475 resultados para quantum dot lasers


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The turn-on delay time jitter of four different unbiased gain-switched laser types is determined by measuring the temporal probability distribution of the leading edge of the emitted optical pulse. One single-mode 1.5-mu-m distributed feed-back laser and three multimode Fabry-Perot lasers emitting at 750 nm and 1.3-mu-m are investigated. The jitter is found to decrease for all lasers with increasing injection current. For multimode lasers it decreases from 8 ps excited slightly above threshold down to below 2 ps at three times the threshold current. The jitter of the distributed feedback (DFB) laser is a factor of 3-5 larger than the jitter of the three multimode lasers. A new model to predict the turn-on delay time jitter is presented and explains the experiments quantitatively.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A very low CW threshold current of 1.65 mA at room temperature was obtained for an uncoated buried-heterostructure strained layer multiquantum well InGaAs-GaAs laser fabricated using hybrid molecular beam epitaxy and liquid phase epitaxy crystal growth technique. External differential quantum efficiency as high as 44.6% (0.53 mW/mA) and output power of more than 30 mW per facet were achieved in the same laser.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A GaAs/GaAlAs graded-index separate confinement single quantum well heterostructure single-mode ridge waveguide electroabsorption modulator was fabricated and investigated. For the modulator with a quantum well width of 100 angstrom and device length of 700-mu-m, an on/off ratio of 29.7 dB and estimated absorption insertion loss of 3 dB were obtained for TE polarised light with wavelength 8650 angstrom, and for TM polarisation the on/off ratio was 28.5 dB. With a switching voltage of 1 V, an on/off ratio of 15 dB was achieved. Photocurrent spectra exhibited a red shift of 600 angstrom of the absorption edge when the voltage applied to the PIN diode was varied from 0.5 to -7 V. The corresponding shift of the room temperature exciton peak energy was 96 meV.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

High-quality compressively strained In0.63Ga0.37As/InP quantum wells with different well widths (1-11 nm) have been grown coherently on InP substrates using a home-made gas source molecular beam epitaxy (GSMBE) system. The indium composition in the wells of the sample was determined by means of high-resolution X-ray diffraction and its computer simulation. it is found that the exciton transition energies determined by photoluminescence (PL) at 10 K are in good agreement with those calculated using a deformation potential model. Sharp and intense peaks for each well can be well resolved in the 10 K PL spectra. For wells narrower than 4 nm, the line width of the PL peaks are smaller than the theoretical values of the line-width broadening due to 1 hit interface fluctuation, showing that the interface fluctuation of our sample is within 1 ML. For wells of 7 and 9 nm, the PL peak widths are as low as 4.5 meV.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Low-temperature photoluminescence and excitation spectra from InAs monolayer quantum structures, grown on (311)A, (311)B, and (100) GaAs substrates, are investigated, The structures were grown simultaneously by conventional molecular-beam epitaxy (MBE), The experimental results show that the quality of InAs monolayer on (311)B GaAs substrate is obviously better in crystal quality than those on the two other oriented GaAs substrates. In addition, the transition peaks of the InAs layer grown on (311) GaAs substrates shift to higher energy with respect to that from the InAs layer grown on (100) GaAs substrate.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The valence hole subbands, TE and TM mode optical gains, transparency carrier density, and radiative current density of the zinc-blende GaN/Ga0.85Al0.15N strained quantum well (100 Angstrom well width) have been investigated using a 6 X 6 Hamiltonian model including the heavy hole, Light hole, and spin-orbit split-off bands. At the k = 0 point, it is found that the light hole strongly couples with the spin-orbit split-off hole, resulting in the so+lh hybrid states. The heavy hole does not couple with the light hole and the spin-orbit split-off hole. Optical transitions between the valence subbands and the conduction subbands obey the Delta n=0 selection rule. At the k not equal 0 points, there is strong band mixing among the heavy hole, light hole, and spin-orbit split-off hole. The optical transitions do not obey the Delta n=0 selection rule. The compressive strain in the GaN well region increases the energy separation between the so1+lh1 energy level and the hh1 energy level. Consequently, the compressive strain enhances the TE mode optical gain, and strongly depresses the TM mode optical gain. Even when the carrier density is as large as 10(19) cm(-3), there is no positive TM mode optical gain. The TE mode optical gain spectrum has a peak at around 3.26 eV. The transparency carrier density is 6.5 X 10(18) cm(-3), which is larger than that of GaAs quantum well. The compressive strain overall reduces the transparency carrier density. The J(rad) is 0.53 kA/cm(2) for the zero optical gain. The results obtained in this work will be useful in designing quantum well GaN laser diodes and detectors. (C) 1996 American Institute of Physics.