Resumo:
ZnO nanocrystals were synthesized by hydrolysis in methanol. X-ray diffraction and photoluminescence spectra confirm that good crystallized ZnO nanoparticles were formed. Utilizing those ZnO nanoparticles and poly [2- methoxy-5 - (3',7'-dimethyloctyloxy)- 1,4-phenylenevinylene] (MDMO-PPV), light emitting devices with indium tin oxide (ITO)/poly(3,4-oxyethyleneoxy-thiophene):poly(styrene sulfonate) (PEDOT:PSS)/ ZnO:MDMO-PPV/Al and ITO/PEDOT:PSS/MDMO-PPV/Al structures were fabricated. Electrolummescence (EL) spectra reveal that EL yield of hybrid MDMO-PPV and ZnO nanocrystals devices increased greatly as compared with pristine MDMO-PPV devices. The current-voltage characteristics indicate that addition of ZnO nanocrystals can facilitate electrical injection and charge transport. The decreased energy barrier to electron injection is responsible for the increased efficiency of electron injection. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
The fluctuations of the strained layer in a superlattice or quantum well can broaden the width of satellite peaks in double crystal X-ray diffraction (DCXRD) pattern. It is found that the width of the 0(th) peak is directly proportional to the fluctuation of the strained layer if the other related facts are ignored. By this method, the Ge-Si atomic interdiffusion in Ge nano-dots and wetting layers has been investigated by DCXRD. It is found that thermal annealing can activate Ge-Si atomic interdiffusion and the interdiffusion in the nano-dots area is much stronger than that in the wetting layer area. Therefore the fluctuation of the Ge layer decreases and the distribution of Ge atoms becomes homogeneous in the horizontal Ge (GeSi actually) layer, which make the width of the 0(th) peak narrow after annealing.
Resumo:
A high-power continuous wave (cw) mode-locked Nd:YVO4 solid-state laser was demonstrated by use of a semiconductor absorber mirror (SAM). The maximum average output power was 8.1 W and the optic-to-optic conversion efficiency was about 41 %. At the maximum incident pump power, the pulse width was about 8.6 ps and the repetition rate was 130 MHz. Experimental results indicated that this absorber was suitable for high power mode-locked solid-state lasers. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
It is important to acquire the composition of Si1-xGex layer, especially that with high Ge content, epitaxied on Si substrate. Two nondestructive examination methods, double crystals X-ray diffraction (DCXRD) and micro-Raman measurement, were introduced comparatively to determine x value in Si1-xGex: layer, which show that while the two methods are consistent with each other when x is low, the results obtained from double crystals X-ray diffraction are not credible due to the large strain relaxation occurring in Si1-xGex layers when Ge content is higher than about 20%. Micro-Raman measurement is more appropriate for determining high Ge content than DCXRD.
Resumo:
We report on structural characterization of AlGaN/GaN superlattices grown on sapphire. The superlattice formation is evidenced by high-resolution x-ray diffraction and transmission electron microscopy. The high resolution x-ray diffraction spectra exhibit a pattern of satellite peaks. The in-plane lattice constants of the superlattices indicate the coherent growth of the AlGaN layer onto GaN. The average At composition in the superlattices is determined to be 0.08 by Rutherford backscattering spectroscopy. The average parallel and perpendicular elastic strains for the SLs are determined to be (e(parallel to)) = +0.25% and (e(perpendicular to)) = -0.17%. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Wafer bonding between p-Si and an n-InP-based InGaAsP multiple quantum well (MQW) wafer was achieved by a direct wafer bonding method. In order to investigate the strain at different annealing temperatures, four pre-bonded pairs were selected, and pair one was annealed at 150 degrees C, pair two at 250 degrees C, pair three at 350 degrees C, and pair four at 450 degrees C, respectively. The macroscopical strains on the bonded epitaxial layer include two parts, namely the internal strain and the strain caused by the mismatching of the crystalline orientation between InP (100) and Si (100). These strains were measured by the X-ray double crystalline diffraction, and theoretical calculations of the longitudinal and perpendicular thermal strains at different annealing temperatures were calculated using the bi-metal thermostats model, both the internal strain and the thermal strain increase with the annealing temperature. Normal thermal stress and the elastic biaxial thermal strain energy were also calculated using this model. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
We report on the use of very thin GaAsP insertion layers to improve the performance of an InGaAsP/InGaP/AlGaAs single quantum-well laser structure grown by metal organic chemical vapour deposition. Compared to the non-insertion structure, the full width at half maximum of photoluminescence spectrum of the insertion structure measured at room temperature is decreased from 47 to 38 nm indicating sharper interfaces. X-ray diffraction shows that the GaAsP insertion layers between AlGaAs and InGaP compensates for the compressive strain to improve the total interface. The laser performance of the insertion structure is significantly improved as compared with the counterpart without the insertion layers. The threshold current is decreased from 560 to 450mA while the slope efficiency is increased from 0.61 to 0.7W/A and the output power is increased from 370 to 940mW. The slope efficiency improved is very high for the devices without coated facets. The improved laser performance is attributed to the suppression of indium carry-over due to the use of the GaAsP insertion layers.
Resumo:
Wafers with normal light-emitting diode structure were grown by metal organic chemical vapor deposition system. The pressure and temperature were varied during growth of buffer layer in order to grow different types of epilayers. The cathodoluminescence results show that the interface distortion of quantum well plays an important role in radiant efficiency. The electroluminescence detections indicate that the dislocations also influence the external quantum efficiency by lowering the electron injection efficiency. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Sb-assisted GaInNAs/GaAs quantum wells (QWs) with high (42.5%) indium content were investigated systematically. Transmission electron microscopy, reflection high-energy electron diffraction and photoluminescence (PL) measurements reveal that Sb acts as a surfactant to suppress three-dimensional growth. The improvement in the 1.55 mu m range is much more apparent than that in the 1.3 mu m range.. which can be attributed to the difference in N composition. The PL intensity and the full-width at half maximum of the 1.55 mu m single-QW were comparable with that of the 1.3 Am QWs. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Silicon nanoparticles have been fabricated in both oxide and nitride matrices by using plasma-enhanced chemical vapour deposition, for which a low substrate temperature down to 50 degreesC turns out to be most favourable. High-rate deposition onto such a cold substrate results in the formation of nanoscaled silicon particles, which have revealed an amorphous nature under transmission electron microscope (TEM) examination. The particle size can be readily controlled below 3.0 nm, and the number density amounts to over 10(12) cm(-2), as calculated from the TEM micrographs. Strong photoluminescence in the whole visible light range has been observed in the as-deposited Si-in-SiOx and Si-in-SiNx thin films. Without altering the size or structure of the particles, a post-annealing at 300 degreesC for 2 min raised the photoluminescence efficiency to a level comparable to the achievements with nanocrystalline Si-in-SiO2 samples prepared at high temperature. This low-temperature procedure for fabricating light-emitting silicon structures opens up the possibility of manufacturing integrated silicon-based optoelectronics.
Resumo:
In this paper we propose a new method for measuring the thickness of the GaN epilayer, by using the ratio of the integrated intensity of the GaN epilayer X-ray diffraction peaks to that of the sapphire substrate ones. This ratio shows a linear dependence on the GaN epilayer thickness up to 2 mum. The new method is more accurate and convenient than those of using the relationship between the integrated intensity of GaN epilayer diffraction peaks and the GaN thickness. Besides, it can eliminate the absorption effect of the GaN epilayer.
Resumo:
In order to understand the growth feature of GaN on GaAs (0 0 1) substrates grown by metalorganic chemical vapor deposition (MOCVD), the crystallinity of GaN buffer layers with different thicknesses was investigated by using double crystal X-ray diffraction (DCXRD) measurements. The XRD results showed that the buffer layers consist of predominantly hexagonal GaN (h-GaN) and its content increases with buffer layer thickness. The nominal GaN (111) reflections with chi at 54.74degrees can be detected easily, while (0 0 2) reflections are rather weak. The integrated intensity of reflections from (111) planes is 4-6 times that of (0 0 2) reflections. Possible explanations are presented. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
A new method of measuring the thickness of GaN epilayers on sapphire (0 0 0 1) substrates by using double crystal X-ray diffraction was proposed. The ratio of the integrated intensity between the GaN epilayer and the sapphire substrate showed a linear relationship with the GaN epilayer thickness up to 2.12 mum. It is practical and convenient to measure the GaN epilayer thickness using this ratio, and can mostly eliminate the effect of the reabsorption, the extinction and other scattering factors of the GaN epilayers. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
Silicon nanocrystals in SiO2 matrix are fabricated by plasma enhanced chemical vapor deposition followed by thermal annealing. The structure and photoluminescence (PL) of the resulting films is investigated as a function of deposition temperature. Drastic improvement of PL efficiency up to 12% is achieved when the deposition temperature is reduced from 250 degreesC to room temperature. Low-temperature deposition is found to result in a high quality final structure of the films in which the silicon nanocrystals are nearly strain-free, and the Si/SiO2 interface sharp. The demonstration of the superior structural and optical properties of the films represents an important step towards the development of silicon-based light emitters. (C) 2002 American Institute of Physics.
Resumo:
A model for analyzing point defects in compound crystals was improved. Based on this modified model, a method for measuring Mn content in GaMnAs was established. A technique for eliminating the zero-drift-error was also established in the experiments of X-ray diffraction. With these methods, the Mn content in GaMnAs single crystals fabricated by the ion-beam epitaxy system was analyzed.