353 resultados para Laser induced poling
Resumo:
The possibility of lifetime measurement in a flowing medium with phase fluorometry is investigated theoretically. A 3-D time dependent partial differential equation of the number density of atoms (or molecules) in the upper level of the fluorescence transition is solved analytically, taking flow, diffusion, optical excitation, decay, Doppler shift, and thickness of the excitation light sheet into account. An analytical expression of the intensity of the fluorescence signal in the flowing medium is deduced. Conditions are given, in which the principle of lifetime measurement with phase fluorometry in the static sample cell can be used in a flowing medium.
Resumo:
A new method for measuring the density, temperature and velocity of N2 gas flow by laser induced biacetyl phosphorescence is proposed. The characteristics of the laser induced phosphorescence of biacetyl mixed with N2 are investigated both in static gas and in one-dimensional flow along a pipe with constant cross section. The theoretical and experimental investigations show that the temperature and density of N2 gas flow could be measured by observing the phosphorescence lifetime and initial intensity of biacetyl triplet (3Au) respectively. The velocity could be measured by observing the time-of-flight of the phosphorescent gas after pulsed laser excitation. The prospect of this method is also discussed.
Resumo:
Investigation of kerosene combustion in a Mach 2.5 flow was carried out using a model supersonic combustor with cross-section area of 51 mm?70 mm, with special emphases on the characterization of effervescent atomization and the flameholdering mechanism using different integrated fuel injector/flameholder cavity modules. Direct photography, Schlieren imaging, and Planar Laser Induced Fluorescence (PLIF) imaging of OH were utilized to examine the cavity characteristics and spray structure, with and without gas barbotage. Schlieren images illustrate the effectiveness of gas barbotage in facilitating atomization and the importance of secondary atomization when kerosene sprays interacting with a supersonic crossflow. OH-PLIF images further substantiate our previous finding that there exists a local high temperature radical pool within the cavity flameholder and this radical pool plays a crucial role in promoting kerosene combustion in a supersonic combustor. The present results also demonstrate that the cavity characteristics can be different in non-reacting and reacting supersonic flows. As such, the conventional definition of cavity characteristics based on non-reacting flows needs to be revised.
Resumo:
利用有限元方法建立了二维模型,研究了飞秒激光作用下石英玻璃中导带电子的产生、激光能量的沉积、导带电子和能量扩散等微观过程.计算了导带电子扩散引起的局部净电荷及其形成的静电场分布,初步揭示了微爆炸的演化过程.
Resumo:
设计和制备了全向高反膜SiO2/TiO2,研究了它在不同脉冲宽度、不同脉冲能量的飞秒激光作用下的破坏阈值和烧蚀深度.利用发展的抽运.探针方法,研究了抽运脉冲作用下材料中导带电子的超快激发和能量沉积过程,建立并求解了飞秒激光激发材料和材料的激发对抽运光自身反作用的耦合动力学模型.模型较好地揭示了材料破坏的激发过程.
Resumo:
用扫描电镜(SEM)研究了氟化镁在800nm超短脉冲激光作用下的单枪表面烧蚀形貌.根据烧蚀斑面积与激光脉冲能量间的对数关系,测得烧蚀阈值与激光脉宽的关系曲线(55—750fs).计算了导带电子的双光子吸收,改进了多速率方程模型.很好地解释了实验结果.
Resumo:
基于固体的能带理论和能量守恒原理建立了一个描述激光与非金属材料作用时载流子随时间空间变化的理论模型。讨论了材料的破坏阈值、烧蚀深度与激光脉宽、波长和强度之间的关系,同时也讨论了破坏阈值、烧蚀深度与材料禁带宽度等特性之间的关系。讨论了多光子电离、隧道电离和雪崩电离在激光对材料破坏过程中的不同地位,理论结果表明,光电离在超短脉冲激光对非金属材料破坏过程中对破坏阈值的影响最大。
Resumo:
激光诱导周期性纳米微结构在多种材料包括电介质、半导体、金属和聚合物中观察到。研究了800 nm和400 nm飞秒激光垂直聚焦于6H SiC晶体表面制备纳米微结构。实验观察到800 nm和400 nm线偏光照射样品表面分别得到周期为150 nm和80 nm的干涉条纹, 800 nm圆偏振激光单独照射样品表面得到粒径约100 nm的纳米颗粒。偏振相互垂直的800 nm和400 nm激光同时照射晶体得到粒径约100 nm的纳米颗粒阵列, 该纳米阵列的方向随400 nm激光强度增加而向400 nm偏振方向偏转。利
Resumo:
报道了在铌酸锂晶体中实现紫外激光诱导畴反转的实验。在一定外加均匀电场下,铌酸锂晶体中通过波长365nm的紫外激光,由于紫外光的照射降低了矫顽电场只在通光区实现畴反转。研究表明,该方案可用于周期性极化铌酸锂的制备,并有望成为制作精细周期性畴结构的有效技术方案。
Resumo:
对紫外激光诱导近化学计量比钽酸锂晶体铁电畴反转进行了实验研究。波长为351 nm的连续紫外激光被聚焦在近化学计量比钽酸锂晶体的-z表面,同时沿与晶体自发极化相反的方向施加均匀外电场。实验证实紫外激光辐照可以有效地降低晶体畴反转所需的矫顽电场,采用数字全息干涉测量技术检测证实在激光辐照区域实现局域畴反转。研究表明采用紫外激光诱导可以实现对近化学计量比钽酸锂晶体铁电畴反转的局域控制。提出了物理机理的理论分析,认为外电场和激光辐照场的共同作用在晶体内部产生高浓度、大尺寸的缺陷结构,缺陷一定程度上降低畴体成核和畴
Resumo:
以硅酸四乙酯(TEOS)和甲基三乙氧基硅烷(MTEOS)为前驱材料,用溶胶-凝胶(sol-gel)方法在钛宝石表面制备得到均匀性良好且具有高激光损伤阈值的有机硅复合凝胶增透膜。膜层在钛宝石激光器输出波段(750~850nm)的增透效果显著,其平均透过率超过98.6%;激光破坏阈值为2.2J/cm^2(800nm,300ps);膜层表面均匀性达到激光波面的要求,在皮秒、飞秒超短脉冲高功率激光领域具有应用价值。溶胶的性能测试结果表明,溶胶粘度和成膜折射率均随溶液中CH3SiO1.5溶胶体含量的增加而增大,而膜
Resumo:
采用醇热法水解氧氯化锆(ZrOCl2·8H2O)制备ZrO2溶胶,提拉法涂膜。采用粘度、粒度分布、折射率、IR、DSC、AFM等测试手段对溶胶和薄膜性能进行表征。结果表明,ZrO2溶胶颗粒的平均粒径为18.9nm,薄膜经300℃热处理后折射率可高达1.95,膜层表面均匀平整,表面平均粗糙度仅为0.561nm,膜层的激光损伤阈值为14J/cm^2(1064nm,1ns)。
Resumo:
散粒磨料研磨与固着磨料研磨是光学研磨加工过程中的两种主要手段,但两者材料去除的机制不同。目前针对高功率固体激光装置中的主要工作物质——磷酸盐激光钕玻璃的亚表面缺陷(SSD)研究相对较少,因此在实验的基础上,通过系统地研究固着磨料对磷酸盐激光钕玻璃的研磨工艺过程,分析了多种因素,如磨料粒径、载荷大小、机床转速,以及结合剂材料与冷却液等对钕玻璃亚表面缺陷形成的影响,并与散粒磨料研磨工艺所产生的亚表面缺陷进行了比较,对关键工艺参数进行定量,为高质量钕玻璃制造工艺的选型以及进一步优化亚表面缺陷提供了重要的参考数据。
Resumo:
We present a destructive method for detecting and measuring subsurface damage of Nd-doped phosphate glasses. An instrument based on the dimple method - a destructive method - was developed. Subsurface damage depth produced in each fabrication procedure was obtained. We extend the surface roughness-subsurface damage relation to Nd-doped phosphate glasses. The constant ratio of subsurface damage and surface roughness was obtained as well. We also analyse the relation of abrasive size and subsurface damage experimentally. From a measurement of the surface roughness or abrasive size, one can obtain an accurate estimate of the damage layer thickness that must be eliminated by polishing or subsequent grinding operations. (C) 2007 Elsevier GmbH. All rights reserved.
Resumo:
系统地研究了光学研磨过程中,磨料粒径、载荷大小以及机床转速对钕玻璃表面及亚表面损伤的影响。结果表明,机床转速和载荷基本不改变材料表面粗糙度,而较大载荷或较低机床转速产生较大的亚表面缺陷,表面粗糙度和亚表面缺陷缺陷深度基本与最大磨料粒径呈正比,载荷增倍使亚表面缺陷与表面粗糙度的常数比值增加0.05。研究结果为钕玻璃加工工艺改进提供了参考依据。