InGaN based light emitting devices (LEDs) with asymmetric coupled quantum wells (AS-QWs) and conventional symmetric coupled quantum wells (CS-QWs) active structures were grown by metal-organic chemical vapor deposition technique. The LEDs with AS-QWs active region show improved light emission intensity and reduced forward voltage compared with LEDs with CS-QWs active region. Based on the electroluminescence measurements and the devices structure analysis, it can be concluded that these improvements are mainly attributed to the efficient hole tunneling through barriers and consequently the uniform distribution of carriers in the AS-QWs. (C) 2009 American Institute of Physics. [doi: 10.1063/1.3254232]

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We have demonstrated a passively mode-locked diode end-pumped all-solid-state laser, which is composed of a Nd:Gd0.5Y0.5VO4 crystal and a folded cavity with a semiconductor saturable-absorber mirror grown by metal-organic chemical-vapor deposition. Stable cw mode locking with a 3.8-ps pulse duration at a repetition rate of 112 MHz was obtained. At 13.6 W of the incident pump power, a clean mode-locked fundamental-mode average output power of 3.9 W was achieved with an overall optical-to-optical efficiency of 29.0%, and the slope efficiency was 38.1%. (C) 2004 Optical Society of America.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Raman measurements and photoluminescence (PL) were performed on the metal-organic chemical-vapor deposition epitaxially grown GaN before and after the implantation with Er and Er+O. Several Raman defect modes have emerged from the implantation-damaged samples. The structures around 300 and 595 cm(-1) modes are attributed to the disorder-activated Raman scattering, whereas the 670 cm(-1) peak is assigned to nitrogen-vacancy-related defect scattering. One additional peak at 360 cm(-1) arises after Er+O coimplantation. This Raman peak is attributed to the O-implantation-induced defect complex. The appearance of the 360 cm(-1) mode results in the decrease of the Er3+ -related infrared PL intensity for the GaN:Er+O samples. (C) 2004 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The relaxation of the misfit strain by the formation of misfit dislocations in InxGa1-xN/GaN multiple quantum wells grown by metal-organic chemical-vapor deposition was investigated by the cross-sectional transmission electron microscopy, double crystal x-ray diffraction, and temperature-dependent photoluminescence. It is found that the misfit dislocations generated from strain relaxation are all pure-edge threading dislocations with burgers vectors of b=1/3<11 (2) over bar0>. The misfit dislocations arise from the strain relaxation due to the thickness of strained layer greater than the critical thickness. The relaxation of strained layer was mainly achieved by the formation of dislocations and localization of In, while the dislocations changed their slip planes from {0001} to {10 (1) over bar0}. With the increasing temperature, the efficiency of photoluminescence decrease sharply. It indicates that the relaxation of the misfit strain has a strong effect on optical efficiency of film. (C) 2004 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The strain state of 570nm AlXGa1-xN layers grown on 600nm GaN template by metal organic chemical vapor deposition was studied using Rutherford backscattering (RBS)/channeling and triple-axis X-ray diffraction measurements. The results showed that the degree of relaxation (R) of AlxGa1-xN layers increased almost linearly when x less than or equal to 0.42 and reached to 70% when x = 0.42. Above 0.42, the value of R varied slowly and AI(x)Ga(1-x)N layers almost full relaxed when x = 1 (AIN). In this work the underlying GaN layer was in compressive strain, which resulted in the reduction of lattice misfit between GaN and AlxGa1-xN, and a 570nm AlxGa1-xN layer with the composition of about 0.16 might be grown on GaN coherently from the extrapolation. The different shape of (0004) diffraction peak was discussed to be related to the relaxation. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Hydrogenated amorphous silicon-carbon (a-SiC:H) films were deposited by plasma enhanced chemical vapor deposition (PECVD) with a fixed methane to silane ratio ([CH4]/[SiH4]) of 1.2 and a wide range of hydrogen dilution (R-H=[H-2]/[SiH4 + CH4]) values of 12, 22, 33, 102 and 135. The impacts of RH on the structural and optical properties of the films were investigated by using UV-VIS transmission, Fourier transform infrared (FTIR) absorption, Raman scattering and photoluminescence (PL) measurements. The effects of high temperature annealing on the films were also probed. It is found that with increasing hydrogen dilution, the optical band gap increases, and the PL peak blueshifts from similar to1.43 to 1.62 eV. In annealed state, the room temperature PL peak for the low R-H samples disappears, while the PL peak for the high R-H samples appears at similar to 2.08 eV, which is attributed to nanocrystalline Si particles confined by Si-C and Si-O bonds.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of silicon film samples were prepared by plasma enhanced chemical vapor deposition (PECVD) near the threshold from amorphous to nanocrystalline state by adjusting the plasma parameters and properly increasing the reactions between the hydrogen plasma and the growing surface. The microstucture of the films was studied by micro-Raman and Fourier transform infrared (FTIR) spectroscopy. The influences of the hydrogen dilution ratio of silane (R-H = [H-2]/[SiH4]) and the substrate temperature (T-s) on the microstructural and photoelectronic properties of silicon films were investigated in detail. With the increase of RH from 10 to 100, a notable improvement in the medium-range order (MRO) of the films was observed, and then the phase transition from amorphous to nanocrystalline phase occurred, which lead to the formation of diatomic hydrogen complex, H-2* and their congeries. With the increase of T-s from 150 to 275 degreesC, both the short-range order and the medium range order of the silicon films are obviously improved. The photoconductivity spectra and the light induced changes of the films show that the diphasic nc-Si/a-Si:H films with fine medium-range order present a broader light spectral response range in the longer wavelength and a lower degradation upon illumination than conventional a-Si:H films. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polycrystalline GaN thin films have been deposited epitaxially on a ZnO-buffered (111)-oriented Si substrate by molecular beam epitaxy. The microstructural and compositional characteristics of the films were studied by analytical transmission electron microscopy (TEM). A SiO2 amorphous layer about 3.5 nm in thickness between the Si/ZnO interface has been identified by means of spatially resolved electron energy loss spectroscopy. Cross-sectional and plan-view TEM investigations reveal (GaN/ZnO/SiO2/Si) layers exhibiting definite a crystallographic relationship: [111](Si)//[111](ZnO)//[0001](GaN) along the epitaxy direction. GaN films are polycrystalline with nanoscale grains (similar to100 nm in size) grown along [0001] direction with about 20degrees between the (1 (1) over bar 00) planes of adjacent grains. A three-dimensional growth mode for the buffer layer and the film is proposed to explain the formation of the as-grown polycrystalline GaN films and the functionality of the buffer layer. (C) 2004 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Preferred growth of nanocrystalline silicon (nc-Si) was first found in boron-doped hydrogenated nanocrystalline (nc-Si:H) films prepared using plasma-enhanced chemical vapor deposition system. The films were characterized by high-resolution transmission electron microscope, X-ray diffraction (XRD) spectrum and Raman Scattering spectrum. The results showed that the diffraction peaks in XRD spectrum were at 2theta approximate to 47degrees and the exponent of crystalline plane of nc-Si in the film was (220). A considerable reason was electric field derived from dc bias made the bonds of Si-Si array according to a certain orient. The size and crystalline volume fraction of nc-Si in boron-doped films were intensively depended on the deposited parameters: diborane (B2H6) doping ratio in silane (SiH4), silane dilution ratio in hydrogen (H-2), rf power density, substrate's temperature and reactive pressure, respectively. But preferred growth of nc-Si in the boron-doped nc-Si:H films cannot be obtained by changing these parameters. (C) 2004 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Raman scattering and photoluminescence (PL) of boron-doped silicon nanowires have been investigated. Raman spectra showed a band at 480 cm(-1), indicating that the crystallinity of the nanowires was suppressed by boron doping. PL taken from B-doped SiNWS at room temperature exhibited three distinct emission peaks at 1.34, 1.42. and 1.47 eV and the PL intensity was much stronger than that of undoped SiNWS. The increased PL intensity should be very profitable for nano-optoelectronics. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The hydrogen dilution profiling (HDP) technique has been developed to improve the quality and the crystalline uniformity in the growth direction of mu c-Si:H thin films prepared by hot-wire chemical-vapor deposition. The high H dilution in the initial growth stage reduces the amorphous transition layer from 30-50 to less than 10 nm. The uniformity of crystalline content X-c in the growth direction was much improved by the proper design of hydrogen dilution profiling which effectively controls the nonuniform transition region of Xc from 300 to less than 30 nm. Furthermore, the HDP approach restrains the formation of microvoids in mu c-Si: H thin films with a high Xc and enhances the compactness of the film. As a result the stability of mu c-Si: H thin films by HDP against the oxygen diffusion, as well as the electrical property, is much improved. (c) 2005 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The influences of a high-temperature (HT) AlN interlayer (IL) on the phase separation in crack-free AlGaN grown on GaN have been studied. The depth-dependent cathodoluminescence (CL) spectra indicate a relatively uniform Al distribution in the growth direction, but the monochromatic CL images and the CL spectra obtained by line scan measurements reveal a lateral phase separation in AlGaN grown on relatively thick HT-AlN ILs. Moreover, when increasing the thickness of HT-AlN IL, the domain-like distribution of the AlN mole fraction in AlGaN layers is significantly enhanced through a great reduction of the domain size. The morphology of mesa-like small islands separated by V trenches in the HT-AlN IL, and the grain template formed by the coalescence of these islands during the subsequent AlGaN lateral overgrowth, are attributed to be responsible for the formation of domain-like structures in the AlGaN layer. (c) 2005 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of hydrogenated silicon films near the threshold of crystallinity was prepared by very high frequency plasma enhanced chemical vapor deposition (VHF-PECVD) from a mixture of SiH4 diluted in H, The effect of hydrogen dilution ratios R-H = [H-2]/[SiH4] on microstructure of the films was investigated. Photoelectronic properties and stability of the films were studied as a function of crystalline fraction. The results show that more the crystalline volume fraction in the silicon films, the higher mobility life-time product (mu tau), better the stability and lower the photosensitivity. Those diphasic films contained 8%-31% crystalline volume fraction can gain both the fine photoelectronic properties and high stability. in the diphasic (contained 12% crystalline volume fraction) solar cell, we obtained a much lower light-induced degradation of similar to 2.9%, with a high initial efficiency of 10.01% and a stabilized efficiency of 9.72% (AM1.5, 100 mW/cm(2)). (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We have demonstrated stable self-starting passive mode locking in a diode-end-pumped Nd:Gd-0.8-Y0.5VO4 laser by using an In0.25Ga0.75As absorber grown at low temperature (LT In0.25Ga0.75As absorber). An In0.25Ga0.75As single-quantum-well absorber, which was grown directly on the GaAs buffer by use of the metal-organic chemical-vapor deposition technique, acts simultaneously as a passive mode-locking device and as an output coupler. Continuous-wave mode-locked pulses were obtained at 1063.5 nm. We achieved a pulse duration of 2.6 ps and an average output power of 2.15 W at a repetition rate of 96.4 MHz. (c) 2005 Optical Society of America.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of hydrogenated silicon films near the threshold of crystallinity was prepared by very high frequency plasmaenhanced chemical vapor deposition (VHF-PECVD)from a mixture of SiH4 diluted in H-2. The effect of hydrogen dilution ratios R = [H-2]/[SiH4] on the microstructure of the films was investigated. The photoelectronic properties and stability of the films were studied as a function of crystalline fraction. The results show that the diphasic films gain both the fine photoelectric properties like a-Si: H and high stability like mu w-Si:H. By using the diphasic silicon films as the intrinsic layer, p-i-n junction solar cells were prepared. Current-voltage (J-V) characteristics and stability of the solar cells were measured under an AM1.5 solar simulator. We observed a light-induced increase of 5.2% in the open-circuit voltage (V-oc) and a light-induced degradation of similar to 2.9% inefficiency.