806 resultados para hydrolytically degradable polymer


Relevância:

100.00% 100.00%

Publicador:

Resumo:

This study investigated the differences in clinical outcomes between patients with bifurcation lesions (BL) treated with a biolimus-eluting stent (BES) with a biodegradable polymer, and a sirolimus-eluting stent (SES) with a durable polymer.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Bioresorbable polymeric films were prepared by solvent casting using a tyrosine-derived polycarbonate and metronidazole (MDZ) as the model drug at 2.5%, 5% and 10% (w/w). Drug loading did not affect the water uptake, drug release, polymer degradation or erosion profiles. All devices released approximately 85% (w/w) of the drug within a 1.5 h period. This may be attributed to the rapid water uptake of the polymer. An increase in the water uptake correlated with a linear rate increase of the polymer degradation (0.968 ≤ R2 ≤ 0.999). Moreover, MDZ presented a remarkable plasticizing effect for the polymer and drug loading exerted a significant impact on the mechanical properties of the obtained films. The results obtained can be used to further the development of novel biocompatible and biodegradable polymeric platforms for the delivery of metronidazole and other drugs in a broad range of pharmaceutical applications.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

OBJECTIVES: We assessed the impact of vessel size on outcomes of stenting with biolimus-eluting degradable polymer stent (BES) and sirolimus-eluting permanent polymer stent (SES) within a randomized multicenter trial (LEADERS). BACKGROUND: Stenting of small vessels might be associated with higher rates of adverse events. METHODS: "All-comer" patients (n = 1,707) were randomized to BES and SES. Post-hoc-stratified analysis of angiographic and clinical outcomes at 9 months and 1 year, respectively, was performed for vessels with reference diameter 2.75 mm. RESULTS: Of 1,707 patients, 429 patients in the BES group with 576 lesions and 434 patients in the SES group with 557 lesions had only small vessels treated (50.6% of the patient cohort). In patients with small vessels there was no significant difference in overall major adverse cardiac events (MACE) rate (12.1% vs. 11.8%; p = 0.89) or target lesion revascularization (TLR) rate (9.6% vs. 7.4%; p = 0.26) between BES and SES. The MACE and TLR rates in the small-vessel patient population were higher than in the large-vessel population. The TLR rate was 9.6% versus 2.6%, and MACE rate was 12.1% versus 7.1% for small versus large vessels in the BES arm (TLR: hazard ratio [HR] = 3.724, p = 0.0013; MACE: HR = 1.720, p = 0.0412). In the SES arm, TLR was 7.4% versus 5.1%, and MACE was 11.8% versus 10.3% in small versus large vessels (TLR: HR = 1.435, p = 0.2594; MACE: HR = 1.149, p = 0.5546). CONCLUSIONS: Prevalence of small vessel disease is high in an "all-comer" population with higher TLR and MACE rates. The BES and SES seem equivalent in treatment outcomes of small vessels in this "all-comer" patient population.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The criteria involved in the degradation of polyethylene-based degradable polymer samples have been investigated, with a view to obtaining a clearer mechanism of photo-biodegradation. The compatibility of degradable polymer samples during materials recycling was also studied. Commercial and laboratory prepared degradable polymer samples were oxidised in different environments and the oxidation products formed were studied using various analytical chromatographic and spectroscopic techniques such as HPLC, FT-IR and NMR. It was found that commercial degradable polymer samples which are based on the ECO systems, degrade predominantly via the Norrish II process, whereas the other degradable systems studied (starch-filled polyethylene systems, transition metal systems, including metal carboxylate based polyethylene systems and the photoantioxidant-activator systems) photodegrade essentially via the Norrish I process. In all cases, the major photoxidation products extracted from the degradable polymer samples were found to be carboxylic acids, although, in the polymer itself a mixture of carbonyl containing products such as esters, lactones, ketones and aldehydes was observed. The study also found that the formation of these hydrophilic carbonyl products causes surface swelling of the polymer, thus making bioerosion possible. It was thus concluded that environmental degradation of LDPE is a two step process, the initiation stage being oxidation of the polymer which gives rise to bioassimilable products, which are consequently bioeroded in the second stage, (the biodegradation step). Recycling of the degradable polymer samples as 10% homogeneous and heterogeneous blends was carried out using a single screw extruder (180°C and 210°C) and an internal mixer (190°C). The study showed that commercial degradable polymer samples may be recycled with a minimal loss in their properties.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Current artificial heart valves are classified as mechanical and bioprosthetic. An appealing pathway that promises to overcome the shortcomings of commercially available heart valves is offered by the interdisciplinary approach of cardiovascular tissue engineering. However, the mechanical properties of the Tissue Engineering Heart Valves (TEHV) are limited and generally fail in the long-term use. To meet this performance challenge novel biodegradable triblock copolymer poly(ethylene oxide)-polypropylene oxide)-poly(ethylene oxide) (PEO-PPO-PEO or F108) crosslinked to Silk Fibroin (F108-SilkC) to be used as tri-leaflet heart valve material was investigated. ^ Synthesis of ten polymers with varying concentration and thickness (55 µm, 75 µm and 100 µm) was achieved via a covalent crosslinking scheme using bifunctional polyethylene glycol diglycidyl ether (PEGDE). Static and fatigue testing were used to assess mechanical properties of films, and hydrodynamic testing was performed to determine performance under a simulated left ventricular flow regime. The crosslinked copolymer (F108-Silk C) showed greater flexibility and resilience, but inferior ultimate tensile strength, by increasing concentration of PEGDE. Concentration molar ratio of 80:1 (F108: Silk) and thickness of 75 µm showed longer fatigue life for both tension-tension and bending fatigue tests. Four valves out of twelve designed satisfactorily complied with minimum performance requirement ISO 5840, 2005. ^ In conclusion, it was demonstrated that the applicability of a degradable polymer in conjugation with silk fibroin for tissue engineering cardiovascular use, specifically for aortic valve leaflet design, met the performance demands. Thinner thicknesses (t<75 µm) in conjunction with stiffness lower than 320 MPa (80:1, F108: Silk) are essential for the correct functionality of proposed heart valve biomaterial F108-SilkC. Fatigue tests were demonstrated to be a useful tool to characterize biomaterials that undergo cyclic loading. ^

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Les acides biliaires sont des composés naturels existants dans le corps humain. Leur biocompatibilité, leur caractère amphiphile et la rigidité de leur noyau stéroïdien, ainsi que l’excellent contrôle de leurs modifications chimiques, en font de remarquables candidats pour la préparation de matériaux biodégradables pour le relargage de médicaments et l'ingénierie tissulaire. Nous avons préparé une variété de polymères à base d’acides biliaires ayant de hautes masses molaires. Des monomères macrocycliques ont été synthétisés à partir de diènes composés de chaînes alkyles flexibles attachées à un noyau d'acide biliaire via des liens esters ou amides. Ces synthèses ont été réalisées par la fermeture de cycle par métathèse, utilisant le catalyseur de Grubbs de première génération. Les macrocycles obtenus ont ensuite été polymérisés par ouverture de cycle, entropiquement induite le catalyseur de Grubbs de seconde génération. Des copolymères ont également été préparés à partir de monolactones d'acide ricinoléique et de monomères cycliques de triester d’acide cholique via la même méthode. Les propriétés thermiques et mécaniques et la dégradabilité de ces polymères ont été étudiées. Elles peuvent être modulées en modifiant les différents groupes fonctionnels décorant l’acide biliaire et en ayant recours à la copolymérisation. La variation des caractéristiques physiques de ces polymères biocompatibles permet de moduler d’autres propriétés utiles, tel que l’effet de mémoire de forme qui est important pour des applications biomédicales.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Designing degradable hydrogels is complicated by the structural and temporal complexities of the gel and evolving tissue. A major challenge is to create scaffolds with sufficient mechanical properties to restore initial function while simultaneously controlling temporal changes in the gel structure to facilitate tissue formation. Poly(ethylene glycol) was used in this work, to form biodegradable poly(ethylene glycol)-based hydrogels with hydrolyzable poly-l-lactide segments in the backbone. Non-degradable poly(ethylene glycol) was also introduced in the formulation to obtain control of the degradation profile that encompasses cell growth and new tissue formation. The dependence on polymer composition was observed by higher degradation profiles and decreased mechanical properties as the content of degradable segments was increased in the formulation. Based on in vitro tests, no toxicity of extracts or biomaterial in direct contact with human adipose tissue stem cells was observed, and the ultraviolet light treatment did not affect the proliferation capacity of the cells.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

There are currently few biomaterials which combine controlled degradation rates with ease of melt processability. There are however, many applications ranging from surgical fixation devices to drug delivery systems which require such combination properties. The work in this thesis is an attempt to increase the availability of such materials. Polyhydroxybutyrate-polyhydroxyvalerate copolymers are a new class of potentially biodegradable materials, although little quantitative data relating to their in vitro and in vivo degradation behaviour exists. The hydrolytic degradation of these copolymers has been examined in vitro under conditions ranging from `physiological' to extremes of pH and elevated temperature. Progress of the degradation process was monitored by weight loss and water uptake measurement, x-ray diffractometry, optical and electron microscopy, together with changes in molecular weight by gel permeation chromatography. The extent to which the degradation mechanism could be modified by forming blends with polysaccharides and polycaprolactone was also investigated. Influence of the valerate content, molecular weight, crystallinity, together with the physical form of the sample, the pH and the temperature of the aqueous medium on the hydrolytic degradation was investigated. Its progress was characterised by an initial increase in the wet weight, with concurrent decrease in the dry weight as the amorphous regions of the polymer are eroded, thereby producing an increase in matrix porosity. With the polysaccharide blends, this initial rate is dramatically affected, and erosion of the polysaccharide from the matrix markedly increases the internal porosity which leads to the eventual collapse of the matrix, a process which occurs, but less rapidly, in the degradation of the unblended polyhydroxybutyrate-polyhydroxyvalerate copolymers. Surface energy measurement and goniophotometry proved potentially useful in monitoring the early stages of the degradation, where surface rather than bulk processes predominate and are characterised by little weight loss.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The purpose of this study was to evaluate the impact and fracture resistance of acrylic resins: a heat-polymerized resin, a high-impact resin and an experimental polymethyl methacrylate with elastomer in different proportions (10, 20, 40 and 60%). 120 specimens were fabricated and submitted to conventional heat-polymerization. For impact test, a Charpy-type impact tester was used. Fracture resistance was assessed with a 3-point bending test by using a mechanical testing machine. Ten specimens were used for each test. Fracture (MPa) and impact resistance values (J.m-1) were submitted to ANOVA - Bonferroni's test - 5% significance level. Materials with higher amount of elastomer had statistically significant differences regarding to impact resistance (p < 0.05). Fracture resistance was superior (p < 0.01) for high-resistance acrylic resin. The increase in elastomer concentration added to polymethyl methacrylate raised the impact resistance and decreased the fracture resistance. Processing the material by injection decreased its resistance to impact and fracture.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work three capillary columns, one with uncoated inner wall and two with covalently-bound internal coatings - poly(vinyl alcohol) (PVA) and poly(dimethylacrylamide) (PDMA) - both covalently covered - were used to separate DNA fragments and compared to DNA separation using replaceable polymer solutions. The separations were performed using hydroxyethylcellulose (HEC) (90-105 kDa) in concentrations ranging from 0.00 to 2.00% m/v. The results indicated that the separation efficiency was higher in the PVA capillary than in the PDMA in all evaluated concentrations of HEC. In addition, higher resolution was also observed in PVA-coated capillary since in PDMA the shape of the peaks was not reproducible when subsequent runs were performed. Contrary to what has previously been reported in the literature, no reasonable separation was possible in bare fused silica.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends formed by electrochemical polymerization of polypyrrole (PPy) into polyacrylamide (PAAm) hydrogels were used as devices for controlled drug release. The influence of several parameters in the synthesis, such as type of hydrogel matrix and polymerization conditions was studied by using a fractional factorial design. The final goal was to obtain an adequate device for use in controlled release tests, based on electrochemical potential control. For controlled release tests, Safranin was used as model drug and release curves (amount of drug vs. time) have shown that these blends are promising materials for this use. The optimized blends obtained were characterized by cyclic voltammetry and Raman spectroscopy.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have investigated the structure of disordered gold-polymer thin films using small angle x-ray scattering and compared the results with the predictions of a theoretical model based on two approaches-a structure form factor approach and the generalized Porod law. The films are formed of polymer-embedded gold nanoclusters and were fabricated by very low energy gold ion implantation into polymethylmethacrylate (PMMA). The composite films span (with dose variation) the transition from electrically insulating to electrically conducting regimes, a range of interest fundamentally and technologically. We find excellent agreement with theory and show that the PMMA-Au films have monodispersive or polydispersive characteristics depending on the implanted ion dose. (C) 2010 American Institute of Physics. [doi:10.1063/1.3493241]

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Shallow subsurface layers of gold nanoclusters were formed in polymethylmethacrylate (PMMA) polymer by very low energy (49 eV) gold ion implantation. The ion implantation process was modeled by computer simulation and accurately predicted the layer depth and width. Transmission electron microscopy (TEM) was used to image the buried layer and individual nanoclusters; the layer width was similar to 6-8 nm and the cluster diameter was similar to 5-6 nm. Surface plasmon resonance (SPR) absorption effects were observed by UV-visible spectroscopy. The TEM and SPR results were related to prior measurements of electrical conductivity of Au-doped PMMA, and excellent consistency was found with a model of electrical conductivity in which either at low implantation dose the individual nanoclusters are separated and do not physically touch each other, or at higher implantation dose the nanoclusters touch each other to form a random resistor network (percolation model). (C) 2009 American Vacuum Society. [DOI: 10.1116/1.3231449]

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have investigated the fundamental structural properties of conducting thin films formed by implanting gold ions into polymethylmethacrylate (PMMA) polymer at 49 eV using a repetitively pulsed cathodic arc plasma gun. Transmission electron microscopy images of these composites show that the implanted ions form gold clusters of diameter similar to 2-12 nm distributed throughout a shallow, buried layer of average thickness 7 nm, and small angle x-ray scattering (SAXS) reveals the structural properties of the PMMA-gold buried layer. The SAXS data have been interpreted using a theoretical model that accounts for peculiarities of disordered systems.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A buried conducting layer of metal/polymer nanocomposite was formed by very low energy gold ion implantation into polymethylmethacrylate. The conducting layer is similar to 3 nm deep and of width similar to 1 nm. In situ resistivity measurements were performed as the implantation proceeded, and the conductivity thus obtained as a function of buried gold concentration. The measured conductivity obeys the behavior well established for composites in the percolation regime. The critical concentration, below which the polymer remains an insulator, is attained at a dose similar to 1.0 x 10(16) atoms/cm(2) of implanted gold ions. (C) 2008 American Institute of Physics.