263 resultados para array microstructure


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thin films of ZrO2, HfO2 and TiO2 were deposited on kinds of substrates by electron beam evaporation (EB), ion assisted deposition (IAD) and dual ion beam sputtering (DIBS). Then some of them were annealed at different temperatures. X-ray diffraction (XRD) was applied to determine the crystalline phase and the grain size of these films, and the results revealed that their microstructures strongly depended on the deposition conditions such as substrate, deposition temperature, deposition method and annealing temperature. Theory of crystal growth and migratory diffusion were applied to explain the difference of crystalline structures between these thin films deposited and treated under various conditions. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Hot pressing (HP) at higher sintering temperature has been a traditional and prevalent technique for the fabrication of alpha-SiAlON. In order to prepare translucent SiAlON more easily, LiF was used as a non-oxide sintering additive to lower the sintering temperature to <= 1650 degrees C. As a result, all of the samples possessed a good hardness and fracture toughness. At the same time, the lower temperature sintered samples showed a higher optical transmittance in the range of 2.5-5.5 mu m wavelength (0.5 mm in thickness). The maximum infrared transmission reached 68% at a wavelength of 3.3 mu m. The present work shows that the sintering process has a strong effect on microstructure and property of alpha-SiAlON. To be exact, a lower sintering temperature and longer holding time can produce some fully-developed microstrcture, which is beneficial for the optical transmittance. (C) 2008 The Ceramic Society of Japan. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The evolution of microstructure and optical properties of TiO2 sculptured thin films under thermal annealing is reported. XRD, field emission SEM, UV-Vis-NIR spectra are employed to characterize the microstructural and optical properties. It is found that the optimum annealing temperature for linear birefringence is 500 degrees C. The maximum of transmission difference for linear birefringence is up to 18%, which is more than twice of that in as-deposited thin films. In addition, the sample annealed at 500 degrees C has a minimum of column angle about 12 degrees C. The competitive process between the microstructural and optical properties is discussed in detail. Post-annealing is a useful method to improve the linear birefringence in sculptured thin films for practical applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Y2O3 stabilized ZrO2 (YSZ) thin films with different Y2O3 molar contents (0, 3, 7, and 12 mol%) are deposited on BK7 substrates by electron-beam evaporation technique. The effects of different Y2O3 contents on residual stresses and structures of YSZ thin films are studied. Residual stresses are investigated by means of two different techniques: the curvature measurement and x- ray diffraction method. It is found that the evolution of residual stresses of YSZ thin films by the two different methods is consistent. Residual stresses of films transform from compressive stress into tensile stress and the tensile stress increases monotonically with the increase of Y2O3 content. At the same time, the structures of these films change from the mixture of amorphous and monoclinic phases into high temperature cubic phase. The variations of residual stress correspond to the evolution of structures induced by adding of Y2O3 content.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study investigates the optical properties and microstructure of Ta2O5 film deposited with the glancing angle deposition technique. The tilted nanocolumn microstructure, examined with scanning electron microscopy, induces the optical anisotropy of thin film. The optical properties of thin film are characterized with an inverse synthesis method. Based on the Cauchy model, the dispersion equations of optical constants of film are determined from the transmittance spectra measured at normal and oblique incidence over 400-800 nm. The starting values derived with an envelope method quicken the optimization process greatly. The dispersion of the principal indices N-1, N-2, and N-3 and the thickness d of thin film are presented statistically. A good agreement between the measured optical properties and theoretical calculation is obtained, which validates the model established for thin film produced by glancing angle deposition. (C) 2008 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Many efforts based on complete mitochondrial DNA (mtDNA) genomes have been made to depict the global mtDNA landscape, but the phylogeny of Indian macrohaplogroup M has not yet been resolved in detail. To fill this lacuna, we took the same strategy as in o

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Otolith microstructure of Oxygymnocypris stewartii collected from the Lhasa River was examined and described with regards to the early life history events. The monthly changes in the number of microincrements on the margin of the otolith were examined to validate the approximately daily periodicity of otolith increment formation. The microstructure of otoliths was used to detect changes in microincrement deposition patterns corresponding with events during early life. The annuli, microincrements and checks including the hatch check, yolk absorption check and several recurrent patterns in the otolith were described. Periodicity of the recurrent patterns was weekly, fortnightly and monthly. Through counting the number of the microincrements, it was confirmed that the primary growth of O. stewartii was in a period of 7 or 8 months from late March to October; it was estimated that O. stewartii might hatch between April and May.