626 resultados para Crystal Growth, Purple Bronze, Low Dimensionality, Superconductivity
Resumo:
The effect of ion-induced damage on GaNAs/GaAs quantum wells (QWs) grown by molecular beam epitaxy employing a DC plasma as the N source was investigated. Ion-induced damage results in: (i) an observed disappearance of pendellosung fringes in the X-ray diffraction pattern of the sample; (ii) a drastic decrease in intensity and a broadening in the full-width at half-maximum of photoluminescence spectra. It was shown that ion-induced damage strongly affected the bandedge potential fluctuations of the QWs. The bandedge potential fluctuations for the samples grown with and without ion removal magnets (IRMs) are 44 and 63 meV, respectively. It was found that the N-As atomic interdiffusion at the interfaces of the QWs was enhanced by the ion damage-induced defects. The estimated activation energies of the N-As atomic interdiffusion for the samples grown with and without IRMs are 3.34 and 1.78 eV, respectively. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
The effects of in situ annealing treatment in the initial growth stage and In-doping during growth of the GaN on the material properties were investigated. GaN was grown by LP-MOVPE. In situ annealing reduced the full-width at half-maximum (FWHM) of X-ray rocking curves and reduced etch pit density of GaN films. It improved the optical properties of the epilayer. Undoped and In-doped GaN films of initial growth stage were investigated. It was found that morphology and optical properties were improved in In-doped samples. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Quantum cascade (QC) lasers based on strain-compensated InxGa(1-x)As/InyAl(1-y)As grown on InP substrate using molecular beam epitaxy is reported. The epitaxial quality is demonstrated by the abundant narrow satellite peaks of double-crystal X-ray diffraction and cross-section transmission electron microscopy of the QC laser wafer. Laser action in quasi-continuous wave operation is achieved at lambda approximate to 3.6-3.7 mum at room temperature (34 degreesC) for 20 mum x 1.6 mm devices, with peak output powers of similar to 10.6mW and threshold current density of 2.7kA/cm(2) at this temperature. (C) 2000 Published by Elsevier Science B.V.
Resumo:
We have studied the effects of postgrowth rapid thermal annealing on the optical properties of 3-nm-height InAs/GaAs quantum dots covered by 3-nm-thick InxGa1-xAs (x = 0, 0.1, and 0.2) overgrowth layer. At higher annealing temperature (T greater than or equal to 750 degreesC), the photoluminescence peak of InGaAs layer has been observed at lower-energy side of the InAs quantum-dot peak. In addition, the blueshift in photoluminescence (PL) emission energy is found to he similar for all samples with increasing the annealing temperature from 650 to 850 degreesC. However, the trend of narrowing of photoluminescence linewidth is significantly different for InAs quantum dots with different In mole fractions in InGaAs overgrowth layer. These results suggest that the intermixing in the lateral direction plays an important role in helping to understand the modification of optical properties induced by rapid thermal annealing. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Strained InAs nanostructures have been grown by solid-source molecular beam epitaxy in In0.52Al0.48As matrix on different InP substrate surfaces ((0 0 1) and (1 1 n)A/B (n = 1 - 5)). The morphology of the nanostructures was characterized using atomic force microscopy (AFM). The AFM results reveal interesting differences in the size, shape, and alignment of the nanostructures between different oriented surfaces. It was found that some faceted nanostructures tend to form on A-type surfaces, the shape and the alignment of these nanostructures show clear dependence on the substrate orientation. Samples grown on (0 0 1) and B-type surfaces showed preferentially dense round dots. Dots formed on (1 1 3)B, (1 1 3)B and (1 1 5)B surfaces have a higher dot density and size homogeneity, which shows a potential for the production of high-quality and customized self-assembled quantum dots for photonics applications. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Self-assembled InAs nanostructures on (0 0 1)InP substrate have been grown by molecular beam epitaxy (MBE) and evaluated by transmission electron microscopy (TEM) and photoluminescence (PL). It is found that the morphologies of InAs nanostructures depend strongly on the underlying alloy. Through introducing a lattice-matched underlying InAlGaAs layer on InAlAs buffer layer, the InAs quantum dots (QDs) can be much more uniform in size and great improvement in PL properties can be attained at the same time. In particular, 1.55 mu m luminescence at room temperature (RT) can be realized in InAs QDs deposited on (0 0 1)InP substrate with underlying InAlGaAs layer. (C) 2000 Published by Elsevier Science B.V. All rights reserved.
Resumo:
Self-assembled InAs quantum dots (QDs) in InAlAs grown on (001) and (311)B InP substrates by molecular beam epitaxy (MBE) have been comparatively investigated. A correlated study of atomic force microscopy (AFM) and photoluminescence (PL) disclosed that InAs QDs grown on high-index InP substrates can lead to high density and uniformity. By introducing a lattice-matched InAlGaAs overlayer on InAlAs buffer, still more dense and uniform InAs QDs were obtained in comparison with InAs QDs formed with only InAlAs matrix. Moreover, two-dimensional well-ordered InAs dots with regular shape grown on (311)B InP substrates are reported for the first time. We explained this exceptional phenomenon from strain energy combined with kinetics point of view. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Self-assembled InAs quantum wires (QWRs) embedded in In0.52Al0.48As, In0.53Ga0.47As, and (In0.52Al0.48As)(n)/(In0.53Ga0.47As)(m)-short-period-lattice matrices on InP(001) were fabricated with molecular beam epitaxy (MBE). These QWR lines are along [110], x 4 direction in the 2 x 4 reconstructed (001) surface as revealed with reflection high-energy electron diffraction (RHEED). Alignment of quantum wires in different layers in the InAs/spacer multilayer structures depends on the composition of spacer layers. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Interdigital metal-semiconductor-metal (MSM) ultraviolet photoconductive detectors have been fabricated on undoped GaN films grown by molecular beam epitaxy (MBE), Response dependence on wavelength, applied current, excitation powers and chopper frequency has been extensively investigated. It is shown that the photodetector's spectral response remained nearly constant for wavelengths above the band gap and dropped sharply by almost three orders of magnitude for wavelengths longer than the band gap. It increases linearly with the applied constant current, but very nonlinearly with illuminating power. The photodetectors showed high photoconductor gains resulting from trapping of minority carriers (holes) at acceptor impurities or defects. The results demonstrated the high quality of the GaN crystal used to fabricate these devices. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Deep levels in undoped GaN materials grown by modified molecular beam epitaxy (MBE) are investigated by photoluminescence (PL) and optical quenching of photoconductivity measurements. A broad band which extends from 2.1 to 3.0 eV with a maximum at about 2.7 eV is observed, and four prominent quenching bands were found located at 2.18, 2.40, 2.71, and 2.78 eV above the valence band, respectively. These levels are attributed to four holes trap levels existence in the material. The defects cannot be firmly identified at present. (C) 2000 Elsevier Science B.V, All rights reserved.
Resumo:
Al-related DX-like centers were observed in n-type Al-doped ZnS1-xTex epilayers grown by molecular-beam epitaxy on GaAs substrates. The capacitance-voltage measurement, deep-level transient spectroscopy, and photoconductivity spectroscopy revealed that the behaviors of Al donors in ZnS1-xTex were similar to the so-called DX centers in AlxGa1-xAs. The optical ionization energies (E-i) and emission barriers (E-e) for the observed two Al-related DX-like centers were determined as E-i similar to 1.0 and 2.0cV and E-e similar to 0.21 and 0.39 eV, respectively. It was also shown that the formation of Al-related DX-like centers resulted in a significantly large lattice relaxation in ZnS1-xTex. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Swirl defects in dislocation-free Czochralski (CZ) silicon crystals have been investigated by preferential etching, transmission electron microscopy (TER I) and electron energy loss spectroscopy (EELS) mode of a scanning transmission electron microscope (STEM). Two kinds of Swirl defects have been found with a good correspondence between striated pattern consisting of hillocks and the buried micro-defects. The Swirl defects were identified as perfect dislocation loop cluster and tetrahedral precipitate, respectively. In addition, a kind of tiny micro-defects is found to be distributed preferentially in the vicinity of the Swirl pattern although there is no detectable correspondence between hillocks and the micro-defects. The energy-filtered images have been obtained by the plasma peaks at different parts of a coherent precipitate with the Si matrix. The experimental results show some indications of the existence of oxygen and carbon in the core of the precipitate and suggest that oxygen and carbon may play important roles in the formation of Swirl defect. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
The effects of gravity and crystal orientation on the dissolution of GaSb into InSb melt and the recrystallization of InGaSb were investigated under microgravity condition using a Chinese recoverable satellite and under normal gravity condition on earth. To investigate the effect of gravity on the solid/liquid interface and compositional profiles. a numerical simulation was carried out. The InSb crystal melted at 525 degrees C and then a part of GaSb dissolved into the InSb melt during heating to 706 degrees C and this process led to the formation of InGaSb solution. InGaSb solidified during the cooling process. The experimental and calculation results clearly show that the shape of the solid/liquid interface and compositional profiles in the solution were significantly affected by gravity. Under microgravity, as the Ga compositional profiles were uniform in the radial direction. the interfaces were almost parallel. On the contrary, for normal gravity condition, as large amounts of Ga moved up in the upper region due to buoyancy, the dissolved zone broadened towards gravitational direction. Also. during the cooling process, needle crystals of InGaSb started appearing and the value of x of InxGa1-xSb crystals increased with the decrease of temperature. The GaSb with the (111)B plane dissolved into the InSb melt much more than that of the (111)A plane. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
We have studied the optical and structural properties of InAs/GaAs QDs covered by InxGa1-xAs (0 less than or equal to x less than or equal to 0.3) layer using transmission electron microscopy, photoluminescence (PL) spectra and atomic force microscopy. We find that the strain reduces in the growth direction of InAs islands covered by InGaAs instead of GaAs layer. Significant redshift of PL peak energy and narrowing of PL linewidth are observed for the InAs QDs covered by 3 nm thick InGaAs layer. In addition, atomic force microscopy measurements indicate that the InGaAs islands will nucleate on top of InAs quantum dots, when 3 nm In0.3Ga0.7As overgrowth layer is deposited. This result can well explain the PL intensify degradation and linewidth increment of quantum dots with a higher In-mole-fraction InGaAs layer. The energy gap change of InAs QDs covered by InGaAs may be explained in terms of reducing strain, suppressing compositional mixing and increasing island height. (C) 2000 Elsevier Science B.V. All rights reserved.