A high-power Ytterbium-doped fiber laser (YDFL) with homemade double clad fiber (DCF) is introduced in this paper. The output power characteristics of a linear cavity fiber laser have been studied theoretically by solving the rate equations and experimentally tested with single- and double-end-pumping configurations. When both ends of the fiber are pumped by two high-power laser diodes with a launched power of similar to 300 W each, a maximum CW output of 444 W is obtained with a slope efficiency of similar to 75%. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, high optical quality cerium-doped lutetium pyrosilicate(LPS:Ce) crystal has been grown by Czochralski method with the seed oriented along cleavage plane (1 1 0). The structure, segregation coefficient of Ce3+ and optical characterization of LPS:Ce crystal have been compared with those of LSO:Ce crystal. The results show that LPS:Ce has the advantage over LSO:Ce by having a larger segregation coefficient of Ce3+, lower cost of starting material, lower melting point and only one luminescence mechanism. Thus, LPS:Ce crystal offers an attractive alternative to LSO:Ce for scintillator applications. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Yb: YAlO3 (YAP) (15 at %) and Yb: Y3Al5O12 (YAG)(15 at %) have been grown using the Czochralski method. Their absorption and fluorescence spectra were measured at room temperature and important spectroscopic parameters were calculated. Through the comparison of spectroscopic parameters of Yb:YAP and Yb: YAG, all results indicate that 15 at % Yb:YAP crystal is a potential candidate used for compact, efficient thin chip lasers when the laser output wavelength is 1012 or 103 8 nm. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Large sized neodymium-doped Y3Al5O12 (Nd:YAG) laser crystals have been grown by temperature gradient technique (TGT) method and compared with Czochralski (Cz) method. The comparison of these two crystal growth methods has been listed. The results showed that the TGT method has many advantages over the Cz method. The concentration distribution of Nd ions in the crystals was determined and the absorption spectra of these crystals have been investigated and compared. The TGT grown highly doped Nd:YAG crystal has a larger absorption FWHM than that of Cz grown Nd:YAG crysral. Highly doped Nd:YAG (similar to 2.8 at. pct) crystals could be obtained by TGT.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

About Phi 45 mm LiAlO2 single crystal was grown by Czochralski (Cz) technique. However, the full-width at half-maximum (FWHM) value was high to 116.9 arcsec. After three vapor transport equilibration (VTE) processes, we can obtain high-quality LiAlO2 slice with the FWHM value of 44.2 arcsec. ZnO films were fabricated on as-grown slices and after-VTE ones by pulsed laser deposition (PLD). It was found that ZnO films on the two slices have similar crystallinity, optical transmittance and optical band gap at room temperature. These results not only show that LAO substrate is suitable for ZnO growth, but also prove that the crystal quality of LAO substrate slightly affects the structural and optical properties of ZnO film.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Yb:Y3Al5O12 (Yb:YAG) single crystals with Yb doping concentration 0.5 at.%, 5 at.%, 15 at.%, 25 at.%, 50 at.%, 100 at.% and Yb:YAlO3 (Yb:YAP) single crystals with Yb doping concentration 0.5 at.%, 5 at.%, 15 at.%, 30 at.% were grown by the Czochralski process. The fluorescence spectra of these crystals and the effects of self-absorption on the shape of the fluorescence spectra were studied. Through comparing the fluorescence spectra of Yb:YAG and Yb:YAP, all results indicate that the effects of self-absorption on the fluorescence spectra of Yb:YAP are remarkably stronger than that of Yb:YAG at the same Yb concentration. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Adhesion between the interface of pure silver thin film and three kinds of low refractive index coatings MgF2, Al2O3, SiO2 were compared in this article. The results indicated that the adhesion of Al2O3 and Ag was evidently superior to that of MgF2 and Ag, and the adhesion of MgF2 and Ag was evidently superior to that Of SiO2 and Ag. Reasons were analyzed accordingly. On the other hand, we compared the effect on the optical characteristic of Ag film when these three kinds of films were used as protective coatings and enhanced coatings. Considering the difference of the adhesion between Ag and MgF2, Al2O3, SiO2, suited uses are given for each other. © 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

TiO2 and ZrO2 films are deposited by electron-beam (EB) evaporation and by sol-gel process. The film properties are characterized by visible and Fourier-transform infrared spectrometry, x-ray diffraction analysis, surface roughness measure, absorption and laser-induced damage threshold (LIDT) test. It is found that the sol-gel Elms have lower refractive index, packing density and roughness than EB deposited films due to their amorphous structure and high OH group concentration in the film. The high LIDT of sol-gel films is mainly due to their amorphous and porous structure, and low absorption. LIDT of EB deposited film is considerably affected by defects in the Elm, and LIDT of sol-gel deposited film is mainly effected by residual organic impurities and solvent trapped in the film.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

HfO2 single layers, 800 run high-reflective (HR) coating, and 1064 ran HR coating were prepared by electron-beam evaporation. The laser-induced damage thresholds (LIDTs) and damage morphologies of these samples were investigated with single-pulse femtosecond and nanosecond lasers. It is found that the LIDT of the HfO2 single layer is higher than the HfO2-SiO2 HR coating in the femtosecond regime, while the situation is opposite in the nanosecond regime. Different damage mechanisms are applied to study this phenomenon. Damage morphologies of all samples due to different laser irradiations are displayed. (c) 2007 Optical Society of America.