221 resultados para Growth and survival
Resumo:
For the first time, a high optical quality Yb3+-doped lutetium pyrosilicate laser crystal Lu2Si2O7 (LPS) was grown by the Czochralski (Cz) method. The segregation coefficient of ytterbium ion in Yb:LPS crystal detected by the inductively coupled plasma atomic emission spectrometer (TCP-AES) method is equal to 0.847. X-ray powder diffraction result confirms the C2/m phase monoclinic space group of the grown crystal and the peaks corresponding to different phases were indexed. The absorption and fluorescence spectra, as well as fluorescence decay lifetime of Yb3+ ion in LPS have been investigated. The absorption and fluorescence cross-sections of the transitions F-2(7/2) <-> F-2(5/2) of Yb3+ ion in LPS crystal have been determined. The advantages of the Yb:LPS crystal including high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections (1.33 x 10(-2) cm(2)) and particularly broad emission bandwidth (similar to 62 nm) indicated that the Yb:LPS crystal seemed to be a promising candidate used as compact, efficient thin chip lasers when LD is pumped at 940 and 980 nm due to its low-symmetry monoclinic structure and single crystallographic site. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
In this paper, single crystal of ytterbium (Yb) doped Ca-5(PO4)(3)F (FAP) has been grown along the c-axis by using the Czochralski method. The segregation coefficients of Yb3+ in the Yb:FAP crystal has been determined by ICP-AES method. The absorption spectrum, fluorescence spectrum and fluorescence lifetime of the Yb:FAP crystal has been also measured at room temperature. In the absorption spectra, there are two absorption bands at 904 and 982 nm, respectively, which are suitable for InGaAs diode laser pumping. The absorption cross-section (sigma(abs)) is 5.117 x 10(-20) cm(2) with an FWHM of 4 nm at 982 nm. The emission cross-section is (sigma(em)) 3.678 x 10(-20) cm(2) at 1042 nm. Favorable values of the absorption cross-section at about 982 nm are promising candidates for laser diode (LD) pumping. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
ZnO crystals with dimensions of 30 x 38 x 8 turn 3 have been grown by the hydrothermal method using a mixed solution of KOH, LiOH and H2O2. The growing rates for +c(0001) and -c(000 (1) over bar) were 0.17 and 0.09 mm/day, respectively. The crystal color was very light green for +c sector and dark brown for -c sector. For the +c sector, the resistivity at room temperature was 80 0 cm, the carrier concentration was about 10(4)/cm(3), and the mobility was about 100 cm(2)/Vs. The full-width at half-maximum (FWHM) of double axis X-ray rocking curve for the polished Zn face cut from +c sector was 45 arcsec. The photoluminescence (PL) spectrum and the absorption spectrum of +c part of the crystals at room temperature were also reported and discussed in this paper. (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
g-LiAlO2 single crystal is a promising substrate for GaN heteroepitaxy. In this paper, we present the growth of large-sized LiAlO2 crystal by modified Czochralski method. The crystal quality was characterized by high-resolution X-ray diffraction and chemical etching. The results show that the as-grown crystal has perfect quality with the full width at half maximum (FWHM) of 17.7-22.6 arcsec and etch pits density of (0.3-2.2) x 10(4) cm(-2) throughout the crystal boule. The bottom of the crystal boule shows the best quality. The optical transmission spectra from UV to IR exhibits that the crystal is transparent from 0.2 to 5.5 mu m and becomes completely absorbing around 6.7 mu m wavelength. The optical absorption edge in near UV region is about 191 nm.
Resumo:
ZnO films were fabricated on LiGaO2 (0 0 1), (10 0) and (0 10) planes by RF magnetron sputtering. The structural, morphological and optical properties of as-grown ZnO films were investigated by X-ray diffraction (XRD), atomic force microscopy (AFM), Raman spectra and photoluminescence (PL) spectra. It is found that the orientation of ZnO films is strongly dependent on the substrate plane. [0 0 0 11, [1 (1) over bar 00] and [11 (2) over bar0] oriented ZnO films are deposited on LiGaO2 (001), (100) and (010), respectively. AFM shows the (0001) ZnO film consists of well-aligned regular hexagonal grains. Raman spectra reveal a tensile stress in the (0 0 0 1) ZnO film and a compressive stress in (110 0) and (112 0) ZnO films. PL spectra of all ZnO films exhibit only a near-band-edge UV emission peak. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Er3+ -doped Gd2SiO5 (Er:GSO) single crystal with dimensions of circle divide 35 x 40 mm(3) has been grown by the Czochralski method. The absorption and fluorescence spectra of the Er:GSO crystal were measured at room temperature. The spectral parameters were calculated based on Judd-Ofelt theory, and the intensity parameters Omega(2), Omega(4) and Omega 6 are obtained to be 6.168 x 10(-20), 1.878 x 10(-20), and 1.255 x 10(-20) cm(2), respectively. The emission cross-section has been calculated by Fuechtbauer-Ladenbury formula. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
The YAG crystal codoped with Yb3+ and Tm3+ has been grown by Czochralski (Cz) method. The crystal structure of the crystal has been determined by X-ray diffraction analysis. The absorption and emission spectra of Yb,Tm:YAG crystal at room temperature have also been studied. The emission cross-sections have been calculated by Fuechtbauer-Ladenburg formula and reciprocity method. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
A bulk crystal of Yb:Sc2SiO5 (Yb:SSO) with favorable thermal properties was successfully obtained by the Czochralski method. The energy level diagrams for Yb:SSO crystal were determined by optical spectroscopic analysis and semi-empirical crystal-field calculations using the simple overlap model. The full width at half maximum of the absorption band centering at 976 nm was calculated to be 24 nm with a peak absorption cross-section of 9.2x10(-21) cm(2). The largest ground-state splitting of Yb3+ ions is up to 1027 cm(-1) in a SSO crystal host. Efficient diode-pumped laser performance of Yb:SSO was primarily demonstrated with a slope efficiency of 45% and output power of 3.55 W.
Resumo:
The 2 at.% Sm:GdVO4 crystal was grown by the Czochralski method. The segregation coefficient of Sm3+ ion in this crystal is 0.98. The crystal structure of the Sm:GdVO4 crystal was determined by X-ray diffraction analysis. Judd-Ofelt theory was used to calculate the intensity parameters (Omega(i)), the spontaneous emission probability, the luminary branching ratio and the radiative lifetime of the state (4)G(5/2). The stimulated emission cross-sections at 567, 604 and 646 nm are calculated to be 5.92 x 10(-21), 7.62 x 10(-21) and 5.88 x 10(-21) cm(2), respectively. The emission cross-section at 604 nm is 4.4 times lager than that in Sm: YAP at 607 nm. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Mg0.4Al2.4O4 single crystals with good optical quality were successfully grown by the Czochralski method. The transmission spectrum indicated that the absorption edge of the crystal was at 220nm, while no apparent absorption peaks were found. The X-ray diffraction and DSC curve analysis showed that Mg0.4Al2.4O4 crystal was stable at room temperature. While after annealing in the air and hydrogen atmosphere at about 1200 degrees C,Mg0.4Al2.4O4 decomposed into Al2O3 and (MgO)(0.4)(Al2O3)(x) (0.4 < x < 1.2). The reaction mainly occurred on the crystal surface, barely inside. (C) 2008 Elsevier B.V. All rights reserved.