130 resultados para ELECTRON-ION COLLIDER
Resumo:
Semiconducting manganese silicide, Mn27Si47 and Mn15Si26, were obtained using mass-analyzed low energy dual ion beam epitaxy technique, Auger electron spectroscopy depth profiles showed that some of the Mn ions were deposited on single-crystal silicon substrate and formed a 37.5 nm thick Mn film, and the other Mn ions were successfully implanted into the Si substrate with the implantation depth of 618 nm. Some samples were annealed in the atmosphere of flowing N-2 at 840 degreesC. X-ray diffraction measurements showed that the annealing was beneficial to the formation of Mn27Si47 and Mn15Si26 (C) 2001 Published by Elsevier Science B.V.
Resumo:
Carbon films were deposited by mass-selected ion beam technique with ion energies 50-200eV at a substrate temperature from room temperature to 80 degreesC,. For the energies used, smooth diamond-like carbon films were deposited at room temperature. When the substrate temperature was 600 degreesC,rough graphitic films were produced. But highly oriented carbon tubes were observed when the energies were larger than 140eV at 800 degreesC. They were perpendicular to the surface and parallel to each other. preferred orientation of graphite basic plane was observed by high-resolution electron microscopy. Shallow ion implantation and stress are responsible for this orientation.
Resumo:
By mass-selected low energy ion beam deposition, amorphous carbon film was obtained. X-ray diffraction, Raman and Auger electron spectroscopy depth line shape measurements showed that such carbon films contained diamond particles. The main growth mechanism is subsurface implantation. Furthermore, it was indicated in a different way that ion bombardment played a decisive role in bias enhanced nucleation of chemical vapor deposition diamond.
Resumo:
Epitaxial cerium dioxide films on single-crystal silicon substrates (CeO2/Si) have been grown by a dual mass-analyzed low-energy ion beam deposition (IBD) system. By double-crystal X-ray diffraction (XRD), Full Width at Half Maximum (FWHM) are 23' and 33' in the rocking curves for (222) and (111) faces of the CeO2 film, respectively, and the lattice-mismatch Delta a/a with the substrate is about - 0.123%. The results show that the CeO2/Si grown by IBD is of high crystalline quality. In this work, the CeO2/Si heterostructure were investigated by X-ray Photoelectron Spectroscopy (XPS) and Auger Electron Spectroscopy (AES) measurements. Especially, XPS and AES depth profiling was used to analyze the compositions and structures in the interface regions of the as-grown and post-annealed CeO2/Si. It was found that there was no silicon oxide in the interface region of the as-grown sample but silicon oxide in the post-annealed sample. The reason for obtaining such high quality heterostructure mainly depends on the absence of silicon oxide in the surface at the beginning of the deposition. (C) 1998 Elsevier Science Ltd. All rights reserved.
Resumo:
Strain relaxation in the As ion implanted Si0.57Ge0.43 epilayers was studied by double-crystal x-ray diffractometry and transmission electron microscopy, and was compared to that in the nonimplanted Si0.57Ge0.43 epilayers. Experimental results show that after rapid thermal annealing (RTA) the x-ray linewidth of the As+-implanted Si0.57Ge0.43 epilayers is narrower than that of the nonimplanted epilayers, and than that of the partially relaxed as-grown samples, which is due primarily to low density of misfit dislocations in the As+-implanted SiGe epilayers. RTA at higher than 950 degrees C results in the formation of misfit dislocations for the nonimplanted structures, and of combinations of dislocations and precipitates (tentatively identified as GeAs) for the As+-implanted epilayers. The results mean that the strain relaxation mechanism of the As+-implanted Si1-xGex epilayers may be different from that of the nonimplanted Si1-xGex epilayers. (C) 1998 American Institute of Physics.
Resumo:
An anomalous behavior was observed in X-ray photoelectron Spectroscopy (XPS) depth profile measurements conducted on CeO2/Si epilayers grown by ion beam epitaxy (IBE): the signals of Ce3+ and Ce4+ co-exist, and the ratio between them increases during the etching time and then tends to maintain a constant level before increasing again. The results of X-ray Diffraction (XRD), Auger Electron Spectroscopy (AES), and Rutherford Back-Scattering (RES) measurements proved that the reduction chemical reaction of CeO2 is induced by ion-etching. (C) 1998 Elsevier Science Ltd. All rights reserved.
Resumo:
Fe-N films containing the Fe16N2 phase were prepared in a high-vacuum system of ion-beam-assisted deposition (IBAD). The composition and structure of the films were analysed by Auger electron spectroscopy (AES) and X-ray diffraction (XRD), respectively. Magnetic properties of the films were measured by a vibrating sample magnetometer (VSM). The phase composition of Fe-N films depend sensitively on the N/Fe atomic arrival ratio and the deposition temperature. An Fe16N2 film was deposited successfully on a GaAs (1 0 0) substrate by IBAD at a N/Fe atomic arrival ratio of 0.12. The gram-saturation magnetic moment of the Fe16N2 film obtained is 237 emu/g at room temperature, the possible cause has been analysed and discussed. Hysteresis loops of Fe16N2 have been measured, the coercive force H-c is about 120 Oe, which is much larger than the value for Fe, this means the Fe16N2 sample exhibits a large uniaxial magnetocrystalline anisotropy. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
Raman scattering measurements have been performed in diluted magnetic semiconductor Ga1-xMnxAs prepared by Mn-ion implantation, deposition, and post-annealing technique. It is found that the Raman spectrum measured from the implanted surface of the sample shows some new weak modes in addition to the GaAs-like modes which are observed from the unimplanted surface. The new vibrational modes observed are assigned to MnAs-like modes. The coupled LO-phonon plasmon mode, and Mn and As related vibrational modes caused by Mn-ion implantation, deposition, and post-annealing are also observed. Furthermore, the GaAs-like modes are found to be shifted by approximately 4 cm(-1) in the lower frequency side, compared with those observed from the unimplanted surface.
Resumo:
Direct ion beam deposition of carbon films on silicon in the ion energy range of 15-500 eV and temperature range of 25-800-degrees-C has been studied. The work was carried out using mass-separated C+ and CH3+ ions under ultrahigh vacuum. The films were characterized with x-ray photoelectron spectroscopy, Raman spectroscopy, transmission electron microscopy, and transmission electron diffraction analysis. In the initial stage of the deposition, carbon implanted into silicon induced the formation of silicon carbide, even at room temperature. Further carbon ion bombardment then led to the formation of a carbon film. The film properties were sensitive to the deposition temperature but not to the ion energy. Films deposited at room temperature consisted mainly of amorphous carbon. Deposition at a higher temperature, or post-deposition annealing, led to the formation of microcrystalline graphite. A deposition temperature above 800-degrees-C favored the formation of microcrystalline graphite with a preferred orientation in the (0001) direction. No evidence of diamond formation in these films was observed.
Resumo:
Thermally stimulated redistribution and precipitation of excess arsenic in Ge0.5Si0.5 alloy has been studied by X-ray photoelectron spectroscopy (XPS), cross sectional transmission electron microscopy (XTEM) and X-ray energy disperse spectrometry (EDS). Samples were prepared by the implantation of 6 X 10(6) As+ cm(-2) and 100 keV with subsequent thermal processing at 800 degrees C and 1000 degrees C for 1 h. The XPS depth profiles from the implanted samples before and after the thermal annealing indicate that there is marked redistribution of the elements in heavily arsenic-implanted Ge0.5Si0.5 alloys during the annealing, including: (1) diffusion of As from the implanted region to the surface; (2) aggregation of Ge in the vicinity of the surface. A high density of precipitates was observed near the surface which were by XTEM and EDS identified as an arsenide. It is suggested that most of the implanted As in Ge0.5Si0.5 alloy exists in the form of GeAs.
Resumo:
Medium energy (5-25 keV) C-13(+) ion implantation into diamond (100) to a fluence ranging from 10(16) cm(-2) to 10(18) cm(-2) was performed for the study of diamond growth via the approach of ion beam implantation. The samples were characterized with Rutherford backscattering/channelling spectroscopy, Raman spectroscopy, X-ray photoemission spectroscopy and Auger electron spectroscopy. Extended defects are formed in the cascade collision volume during bombardment at high temperatures. Carbon incorporation indeed induces a volume growth but the diamond (100) samples receiving a fluence of 4 x 10(17) to 2 x 10(18) at. cm(-2) (with a dose rate of 5 x 10(15) at. cm(-2) s(-1) at 5 to 25 keV and 800 degrees C) showed no He-ion channelling. Common to these samples is that the top surface layer of a few nanometers has a substantial amount of graphite which can be removed by chemical etching. The rest of the grown layer is polycrystalline diamond with a very high density of extended defects.
Resumo:
The paper reports a method of depositing SiO2, SiNx, a:Si, Si3N4 and SiOxNy dielectric thin films by electron cyclotron resonance plasma chemical vapor deposition (ECR CVD) on InP, InGaAs and other compound semiconductor optoelectronic devices,and give a technology of depositing dielectric thin films and optical coatings by ECR CVD on Laser's Bars. The experiment results show the dielectric thin films and optical coatings are stable at thermomechanical property,optical properties and the other properties. In addition, the dielectric thin film deposition that there is low leakage current is reported for using as diffusion and ion implatation masks in the paper. In the finally, the dielectric film refractive index can be accurately controlled by the N-2/O-2/Ar gas flow rate.
Resumo:
Fe-N films containing the Fe16N2 phase were prepared in a high-vacuum system of ion-beam-assisted deposition (IBAD). The composition and structure of the films were analysed by Auger electron spectroscopy (AES) and X-ray diffraction (XRD), respectively. Magnetic properties of the films were measured by a vibrating sample magnetometer (VSM). The phase composition of Fe-N films depend sensitively on the N/Fe atomic arrival ratio and the deposition temperature. An Fe16N2 film was deposited successfully on a GaAs (1 0 0) substrate by IBAD at a N/Fe atomic arrival ratio of 0.12. The gram-saturation magnetic moment of the Fe16N2 film obtained is 237 emu/g at room temperature, the possible cause has been analysed and discussed. Hysteresis loops of Fe16N2 have been measured, the coercive force H-c is about 120 Oe, which is much larger than the value for Fe, this means the Fe16N2 sample exhibits a large uniaxial magnetocrystalline anisotropy. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
In this paper, we present results of the synthesis of gold nanoclusters in sapphire, using Ar ion implantation and annealing in air. Unlike the conventional method of Au implantation followed by thermal annealing, Au was deposited on the surface of m- and a- cut sapphire single crystal samples including those pre-implanted with Ar ions. Au atoms were brought into the substrate by subsequent implantation of Ar ions to form Au nanoparticles. Samples were finally annealed stepwisely in air at temperatures ranging from 400 to 800 C and then studied using UV–vis absorption spectrometry, transmission electron microscopy and Rutherford backscattered spectrometry. Evidence of the formation Au nanoparticles...