909 resultados para Silicon concentration
Resumo:
Silicon (Si) accumulation in organs and cells is one of the most prominent characteristics of plants of the family Poaceae. Many species from this family are used as forage plants for animal feeding. The present study investigates in Brachiaria brizantha (Hochst. ex A. Rich.) Stapf. cv. Marandu: (1) the dry matter production and Si content in shoot due to soil Si fertilizations; (2) the Si distribution among shoot parts; and (3) the silica deposition and localization in leaves. Plants of B. brizantha cv. Marandu were grown under contrasting Si supplies in soil and nutrient solution. Silica deposition and distribution in grass leaf blades were observed using light microscope and scanning electron microscope equipped with an energy dispersive X-ray spectrometer (SEM-EDXS). Silicon concentration in the B. brizantha shoot increased according to the Si supply. Silicon in grass leaves decreased following the order: mature leaf blades > recently expanded leaf blades > non-expanded leaf blades. Silicon accumulates mainly on the upper (adaxial) epidermis of the grass leaf blades and, especially, on the bulliform cells. The Si distribution on adaxial leaf blade surface is non uniform and reflects a silica deposition exclusively on the cell wall of bulliform cells.
Resumo:
The effect of increasing the amount of added grain refiner on grain size and morphology has been investigated for a range of hypoeutectic Al-Si alloys. The results show a transition in grain size at a silicon concentration of about 3 wt% in unrefined alloys; the grain size decreasing with silicon content before the transition, and increasing beyond the transition point. A change in morphology also occurs with increased silicon content. The addition of grain refiner leads to greater refinement for silicon contents below the transition point than for those contents above the transition point, while the transition point seems to remain unchanged. The slope of the grain size versus silicon content curve after the transition seems to be unaffected by the degree of grain refinement. The results are related to the competitive processes of nucleation and constitutional effects during growth and their impact on nucleation kinetics. (C) 1999 Elsevier Science S.A. All rights reserved.
Resumo:
In this work we report studies of the photoluminescence emission in samples based on Si/SiOx films deposited by the Pulsed Electron Beam Ablation (PEBA) technique. The samples were prepared at room temperature using targets with different Si/SiO2 concentrations. The samples were characterized using X-ray Absorption Edge Spectroscopy (XANES) at the Si-K edge, Raman spectroscopy, Photoluminescence (PL) and X-ray Photoelectron Spectroscopy (XPS). The concentration of a-Si and nc-Si in the film was dependent on the silicon concentration in the target. It was also observed that the PL is strongly dependent on the structural amorphous/crystalline arrangement. Crown Copyright (C) 2011 Published by Elsevier B.V. All rights reserved.
Resumo:
An experimental programme has been undertaken to determine which of the grain formation mechanisms of equiaxed crystals are dominant in the solidification of Al-Si foundry alloys. Small ingots were cast from alloys of varying silicon concentration with and without gauze barriers, using different types of mould materials and different mould preheats. The results show that two mechanisms of grain nucleation are operating. The first is a wall mechanism where crystals are nucleated either on or near the mould wall owing to thermal undercooling. The second is a constitutional supercooling mechanism where nucleants are activated in the constitutionally undercooled zone ahead of the advancing interface. As a consequence, the grain size decreases with increasing silicon content. However a transition in the growth mode occurs once a critical degree of constitutional undercooling is exceeded. This change in growth is accompanied by an increase in grain size. The transition point can be shifted with respect to solute content by changing the casting conditions, and a mechanism is proposed to explain this effect. MST/4109
Resumo:
The dendrite coherency point of Al-Si-Cu alloys was determined by thermal analysis and rheological measurement methods by performing parallel measurements at two cooling rates for aluminum alloys across a wide range of silicon and copper contents. Contrary to previous findings, the two methods yield significantly different values for the fraction solid at the dendrite coherency point. This disparity is greatest for alloys of low solute concentration. The results from this study also contradict previously reported tl ends in the effect of cooling rate on the dendritic coherency point. Consideration of the results shows that thermal analysis is not a valid technique for the measurement of coherency. Analysis of the results from rheological testing indicates that silicon concentration has a dominant effect on grain size and dendritic morphology, independent of cooling rate and copper content, and thus is the factor that determines the fraction solid at dendrite coherency for Al-Si-Cu alloys.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pós-graduação em Ciência Florestal - FCA
Resumo:
These studies were performed from September 10 to 29, 2007 in the Kara Sea in transects westward of the Yamal Peninsula, near the St. Anna Trough, in the Ob River estuary (Obskay Guba), and on the adjacent shelf. Concentration of chlorophyll a in the euphotic layer varied from 0.02 to 4.37 µg/l, aver. 0.76 µg/l. Primary production in the water column varied from 10.9 to 148.0 mg C/m**2/day (aver. 56.9 mg C/m**2/day). It was shown that frontal zones divided the Kara Sea into distinct areas with different productivities. Maximum levels of primary production were measured in the deep part of the Yamal transect (132.4 mg C/m**2/day) and the shallow Kara Sea shelf near the Ob River estuary (74.9 mg C/m**2/day). Characteristics of these regions were low salinity of the surface water layer (19-25 psu) and elevated silicon concentration (12.8-28.1 µg-atom/l). It is explainable by river runoff. Frontal zones of the Yamal current within the Yamal and Ob transects showed high assimilation numbers reached to 2.32 and 1.49 mg C/mg Chl/hr, respectively; they were maximal for studied areas.
Resumo:
Results of studies during Project of an international expedition onboard R/V Vladimir Parshin in September-October 2005 are presented. Intensive development of Bacillariophyceae and Dynophyceae was recorded in coastal waters of Bulgaria, Turkey, and in the Danube River delta during period of investigations. Increase in algae population was accompanied by rising of chlorophyll a concentration up to 2.0-5.5 µg/l. In the deep water region it did not exceed 0.5 µg/l. Phytoplankton growth rate in the surface water layer varied from 0.1 to 1.0 1/day. This parameter and NO2+NO3 concentration, as well as the silicon concentration were correlative, as was described by the Michaelis-Menten equation. Phytoplankton growth was affected by basic nutrients. Zooplankton grazing varied from 0.10 to 0.69 1/day and average values in different regions varied by 1.5 times. Microalgae size range is one of major factors of grazing regulation. Rate of phytoplankton consumption was decreasing with increasing the largest diatom Pseudosolenia calcar-avis impact on total biomass of nano- and microphytoplankton.
Resumo:
A novel HCPV nonimaging concentrator concept with high concentration (>500×) is presented. It uses the combination of a commercial concentration GaInP∕GaInAs∕Ge 3J cell and a concentration Back‐Point‐Contact (BPC) concentration silicon cell for efficient spectral utilization, and external confinement techniques for recovering the 3J cell′s reflection. The primary optical element (POE) is a flat Fresnel lens and the secondary optical element (SOE) is a free‐form RXI‐type concentrator with a band‐pass filter embedded it, both POE and SOE performing Köhler integration to produce light homogenization. The band‐pass filter sends the IR photons in the 900–1200 nm band to the silicon cell. Computer simulations predict that four‐terminal terminal designs could achieve ∼46% added cell efficiencies using commercial 39% 3J and 26% Si cells. A first proof‐of concept receiver prototype has been manufactured using a simpler optical architecture (with a lower concentration, ∼ 100× and lower simulated added efficiency), and experimental measurements have shown up to 39.8% 4J receiver efficiency using a 3J with peak efficiency of 36.9%
Resumo:
Recently it has been shown that modification with strontium causes an increase in the size of eutectic grains. The eutectic grain size increases because there are fewer nucleation events, possibly due to the poisoning of phosphorus-based nuclei that are active in the unmodified alloy. The current paper investigates the effect of strontium concentration on the eutectic grain size. In the aluminium-10 wt.% silicon alloy used in this research, for fixed casting conditions, the eutectic grain size increases as the strontium concentration increases up to approximately 150ppm, beyond which the grain size is relatively stable. This critical strontium concentration is likely to differ depending on the composition of the base alloy, including the concentration of minor elements and impurities. It is concluded that processing and in-service properties of strontium modified aluminium-silicon castings are likely to be more stable if a minimum critical strontium concentration is exceeded. If operating below this critical strontium concentration exceptional control over composition and casting conditions is required. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
In this paper, we use a model of hydrogenated amorphous silicon generated from molecular dynamics with density functional theory calculations to examine how the atomic geometry and the optical and mobility gaps are influenced by mild hydrogen oversaturation. The optical and mobility gaps show a volcano curve as the hydrogen content varies from undersaturation to mild oversaturation, with largest gaps obtained at the saturation hydrogen concentration. At the same time, mid-gap states associated with dangling bonds and strained Si-Si bonds disappear at saturation but reappear at mild oversaturation, which is consistent with the evolution of optical gap. The distribution of Si-Si bond distances provides the key to the change in electronic properties. In the undersaturation regime, the new electronic states in the gap arise from the presence of dangling bonds and strained Si-Si bonds, which are longer than the equilibrium Si-Si distance. Increasing hydrogen concentration up to saturation reduces the strained bonds and removes dangling bonds. In the case of mild oversaturation, the mid-gap states arise exclusively from an increase in the density of strained Si-Si bonds. Analysis of our structure shows that the extra hydrogen atoms form a bridge between neighbouring silicon atoms, thus increasing the Si-Si distance and increasing disorder in the sample.
Resumo:
The influence of annealing on the mechanical properties of high-silicon cast iron for three alloys with distinct chromium levels was investigated. Each alloy was melted either with or without the addition of Ti and Mg. These changes in the chemical composition and heat treatment aimed to improve the material's mechanical properties by inhibiting the formation of large columnar crystals, netlike laminae, precipitation of coarse packs of graphite, changing the length and morphology of graphite, and rounding the extremities of the flakes to minimize the stress concentration. For alloys with 0.07 wt.% Cr, the annealing reduced the impact resistance and tensile strength due to an enhanced precipitation of refined carbides and the formation of interdendritic complex nets. Annealing the alloys containing Ti and Mg led to a decrease in the mechanical strength and an increase in the toughness. Alloys containing approximately 2 wt.% Cr achieved better mechanical properties as compared to the original alloy. However, with the addition of Ti and Mg to alloys containing 2% Cr, the chromium carbide formation was inhibited, impairing the mechanical properties. In the third alloy, with 3.5 wt.% of Cr additions, the mechanical strength improved. The annealing promoted a decrease in both hardness and amount of iron and silicon complex carbides. However, it led to a chromium carbide formation, which influenced the mechanical characteristics of the matrix of the studied material.
Resumo:
Silicon nitride particles were incorporated to electrolytic copper by co-electrodeposition in acidic sulfate bath, aiming the improvement of its mechanical resistance. Smooth deposits containing well-distributed silicon nitride particles were obtained. The current density did not show significant influence on incorporated particle volume fraction, whereas the variation of particle concentration in the bath had a more pronounced effect. The microhardness of the composite layers was higher than that of pure copper deposits obtained under the same conditions and increased with the increase of incorporated particle volume fraction. The microhardness of composites also increased with the increase of current density due to copper matrix grain refining. The composite coatings were slightly more corrosion resistant than pure copper deposits in 3.5% NaCl solutions.