Resumo:
Wafers with normal light-emitting diode structure were grown by metal organic chemical vapor deposition system. The pressure and temperature were varied during growth of buffer layer in order to grow different types of epilayers. The cathodoluminescence results show that the interface distortion of quantum well plays an important role in radiant efficiency. The electroluminescence detections indicate that the dislocations also influence the external quantum efficiency by lowering the electron injection efficiency. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
InAs quantum dots (QDs) were grown on In0.15Ga0.85As strained layers by molecular beam epitaxy on GaAs (0 0 1) substrates. Atomic force microscopy and transmission electron microscopy study have indicated that In0.15Ga0.85As ridges and InAs QDs formed at the inclined upside of interface misfit dislocations (MDs). By testifying the MDs are mixed 60 degrees dislocations and calculating the surface stress over them when they are 12-180 nm below the surface, we found the QDs prefer nucleating on the side with tensile stress of the MDs and this explained why the ordering of QDs is weak when the InGaAs layer is relatively thick. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
We investigate the effects of lightly Si doping on the minority carrier diffusion length in n-type GaN films by analyzing photovoltaic spectra and positron annihilation measurements. We find that the minority carrier diffusion length in undoped n-type GaN is much larger than in lightly Si-doped GaN. Positron annihilation analysis demonstrates that the concentration of Ga vacancies is much higher in lightly Si-doped GaN and suggests that the Ga vacancies instead of dislocations are responsible for the smaller minority carrier diffusion length in the investigated Si-doped GaN samples due to the effects of deep level defects. (c) 2006 American Institute of Physics.
Resumo:
Zinc-blende CrSb (zb-CrSb) layers with room-temperature ferromagnetism have been grown on (In,Ga)As buffer layers epitaxially prepared on (001) GaAs substrates by molecular-beam epitaxy. Compared with the typical thickness [2-3 ML (ML denotes monolayers)] of zb-CrSb grown directly on GaAs, the thickness of zb-CrSb grown on (In,Ga)As has been increased largely; the maximum can be up to similar to 9 ML. High-resolution cross sectional transmission electron microscopy images show that the zb-CrSb layer is combined with (In,Ga)As buffer layer without any dislocations at the interface. (C) 2006 American Institute of Physics.
Resumo:
Er-doped Si nanoclusters embedded in SiO2 (NCSO) films were prepared by radio frequency magnetron sputtering on either silicon or quartz substrates. A 1.16 mu m (1.08 eV) photoluminescence (PL) peak was observed from an Er-doped NCSO film deposited on a Si substrate. This 1.16 mu m peak is attributed to misfit dislocations at the NCSO/Si interface. The emission properties of the 1.16 mu m peak and its correlation with the Er3+ emission (1.54 mu m) have been studied in detail. The observed behavior suggests that the excitation mechanism of the 1.16 mu m PL is in a fashion similar to that shown for Er-doped Si nanoclusters embedded in a SiO2 matrix. (C) 2006 American Institute of Physics.
Resumo:
Both cracked and crack-free GaN/Al0.55Ga0.45N multiple quantum wells (MQWs) grown on GaN template by metalorganic chemical vapor deposition have been studied by triple-axis X-ray diffraction, grazing-incidence X-ray reflectivity, atomic force microscope, photoluminescence spectroscopy and low-energy positron annihilation spectroscopy. The experimental results show that cracks generation not only deteriorates the surface morphology, but also leads to a period dispersion and roughens the interfaces of MQWs. The mean density of dislocations in MQWs, determined from the average full-width at half-maximum of to-scan of each satellite peak, has been significantly enhanced by the cracks generation. Furthermore, the measurement of annihilation-line Doppler broadening reveals a higher concentration of negatively charged vacancies in the cracked MQWs. The combination of these vacancies and the high density of edge dislocations are assumed to contribute to the highly enhanced yellow luminescence in the cracked sample. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Effect of rapid thermal annealing on photoluminescence (PL) properties of InGaAs, InGaNAs, InGaAsSb, and InGaNAsSb quantum wells (QWs) grown by molecular-beam epitaxy was systematically investigated. Variations of PL intensity and full width at half maximum were recorded from the samples annealed at different conditions. The PL peak intensities of InGaAs and InGaNAs QWs initially increase and then decrease when the annealing temperature increased from 600 to 900 degrees C, but the drawing lines of InGaAsSb and InGaNAsSb take on an "M" shape. The enhancement of the PL intensity and the decrease of the full width at half maximum in our samples are likely due to the removal of defects and dislocations as well as the composition's homogenization. In the 800-900 degrees C high-temperature region, interdiffusion is likely the main factor influencing the PL intensity. In-N is easily formed during annealing which will prevent In out diffusion, so the largest blueshift was observed in InGaAsSb in the high-temperature region. (c) 2006 American Institute of Physics.
Resumo:
Transport properties of two-dimensional electron gas (2DEG) are crucial to metamorphic high-electron-mobility transistors (MM-HEMT). We have investigated the variations of subband electron mobility and concentration versus temperature from Shubnikov-de Hass oscillations., and variable temperature Hall measurements. The results indicate that the electrical performance is the best when the In content is 0.65 in the channel for MM-HEMT. When the In content exceeds 0.65, a large lattice mismatch will cause dislocations and result in the decrease of mobility and the fall of performance in materials and devices.
Resumo:
Microdefects originating from impurity-dislocation interactions in undoped InP that had been annealed in phosphorus and iron phosphide ambiances have been studied using optical microscopy. The electrical uniformity of the annealed wafer is improved by removing impurity aggregation around dislocations and by eliminating impurity striations in the annealing process. Compared to as-grown Fe-doped semi-insulating (SI) material, SI wafers obtained by annealing undoped InP in iron phosphide ambiances have better uniformity. This is attributed to the avoidance of Fe aggregation around dislocations and dislocation clusters, Fe precipitation and impurity striations, and is related to the use of a low concentration of Fe in the annealed material. The influence of Fe diffusion on the migration of dislocations in the annealing process has been studied and reviewed. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
We report the transmission-electron microscopy study of the defects in wurtzitic GaN films grown on Si(111) substrates with AIN buffer layers by the metal-organic chemical vapour deposition method. The In0.1Ga0.9N/GaN multiple quantum well (MQW) reduced the dislocation density by obstructing the mixed and screw dislocations passing through the MQW. No evident reduction of the edge dislocations density by the MQW was observed. It was found that dislocations with screw component can be located at the boundaries of sub-grains slightly in-plane misoriented.
Resumo:
We report the transmission electron microscopy (TEM) study of the microstructure of wurtzitic GaN films grown on Si(I I I) substrates with AlN buffer layers by metalorganic chemical vapor deposition (MOCVD) method. An amorphous layer was formed at the interface between Si and AlN when thick GaN film was grown. We propose the amorphous layer was induced by the large stress at the interface when thick GaN was grown. The In0.1Ga0.9N/GaN multiple quantum well (MQW) reduced the dislocation density by obstructing the mixed and screw dislocations from passing through the MQW. But no evident reduction of the edge dislocations by the MQW was observed. It was found that dislocations located at the boundaries of grains slightly in-plane misoriented have screw component. Inversion domain is also observed. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
The influence of reactor pressure on GaN nucleation layer (NL) and the quality of subsequent GaN on sapphire is studied. The layers were grown by low-pressure metalorganic chemical vapor deposition (MOCVD) on c-plane sapphire substrates and investigated by in situ laser reflectometry, atomic force microscope, scanning electron microscope, X-ray diffraction and photoluminescence. With the increase of reactor pressure prior to high-temperature GaN growth, the size of GaN nuclei formed after annealing decreases, the spacing between nucleation sites increases and the coalescence of GaN nuclei is deferred. The optical and crystalline qualities of GaN epilayer were improved when NLs were deposited at high pressure. The elongated lateral overgrowth of GaN islands is responsible for the quality improvement. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
Epitaxial growth of InN on GaN(0001) by plasma-assisted molecular-beam epitaxy is investigated over a range of growth parameters including source flux and substrate temperature. Combining reflection high-energy electron diffraction (RHEED) and scanning tunneling microscopy (STM), we establish a relationship between film growth mode and the deposition condition. Both two-dimensional (2D) and three-dimensional (3D) growth modes of the film are observed. For 2D growth, sustained RHEED intensity oscillations are recorded while STM reveals 2D nucleation islands. For 3D growth, less than three oscillation periods are observed indicating the Stranski-Krastanov (SK) growth mode of the film. Simultaneous measurements of (reciprocal) lattice constant by RHEED suggest a gradual relaxation of the strain in film, which commences during the first bilayer (BL) deposition and almost completes after 2-4 BLs. For SK growth, 3D islanding initiates after the strain has mostly been relieved, presumably by dislocations, so the islands are likely strain free. (C) 2002 American Institute of Physics.
Resumo:
The crystallographic tilt in GaN layers grown by epitaxial lateral overgrowth (ELO) on sapphire (0001) substrates was investigated by using double crystal X-ray diffraction (DC-XRD). It was found that ELO GaN stripes bent towards the SiNx mask in the direction perpendicular to seeding lines. Each side of GaN (0002) peak in DC-XRD rocking curves was a broad peak related with the crystallographic tilt. This broad peak split into two peaks (denoted as A and B), and peak B disappeared gradually when the mask began to be removed by selective etching. Only narrow peak A remained when the SiNx mask was removed completely. A model based on these results has been developed to show that there are two factors responsible for the crystallographic tilt: One is the non-uniformity elastic deformation caused by the interphase force between the ELO GaN layer and the SiNx mask. The other is the plastic deformation, which is attributed to the change of the threading dislocations (TDs)-from vertical in the window regions to the lateral in the regions over the mask.
Resumo:
The crystallographic tilt of the lateral epitaxial overgrown (LEO) GaN on sapphire Substrate with SiNx mask is investiaated by double crystal X-ray diffraction. Two wing peaks beside the GaN 0002 peak can be observed for the as-grown LEO GaN. During the selective etching of SiNx mask, each wing peak splits into two peaks, one of which disappears as the mask is removed, while the other remains unchanged. This indicates that the crystallographic tilt of the overgrown region is caused not only by the plastic deformation resulted from the bending of threading dislocations, but by the non-uniformity elastic deformation related with the GaN, SiNx interfacial forces. The widths of these two peaks are also studied in this paper. (C) 2002 Elsevier Science B.V. All rights reserved.