142 resultados para Bengal Fan
Resumo:
Using the stratified gas flow model for calculating the conductance of long tubes with constant cross section, an analytical expression for calculating the conductance of along tube with equilateral triangle cross section has been derived. The formula given is applicable to the full pressure range. A minimum in the conductance in the intermediate flow state is shown. 2002 American vacuum Society.
Resumo:
ZrO2, films were deposited by electron-beam evaporation with the oxygen partial pressure varying from 3 X 10(-3) Pa to I I X 10(-3) Pa. The phase structure of the samples was characterized by x-ray diffraction (XRD). The thermal absorption of the films was measured by the surface thermal lensing technique. A spectrophotometer was employed to measure the refractive indices of the samples. The laser-induced damage threshold (LIDT) was assessed using a 1064, nm Nd: yttritium-aluminium-garnet pulsed laser at pulse width of 12 ns. The influence of oxygen partial pressure on the microstructure and LIDT of ZrO2 films was investigated. XRD data revealed that the films changed from polycrystalline to amorphous as the oxygen partial pressure increased. The variation of refractive index at 550 nm wavelength indicated that the packing density of the films decreased gradually with increasing oxygen partial pressure. The absorptance of the samples decreased monotonically from 125.2 to 84.5 ppm with increasing oxygen partial pressure. The damage threshold, values increased from 18.5 to 26.7 J/cm(2) for oxygen partial pressures varying from 3 X 10(-3) Pa to 9 X 10(-3) Pa, but decreased to 17.3 J/cm(2) in the case of I I X 10(-3) Pa. (C) 2005 American Vacuum Society.
Resumo:
There are two different effects to generate group delay dispersion by multilayer thin film mirrors: chirper effect and Gires-Tournois effect. Both effects are employed to introduce desired dispersion in the designed mirror. Thus the designed mirror provides large dispersion throughout broad waveband. Such mirror can be used for dispersion compensation in Ti:sapphire femtosecond lasers. Most group delay dispersion of a 5-mm Ti:sapphire crystal can be compensated perfectly with only four bounces of the designed mirror.
Resumo:
ZrO2, films were deposited by electron-beam evaporation with the oxygen partial pressure varying from 3 X 10(-3) Pa to I I X 10(-3) Pa. The phase structure of the samples was characterized by x-ray diffraction (XRD). The thermal absorption of the films was measured by the surface thermal lensing technique. A spectrophotometer was employed to measure the refractive indices of the samples. The laser-induced damage threshold (LIDT) was assessed using a 1064, nm Nd: yttritium-aluminium-garnet pulsed laser at pulse width of 12 ns. The influence of oxygen partial pressure on the microstructure and LIDT of ZrO2 films was investigated. XRD data revealed that the films changed from polycrystalline to amorphous as the oxygen partial pressure increased. The variation of refractive index at 550 nm wavelength indicated that the packing density of the films decreased gradually with increasing oxygen partial pressure. The absorptance of the samples decreased monotonically from 125.2 to 84.5 ppm with increasing oxygen partial pressure. The damage threshold, values increased from 18.5 to 26.7 J/cm(2) for oxygen partial pressures varying from 3 X 10(-3) Pa to 9 X 10(-3) Pa, but decreased to 17.3 J/cm(2) in the case of I I X 10(-3) Pa. (C) 2005 American Vacuum Society.
Resumo:
Laser conditioning effects of the dielectric mirror coatings with different designs were investigated. Simple quarter-wave ZrO2:Y2O3/SiO2 mirrors and half-wave SiO2 over-coated ZrO2:Y2O3/SiO2 mirror coatings were fabricated by E-beam evaporation (EBE). The absorbance of the samples before and after laser conditioning was measured by surface thermal lensing (STL) technology and the defects density was detected under Nomarski microscope. The enhancement of the laser damage resistance was found after laser conditioning. The dependence of the laser conditioning on the coating design was also observed and the over-coated sample obtained greatest enhancement, whereas the absorbance of the samples did not change obviously. During the sub-threshold fluence raster scanning, the minor damage about defects size was found and the assumption of pre-damage mechanism, based on the functional damage concept, was put forward. The improvement of the laser induced damage threshold (LIDT) was attributed to the benign damage of the defects and the dependence on the coating design owed to the damage growth behavior of different coating designs. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
The laser-induced damage (LID) behavior of narrow-band interference filters was investigated with a Nd:YAG laser at 1064 nm under single-pulse mode and free-running mode. The absorption measurement of such coatings was performed with surface thermal lensing (STL) technique. The damage morphologies under the two different laser modes were also studied in detail. It was found that all the filters exhibited a pass-band-center-dependent absorption and laser-induced damage threshold (LIDT) behavior, but the damage morphologies were diverse. The explanation was given with the analysis of the electric field distribution and the operational behavior of the irradiation laser. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
HfO2 films were deposited by electron beam evaporation with different deposition parameters. The properties such as refractive index, weak absorption, and laser induced damage thresholds (LIDTs) of these films have been investigated. It was found that when pulsed Nd:YAG 1064 nm laser is used to investigate LIDT of films: Metallic character is the main factor that influences LIDTs of films obtained from Hf starting material by ion-assisted reaction, and films prepared with higher momentum transfer parameter P have fewer metallic character; The ion-assisted reaction parameters are key points for preparing high LIDT films and if the parameters are chose properly, high LIDT films can be obtained. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
Glancing angle deposition is a novel method to prepare graded index coatings. By using this method and physical vapour deposition, ZrO2 is used to engineer graded index filter on BK7 glass substrate. Controlling the deposition rate and the periodic oscillation of oblique angle of deposited material, a 10-period graded index ZrO2 filter with high reflection near 532 nm and high transmittance at wavelength 1064 nm is fabricated. The causes of difference between the theoretical and experimental results are discussed in detail. The material properties and electron gun nonlinearity are possibly the main origins of the difference, which result in the variations in both thickness control and deposition rate of the Elm material.
Resumo:
TiO2 and ZrO2 films are deposited by electron-beam (EB) evaporation and by sol-gel process. The film properties are characterized by visible and Fourier-transform infrared spectrometry, x-ray diffraction analysis, surface roughness measure, absorption and laser-induced damage threshold (LIDT) test. It is found that the sol-gel Elms have lower refractive index, packing density and roughness than EB deposited films due to their amorphous structure and high OH group concentration in the film. The high LIDT of sol-gel films is mainly due to their amorphous and porous structure, and low absorption. LIDT of EB deposited film is considerably affected by defects in the Elm, and LIDT of sol-gel deposited film is mainly effected by residual organic impurities and solvent trapped in the film.
Resumo:
We investigate the laser damage behaviour of an electron-beam-deposited TiO2 monolayer at different process parameters. The optical properties, chemical composition, surface defects, absorption and laser-induced damage threshold (LIDT) of Elms are measured. It is found that TiO2 Elms with the minimum absorption and the highest LIDT can be fabricated using a TiO2 starting material after annealing. LIDT is mainly related to absorption and is influenced by the non-stoichiometric defects for TiO2 films. Surface defects show no evident effects on LIDT in this experiment.
Resumo:
We investigate the influence of vacuum organic contaminations on laser-induced damage threshold (LIDT) of optical coatings. Anti-reflective (AR) coatings at 1064 nm made by Ta2O5/SiO2 are deposited by the ion beam sputtering method. The LIDTs of AR coatings are measured in vacuum and in atmosphere, respectively. It is exhibited that contaminations in vacuum are easily to be absorbed onto optical surface because of lower pressure, and they become origins of damage, resulting in the decrease of LIDT from 24.5 J/cm(2) in air to 15.7 J/cm(2) in vacuum. The LIDT of coatings in vacuum has is slightly changed compared with the value in atmosphere after the organic contaminations are wiped off. These results indicate that organic contaminations are the main reason of the LIDT decrease in vacuum. Additionally, damage morphologies have distinct changes from vacuum to atmosphere because of the differences between the residual stress and thermal decomposability of filmy materials.
Resumo:
As the principal section consistent with the principal plane, electromagnetic propagation in a uniaxially birefingent thin film can be described with a concise 2 x 2 characteristic matrix, in which the refractive indices of the forward and backward propagating extraordinary rays are different and dependent. In this letter, based on Huygen's construction, the refractive indices and effective optical admittances of the forward and backward propagating extraordinary rays are discussed further, and the 2 x 2 characteristic matrix is simplified. Furthermore, the input optical admittance, reflectance and transmittance of assembly is presented, just as an isotropic thin film. The result can be extended to the general case of multilayer uniaxially birefringent thin films with their optic axes in the incident plane. Copyright (c) EPLA, 2007.