Single-walled carbon nanotubes (SWNTs) have been considered as the leading candidate for nano-device applications ranging from gene therapy and novel drug delivery to membrane separations. The miniaturization of DNA-nanotube devices for biological applications requires fully understanding DNA-nanotube interaction mechanism. We report here, for the first time, that DNA destabilization and conformational transition induced by SWNTs are sequence-dependent. Contrasting changes for SWNTs binding to poly[dGdC]:poly[dGdC] and poly[dAdT]:poly[dAdT] were observed. For GC homopolymer, DNA melting temperature was decreased 40 degrees C by SWNTs but no change for AT-DNA. SWNTs can induce B-A transition for GC-DNA but AT-DNA resisted the transition. Our circular dichroism, competitive binding assay and triplex destabilization studies provide direct evidence that SWNTs induce DNA B-A transition in solution and they bind to the DNA major groove with GC preference.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Effects of chain flexibility on the conformation of homopolymers in good solvents have been investigated by Monte Carlo simulation. Bond angle constraint coupled with persistence length of polymer chains has been introduced in the modified eight-site bond fluctuation simulation model. The study about the effects of chain flexibility on polymer sizes reveals that the orientation of polymer chains under confinement is driven by the loss of conformation entropy. The conformation of polymer chains undergoing a gradual change from spherical iso-diametric ellipsoid to rodlike iso-diametric ellipsoid with the decrease of polymer chain flexibility in a wide region has been clearly illustrated from several aspects. Furthermore, a comparison of the freely jointed chain (FJC) model and the wormlike chain (WLC) model has also been made to describe the polymer sizes in terms of chain flexibility and quasi-quantitative boundary toward the suitability of the models.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Four different sizes of citrate-protected silver nanoplates with the corresponding in-plane dipole resonance band at 530, 619, 778, and 858 nm, respectively, are synthesized for surface-enhanced Raman scattering (SERS) study. Their aggregation behaviors are monitored by use of UV-vis spectroscopy. During the aggregation process, a marked red shift of the in-plane dipole resonance of silver nanoplates is observed, whereas other resonance modes of them only have small alterations in the site or intensity. Aggregated silver nanoplates can serve as active SERS substrates with an enhancement factor of about 4.5 x 10(5) using 2-aminothiophenol as a probing molecule. The SERS performance of silver nanoplates is even superior to the commonly used Lee-Meisel silver colloid, making them very attractive for SERS applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have investigated the inverted phase formation and the transition from inverted to normal phase for a cylinder-forming polystyrene-block-poly(methyl methacrylate) (PS-b-PMMA) diblock copolymer in solution-cast films with thickness about 300 nm during the process of the solution concentrating by slow solvent evaporation. The cast solvent is 1, 1,2,2-tetrachloroethane (Tetra-CE), a good solvent for both blocks but having preferential affinity for the minority PMMA block. During such solution concentrating process, the phase behavior was examined by freeze-drying the samples at different evaporation time, corresponding to at different block copolymer concentrations, phi. As phi increases from similar to 0.1 % (nu/nu), the phase structure evolved from the disordered sphere phase (DS), consisting of random arranged spheres with the majority PS block as I core and the minority PMMA block as a corona, to ordered inverted phases including inverted spheres (IS), inverted cylinders (IC), and inverted hexagonally perforated lamellae (IHPL) with the minority PMMA block comprising the continuum phase, and then to the lamellar (LAM) phase with alternate layers of the two blocks, and finally to the normal cylinder (NC) phase with the majority PS block comprising the continuum phase. The solvent nature and the copolymer solution concentration are shown to be mainly responsible for the inverted phase formation and the phase transition process.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Crystallization and phase behavior in solution-cast thin films of crystalline syndiotactic 1,2-polybutadiene (s-1,2-PB) and isotactic polypropylene (i-PP) blends have been investigated by transmission electron microscopy (TEM), atomic force microscopy (AFM) and field-emission scanning electron microscopy (FESEM) techniques. Thin films of pure s-1,2-PB consist of parallel lamellae with the c-axis perpendicular to the film plane and the lateral scale in micrometer size, while those of i-PP are composed of cross-hatched and single-crystal-like lamellae. For the blends, TEM and AFM observations show that with addition of i-PP, the s-1,2-PB long lamellae become bended and i-PP itself tends to form dispersed convex regions oil a continuous s-1,2-PB phase even when i-PP is the predominant component, which indicates a strong phase separation between the two polymers during film formation. FESEM micrographs of both lower and upper surfaces of the films reveal that the s-1,2-PB lamellae pass through i-PPconvex regions from the bottom, i.e. the dispersed i-PP regions lie on the continuous s-1,2-PB phase. The structural development is attributed to an interplay of crystallization and phase separation of the blends in the film forming process.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Monodisperse oligo[(1,4-phenyleneethynylene)-alt-(2,5-thiopheneethynylene)]s, new candidates for molecular wires, were rapidly synthesized via an iterative divergent/convergent doubling strategy in solution as well as on Merrifield's resin.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of metal cations in solution on the oxidation of methanol on the electrode surface of platinum is a neglected aspect to direct methanol fuel cell (DMFC). In this paper, a smooth platinum electrode absorbing metal cations as the working electrode was applied to investigate the methanol oxidation with the cyclic voltammetry (CV) in 1.0 mol L-1 H2SO4. From the analysis of experiment, it is found that the cations, Li+, Ce4+, Mn2+, Ni2+, Cu2+, have some negative effect on the catalytic oxidation of methanol on the surface of platinum. The degree of the effect from different cations was analyzed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

4-Aminobenzoic acid (4-ABA) was covalently grafted on a glassy carbon electrode (GCE) by amine cation radical formation during the electrooxidation process in 0.1 M KCl aqueous Solution. X-ray photoelectron spectroscopy (XPS) measurement proves the presence of 4-carboxylphenylamine on the GCE. Electron transfer processes of Fe(CN)(6)(3-) in solutions of various pHs at the modified electrode are studied by both cyclic voltammetry (CV) and electrochemical impedance spectroscopy (EIS). Changing the solution pH would result in the variation of the terminal group's charge state, based on which the surface pK(a) values were estimated. The copper hexacyanoferrate (CuHCF) multilayer films were formed on 4-ABA/GCE prepared in aqueous solution, and which exhibit good electrochemical behavior with high stability.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of novel cyclometalated iridium(III) complexes bearing 2,4-diphenylquinoline ligands with fluorinated substituent were prepared and characterized by elemental analysis, NMR and mass spectroscopy. The cyclic voltammetry, absorption, emission and electroluminescent properties of these complexes were systematically investigated. Electrochemical studies showed that the oxidation of the fluorinated complexes occurred at more positive potentials (in the range 0.57-0.69 V) than the unfluorinated complex 1 (0.42 V). In view of the energy level, the lowering of the LUMO by fluorination is significantly less than that of the HOMO. The weak and low energies absorption bands in the range of 300-600 nm are well resolved, likely associated with MLCT and (3)pi-pi* transitions. These complexes show strong orange red emission both in the solution and solid state. The emission maxima of the fluorinated complexes showed blue shift by 9, 24 and 15 nm for 2, 3 and 4, respectively, with respect to the unfluorinated analogous 1. Multilayered organic light-emitting diodes (OLEDs) were fabricated by using the complexes as dopant materials. Significantly higher performance and lower turn-on voltage were achieved using the fluorinated complexes as the emitter than that using the unfluorinated counterpart 1 under the same doping level.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have used Monte Carlo simulation to study the micellization of ABC 3-miktoarm star terpolymers in a selective solvent (good to A segment, bad to B and C segments). The simulation results reveal that the self-assembled morphology is determined by the block length, molecular architecture, terpolymer concentration and insolubility of insoluble block in the solvent. In dilute solution, symmetric terpolymers (N-B = N-C = 30) tend to aggregate into a novel wormlike pearl-necklace structure linked by an alternating arrangement of B and C spheres, whereas the asymmetric terpolymers (NB = 10, NC = 50) are likely to aggregate into spherical or cylindrical micelles (formed by C blocks) connected with some small B spheres, when the concentration of terpolymer is relatively low (chain number is 100). However, when the concentration of terpolymer is relatively high (chain number is 250), the symmetric terpolymers tend to aggregate into a netlike structure linked by an alternation of B and C spheres, whereas the asymmetric terpolymers are likely to aggregate into wormlike micelles (formed by C blocks) connected with some of small spheres (formed by B blocks). Moreover, when the insolubility of insoluble block in the solvent is weak, the insoluble blocks aggregate into some incompact micelles.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fourier-transform (FT)-Raman and -infrared (IR) spectroscopy were employed to investigate the function of the aqueous 2-hydroxyethylmethacrylate/glutaraldehyde solution (Gluma) as a desensitizer. 2-Hydroxyethylmethacrylate (HEMA), glutaraldehyde (GA), and the mixture of HEMA/GA (i.e. Gluma) were used to interact with dentin, collagen, hydroxyapatite (HAP), and bovine serum albumin (BSA) individually. All the interactions were monitored by an FT-Raman spectrometer. FT-IR spectroscopy was also used in this study. The results show that HEMA could be absorbed by dentin and collagen; GA could cross-link collagen and BSA; and when BSA was added to Gluma, polymerization of HEMA occurred. The results suggest that Gluma acts as a desensitizer whereby, first, GA reacts with part of the serum albumin in dentinal fluid, which induces a precipitation of serum albumin, then, second, a reaction of GA with serum albumin induces polymerization of HEMA. The function of Gluma as a desensitizer to block dentinal tubules occurs via these two reactions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dispersion copolymerization of acrylamide (AM) with 2-methylacryloylxyethyl trimethyl ammonium chloride (DMC) has been carried out in aqueous salts solution containing ammonium sulfate and sodium chloride with poly(acryloylxyethyl trimethyl ammonium chloride) (PDAC) as the stabilizer and 2,2'-azobis[2-(2-inidazolin-2-yl)propane]-dihydro chloride (VA-044) as the initiator. A new particle formation mechanism of the dispersion polymerization for the present system has been proposed. The effects of inorganic salts and stabilizer concentration on dispersion polymerization have been investigated. The results show that varying the salt concentration could affect the morphology and molecular weight of the resultant copolymer particles significantly. With increasing the stabilizer concentration, the particle size decreased at first and then increased, meanwhile the effect on the copolymer molecular weight was the contrary. These results had been rationalized based on the proposed mechanism.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, a novel substitutional solid solution (W0.8Al0.2)C was synthesized by mechanically activated high-temperature reaction. X-ray diffraction was used for phase identification during the whole reaction process. Environment scanning electronic microscopy-field emission gun and energy dispersive x-ray were used to investigate the microstructure and the quantitative material composition of the specimen. (W(0.8)A(10.2))C was found to crystallize in the WC-type, and the cell parameters were a = 2.907(1) angstrom and c = 2.837(1) angstrom. The hardness of (W0.8Al0.2)C was tested to be 19.3 +/- 1 GPa, and the density was 13.19 +/- 0.05 g cm(-3).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel solution-phase method for the preparation of Au@ZnO core-shell composites was described. With this method, the composites were grown without heating that is usually needed in other solution methods. Atomic force microscopy (AFM) results show that the diameter of Au@ZnO core-shell composites is about 10.5 nm. X-ray photoelectron spectroscopy (XPS) was applied to characterize Au@ZnO core-shell composites. The optical properties of Au@ZnO core-shell composites, including UV-vis absorption and photo luminescence (PL), were observed at room temperature.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dispersion copolymerization of acrylamide with acrylic acid in an aqueous solution of ammonium sulfate using poly(2-acrylamido-2-methylpropanesulfonic acid sodium) as the stabilizer and ammonium persulfate (APS) as the initiator was investigated. The influence of initiator concentration, stabilizer concentration, ammonium sulfate concentration, chain-transfer agent concentration, and polymerization temperature on the copolymerization was discussed. The results showed that varying the ammonium sulfate concentration could affect the particle size and the intrinsic viscosity of the copolymer significantly. With increasing the stabilizer concentration, the particle size of the copolymer decreased first, and then increased, meanwhile the intrinsic viscosity of the copolymer decreased. The increase of initiator concentration, chain-transfer agent concentration, and polymerization temperature resulted in the increase in the particle size. Polydisperse spherical particles were formed in the system, and the kinetics for the dispersion copolymerization were discussed.