222 resultados para annealing conditions


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Based on the 2 x 2 (electric field) cross-spectral density matrix, a model for an electromagnetic J(0)-correlated Schell-model beam is given that is a generalization of the scalar J(0)-correlated Schell-model beam. The conditions that the matrix for the source to generate an electromagnetic J(0)-correlated Schell-model beam are obtained. The condition for the source to generate a scalar J(0)-correlated Schell-model beam can be considered as a special case. (C) 2008 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

YAlO3 single crystal doped with Ce3+ at concentration 1% was grown by the temperature gradient technique. The as-grown crystal was pink. After H-2 annealing or air annealing at 1400degreesC for 20 h, the crystal was turned into colorless. We concluded there were two kinds of color centers in the as-grown crystal. One is F+ center attributed to absorption band peaking at about 530 nm, the other is O- center attributed to absorption band peaking at about 390 nm. This color centers model can be applied in explaining the experiment phenomena including the color changes, the absorption spectra changes, and the light yield changes of Ce:YAP crystals before and after annealing. (C) 2004 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The annealing effects of sapphire substrate on the quality of epitaxial ZnO films grown by metalorganic chemical vapor deposition (MOCVD) were studied. The atomic steps formed on (0 0 0 1) sapphire (alpha-Al2O3) substrate surface by annealing at high temperature was analyzed by atomic force microscopy (AFM). The annealing effects of sapphire substrate on the ZnO films were examined by X-ray diffraction (XRD), AFM and photoluminescence (PL) measurements. Experimental results indicate that the film quality is strongly affected by annealing treatment of the sapphire substrate surface., The optimum annealing temperature of sapphire substrates is given. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnO films were grown on (0 0 0 1) LiNbO3 substrates by metal organic chemical vapor deposition (MOCVD). Annealing of ZnO films was performed in air for I h at 800 degrees C. The effects of annealing on the structural and optical properties of ZnO thin films on LiNbO3 substrates were investigated using X-ray diffraction (XRD), atomic force microscopy (AFM) and photoluminescence (PL) measurements. XRD patterns and AFM showed that the as-grown and the annealed ZnO films grown on LiNbO3 substrates had c-axis preferential orientation, the crystallinity of the ZnO films grown on LiNbO3 Substrates was improved, and the grain size increased by annealing. The PL spectra showed that the intensity of the UV near-band-edge peak was increased after annealing, while the intensity of visible peak (deep-level emission) decreased. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Defects in as-grown U3+ : CaF2 crystals grown with or without PbF2 as an oxygen scavenger were studied using Raman spectra, thermoluminescence glow curves, and additional absorption (AA) spectra induced by heating and gamma-irradiation. The effects of heating and irradiation on as-grown U3+: CaF2 crystals are similar, accompanied by the elimination of H-type centers and production of F-type centers. U3+ is demonstrated to act as an electron donor in the CaF2 lattice, which is oxidized to the tetravalent form by thermal activation or gamma-irradiation. In the absence of PbF(2)as an oxygen scavenger, the as-grown U3+:CaF2 crystals contain many more lattice defects in terms of both quantity and type, due to the presence of O2- impurities. Some of these defects can recombine with each other in the process of heating and gamma-irradiation. (c) 2005 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of gamma irradiation on as-grown 5 at% Yb:YAlO3 (YAP) and air annealing on gamma-irradiated 5 at% Yb: YAP have been studied by the difference in the absorption spectra before and after treatment. The gamma irradiation and air annealing led to opposite changes of the absorption properties of the Yb: YAP crystal. After air annealing, the gamma-irradiation effects were totally removed over the wavelength range 390-800 nm and the concentrations of Fe3+ and Yb3+ were slightly increased. For the first time, the gamma-irradiation-induced valence changes between Yb3+ and Yb2+ ions in Yb: YAP crystals have been observed. (c) 2005 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Five absorption hands, at 227, 300 340, 370 and 457nm, were observed in the optical absorption spectrum of Ce:Y3Al5O12 (Ce:YAG) crystals grown by the temperature gradient technique (TGT). The absorption bands at 227, 340, and 457 nm were identified Lis belonging to the Ce3+ -ion in the YAG crystal. A near UV optical emission band at 398nm was observed. with an excitation spectrum containing two bands, at 235 and 370nm. No fluorescence was detected under 300 nm excitation. The pair of absorption bands at 235 and 370 nm and the absorption band at 300 nm were attributed to the F- and F+-type color centers, respectively. The color centers model was also applied to explain the spectral changes in the Ce:YAG (TGT) crystal, including the reduction in the Ce 31 -ion absorption intensity, after annealing in an oxidizing atmosphere (air). (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The absorption spectra of the undoped Y2SiO5 and Eu3+-doped Y2SiO5 crystals grown by the Czochralski technique were compared before and after annealing and, similarly, the unannealed and annealed crystals after gamma-ray irradiation. The absorption bands of Eu2+ ions with peaks at 300 and 390 nm were observed in the as-grown Y2SiO5:Eu3+ crystal. These peaks were more intense in H-2-annealed and irradiated Y2SiO5:Eu3+ crystals. The additional absorption peaks at 260 and 320-330 nm which were attributed to F color centers and O- hole centers were observed in irradiated undoped Y2SiO5 and Y2SiO5:Eu3+ crystals, respectively. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The annealing effects of sapphire substrates on the quality of epitaxial ZnO films grown by dc reactive magnetron sputtering were studied. The atomic steps formed on (0001) sapphire (alpha-Al2O3) substrates surface by annealing at high temperature were analyzed by atomic force microscopy. Their influence on the growth of ZnO films was examined by X-ray diffraction and photoluminescence measurements. Experimental results indicate that the film quality is strongly affected by annealing treatment of the sapphire substrate surface. The optimum annealing temperature of sapphire substrates for ZnO grown by magnetron sputtering is 1400 degrees C for 1 h in air.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of gamma-irradiation on the air-annealed 10 at.% Yb:Y3Al5O12 (YAG) and air annealing on the gamma-irradiated 10at.% Yb:YAG have been studied by the difference absorption spectra before and after treatment. The gamma-irradiation and air annealing led to opposite changes of the absorption properties of the Yb:YAG crystal. After air annealing, the gamma-irradiation induced centers were totally removed and the concentration of Fe3+ and Yb3+ were lightly increased. For the first time, the gamma-irradiation induced valence changes between Yb3+ and Yb2+ ions in Yb:YAG crystals have been observed. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mg0.4Al2.4O4 single crystals with good optical quality were successfully grown by the Czochralski method. The transmission spectrum indicated that the absorption edge of the crystal was at 220nm, while no apparent absorption peaks were found. The X-ray diffraction and DSC curve analysis showed that Mg0.4Al2.4O4 crystal was stable at room temperature. While after annealing in the air and hydrogen atmosphere at about 1200 degrees C,Mg0.4Al2.4O4 decomposed into Al2O3 and (MgO)(0.4)(Al2O3)(x) (0.4 < x < 1.2). The reaction mainly occurred on the crystal surface, barely inside. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZrO2 coatings were deposited on different substrates of Yb:YAG and fused silica by electron beam evaporation. After annealed for 12 h at 673 and 1073 K, respectively, weak absorption of coatings was measured by surface thermal lensing (STL) technique, and then laser-induced damage threshold (LIDT) was determined also. The crystalline phase of ZrO2 coatings and the size of the crystal grain were investigated by X-ray diffraction. It was found that microstructure of ZrO2 coatings was dependent on both annealing temperature and substrate structure, and coatings containing monoclinic phases had higher damage threshold than others. Due to the strong absorption of Yb:YAG, damage threshold of coatings on Yb:YAG was much less than that on fused silica. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnO:Zn phosphor thin films were prepared by face-to-face annealing at 450 degrees C in air. The effects of the face-to-face annealing on the structural and optical properties of the ZnO films were investigated by X-ray diffraction (XRD), photoluminescence (PL), optical transmittance and absorption measurements. Measurement results showed that the crystal quality of ZnO films was improved by face-to-face annealing. Both UV light emission and visible light emission were enhanced compared to those of open annealing films. The UV emission peak was observed to have a blueshift towards higher energy. The optical band-gap edge of as-annealed films shifted towards longer wavelength. (c) 2005 Elsevier B.V.. All rights reserved.