139 resultados para Solid-state absorption
Resumo:
In this paper, a highly efficient Ti:sapphire end-pumped 1 at.-% Nd:YAG ceramic laser that is comparable in efficiency with Nd:YAG single crystal lasers has been developed. Optical absorption and emission spectra for Nd:YAG ceramics have been measured. With 673-mW pumping, 295-mW laser output at 1064 nm has been obtained. The laser threshold is only 13 mW. Deducted the transmitted light, the corresponding optical-to-optical conversion efficiency is 58.4%. The lasing characteristics of Nd:YAG ceramic are nearly equal to those of Nd:YAG single crystal.
Resumo:
The Raman spectra, infrared spectra and upconversion luminescence spectra were studied, and the effect mechanism of OH- groups on the upconversion luminescence of Er3+-doped oxyhalide tellurite glasses was analyzed. The results show that the phonon energy of lead chloride tellurite (PCT) glass was lower than that of lead fluoride tellurite (PFT) glass, but upconversion luminescence intensity of Er3+-doped PFT glass was higher than that of Er3+-doped PCT glass. The analysis considers that it was attributed mainly to the effect of OH- groups. The lower the absorption coefficient of the OH- groups, the higher the fluorescence lifetime of Er3+, and as a result the higher upconversion luminescence intensity of Er3+. In this work, the effect of OH groups on the upconversion luminescence of Er3+ was bigger than that of the phonon energy. (c) 2005 Elsevier Inc. All rights reserved.
Resumo:
Effect of PbF2 on Yb3+ -doped fluorophosphate glasses is studied. Results indicate that proper amount of PbF2 has absolute advantages in improving the crystallization stability of fluorophosphate glasses. T, value performs a decreasing and increasing tendency with 25 mol% PbF2 as the turning-point. And the spectroscopic properties such as absorption and emission cross section, effective fluorescence linewidth are apparently enhanced with PbF2 over 25 mol%. Lasing parameters beta, I-sat and I-min increase slightly with the addition of PbF2. Raman analysis proves that over 20 mol% PbF2, destroys the phosphate vibration groups greatly. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
Infrared-to-visible upconversion fluorescence property of Er3+/Yb3+ codoped novel bismuth-germanium glass under 975 nm LD excitation has been studied. Intense green and red emissions centered at 525, 546 and 657 nm, corresponding to the transitions H-2(11/2) -> I-4(15/2), S-4(3/2) -> I-4(15/2), and F-4(9/2) -> I-4(15/2), respectively, were observed at room temperature. The quadratic dependence of the 525, 546 and 657 nm emissions on excitation power indicates that a two-photon absorption process occurs. The structure of the bismuth-germanium glass has been investigated by peak-deconvolution of FT-Raman spectrum, and the structural information was obtained from the peak wavenumbers. This novel bismuth-germanium glass with low maximum phonon energy (similar to 750 cm(-1)) can be used as potential host material for upconversion lasers. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
Structural and infrared-to-visible upconversion fluorescence properties of Er3+/Yb3+-codoped oxychloride lead-germanium-bismuth glass have been studied. The Raman spectrum investigation indicates that PbCl2 plays an important role in the formation of glass network, and has an important influence on the upconversion luminescence owing to lower phonon energy. Intense green and red emissions centered at 525, 546, and 657 nm, corresponding to the transitions H-2(11/2)-->I-4(15/2,) I-4(3/2)-->I-4(15/2), and F-4(9/2)-->I-4(15/2), respectively, were observed at room temperature. The quadratic dependence of the 525, 546, and 657 nm emissions on excitation power indicates that a two-photon absorption process occurs under 975 nm excitation. (C) 2004 Elsevier Ltd. All rights reserved.
Resumo:
A new Yb-doped oxyorthosilicate laser crystal, Yb:Gd2SiO5 (Yb:GSO), has been grown by the Czochralski (Cz) method. The crystal structure was determined by means of X-ray diffraction analysis. Room temperature absorption and fluorescence spectra of Yb3+ ions in GSO crystal were measured. Then. spectroscopic parameters of Yb:GSO were calculated and compared with those of another Yb-doped oxyorthosilicate crystal Yb:YSO. Results indicated that Yb:GSO crystal seemed to be a very promising laser gain media in generating ultra-pulses and tunable solid state laser applications. As expected, the output power of 2.72 W at 1089 nm was achieved in Yb:GSO crystal with absorbed power of only 4.22 W at 976 nm, corresponding to the slope efficiency of 71.2% through the preliminary laser experiment. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
High-quality Nd:LuVO4 single crystal was successfully grown by Czochralski method. The assessment of the crystalline quality by the chemical etching method and Conoscope image was reported. The absorption spectra from 300 to 1000 nm and emission spectra from 960 to 1450 nm of Nd: LuVO4 were measured. Laser performance was achieved with Nd:LUVO4 crystal for the transition of F-4(3/2) -> I-4(11/2) (corresponding wavelength 1065.8 nm) in an actively Q-switched operation, and the average output power reached 5.42 W at a pulse repetition frequency (PRF) of 40 kHz under pump power of 18 W, giving an optical conversion efficiency of 30.1%. The pulse energy and peak power reached 138 mu J and 16.2 kW at PRF of 25 kHz under pump power of 14.2 W, and the pulse duration was 8.5 ns. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
For the first time to our knowledge, the laser performance of Yb3+, Na+-codoped CaF2 single crystals was demonstrated. Self-Q-switched laser operation at 1050nm was observed for 976 nm diode pumping at room temperature. On 5 W of incident power, the repetition rate and width of the self-Q-switched pulses reached 28 kHz and 1.5 mu s, respectively. A maximal slope efficiency of 20.3% and minimal threshold absorbed pump power of 30 mW were respectively achieved with different output couplers, showing the promising application of Yb3+, Na+-codoped CaF2 crystals as compact and efficient solid-state lasers. (C) 2005 Optical Society of America.
Resumo:
For the first time, a high optical quality 10 at.% Yb3+-doped gadolinium oxyorthosilicate laser crystal Gd2SiO5 (GSO) was grown by the Czochralski (Cz) method. The segregation coefficient of Yb3+ was studied by the inductively coupled plasma atomic emission spectrometer (ICP-AES) method. The crystal structure has monoclinic symmetry with space group P2(1)/c; this was determined by means of an x-ray diffraction analysis. The absorption spectra, fluorescence spectra and fluorescence decay curves of Yb3+ ions in a GSO crystal at room temperature were also studied. Then, the spectroscopic parameters of Yb:GSO were calculated. The advantages of the Yb:GSO crystal include high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections and particularly broad emission bandwidth (similar to 72 nm). The results indicated that the Yb:GSO crystal seemed to be a very promising laser gain medium in diode-pumped femtosecond laser and tunable solid state laser applications when LD pumped at 940 and 980 nm.
Resumo:
Blue frequency-upconversion fluorescence emission has been observed in Ce3+-doped Gd2SiO5 single crystals, pumped with 120-fs 800 nm IR laser pulses. The observed fluorescence emission peaks at about 440nm is due to 5d -> 4f transition of Ce3+ ions. The intensity dependence of the blue fluorescence emission on the IR excitation laser power obeys the cubic law, demonstrating three-photon absorption process. Analysis suggested that three-photon simultaneous absorption induced population inversion should be the predominant frequency upconversion mechanism. (c) 2006 Optical Society of America.
Resumo:
The effects of Na+ doping level on the thermal conductivities, absorption and emission spectra, and fluorescence lifetimes of Yb3+ ,Na+ :CaF2 crystals were systematically studied. Sites structure, covalent force, and crystal field strength of Yb3+ :CaF2 crystals were markedly varied by codoping Na+ as charge compensator. The 2.0at% Yb3+ and 3.0at% Na+-codoped CaF2 crystal was demonstrated to operate in diode-pumped passively mode-locking scheme. Transform-limited 1 ps laser pulses were obtained, showing the crystal capable of producing ultra-short laser pulses. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Transparent polycrystalline MgO and TiO2 codoped Al2O3 ceramics were fabricated by conventional solid-state pressureless processing. The absorption, emission and excitation spectra of ( Mg, Ti : Al2O3 ceramics were measured. Owing to charge compensation of Mg2+, only UV absorption around 250nm was observed due to O2- -> Ti4+ charge transfer transitions (CT) when Ti content was low. As a result, the emission peaks of isolated Ti4+ ion located at 280-290nm and 410-420nm were observed. Besides absorption peak of V, ion, the characteristic absorption peak of V, ion centered at 490nm was observed in Mg, Ti) : Al2O3 ceramics when Ti content was high. The emission spectra of Ti3+, ion in polycrystalline Al2O3 ceramics coincide with that of Ti: Al2O3 single crystal.
Resumo:
用提拉法生长了掺铬、钕的钆镓石榴石(Cr^4+,Nd^3+:GGG)自调Q激光品体。报道了室温下的吸收光谱和荧光光谱特性。分析了Cr离子浓度对光谱性质的影响。比较了Cr^4+:GGG,Nd^3+:GGG和(Cr^4+,Nd^3+):GGG晶体吸收光谱的关系。测量了(Cr^4+,Nd^3+):GGG晶体和Nd^3+:GGG晶体的荧光寿命,它们分别是33μs和250μs。实验表明,(Cr^4+,Nd^3+):GGG晶体是一种非常有潜力的自调Q激光晶体,可以实现大功率激光器的小型化和全固态化。
Resumo:
Optical properties for ZnO thin films grown on (100) γ-LiAlO2 (LAO) substrate by pulsed laser deposition method were investigated. The c-axis oriented ZnO films were grown on (100) γ-LiAlO2 substrates at the substrate temperature of 550 Celsius degrees. The transmittance of the films was over 85%. Peaks attributed to excitons were shown in absorption spectra, which indicated that thin films had high crystallinity. Photoluminescence spectra with the maximum peak at 540 nm were observed at room temperature, which seemed to be ascribed to oxygen vacancy in the ZnO films caused by diffusion of Li from the substrates into the films during the deposition.
Resumo:
采用传统无压烧结工艺制备出透明性良好的掺Cr3+氧化铝陶瓷;测定了陶瓷的吸收光谱、发射光谱和激发光谱。结果表明,氧化铝陶瓷吸收峰与红宝石单晶一致,吸收截面大小与单晶相近;陶瓷中Cr3+离子所处格位的晶体场强较单晶弱,但其发射谱仍有较好的锐线发射;陶瓷中微量添加剂以及晶界的存在使得Al2O3晶胞发生畸变,造成其发射峰宽化。