junction with such a recombination layer has a small resistance, a nearly ohmic contact, and a negligible optical absorption.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Erbium-implanted silicones were treated by lamp-heating rapid thermal annealing (RTA). Two types of erbium-related photoluminescence spectra appear under different anneal temperatures. 750 degrees C annealing optimizes the luminescence intensity, which does not change with anneal time. Exciton-mediated energy transfer model in erbium-doped silicon was presented. The emission intensity is related to optical active erbium concentration, lifetime of excited Er3+ ion and spontaneous emission time. The thermal quenching of the erbium luminescence in Si is caused by thermal ionization of erbium-bound exciton complex and nonradiative energy backtransfer processes, which correspond to the activation energy of 6.6 meV and 47.4 meV respectively.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Exciton-mediated energy transfer model in Er-doped silicon was presented. The emission intensity is related to optically active Er concentration, lifetime of excited Er3+ ion and spontaneous emission. The thermal quenching of the Er luminescence in Si is caused by thermal ionization of Er-bound exciton complex and nonradiative energy back-transfer processes, which correspond to the activation energy of 6.6 and 47.4 meV, respectively. Er doping in silicon introduces donor states, a large enhancement in the electrical activation of Er (up to two orders of magnitude) is obtained by co-implanting Er with O. It appears that the donor states are the gateway to the optically active Er. (C) 2000 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The erbium-doped hydrogenated amorphous silicon suboxide films containing amorphous silicon clusters were prepared. The samples exhibited photoluminescence peaks at around 750 nm and 1.54 mum, which could be assigned to the electron-hole recombination in amorphous silicon clusters and the intra-4f transition in Er3+, respectively. Correlations between the intensities of these two photoluminescence peaks and oxidation and dehydrogenation of the films during annealing were studied. It was found that the oxidation is triggered by dehydrogenation of the films even at low annealing temperatures, which decisively changes the intensities of the two photoluminescence peaks. On the other hand, the increase of Er content in the erbium-doped hydrogenated amorphous silicon suboxide film will enhance Er3+ emission at 1.54 mum, while quench amorphous silicon cluster emission at 750 nm, such a competitive relationship, was also observed in the erbium-doped silicon nanocrystals embedded in SiO2 matrix. Moreover, we found that Er3+ emission is not sensitive to whether silicon clusters are crystalline or amorphous. The amorphous silicon clusters can be as sensitizer on Er3+ emission as that of silicon nanocrystals. (C) 2003 American Institute of Physics.