Resumo:
CW laser output has been demonstrated for polycrystalline transparent 10 at.% Yb3+-doped Y2O3 ceramics. End-pumped with 970 nm laser diode, a maximum output power of 5.5 W has been obtained with absorbed pump power of 31.1 W. The slope efficiency is 25% while the threshold pump power is 5.6 W. Saturation is not observed in our experiments, indicating higher laser output can be expected with higher pump power. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
We investigate a new structure of high-power 660-nm AlGaInP laser diodes. In the structure, a p-GaAs layer is grown on the ridge waveguide serving as the current-blocking layer, and nonabsorbing windows are only fabricated near the cavity facets to increase the catastrophic-optical-damage level. Stable fundamental mode operation was achieved at up to 80 mW without kinks, and the maximum output power was 184 mW at 22 degrees C. The threshold current was 40 mA.
Resumo:
A cladding-pumped ytterbium-doped fiber laser is described in this letter. Using unusual pumping source with 915-nm wavelength, slope efficiency up to 75% with respect to absorbed input power and output power is obtained, a maximum output power of 4.006 W with fundamental mode is measured.
Resumo:
An electrical-to-green efficiency of more than 10% was demonstrated by intracavity-frequency-doubling a Q-switched diode-side-pumped Nd:YAG laser with a type II lithium triborate (LBO) crystal in a straight plano-concave cavity. An average power of 69.2 W at 532 nm was generated when electrical input power was 666 W. The corresponding electrical-to-green conversion efficiency is 10.4%. To the best of our knowledge, this is the highest electrical-to-green efficiency of second harmonic generation laser systems with side-pumped laser modules, ever reported. At about 66 W of green output power, the power fluctuation over 4 hours was better than +/-0.86%.
Resumo:
The pulse-shaping technique has found widespread applications in nonlinear optics and material processing. Experimental research on laser-induced plasma shutter to control the 532 nm pulse width is conducted. The impacts of the total pulse output energy on pulse compression are investigated, and a useful conclusion can be drawn that there exists an optimal value of pulse energy at which the shortest output pulse of 3.23 ns can be obtained without a device for delay-time. Once the device for delay-time is employed to change the optical differences between two laser paths, the pulse width can be further shortened to 1.51 ns. In short, the 1.5-12 ns width-tunable 532 nm laser pulses have been obtained by adopting the laser-induced plasma shutter technique. (C) 2007 Elsevier GmbH. All rights reserved.
Resumo:
A Nd:GdVO4 crystal is pumped directly into its emitting level at 913 nm for the first time to the best of our knowledge. 3.35 W output laser emitting at 1063 nm is achieved in a 1.1 at.% Nd-doped Nd:GdVO4. The crystal absorbs pumping light of 4.30 W at 913 nm and produces a very low quantity of heat with the opto-optic conversion efficiency of 77.2%. The average slope efficiency is 81.2% from 0.21 W, at the threshold, to 4.30 W of absorbed pump power. Because of the very weakly thermal effect, the near-diffraction-limit beam is easily obtained with beam quality factor of M-2 approximate to 1.1.
Resumo:
A 32.1 W laser-diode-stack pumped acoustic-optic Q-switched Nd:YVO4 slab laser with hybrid resonator at 1064 nm was demonstrated with the pumping power of 112 W and repetition rate of 40 kHz, the pulse duration was 32.47 ns. The slope efficiency and optical-to-optical efficiency were 37 and 28.7%, respectively. At the repetition rate of 20 kHz and pumping power of 90 W, the average output power and pulse duration were 20.4 W and 20.43 ns, respectively. With the pumping power of 112 W, the beam quality M-2 factors in CW operation were measured to be 1.3 in stable direction and 1.6 in unstable direction.
Resumo:
The ablation in zinc selenide (ZnSe) crystal is studied by using 150-fs, 800-nm laser system. The images of the ablation pit measured by scanning electronic microscope (SEM) show no thermal stress and melting dynamics. The threshold fluence is measured to be 0.7 J/cm2. The ultrafast ablation dynamics is studied by using pump and probe method. The result suggests that optical breakdown and ultrafast melting take place in ZnSe irradiated under femtosecond laser pulses.
Resumo:
Single-shot laser damage threshold of MgO for 40-986 fs, 800 nm laser pulses is reported. The pump-probe measurements with femtosecond pulses were carried out to investigate the time-resolved electronic excitation processes. A theoretical model including conduction band electrons (CBE) production and laser energy deposition was applied to discuss the roles of multiphoton ionization (MPI) and avalanche ionization in femtosecond laser-induced dielectric breakdown. The results indicate that avalanche ionization plays the dominant role in the femtosecond laser-induced breakdown in MgO near the damage threshold. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
We demonstrated optical amplification at 1550 nm with a carbon tetrachloride solution of Er3+-Yb3+ codoped NaYF4 nanocubes synthesized with solvo-thermal route. Upon excitation with a 980 nm laser diode, the nanocube solution exhibited strong near-infrared emission by the I-4(13/2) -> I-4(15/2) transition of Er3+ ions due to energy transfer from Yb3+ ions. We obtained the highest optical gain coefficient at 1550 nm of 0.58 cm(-1) for the solution with the pumping power of 200 mW. This colloidal solution might be a promising candidate as a liquid medium for optical amplifier and laser at the optical communication wavelength. (C) 2009 Optical Society of America
Resumo:
Periodic nanostructures are observed on the surface of ZnSe after irradiation by a focused beam of a femtosecond Ti:sapphire laser, which are aligned perpendicular to the laser polarization direction. The period of self-organized grating structures is about 160 nm. The phenomenon is interpreted in terms of interference between the incident light field and the surface scattered wave of 800-nm laser pulses. With the laser polarization parallel to the moving direction we produce long-range Bragg-like gratings by slowly moving the crystal under a fixed laser focus. The nanograting orientation is adjusted by laser polarization and the accumulation effect.
Resumo:
Damage threshold of crystals SiO2 and YAG against 60-900 fs, 800 nm laser pulses are reported. The breakdown mechanisms were discussed based on the double-flux model and Keldysh theory. We found that impact ionization plays the important role in the femtosecond laser-induced damage in crystalline SiO2, while the roles of photoionization and impact ionization in YAG crystals depend on the laser pulse durations. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Stable single-frequency and single-polarization distributed-feedback (DFB) fiber laser was realized by giving a pressure on the phase shift region of the fiber grating. The output wavelength of the DFB fiber laser is 1053 nm. When the pump power of 980 nm laser diode is 100 and 254 mW, the output power can reach 8.3 and 37.1 mW and the polarization extinction ratio was 26 and 20 dB, respectively. After chopped by Acousto-optic modulator (0.3 Hz), the pulse peak value variance is 4.65%(peak to peak) and 1.098% (RMS) for 31 min. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
由于硝酸钡晶体具有很强的对称振动(频率1047 cm^-1)和较高的拉曼增益,可以用来产生受激拉曼激光.采用单端泵浦的外置拉曼振荡腔与双棱镜分光装置进行了硝酸钡晶体拉曼激光实验,泵浦源为倍频Nd: YAG的532 nm激光,硝酸钡晶体通过水溶液降温法生长,尺寸为10 mm×10 mm×48 mm,采用特殊镀膜的腔镜对各阶斯托克斯光进行优化选择.在泵浦源达到65 mJ时,获得21 mJ一阶斯托克斯光,输出波长为563 nm,以及16 mJ的二阶斯托克斯光,输出波长为599 nm,受激拉曼散射SRS最大的整体