Titanium alloys, alloys, especially beta-type alloys containing beta-stabilizing elements, constitute a highly versatile category of metallic materials that have been under constant development for application in orthopedics and dentistry. This type of alloy generally presents a high mechanical strength-to-weight ratio, excellent corrosion resistance and low elastic modulus. The purpose of this study is to evaluate the cytotoxicity and adhesion of fibroblast cells on titanium alloy substrates containing Nb, Ta, Zr, Cu, Sn and Mo alloying elements. Cells cultured on polystyrene were used as controls. In vitro results with Vero cells demonstrated that the tested materials, except Cu-based alloy, presented high viability in short-term testing. Adhesion of cells cultured on disks showed no differences between the materials and reference except for the Ti-Cu alloy, which showed reduced adhesion attributed to poor metabolic activity. Titanium alloys with the addition of Nb, Ta, Zr, Sn and Mo elements show a promising potential for biomedical applications. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Ti-Mo alloys from 4 to 20 Mo wt.% were arc-melted. Their compositions and surfaces were analyzed by EDX, XRF and SEM. The Mo mapping shows a homogeneous distribution for all alloys. The XRD analysis showed that the crystal structure of the alloys is sensitive to the Mo concentration; a mixture of the hexagonal alpha' and orthorhombic alpha '' phases was observed for the Ti-4Mo alloy, and the alpha '' phase is observed almost exclusively when the concentration of Mo added to the Ti reaches 6%. A significant retention of the beta phase is observed for the alloy containing 10% Mo, while at higher Mo concentrations (15% and 20%), retention of phase beta is only verified. Preliminary electrochemical studies have indicated a valve-metal behavior and good corrosion resistance in aerated Ringer solution for all alloys. (c) 2006 Published by Elsevier B.V.
Resumo:
An electron-beam melting and centrifugal splat-quenching technique for the production of microflakes of Ti-6A1-4V (wt%) alloy quenched at an average cooling rate of about 105 K sec–1 is described. The effect of substrate angle on the shape, size, microstructure and average cooling rate of the flakes of major sieve fractions is discussed. Morphologies of particles of minor sieve fractions are dealt with briefly.
Resumo:
The synthesis of nanostructured materials is a critical step in the development elf these novel materials. The basic principles involved in the production of nanocrystals and nanocomposites by rapid solidification are dealt with. An analysis of the various factors influencing the final grain size of the nanocrystals achieved during mechanical alloying has been presented. The devitrification of amorphous phase formed during rapid solidification processing and mechanical alloying provides an alternative and attractive route. Examples of the synthesis of nanostructured materials using these three different routes are drawn from our work on titanium alloys.
Resumo:
In the present study, solidification microstructure and texture evolution in grain-refined Ti-6Al-4V and γ-TiAl alloys via trace boron addition are compared with their baseline counterparts. Boron addition resulted in dramatic grain refinement by almost an order of magnitude. The texture developed in these alloys is also markedly different from the baseline alloys.
Resumo:
Titaniuni and its alloys have many applications in aerospace, marine and other engineering industries. Titanium requires special melting techniques because of its high reactivity at elevated temperatures and needs special mould materials and methods for castings. This paper reviews the development of titanium casting technology.
Resumo:
A metastable nano-scale disordered precipitate with orthorhombic symmetry has been identified using high resolution scanning transmission electron microscopy. The phase, termed O', is metastable, formed by a shuffle mechanism involving a {110}<1<(1)over bar>0> transverse phonon wave in samples of Ti-26Nb-2Zr (at.%) quenched from the beta phase. The addition of 2% Zr to Ti-26Nb appears to suppress significantly the stability of both the {11 (2) over bar}<111> shear and 2/3 <111> longitudinal phonon wave but promotes the {110}<1<(1)over bar>0> transverse shuffle. This results in the nano-size O' phase being homogeneously formed in the parent beta phase matrix rather than the massive alpha `' phase. (C) 2016 Elsevier B.V. All rights reserved.
Resumo:
Cylindrical specimens (4 mm diameter and 4 mm height) of titanium alloy bar were given various heat treatments to provide a wide range of microstructures and mechanical parameters. These specimens were then subjected to high plastic strain at a large strain rate (103 s-1 ) during dynamic compression by a split Hopkinson bar at ambient temperature. The microstructures of the localised shear bands were examined by optical and transmission electron microscopy. The results show that there are two types of localised shear bands: deformed and white shear bands. A detailed observation reveals that there is no difference in the nature of the deformed and white shear bands, but they occur at different stages of localised deformation. It is found that there is a burst of strain, corresponding to a critical strain rate at which the white shear band occurs and no phase transformation occurs in the shear bands.