An efficient diode-pumped laser was demonstrated by using an ytterbium-doped laser crystal, Yb:Gd2SiO5 (Yb:GSO), wherein Yb3+ ions exhibit the largest ground-state splitting among all the ytterbium-doped crystals. The Yb:GSO laser can be operated at a low pumping threshold, and the most efficient laser occurs around 1088 nm since the corresponding emission band has the largest emission cross section and the lowest thermal population. A slope efficiency of 75% was demonstrated for a continuous-wave Yb:GSO laser at 1094 nm, and self-pulsed lasers were achieved within the tunable range of 1091-1105 nm, which are the longest laser wavelengths achieved for Yb3+ lasers. (c) 2006 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A new Yb-doped oxyorthosilicate laser crystal, Yb:Gd2SiO5 (Yb:GSO), has been grown by the Czochralski (Cz) method. The crystal structure was determined by means of X-ray diffraction analysis. Room temperature absorption and fluorescence spectra of Yb3+ ions in GSO crystal were measured. Then. spectroscopic parameters of Yb:GSO were calculated and compared with those of another Yb-doped oxyorthosilicate crystal Yb:YSO. Results indicated that Yb:GSO crystal seemed to be a very promising laser gain media in generating ultra-pulses and tunable solid state laser applications. As expected, the output power of 2.72 W at 1089 nm was achieved in Yb:GSO crystal with absorbed power of only 4.22 W at 976 nm, corresponding to the slope efficiency of 71.2% through the preliminary laser experiment. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Yb:Gd2SiO5 (Yb:GSO) exhibits a large fundamental manifold splitting. Its long-wavelength emission band around 1088 nm, which has the largest emission cross section, encounters the lowest reabsorption losses caused by thermal population of the terminal laser level. As a result, low-threshold and tunable continuous-wave Yb:GSO lasers were demonstrated. A slope efficiency up to 86% and a pumping threshold as low as 127 mW were achieved for a continuous-wave Yb:GSO laser at 1092.5 nm under the pump of a high-brightness laser diode. A continuous tunability between 1000 and 1120 nm was realized with an SF14 prism as the intracavity tuning element. (c) 2006 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report the measured group delay dispersion (GDD) of new crystals Yb:Gd2SiO5 (Yb:GSO), Yb:GdYSiO5 (Yb:GYSO) and Yb:LuYSiO5 (Yb:LYSO) over wavelengths from 1000nm to 1200nm, with a white-light interferometer. Those GDD data should be useful for the dispersion compensation for femtosecond pulse generation in the lasers with these new crystals as the gain media. (C) 2007 Optical Society of America

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Compact femtosecond laser operation of Yb:Gd2SiO5 (Yb:GSO) crystal was demonstrated under high-brightness diode-end-pumping. A semiconductor saturable absorption mirror was used to start passive mode-locking. Stable mode-locking could be realized near the emission bands around 1031, 1048, and 1088 nm, respectively. The mode-locked Yb: GSO laser could be tuned from one stable mode-locking band to another with adjustable pulse durations in the range 1 similar to 100 ps by slightly aligning laser cavity to allow laser oscillations at different central wavelengths. A pair of SF10 prisms was inserted into the laser cavity to compensate for the group velocity dispersion. The mode-locked pulses centered at 1031 nm were compressed to 343 fs under a typical operation situation with a maximum output power of 396 mW. (c) 2007 Optical Society of America.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Gd2SiO5 (GSO) single crystal codoped with Yb3+ and Er3+ (Abbr. as Er:Yb:GSO) was successfully grown by the Czochralski (CZ) method for the first time and the spectral characteristics were investigated. The absorption and fluorescence spectra were measured. The emission lifetime of the I-4(13/2)-Er-level was measured to be 5.84ms and the emission cross-section at 1529nm was calculated to be 1.03 x 10(-20) cm(2). The results indicate that Er:Yb:GSO is a potential laser material at similar to 1. 55 mu m wavelength region. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

For the first time, a high optical quality 10 at.% Yb3+-doped gadolinium oxyorthosilicate laser crystal Gd2SiO5 (GSO) was grown by the Czochralski (Cz) method. The segregation coefficient of Yb3+ was studied by the inductively coupled plasma atomic emission spectrometer (ICP-AES) method. The crystal structure has monoclinic symmetry with space group P2(1)/c; this was determined by means of an x-ray diffraction analysis. The absorption spectra, fluorescence spectra and fluorescence decay curves of Yb3+ ions in a GSO crystal at room temperature were also studied. Then, the spectroscopic parameters of Yb:GSO were calculated. The advantages of the Yb:GSO crystal include high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections and particularly broad emission bandwidth (similar to 72 nm). The results indicated that the Yb:GSO crystal seemed to be a very promising laser gain medium in diode-pumped femtosecond laser and tunable solid state laser applications when LD pumped at 940 and 980 nm.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We report what is believed to be the first demonstration of the laser action of Yb3+ -doped Gd2SiO5 (Yb:GSO) crystal pumped by a 940-nm laser diode at room temperature. The threshold of laser generation is only 0.85 kW/cm(2), which is smaller than the theoretic threshold of Yb:YAG (1.54 kW/cm(2)). The laser wavelength is 1090 mn. With a 2.5% output coupler, the maximum output power is 415 mW under a pump power of 5 W. By using the SESAM, the Q-switched mode locking and CW mode-locked operations are demonstrated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The intensity pulsations of a cw 1030 nm Yb:Phosphate monolithic waveguide laser with distributed feedback are described. We show that the pulsations could result from the coupling of the two orthogonal polarization modes through the two photon process of cooperative luminescence. The predictions of the presented theoretical model agree well with the observed behaviour.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Clusterin is a stress-activated, cytoprotective chaperone that confers broad-spectrum treatment resistance in cancer. However, the molecular mechanisms mediating CLU transcription following anticancer treatment stress remain incompletely defined. We report that Y-box binding protein-1 (YB-1) directly binds to CLU promoter regions to transcriptionally regulate clusterin expression. In response to endoplasmic reticulum stress inducers, including paclitaxel, YB-1 is translocated to the nucleus to transactivate clusterin. Furthermore, higher levels of activated YB-1 and clusterin are seen in taxane-resistant, compared with parental, prostate cancer cells. Knockdown of either YB-1 or clusterin sensitized prostate cancer cells to paclitaxel, whereas their overexpression increased resistance to taxane. Clusterin overexpression rescued cells from increased paclitaxel-induced apoptosis following YB-1 knockdown; in contrast, however, YB-1 overexpression did not rescue cells from increased paclitaxel-induced apoptosis following clusterin knockdown. Collectively, these data indicate that YB-1 transactivation of clusterin in response to stress is a critical mediator of paclitaxel resistance in prostate cancer. Mol Cancer Res; 9(12); 1755–66.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

To study the phase relations in the Bi-2212 and Yb2O3 system, Bi2Sr2Ca1-xYbxCu 2Oy thick films are prepared by partial melt processing via an intermediate reaction between Bi-2212 and Yb2O3. When Bi-2212 and Yb2O3 are partially melted and then slowly cooled, solid solutions of Bi2Sr2Ca 1-xYbxCu2Oy, form by reactions between liquid and solid phases which contain Yb. Following these reactions, Ca is partially replaced in Bi-2212 matrix and participates in the formation of secondary phases, such as Bi-free, (Ca, Sr)Ox and CaO. Variation of the Bi-2212-Yb2O3 ratios and processing parameters changes the balance between the phases and leads to different Yb:Ca ratios in the Bi-2212 matrix of processed thick films. When the partial melting process is optimized for each sample to minimize the growth of secondary phases, x = 0.42-0.46 for the samples prepared at pO2 = 0.01 atm, x = 0.24-0.29 for the samples prepared at pO2 = 0.21 atm, x = 0.18-0.23 for the samples prepared at pO2 = 0.99 atm are obtained regardless to the starting compositions. It is found that superconducting properties of Bi 2Sr2Ca1-xYbxCu2O y thick films strongly depend on the processing conditions, because the conditions result in different Yb content in the Bi-2212 matrix and the volume fraction of the secondary phases. The highest Tc(0) of 77, 90 and 91 K were obtained for the samples processed at 0.01, 0.21 and 0.99 atm of O2, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

He II photoelectron spectra of La, Ce and Yb show features which cannot be explained in terms of single electron excitations. It is proposed that these are due to formation of electron-hole paris.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The valence state of Yb in some of its intermetallics, YbNi2Ge2, YbCu2Si2 and YbPd2Si2 has been investigated by LIII(Yb) absorption edges and X-ray pnotoelectron spectra in the 4f and 4d regions. These studies establish the presence of mixed valence in all three systems and illustrate the utility of 4f and 4d spectra in the study of mixed valence in Yb compounds.