Resumo:

Based on the dimer-monomer equilibrium movement of the fluorescent dye Pyronin Y (PY), a rapid, simple, highly sensitive, label-free method for protein detection was developed by microchip electrophoresis with LIF detection. PY formed a nonfluorescent dimer induced by the premicellar aggregation of an anionic surfactant, SDS, however, the fluorescence intensity of the system increased dramatically when proteins such as BSA, bovine hemoglobin, cytochrome c, and trypsin were added to the solution due to the transition of dimer to fluorescent monomer. Furthermore, 1-ethyl-3-methylimidazolium tetrafluoroborate (EMImBF(4)) instead of PBS was applied as running buffers in microchip electrophoresis.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Polarization self-modulation effect in a free oscillated Nd:YAG laser is investigated after a quarter wave plate is introduced independently in the two positions of the cavity. As described in the previous experiments, the intensity components in the orthogonal directions are modulated with a period of the round-trip time or twice. Different pulse shapes reveal that the seed field from the spontaneous emission is not uniform and seems to be stochastic for each pulse.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

National Natural Science Foundation of China 60506001 60776047 60476021 60576003 60836003;National Basic Research Programme of China 2007CB936700

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A high-power AlGaInP laser diode with current-injection-free region near the facet is successfully fabricated by metaorganic chemical vapor deposition (MOCVD) using the (100) direction n-GaAs substrates with a misorientation of 15 deg toward the (011) direction. The maximum continuous wave output power is about 90 mW for the traditional structure. In comparison, the maximum output power is enhanced by about 67%, and achieves 150 mW for LDs with current-infection-free regions. The fundamental transverse-mode operation is obtained up to 70 mW. Output characteristics at high temperatures are also improved greatly for an LD with a current-injection-free region, and the highest operation temperature is 70 C at 50 mW without kink. The threshold current is about 33 mA, the operation current and the slope efficiency at 100 mW are 120 mA and 0.9 mW/mA, respectively. The lasing wavelength is 658.4 nm at room-temperature 50 mW. (c) 2006 Society of Photo-Optical Instrumentation Engineers.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Bandgap tuning of the InGaAsP/InP multiple quant um well (MQW) laser structure by the impurity-free vacancy diffusion (IFVD) is investigated using photoluminescence. It has been demonstrated that the effects of the plasma bombardment to the:sample surface involved in the IFVD technique can enhance the intermixing of the InGaAsP/InP MQW laser structure. The reliability of the IFVD technique, particularly the effects of the surface decomposition and the intrinsic defects formed in the growth or preparation of the wafer, has been discussed.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The 940 nm Al-free active region laser diodes and bars with a broad waveguide were designed and fabricated. The stuctures were grown by metal organic chemical vapour deposition. The devices show excellent performances. The maximum output power of 6.7 W in the 100 f^m broad-area laser diodes has been measured, and is 2. 5 times higher than that in the Al-containing active region laser diodes with a narrow waveguide and 1. 7 times higher than that in Al-free active region laser diodes with a narrow waveguide. The 19 % fill-factor laser diode bars emit 33 W, and they can operate at 15W with low degradation rates.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A new in situ method was realized by one step laser cladding to produce Ni-base alloy composite coating reinforced by in situ reacted and gradiently distributed TiCp particles. The submicron TiCp particles were formed and uniformly distributed because of the in situ reaction and trapping effect under the rapid solidification condition. And, TiCp particles were of gradient distribution on a macro scale and their volume fraction increased from 1.86% at the layer/substrate interface to a maximum 38.4% at the surface of the layer. Furthermore, the in situ generated TiCp/gamma-Ni interfaces were free from deleterious surface reactions. Additionally, the clad coating also revealed a high microhardness of gradient variation with the layer depth and the superior abrasive wear resistance.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The feasibility of the fabrication of coatings for elevated-temperature structural applications by laser cladding MoSi2 powder on steel was investigated. A dense and crack-free fine coating, well-bonded with the substrate has been obtained by this technique. This coating consists of FeMoSi, Fe2Si and a small amount of Mo5Si3 due to dilution of the substrate in the coating. The microstruelure of the coating is characterized of typical fine dendrites. The dendrites are composed of FeMoSi primary phase, and the interdendritic areas are two eutectic phases of FeMoSi and Fe2Si. The hardness of the coating reaches 845 Hv(0.5), 3.7 times larger than that of the steel substrate (180Hv(0.5)).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

An in situ method was developed to produce an Ni alloy composite coating reinforced by in situ reacted TiC particles with a gradient distribution, using one-step laser cladding with a pre-placed powder mixture on a 5CrMnMo steel substrate. Dispersed and ultra-fine TIC particles were formed in situ in the coating. Most. of the TiC particles, with a marked gradient distribution, were uniformly distributed within interdendritic regions because of the trapping effect of the advancing solid-liquid interface. In addition, the TiC-gamma-Ni interfaces generated in situ were found to be free from any deleterious surface reaction. Finally, the microhardness also showed a gradient variation, with the highest value of 1250 Hv0.2 and the wear properties of the coating were significantly enhanced.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper studies the surface melting in the atmosphere by YAG laser-guided micro-arc discharge. In three kinds of surface conditions (free, oiled, and polyethylene covered), we try to control the diameter and the power density of discharge pit. It is found that the power density of 3 x 10(6) W/cm(2) of discharge pit on the oiled surface is moderate to form the melted layer thicker than that of the others, adapting to strengthen the surface of material, and the power density of 1.07 x 10(7) W/cm(2) of discharge pit on the polyethylene-covered surface is highest to form the deepest discharge pit among them, adapting to remove the material.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The NiAl intermetallic layers and NiAl matrix composite layers with TiC particulate reinforcement were successfully synthesized by laser cladding with coaxial powder feeding of Ni/Al clad powder and Ni/Al + TiC powder mixture, respectively. With optimized processing parameters and powder mixture compositions, the synthesized layers were free of cracks and metallurgical bond with the substrate. The microstructure of the laser-synthesized layers was composed of 6-NiAl phase and a few gamma phases for NiAl intermetallic; unmelted TiC, dispersive fine precipitated TiC particles and refined beta-NiAl phase matrix for TiC reinforced NiAl intermetallic composite. The average microhardness was 355 HV0.1 and 538 HV0.1, respectively. Laser synthesizing and direct metal depositing offer promising approaches for producing NiAl intermetallic and TiC-reinforced NiAl metal matrix composite coatings and for fabricating NiAl intermetallic bulk structure. (C) 2004 Laser Institute of America.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The interface of a laser-discrete-quenched steel substrate and as-deposited chromium electroplate was investigated by ion beam etching, dissolving-substrate-away and using a Vickers microhardness tester, in an attempt to reveal the mechanism that the service life of the chromium-coated parts is increased by the duplex technique of laser pre-quenching plus chromium post-depositing. The laser quenching of the steel substrate can reduce the steep hardness gradient at the substrate/chromium interface and improve the load-bearing capacity of chromium electroplate. Moreover, the laser quenching prior to plating has an extremely great effect on the morphologies and microstructure of the substrate/chromium interface: there is a transient interlayer at the original substrate/chromium interface while there is not at the laser-quenchedzone/chromium interface; the near-substrate surface microstructure and morphologies of the free-standing chromium electrodeposits, whose substrate was dissolved away with nital 30% in volume, inherit the periodically gradient characteristics of the laser-discrete-quenched substrate surface. (c) 2006 Elsevier B.V. All rights reserved.