Resumo:
研究了掺铒TeO2-ZnO-PbCl2碲酸盐基氧卤玻璃在977nm激光二极管抽运下的发光和上转换发光特性,结果发现除红外1.53μm^4I13.2→^4I15/2发光外(荧光半高宽高达69nm),该玻璃还存在很强的^2H11/2→^4I15/2(527nm),^4S3/2→^4I15/2(549nm)和^4R9/2→^4I15/2(666nm)可见上转换发光.应用Judd-Ofelt理论计算得到玻璃强度参数Ω1(t=2,4,6)分别为Ω2=5.87×10^20cm^2,Ω4=2.08×10^2-cm^2,
Resumo:
An erbium-doped phosphate glass fibre has been drawn by the rod-in-tube technique in our laboratory. The gain for the Er3+-doped phosphate glass fibre with different pump powers and with different input signal wavelengths is investigated. The 2.2-cm-long fibre, pumped by a single-mode 980-nm fibre-pigtailed laser diode, can provide a net gain per unit length greater than 1.8dB/cm. The pump threshold is about 50 mW at the wavelength of 1534 nm, and below 70 mW at 1550 nm. The gain linewidth of the Er3+-doped phosphate glass fibre is greater than 34 nm and can cover the C band in optical communication networks.
Resumo:
A novel diffractive-pumping scheme is proposed to improve the evanescent amplification using blazed fiber grating for the first time. We also investigate the cw-pumped-evanescent amplification at 1.55 mu m wavelength with the relative optical gain pumped at 1480 nm of around 2 dB based on side-polished fiber with the effective interaction length as long as 16 mm and with a heavily Er3+-doped (N-Er(3+) > 1.19 x 10(21) ions/cm(3)), low refractive index (n(1550) < 1.47) glass overlay, which has no concentration quenching (tau(f) = 9.0 ms).
Resumo:
我们报道了一种以二极管泵浦的 1.94 μm Tm:YAP激光器为泵浦源,常温下在2.1 μm连续运行的Ho:YAG激光器。最大输出功率1.5 W,相应斜率效率为17.9%,二极管到的转换效率为5.6%。
Resumo:
Infrared (1.2-1.6 mum) luminescence in a yttrium aluminium garnet (YAG) crystal, co-doped with Yb (10 at.%) and Cr (0.05 at.%) ions, was investigated under CW laser diode pumping (lambda = 940 nm). The Cr4+ emission band was observed with its peak at 1.35 mum and measured to be about 6% with respect to Yb3+ IR luminescence (lambda = 1.03 mum). Analysis of the crystal absorption and luminescence spectra allows one to conclude that Yb3+-Cr4+ energy transfer is a mechanism responsible for the B-3(2)(T-3(2))-B-3(1)((3)A(2)) emission of Cr4+ ions. This crystal is promising as an efficient source of the near infrared emission. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Infrared (1.2-1.6 mu m) luminescence in a ytterbium aluminium garnet (YbAG) crystal, doped with Cr (0.05 at.%) ions, was investigated under CW laser diode pumping (lambda = 940 nm). The Cr4+ emission band was observed with its peak at 1.34 mu m and measured to be about 1.3 times with respect to Yb3+ IR luminescence (lambda = 1.03 mu m). We demonstrate that for the excitation wavelength of 940 nm Yb3+ ions act as sensitizers of the B-3(2)(T-3(2))-B-3(1)((3)A(2)) emission of Cr4+ ions. This crystal is promising as a high-efficient system for tunable laser (1.2-1.6 mu m) output. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
Near infrared broadband emission characteristics of bismuth-doped aluminophosphate glass have been investigated. Broad infrared emissions peaking at 1210nm, 1173nm and 1300nm were observed when the glass was pumped by 405nm laser diode (LD), 514nm Ar+ laser and 808nm LD, respectively. The full widths at half maximum (FWHMs) are 235nm, 207nm and 300nm for the emissions at 1210nm, 1173nm and 1300nm, respectively. Based on the energy matching conditions, it is suggested that the infrared emission may be ascribed to P-3(1) --> P-3(0) transition of Bi+. The broadband infrared luminescent characteristics of the glasses indicate that they are promising for broadband optical fiber amplifiers and tunable lasers. (C) 2005 Optical Society of America.
Resumo:
Near-infrared broadband emission from bismuth-tantalum-codoped germanium oxide glasses was observed at room temperature when the glasses were pumped by an 808 nm laser diode. The emission band covered the 0, E, S, C, and L bands (1260-1625 nm), with a maximum peak at similar to 1310 nm, a FWHM broader than 400 nm, and a lifetime longer than 200 lis. The observed broadband luminescence was attributed to bismuth clusters in the glasses. Bismuth-tantalum-codoped germanium oxide glass might be promising as amplification media for broadly tunable lasers and wideband amplifiers in optical communications. (c) 2005 Optical Society of America.
Resumo:
For the first time, a high optical quality 10 at.% Yb3+-doped gadolinium oxyorthosilicate laser crystal Gd2SiO5 (GSO) was grown by the Czochralski (Cz) method. The segregation coefficient of Yb3+ was studied by the inductively coupled plasma atomic emission spectrometer (ICP-AES) method. The crystal structure has monoclinic symmetry with space group P2(1)/c; this was determined by means of an x-ray diffraction analysis. The absorption spectra, fluorescence spectra and fluorescence decay curves of Yb3+ ions in a GSO crystal at room temperature were also studied. Then, the spectroscopic parameters of Yb:GSO were calculated. The advantages of the Yb:GSO crystal include high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections and particularly broad emission bandwidth (similar to 72 nm). The results indicated that the Yb:GSO crystal seemed to be a very promising laser gain medium in diode-pumped femtosecond laser and tunable solid state laser applications when LD pumped at 940 and 980 nm.
Resumo:
We report what we believe to be the first demonstration of laser operation with a novel laser material of Yb3(+) -doped Gd-2 SiO2 (Yb: GSO) pumped by a laser diode at 940 nm. We obtained a low lasing threshold of 1.27 kW/cm(2) with the center wavelength of 1090 nm, which is lower than the value of 1.53 kW/cm(2) predicted for Yb: YAG. The maximal output power of 360 mW was obtained with a 2% output, which corresponds to a slope efficiency up to 19%.
Resumo:
We report on the realization of ZnO homojunction light-emitting diodes (LEDs) fabricated by metalorganic chemical vapor deposition on (0001) ZnO bulk substrate. The p-type ZnO epilayer was formed by nitrogen incorporation using N2O gas as oxidizing and doping sources. Distinct electroluminescence (EL) emissions in the blue and yellow regions were observed at room temperature by the naked eye under forward bias. The EL peak energy coincided with the photoluminescence peak energy of the ZnO epilayer, suggesting that the EL emissions emerge from the ZnO epilayer. In addition, the current-voltage and light output-voltage characteristics of ZnO homojunction LEDs have also been studied. (c) 2006 American Institute of Physics.
Resumo:
The effects of Na+ doping level on the thermal conductivities, absorption and emission spectra, and fluorescence lifetimes of Yb3+ ,Na+ :CaF2 crystals were systematically studied. Sites structure, covalent force, and crystal field strength of Yb3+ :CaF2 crystals were markedly varied by codoping Na+ as charge compensator. The 2.0at% Yb3+ and 3.0at% Na+-codoped CaF2 crystal was demonstrated to operate in diode-pumped passively mode-locking scheme. Transform-limited 1 ps laser pulses were obtained, showing the crystal capable of producing ultra-short laser pulses. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Nd3+-doped Y2-2x La-2x O-3 (x = 0.08) transparent ceramics were fabricated by conventional fabrication process. Spectroscopic properties of the samples were investigated. The absorption band of Nd3+ : Y1.84La0.16O3 was broad covering the wavelength range 780-850 nm. When doped with 1.5at% Nd3+, the cross sections of the sample at 820 nm and laser diode pumped 808 nm were 1.81 x 10(-20) cm(2) and 1.54 x 10(-20) cm(2), respectively. The strongest emission peak of the sample was centered at 1078 mn with long fluorescent lifetime, broad emission bandwidth and high quantum efficiency. Because of the additive La2O3, the spectroscopic quality parameter (X-Nd) of matrix was' decreased from 1.6 to 0.46, thus the fluorescence branch ratio of F-4(3/2) - (4) I-11/2 transition was increased to 56.82%. These properties of Nd3' : Y1.84La0.16O3 transparent ceramic are benefitial to achieve high efficient laser output and ultrashort modelocked pulse.
Resumo:
用提拉法生长了掺铬、钕的钆镓石榴石(Cr^4+,Nd^3+:GGG)自调Q激光品体。报道了室温下的吸收光谱和荧光光谱特性。分析了Cr离子浓度对光谱性质的影响。比较了Cr^4+:GGG,Nd^3+:GGG和(Cr^4+,Nd^3+):GGG晶体吸收光谱的关系。测量了(Cr^4+,Nd^3+):GGG晶体和Nd^3+:GGG晶体的荧光寿命,它们分别是33μs和250μs。实验表明,(Cr^4+,Nd^3+):GGG晶体是一种非常有潜力的自调Q激光晶体,可以实现大功率激光器的小型化和全固态化。