65 resultados para Tucídides, ca. 460-ca. 400 a. C.
Resumo:
ZnO films prepared by the thermal oxidation of the ZnS films through thermal evaporation are reported. The as-deposited ZnS films have transformed to ZnO films completely at 400 degrees C. The 400-700 degrees C annealed films with a preferential c-axis (002) orientation have a hexagonal wurtzite structure. The band gap of ZnO films shifts towards longer wavelength with the increase of the annealing temperature. The relationship between the band gap energy of ZnO films and the grain size is discussed. The shift of the band gap energy can be ascribed to the quantum confinement effect in nanocrystal ZnO films. The photoluminescence spectra of ZnO films show a dominant ultraviolet emission and no deep level or trap state defect emission in the green region. It confirms the absence of interstitial zinc or oxygen vacancies in ZnO films. These results indicate that ZnO film prepared by this simple thermal oxidation method is a promising candidate for optoelectronic devices and UV laser. (c) 2005 Elsevier BN. All rights reserved.
Resumo:
设计并镀制了193nm Al2O3/MgF2反射膜,对它们在空气中分别进行了250-400℃的高温退火,测量了样品的透射率光谱曲线和绝对反射率光谱曲线.发现样品在高反射区的总的光学损耗随退火温度的升高而下降,而后趋于饱和.采用总积分散射的方法对样品在不同退火温度下的散射损耗进行了分析,发现随着退火温度的升高散射损耗有所增加.因此,总的光学损耗的下降是由于吸收损耗而不是散射损耗起主导作用.对Al2O3材料的单层膜进行了同等条件的退火处理,由它们光学性能的变化推导出它们的折射率和消光系数的变化,从而解释了相应
Resumo:
The effects of post-deposited annealing on structure and optical properties of electron-beam evaporated Al2O3 single layers were investigated. The films were annealed in air for 1.5 h at different temperatures from 250 to 400 degrees C. The optical constants and cut-off wavelength were deduced. Microstructure of the samples was characterized by X-ray diffraction (XRD). Profile and surface roughness measurement instrument was used to determine the rms surface roughness. It was found that the cut-off wavelength shifted to short wavelength as the annealing temperature increased and the total optical loss decreased. The film structure remained amorphous even after annealing at 400 degrees C temperature and the samples annealed at higher temperature had the higher rms surface roughness. The decreasing total optical loss with annealing temperature was attributed to the reduction of absorption owing to oxidation of the film by annealing. Guidance to reduce the optical loss of excimer laser mirrors was given. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
HfO2 Elms are deposited on BK7 glass substrates by electron beam evaporation. The influences of annealing between 100 degrees C and 400 degrees C on residual stresses and structures of HfO2 films are studied. It is found that little differences of spectra, residual stresses and structures are obtained after annealing at lower temperatures. After annealing at higher temperatures, the spectra shift to short wavelength, the residual stress increases with the increasing annealing temperature. At the same time, the crystallite size increases and interplanar distance decreases. The variations of optical spectra and residual stress correspond to the evolutions of structures induced by annealing.
Resumo:
The TiOx thin films were prepared by electron beam evaporation using TiO as the starting material. The effect of the annealing temperature on the optical and electrical properties was investigated. The spectra of X-ray photoelectron spectroscopy reveal that Ti in the films mainly exist in the forms of Ti2+ and Ti3+ below 400 degrees C 24h annealing. The charge transfer between different titanium ion contribute greatly to the color, absorption, and electrical resistance of the films. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
用电子束蒸发方法在BK7基底上沉积了HfO2/SiO2多层膜。研究了200℃到400℃的退火对残余应力的影响。结果表明退火前的薄膜残余应力为压应力,在200℃退火后发展为张应力,然后张应力值随着退火温度的升高而增大。在400℃退火后,由于张应力太大,薄膜表面出现了裂纹。同时,随着退火温度的升高,晶粒尺寸长大,晶面间距降低。残余应力的变化与结构的演变相对应。
Resumo:
The resistivity of hydrothermally grown ZnO single crystals increased from similar to 10(3) Omega cm to similar to 10(6) Omega cm after 1.8 MeV electron irradiation with a fluence of similar to 10(16) cm(-2), and to similar to 10(9) Omega cm as the fluence increased to similar to 10(18) cm(-2). Defects in samples were studied by thermally stimulated current (TSC) spectroscopy and positron lifetime spectroscopy (PLS). After the electron irradiation with a fluence of 10(18) cm(-2), the normalized TSC signal increased by a factor of similar to 100. A Zn vacancy was also introduced by the electron irradiation, though with a concentration lower than expected. After annealing in air at 400 degrees C, the resistivity and the deep traps concentrations recovered to the levels of the as-grown sample, and the Zn vacancy was removed.
Resumo:
Vanadium dioxide thin films were fabricated by ion beam sputtering on Si3N4/SiO2/Si after a post reductive annealing process in a nitrogen atmosphere. X-ray Diffraction (XRD), scanning electron microscope (SEM), and X-ray photoelectron spectroscopy (XPS) were employed to analyze the effects of post annealing temperature on crystallinity, morphology, and composition of the vanadium oxide thin films. Transmission properties of vanadium dioxide thin films were measured by Fourier transform-infrared (FT-IR) spectroscopy. The results showed that the as-deposited vanadium oxide thin films were composed of non-crystalline V2O5 and a tetragonal rutile VO2. After annealing at 400 degrees C for 2 h, the mixed phase vanadium oxide (VOx) thin film changed its composition and structure to VO2 and had a (011) oriented monoclinic rutile structure. When increasing the temperature to 450 degrees C, nano VO2 thin films with smaller grains were obtained. FT-IR results showed that the transmission contrast factor of the nano VO2 thin film was more than 0.99 and the transmission of smaller grain nano VO2 thin film was near zero at its switched state. Nano VO2 thin film with smaller grains is an ideal material for application in optical switching devices.
Resumo:
We studied the effects of hydrogen plasma treatment on the electrical and optical properties of ZnO films deposited by radio frequency magnetron sputtering. It is found that the ZnO H film is highly transparent with the average transmittance of 92% in the visible range. Both carrier concentration and mobility are increased after hydrogen plasma treatment, correspondingly, the resistivity of the ZnO H films achieves the order of 10(-3) cm. We suggest that the incorporated hydrogen not only passivates most of the defects and/or acceptors present, but also introduces shallow donor states such as the V-O-H complex and the interstitial hydrogen H-i. Moreover, the annealing data indicate that H-i is unstable in ZnO, while the V-O-H complex remains stable on the whole at 400 degrees C, and the latter diffuses out when the annealing temperature increases to 500 degrees C. These results make ZnO H more attractive for future applications as transparent conducting electrodes.
Resumo:
Metalorganic chemical vapor deposition growth of InN on sapphire substrate has been investigated between 400 degrees C and 500 degrees C to seek the growth condition of InN buffer layer, i.e. the first step of realization of the two-step growth method. Ex situ characterization of the epilayers by means of atomic force microscope, scanning electron microscope and X-ray diffraction, coupled with in situ reflectance curves, has revealed different growth circumstances at these temperatures, and conclusion has been reached that the most suitable temperature for buffer growth is around 450 degrees C. In addition, the growth rate of InN at the optimized temperature with regard to different precursor flow rates is studied at length. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
ZnO thin films with highly c-axis orientation have been fabricated on p-type Si(1 1 1) substrates at 400 degrees C by pulsed laser deposition (PLD) from a metallic Zn target with oxygen pressures between 0.1 and 0.7 mbar. Experimental results indicate that the films deposited at 0.3 and 0.5 mbar have better crystalline and optical quality and flatter surfaces than the films prepared at other pressures. The full width at half maximum (FWHM) of (0 0 0 2) diffraction peak decreases remarkably from 0.46 to 0.19 degrees with increasing annealing temperature for the film prepared at 0.3 mbar. In photoluminescence (PL) spectra at room temperature, the annealed film at 700 degrees C exhibits a smaller ultraviolet (UV) peak FWHM of 108 meV than the as-grown film (119 meV). However, an enhanced deep-level emission is observed. Possible origins to above results are discussed. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Sb-doped and undoped ZnO thin films were deposited on Si (100) substrates by radio frequency (RF) magnetron sputtering. X-ray diffraction (XRD) and scanning electron microscopy (SEM) analyses revealed that all the films had polycrystalline wurtzite structure and c-axis preferred orientation. Room temperature Hall measurements showed that the as-grown films were n-type and conducting (rho similar to 1-10 Omega cm). Annealing in a nitrogen ambient at 400 degrees C for 1 h made both samples highly resistive (rho > 10(3) Omega cm). Increasing the annealing temperature up to 800 C, the resistivity of the ttndoped ZnO film decreased gradually, but it increased for the Sb-doped ZnO film. In the end, the Sb-doped ZnO film annealed at 800 C became semi-insulating with a resistivity of 10(4)Omega cm. In addition, the effects of annealing treatment and Sb-doping on the structural and electrical properties are discussed. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
At a medium substrate temperature of 400 degrees C and a lower As flux, we have grown an ultrafast AlGaAs/GaAs photorefractive multiple quantum well (MQW) structure by molecular beam epitaxy. The as-grown sample exhibits strong photorefractive effect under the transverse Frantz-Keldysh geometry. A peak electroabsorption of 2100 cm(-1) is measured in the as-grown sample in an 11 kV/cm dc electric field, and the peak photorefractive diffraction efficiency can be 1.2%. After postgrowth annealing, the photorefractive effect becomes weak and disappears in samples annealed above 700 degrees C. Using optical transient current spectroscopy, deep levels are measured in these samples. It is found that deep levels are stable against annealing until 700 degrees C. Using a pump-probe technique, carrier lifetimes are measured at room temperature. We find that the as-grown sample has a lifetime of 20 ps, while the 700 degrees C annealed sample has a lifetime of more than 200 ps. The ultrafast lifetime in the as-grown sample is caused by point defects, not by As clusters. Our result show that AlGaAs/GaAs MQW structure grown around 400 degrees C has better performance of the photorefractive effect. (C) 1999 American Institute of Physics. [S0003-6951(99)04036-X].
Resumo:
Photoluminescence (PL) spectroscopy and carrier lifetime measurement has been used to characterize optical properties of defects in the low-temperature (LT) grown GaAs/AlGaAs multiple quantum well structures. Two sets of samples were grown at 400 degrees C by molecular beam epitaxy on nominal (001) and miscut [4 degrees off (001) towards (111) A] GaAs substrates, respectively. After growth, samples were subjected to 30 s rapid thermal annealing at 600-800 degrees C. It is found that after annealing, two defect-related PL features appear in the samples grown on nominal (001) GaAs substrates, but not in those grown on miscut (001) GaAs substrates. The carrier lifetimes are about 31 and 5 ps in as-grown samples grown on nominal and miscut (001) GaAs substrates, respectively. The different PL spectra and carrier lifetimes in two sets of samples are attributed to different structures of the As-Ga-like defects formed during LT growth. (C) 1999 American Institute of Physics. [S0003-6951(99)00230-2].
Resumo:
VOx thin films have been fabricated by low temperature ion beam sputtering and post reductive annealing process. Semiconductor-metal phase transition is observed for the film annealed at 400 degrees C for 2 hours. The film also shows a polycrystal structure with grain size from 50nm to 150nm. The VOx thin films fabricated by this process have a TCR up to -2.7% at room temperature. Our results indicate a promising fabrication method of the nano-structured VOx film with relatively high TCR and semiconductor-metal phase transition.