536 resultados para physical vapor deposition
Resumo:
Highly ordered AlN nanowire arrays were synthesized via a simple physical vapor deposition method on sapphire substrate. The nanowires have an extremely sharp tip < 10 nm, with the average length around 3 mu m. Raman spectroscopy analysis on the AlN nanowire arrays revealed that the lifetime of the phonons is shorter than that in bulk AlN. The transmission spectra of the AlN nanowires showed a blueshift similar to 0.27 eV at the absorption edge with that of the bulk AlN, which is closely related to the small size of the nanowires. (c) 2005 American Institute of Physics.
Resumo:
MnSb films were deposited on porous silicon substrates by physical vapor deposition (PVD) technique. Modulation effects due to the substrate on microstructure and magnetic properties of the MnSb film's were studied by scanning electron microscope (SEM), X-ray diffraction (XRD) and measurements of hysteresis loops. SEM images of the MnSb films indicate that net-like structures were obtained because of the special morphology of the substrates. The net-like MnSb films exhibit some novel magnetic properties different from the unpatterned referenced samples. For example, in the case of net-like morphology, the coercive field is as low as 60 Oe. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Vertically well-aligned ZnO nanoridge, nanorod, nanorod-nanowall junction, and nanotip arrays have been successfully synthesized on Si (100) substrates using a pulsed laser deposition prepared ZnO film as seed layer by thermal evaporation method. Experimental results illustrated that the growth of different morphologies of ZnO nanostructures was strongly dependent upon substrate temperature. X-ray diffraction (XRD) and transmission electron microscopy (TEM) studies showed that the ZnO nanostructures were single crystals with a wurtzite structure. Compared with those of the other nanostructures, the photoluminescence (PL) spectrum of nanorod-nanowall junctions showed the largest intensity ratio of ultraviolet (UV) to yellow-green emission and the smallest full-width at half-maximum (FWHM) of the UV peak, reflecting the high optical quality and nearly defect free of crystal structure. The vertical alignment of the nanowire array on the substrate is attributed to the epitaxial growth of the nanostructures from the ZnO buffer layer. The growth mechanism was also discussed in detail. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Ferromagnetic MnSb films were synthesized on Si wafers by physical vapor deposition. X-ray diffraction revealed that the films primarily consisted of MnSb alloy. Nanorods and nanoleaves were observed in the MnSb films by field-emission scanning electron microscopy. These nanorods had an average diameter of 20nm and a length of up to hundreds of nanometers. The nanoleaves had a width and thickness of about 100 and 20nm, respectively. Magnetic hysteresis loops were measured by an alternative gradient magnetometer, and the loops showed strong geometrical anisotropy.
Resumo:
A selective oxidation technique has been applied to form a diffusion barrier on the Ni-based superalloy substrate by heating the substrate with electron beam of the electron beam-physical vapor deposition (EB-PVD) facility. The interdiffusion behavior, cross-sectional morphology, isothermal and cyclic oxidations were studied for thermal barrier coatings (TBCs) with and without diffusion barrier.
Resumo:
La2Zr2O7 (LZ) and La-2(Zr0.7Ce0.3)(2)O-7 (LZ7C3) as novel candidate materials for thermal barrier coatings (TBCs) were prepared by electron beam-physical vapor deposition (EB-PVD). The adhesive strength of the as-deposited LZ and LZ7C3 coatings were evaluated by transverse scratch test. Meanwhile, the factors affecting the critical load value were also investigated. The critical load value of LZ7C3 coating is larger than that of LZ coating, whereas both values of these two coatings are lower than that of the traditional coating material, i.e. 8 wt% yttria stabilized zirconia (8YSZ). The micro-cracks formed in the scratch channel can partially release the stress in the coating and then enhance the adhesive strength of the coating. The width of the scratch channel and the surface spallation after transverse scratch test are effective factors to evaluate the adhesive strength of LZ and LZ7C3 coatings.
Resumo:
Thermal barrier coatings (TBCs) of La2Zr2O7 (LZ) with the addition of 3 wt.% Y2O3 (LZ3Y) were deposited by electron beam-physical vapor deposition (EB-PVD). The phase stabilities, thermophysical and mechanical properties, and chemical compositions of these ceramics and coatings were studied in detail. The phase stability and thermal expansion behavior of LZ3Y bulk material are identical to those of LZ bulk material, but the mechanical properties of the former are superior to those of the latter. Elemental analysis and X-ray diffraction indicate that compositional deviation of LZ coating can be optimized after doping by 3 wt.% Y2O3, Y2O3 acts as a dopant as well as a process regulator. The optimal composition of LZ3Y coating could be effectively achieved by the addition of excess Y2O3 into the ingot and by properly controlling the current of electron beam (i.e. similar to 650 mA).
Resumo:
Bulk material and coatings of Lanthanum-Cerium Oxide (La2Ce2O7) with a fluorite structure were studied as a candidate material for thermal barrier coating (TBC). It has been showed that such material has the properties of low thermal conductivity about four times lower than YSZ, the difference in the thermal expansion coefficient between La2Ce2O7 and bond coat is smaller than that of YSZ in TBC systems, high phase stability between room temperature and 1673 K, about 300 K higher than that of the YSZ. The coating prepared by electron beam physical vapor deposition (EB-PVD) showed that it has good thermal cycling behavior, implying that Such material can be a promising thermal barrier coating material. The deviation of coating composition from ingot can be overcome by the addition of excess La2O3 during ingot preparation and/or by adjusting the process parameters.
Resumo:
In this paper, recent progresses in optical analysis of dislocation-related physical properties in GaN-based epilayers are surveyed with a brief review. The influence of dislocations on both near-band edge emission and yellow luminescence (YL) is examined either in a statistical way as a function of dislocation density or focused on individual dislocation lines with a high spatial resolution. Threading dislocations may introduce non-radiative recombination centers and enhance YL, but their effects are affected by the structural and chemical environment. The minority carrier diffusion length may be dependent on either dislocation density or impurity doping as confirmed by the result of photovoltaic spectra. The in situ optical monitoring of the strain evolution process is employed during GaN heteroepitaxy using an AIN interlayer. A typical transition of strain from compression to tension is observed and its correlation with the reduction and inclination of threading dislocation lines is revealed. (c) 2007 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
Crystalline beta-BBO layers have been successfully prepared on (0 0 1)-oriented Sr2+-doped alpha-BBO substrates using vapor transport equilibration technique. The layers were characterized by X-ray diffraction, X-ray rocking curve and transmission spectra. The present results manifest that the VTE treatment time and powder ratio are important factors on the preparation of beta-BBO layers. beta-BBO layers with a highly (0 0 l) preferred orientation were obtained according to XRD profiles. The full width at half-maximum of the rocking curve for the layer is as low as about 1000 in., which shows the high crystallinity of the layer. These results reveal the possibility of fabricating beta-BBO (0 0 1) layers on (0 0 1)-oriented Sr2+-doped alpha-BBO substrates by VTE. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Glancing angle deposition is a novel method to prepare graded index coatings. By using this method and physical vapour deposition, ZrO2 is used to engineer graded index filter on BK7 glass substrate. Controlling the deposition rate and the periodic oscillation of oblique angle of deposited material, a 10-period graded index ZrO2 filter with high reflection near 532 nm and high transmittance at wavelength 1064 nm is fabricated. The causes of difference between the theoretical and experimental results are discussed in detail. The material properties and electron gun nonlinearity are possibly the main origins of the difference, which result in the variations in both thickness control and deposition rate of the Elm material.
Resumo:
TiO2 films deposited by electron beam evaporation with glancing angle deposition (GLAD) technique were reported. The influence of flux angle on the surface morphology and the microstructure was investigated by scanning electron microscopy. The GLAD TiO2 films are anisotropy with highly orientated nanostructure of the slanted columns. With the increase of flux angle, refractive index and packing density decrease. This is caused by the shadowing effect dominating film growth. The anisotropic structure of TiO2 films results in optical birefringence, which reaches its maximum at the flux angle alpha = 65 degrees. The maximum birefringence of GLAD TiO2 films is higher than that of common bulk materials. It is suggested that glancing angle deposition may offer an effective method to obtain tailorable refractive index and birefringence in a large continuous range. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
InN nanostructures with and without GaN capping layers were grown by using metal-organic chemical vapor deposition. Morphological, structural, and optical properties were systematically studied by using atomic force microscopy, X-ray diffraction (XRD) and temperature-dependent photoluminescence (PL). XRD results show that an InGaN structure is formed for the sample with a GaN capping layer, which will reduce the quality and the IR PL emission of the InN. The lower emission peak at similar to 0.7 eV was theoretically fitted and assigned as the band edge emission of InN. Temperature-dependent PL shows a good quantum efficiency for the sample without a GaN capping layers; this corresponds to a lower density of dislocations and a small activation energy.
Resumo:
Optimized AlGaN/AlN/GaN high electron mobility transistors (HEMTs) structures were grown on 2-in semi-insulating (SI) 6H-SiC substrate by metal-organic chemical vapor deposition (MOCVD). The 2-in. HEMT wafer exhibited a low average sheet resistance of 305.3 Omega/sq with a uniformity of 3.85%. The fabricated large periphery device with a dimension of 0.35 pm x 2 nun demonstrated high performance, with a maximum DC current density of 1360 mA/mm, a transconductance of 460 mS/mm, a breakdown voltage larger than 80 V, a current gain cut-off frequency of 24 GHz and a maximum oscillation frequency of 34 GHz. Under the condition of continuous-wave (CW) at 9 GHz, the device achieved 18.1 W output power with a power density of 9.05 W/mm and power-added-efficiency (PAE) of 36.4%. While the corresponding results of pulse condition at 8 GHz are 22.4 W output power with 11.2 W/mm power density and 45.3% PAE. These are the state-of-the-art power performance ever reported for this physical dimension of GaN HEMTs based on SiC substrate at 8 GHz. (c) 2008 Elsevier Ltd. All rights reserved.
Resumo:
ZnO nanoflowers are synthesized on AIN films by solution method. The synthesized nanoflowers are composed of nanorods, which are pyramidal and grow from a central point, thus forming structures that are flower-shaped as a whole. The nanoflowers have two typical morphologies: plate-like and bush-like. The XRD spectrum corresponds to the side planes of the ZnO nanorods made up of the nanoflowers. The micro-Raman spectrum of the ZnO nanoflowers exhibits the E-2 (high) mode and the second order multiple-phonon mode. The photoluminescence spectrum of the ZnO nanoflowers exhibits ultraviolet emission centred at 375 nm and a broad green emission centred at 526 nm.