The properties of the wetting layer (WL) of InAs nanorings grown by droplet epitaxy have been studied. The heavy-hole (HH) and light-hole (LH) related transitions of the In(Ga)As WL were observed by reflectance difference spectroscopy. From the temperature dependent photoluminescence behavior of InAs rings, the channel for carriers to redistribute was found to be the compressed GaAs instead of the In(Ga)As layer, which strongly indicated that the wetting layer was depleted around the rings. Futhermore, a complex evolution of the WL with In deposition amount has been observed. (c) 2008 American Institute of Physics.
Resumo:
We grow InN epilayers on different interlayers by metal organic vapour phase epitaxy (MOVPE) method, and investigate the effect of interlayer on the properties and growth mode of InN films. Three InN samples were deposited on nitrided sapphire, low-temperature InN (LT-InN) and high-temperature GaN (HT-GaN), respectively. The InN layer grown directly on nitrided sapphire owns the narrowest x-ray diffraction rocking curve (XRC) width of 300 arcsec among the three samples, and demonstrates a two-dimensional (2D) step-flow-like lateral growth mode, which is much different from the three-dimensional (3D) pillar-like growth mode of LT-InN and HT-GaN buffered samples. It seems that mismatch tensile strain is helpful for the lateral epitaxy of InN film, whereas compressive strain promotes the vertical growth of InN films.
Resumo:
Using the measured capacitance-voltage curves and the photocurrent spectrum obtained from the Ni Schottky contact on a strained Al0.3Ga0.7N/GaN heterostructure, the value of the relative permittivity of the AlGaN barrier layer was analysed and calculated by self-consistently solving Schrodinger's and Poisson's equations. It is shown that the calculated values of the relative permittivity are different from those formerly reported, and reverse biasing the Ni Schottky contact has an influence on the value of the relative permittivity. As the reverse bias increases from 0 V to - 3 V, the value of the relative permittivity decreases from 7.184 to 7.093.
Resumo:
By replacing the flat (Ga1-xAlx)As barrier layer with a trapezoidal AlxGa1-xAs barrier layer, a conventional heterostructure can be operated in enhancement mode. The sheet density of two-dimensional electron gas (2DEG) in the structure can be tuned linearly from N-2D = 0.3 x 10(11) cm(-2) to N-2D = 4.3 x 10(11) cm(-2) by changing the bias on the top gate. The present scheme for gated heterostructures is easy to fabricate and does not require the use of self-alignment photolithography or the deposition of insulating layers. In addition, this scheme facilitates the initial electrical contact to 2DEG. Although, the highest electron mobility obtained for the moment is limited by the background doping level of heterostructures, the mobility should be improved substantially in the future. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
AlGaN/GaN heterostructure using unintentionally doped AlN/GaN superlattices (SLs) as barrier layer is grown on C-plane sapphire by metal organic vapor deposition (MOCVD). Compared with the conventional Si-doped structure, electrical property is improved. An average sheet resistance of 287.1 Omega/square and high resistance uniformity of 0.82% are obtained across the 2-inch epilayer wafer with an equivalent Al composition of 38%. Hall measurement shows that the mobility of two-dimensional electron gas (2DEG) is 1852 cm(2)/V s with a sheet carrier density of 1.2 x 10(13) cm(-2) at room temperature. The root mean square roughness (RMS) value is 0.159 nm with 5 x 5 mu m(2) scan area and the monolayer steps are clearly observed. The reason for the property improvement is discussed. (c) 2008 Elsevier Ltd. All rights reserved.
Resumo:
We have studied the optical matching layers (OMLs) and external quantum efficiency in the evanescent coupling photodiodes (ECPDs) integrating a diluted waveguide as a fibre-to-waveguide coupler, by using the semi-vectorial beam propagation method (BPM). The physical basis of OML has been identified, thereby a general designing rule of OML is developed in such a kind of photodiode. In addition, the external quantum efficiency and the polarization sensitivity versus the absorption and coupling length are analysed. With an optical matching layer, the absorption medium with a length of 30 mu m could absorb 90% of the incident light at 1.55 mu m wavelength, thus the total absorption increases more than 7 times over that of the photodiode without any optical matching layer.
Resumo:
We have investigated the optical properties of AlGaN grown on sapphire. It is found that two main luminescence peaks occur in the cathodoluminescence (CL) spectra of AlGaN films, and their energy separation increases with the increase of Al source flux during the growth. Spatially resolved CL investigations have shown that the line splitting is a result of variation of AlN mole fraction within the layer. The Al composition varies in both lateral and vertical direction. It is suggested that the difference in the surface mobility of Al and Ga atoms, especially, its strong influence on the initial island coalescence process and the formation of island-like regions on the uneven film surface, is responsible for the Al composition inhomogeneity. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
We report on optimizing the GaAs capping layer growth of 1.3 mu m InAs quantum dots (QDs) by a combined two-temperature and annealing process at low temperatures using metalorganic chemical vapor deposition. The initial part (tnm) of the capping layer is deposited at a low temperature of 500 degrees C, which is the same for the growth of both the QDs and a 5-nm-thick In0.15Ga0.85As strain-reducing capping layer on the QDs, while the remaining part is grown at a higher temperature of 560 degrees C after a rapid temperature rise and subsequent annealing period at this temperature. The capping layer is deposited at the low temperatures (<= 560 degrees C) to avoid postgrowth annealing effect that can blueshift the emission wavelength of the QDs. We demonstrate the existence of an optimum t (=5 nm) and a critical annealing time (>= 450s) during the capping, resulting in significantly enhanced photoluminescence from the QDs. This significant enhancement in photoluminescence is attributed to a dramatic reduction of defects due to the optimized capping growth. The technique reported here has important implications for realizing stacked 1.3 mu m InAs/GaAs QD lasers. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
ZnO film of 8 mu m thickness was grown on a sapphire (0 0 1) substrate with a GaN buffer layer by a novel growth technique called metal-source vapor phase epitaxy (MVPE). The surface of ZnO film measured by scanning electron microscope (SEM) is smooth and shows many regular hexagonal features. The full width at half maximum (FWHM) of ZnO(0 0 2) and (1 0 2) omega-scan rocking curves are 119 and 202 arcsec, corresponding a high crystal quality. The status of the strain in ZnO thick film was particularly analyzed by X-ray diffraction (XRD) omega-20 scanning. The results show that the strain in ZnO film is compressive, which is also supported by Raman scattering spectroscopy. The compressive strain can solve the cracking problem in the quick growth of ZnO thick film. (c) 2008 Elsevier Ltd. All rights reserved.
Resumo:
The effect of thickness of the high-temperature (HT) AlN buffer layer on the properties of GaN grown on Si(111) has been investigated. Optical microscopy (OM), atomic force microscopy (AFM) and X-ray diffraction (XRD) are employed to characterize these samples grown by metal-organic chemical vapor deposition (MOCVD). The results demonstrate that the morphology and crystalline properties of the GaN epilayer strongly depend on the thickness of HT AlN buffer layer, and the optimized thickness of the HT AlN buffer layer is about 110 nm. Together with the low-temperature (LT) AlN interlayer, high-quality GaN epilayer with low crack density can be obtained. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
This work discusses the fabrication of two-dimensional photonic crystal mask layer patterns. Photonic crystal patterns having holes with smooth and straight sidewalls are achieved by optimizing electron beam exposure doses during electron beam lithography process. Thereafter, to precisely transfer the patterns from the beam resist to the SiO2 mask layer, we developed a pulse-time etching method and optimize various reaction ion etching conditions. Results show that we can obtain high quality two-dimensional photonic crystal mask layer patterns.
Resumo:
A new method for fabricating electroabsorption modulator integrated with a distributed feedback laser (EML) was proposed. With the method we fabricated a selective area growth double stack active layer EML (SAG-DSAL-EML). Through comparing with other fabrication methods of EMLs, the characters and the merits of the new method presented in this paper were discussed.
Resumo:
Mg-doped p-InGaN layers with In composition of about 10% are grown by metalorganic chemical vapor deposition (MOCVD). The effect of the annealing temperature on the p-type behavior of Mg-doped InGaN is studied. It is found that the hole concentration in p-InGaN increases with a rising annealing temperature in the range of 600 850 C, while the hole mobility remains nearly unchanged until the annealing temperature increases up to 750 C, after which it decreases. On the basis of conductive p-type InGaN growth, the p-In0.1Ga0.9N/i-In0.1Ga0.9N/n-GaN junction structure is grown and fabricated into photodiodes. The spectral responsivity of the InGaN/GaN p-i-n photodiodes shows that the peak responsivity at zero bias is in the wavelength range 350-400 nm.
Resumo:
Polarization effects in AlGaN/GaN heterojunction are simulated based on a traditional semiconductor device simulator. A delta doping layer is purposely inserted at the interface of the heterojunction in the simulation, so the ionized donors or acceptors can represent polarization-induced positive or negative fixed charges. The free electron distribution of single AlGaN/GaN heterostructures with Ga-face and N-face growth is compared, and the results of the simulation show that carrier confinement takes place only in the former structure. The dependence of sheet density of free electrons at the interface of Ga-face growth AlGaN/GaN on Al composition and the thickness of AlGaN is also investigated. The consistency of simulation results with the experiments and calculations reported by other researchers shows that this method can be effectively used to deal with the polarization effects in the simulation of GaN-based heterojunction devices. (C) 2004 Elsevier Ltd. All rights reserved.
Resumo:
GaN epilayers were grown on Si(111) substrate by metalorganic chemical vapor deposition. By using the Al-rich AlN buffer which contains Al beyond stoichiometry, crack-free GaN epilayers with 1 mum thickness were obtained. Through x-ray diffraction (XRD) and secondary ion mass spectroscopy analyses, it was found that a lot of Al atoms have diffused into the under part of the GaN epilayer from the Al-rich AlN buffer, which results in the formation of an AlxGa1-xN layer at least with 300 nm thickness in the 1 mum thick GaN epilayer. The Al fraction x was estimated by XRD to be about 2.5%. X-ray photoelectron spectroscopy depth analysis was also applied to investigate the stoichiometry in the Al-rich buffer before GaN growth. It is suggested that the underlayer AlxGa1-xN originated from Al diffusion probably provides a compressive stress to the upper part of the GaN epilayer, which counterbalances a part of tensile stress in the GaN epilayer during cooling down and consequently reduces the cracks of the film effectively. The method using the Al diffusion effect to form a thick AlGaN layer is really feasible to achieve the crack-free GaN films and obtain a high crystal quality simultaneously. (C) 2004 American Institute of Physics.