ZnO thin films were deposited on the substrates of (100) gamma-LiAlO2 at 400, 550 and 700 degrees C using pulsed laser deposition (PLD) with the fixed oxygen pressure of 20 Pa, respectively. When the substrate temperature is 400 degrees C, the grain size of the film is less than 1 mu m observed by Leitz microscope and measured by X-ray diffraction (XRD). As the substrate temperature increases to 550 degrees C, highly-preferred c-orientation and high-quality ZnO film can be attained. While the substrate temperature rises to 700 degrees C, more defects appears on the surface of film and the ZnO films become polycrystalline again possibly because more Li of the substrate diffused into the ZnO film at high substrate temperature. The photoluminescence (PL) spectra of ZnO films at room temperature show the blue emission peaks centered at 430 nm. We suggest that the blue emission corresponds to the electron transition from the level of interstitial Zn to the valence band. Meanwhile, the films grown on gamma-LiAlO2 (LAO) exhibit green emission centered at 540 nm, which seemed to be ascribed to excess zinc and/or oxygen vacancy in the ZnO films caused by diffusion of Li. from the substrates into the films during the deposition.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Optical properties for ZnO thin films grown on (100) γ-LiAlO2 (LAO) substrate by pulsed laser deposition method were investigated. The c-axis oriented ZnO films were grown on (100) γ-LiAlO2 substrates at the substrate temperature of 550 Celsius degrees. The transmittance of the films was over 85%. Peaks attributed to excitons were shown in absorption spectra, which indicated that thin films had high crystallinity. Photoluminescence spectra with the maximum peak at 540 nm were observed at room temperature, which seemed to be ascribed to oxygen vacancy in the ZnO films caused by diffusion of Li from the substrates into the films during the deposition.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Morphological defects in beta-barium borate (beta-BBO) thin films grown on Sr2+ -doped alpha-BBO substrates by liquid phase epitaxy (LPE) technique were studied by scanning electron micrograph (SEM), atomic force microscopy (AFM) and optical spectroscopy. The present results indicate that the main defects exit in beta-BBO thin films are microcracks and hollow structure. The formation of microcrack is due to the lattice mismatch and the difference of thermal expansion coefficients between substrate and film. The hollow structure might be caused during the combination of islands, which formed in the initial stage. (C) 2006 Elsevier GmbH. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Nonpolar a-plane (1120) ZnO thin films have been fabricated on gamma-LiAlO2 (302) substrates via the low-pressure metal-organic chemical vapor deposition. An obvious intensity variation of the E-2 mode in the Raman spectra indicates that there exhibits in-plane optical anisotropy in the a-plane ZnO thin films. Highly-oriented uniform grains of rectangular shape can be seen from the atomic force microscopy images, which mean that the lateral growth rate of the thin films is also anisotropic. It is demonstrated experimentally that a buffer layer deposited at a low temperature (200 degrees C) can improve the structural and optical properties of the epilayer to a large extent. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO/MgF2/ZnO sandwich structure films were fabricated. The effects of a buffer layer on structure and optical properties of ZnO films were investigated by X-ray diffraction, photoluminescence, optical transmittance and absorption measurements. Measurement results showed that the buffer layer had the effects of improving the quality of ZnO films and releasing the residual stresses in the films. The near-band edge emissions of ZnO films deposited on the MgF2 buffer layer were significantly enhanced compared with those deposited on bare substrate due to the smaller lattice mismatch between MgF2 and ZnO than that between fused silica and ZnO. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO/ITO/ZnO sandwich structure films were fabricated. The effects of buffer layer on the structure and optical properties of ZnO films were investigated by x-ray diffraction (XRD), photoluminescence, optical transmittance, and absorption measurements. XRD spectra indicate that a buffer layer has the effects of lowering the grain orientation of ZnO films and increasing the residual stresses in the films. The near-band-edge emissions of ZnO films deposited on both single indium tin oxide (ITO) buffer and ITO/ZnO double buffers are significantly enhanced compared with that deposited on a bare substrate due to the quantum confinement effect. (C) 2006 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Adhesion between the interface of pure silver thin film and three kinds of low refractive index coatings MgF2, Al2O3, SiO2 were compared in this article. The results indicated that the adhesion of Al2O3 and Ag was evidently superior to that of MgF2 and Ag, and the adhesion of MgF2 and Ag was evidently superior to that Of SiO2 and Ag. Reasons were analyzed accordingly. On the other hand, we compared the effect on the optical characteristic of Ag film when these three kinds of films were used as protective coatings and enhanced coatings. Considering the difference of the adhesion between Ag and MgF2, Al2O3, SiO2, suited uses are given for each other. © 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

TiO2 coatings are prepared on fused silica with conventional electron beam evaporation deposition. After annealed at different temperatures for four hours, the spectra and XRD patterns of TiO2 thin film are obtained. XRD patterns reveal that only anatase phase can be observed in TiO2 coatings regardless of the different annealing temperatures, and with the increasing annealing temperature, the grain size gradually increases. The relationship between the energy gap and microstructure of anatase is determined and discussed. The quantum confinement effect is observed that with the increasing grain size of TiO2 thin film, the band gap energy shifts from 3.4 eV to 3.21 eV. Moreover, other possible influence of the TiO2 thin-film microstructure, such as surface roughness and thin film absorption, on band gap energy is also expected.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of ZnO thin films were deposited on ZnO buffer layers by DC reactive magnetron sputtering. The buffer layer thickness determination of microstructure and optical properties of ZnO films was investigated by X-ray diffraction (XRD), photoluminescence (PL), optical transmittance and absorption measurements. XRD results revealed that the stress of ZnO thin films varied with the buffer layer thickness. With the increase of buffer layer thickness, the band gap edge shifted toward longer wavelength. The near-band-edge (NBE) emission intensity of ZnO films deposited on ZnO buffer layer also varied with the increase of thickness due to the spatial confinement increasing the Coulomb interaction between electrons and holes. The PL measurement showed that the optimum thickness of the ZnO buffer layer was around 12 nm. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZrO2 thin films were deposited bill using an electron beam evaporation technique on three kinds of lithium triborate (LiB3O5 or LBO) substrates with the surfaces at specified crystalline orientations. The influences of the LBO structure on the structural and optical properties of ZrO2 thin films are studied by spectrophotometer and x-ray diffraction. The results indicate that the substrate structure has obvious effects on the structural end optical properties of the film: namely. the ZrO2 thin film deposited on the X-LBO, Y-LBO and Z-LBO orients to m(-212), m(021) and o(130) directions. It is also found that the ZrO2 thin film with m(021) has the highest refractive index and the least lattice misfit.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The refractive indices of thin films, containing dielectric and voids in an oblique columnar structure, are, modelled in the quasi-static limit. The dielectric function is shown to be strongly dependent on the angle of incidence and on the columnar orientation for p-polarized light. This model is applied to model ZnS thin films with oblique columnar structures and the computed results have been given.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The refractive indices of thin films, containing dielectric and voids in an oblique columnar structure, are modeled by extended effective medium in the quasi-static limit. The dielectric function is shown to be strongly dependent on the angle of incidence and on the columnar orientation for p-polarized light. This model is applied to model ZrO2 thin films with oblique columnar structures and the computed results, with the Maxwell Garnett, the Bragg-Pippard, and the Bruggeman formalisms, have been given. (c) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel design for dielectric anisotropic mirrors with birefringent thin films for normal incidence is presented. This mirror consists of a stack of quarter-wave biaxial layers. The biaxial anisotropic layers can be fabricated by oblique deposition. The reflectance is different for two linear polarizations of light incidence on the mirrors. As a numerical example, the design is carried out on glass with TiO2 and ZrO2. These thin films could be applied to anisotropic reflective devices for lasers.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We prepare HfO2 thin films by electron beam evaporation technology. The samples are annealed in air after deposition. With increasing annealing temperature, it is found that the absorption of the samples decreases firstly and then increases. Also, the laser-induced damage threshold (LIDT) increases firstly and then decreases. When annealing temperature is 473K, the sample has the highest LIDT of 2.17J/cm(2), and the lowest absorption of 18 ppm. By investigating the optical and structural characteristics and their relations to LIDT, it is shown that the principal factor dominating the LIDT is absorption.