The TA2 phonon dispersion curves of Ni-Mn-Ga alloys with different compositions which transform to different martensitic structures have been measured over a broad temperature range covering both paramagnetic and ferromagnetic phases. The branches show an anomaly (dip) at a wave number that depends on the particular martensitic structure, and there is softening of these anomalous phonons with decreasing temperature. This softening is enhanced below the Curie point, as a consequence of spin-phonon coupling. This effect is stronger for systems with higher electronic concentration.
Resumo:
The magnetocaloric effect that originates from the martensitic transition in the ferromagnetic Ni-Mn-Gashape-memory alloy is studied. We show that this effect is controlled by the magnetostructural coupling at boththe martensitic variant and magnetic domain length scales. A large entropy change induced by moderatemagnetic fields is obtained for alloys in which the magnetic moment of the two structural phases is not verydifferent. We also show that this entropy change is not associated with the entropy difference between themartensitic and the parent phase arising from the change in the crystallographic structure which has beenfound to be independent of the magnetic field within this range of fields.
Resumo:
We have measured the adiabatic second order elastic constants of two Ni-Mn-Ga magnetic shape memory crystals with different martensitic transition temperatures, using ultrasonic methods. The temperature dependence of the elastic constants has been followed across the ferromagnetic transition and down to the martensitic transition temperature. Within experimental errors no noticeable change in any of the elastic constants has been observed at the Curie point. The temperature dependence of the shear elastic constant C' has been found to be very different for the two alloys. Such a different behavior is in agreement with recent theoretical predictions for systems undergoing multi-stage structural transitions.
Resumo:
Polycrystalline Ni-Mn-Ga thin films have been deposited by the pulsed laser deposition (PLD) technique, using slices of a Ni-Mn-Ga single crystal as targets and onto Si (100) substrates at temperatures ranging from 673 K up to 973 K. Off-stoichiometry thin films were deposited at a base pressure of 1×10-6-Torr or in a 5 mTorr Ar atmosphere. Samples deposited in vacuum and temperatures above 823 K are magnetic at room temperature and show the austenitic {220} reflection in their x-ray diffraction patterns. The temperature dependences of both electrical resistance and magnetic susceptibility suggest that these samples exhibit a structural martensitic transition at around 260 K. The magnetoresistance ratio at low temperature can be as high as 1.3%, suggesting the existence of a granular structure in the films
Resumo:
The magnetocaloric effect that originates from the martensitic transition in the ferromagnetic Ni-Mn-Gashape-memory alloy is studied. We show that this effect is controlled by the magnetostructural coupling at boththe martensitic variant and magnetic domain length scales. A large entropy change induced by moderatemagnetic fields is obtained for alloys in which the magnetic moment of the two structural phases is not verydifferent. We also show that this entropy change is not associated with the entropy difference between themartensitic and the parent phase arising from the change in the crystallographic structure which has beenfound to be independent of the magnetic field within this range of fields.
Resumo:
Traditional methods for studying the magnetic shape memory (MSM) alloys Ni-Mn-Ga include subjecting the entire sample to a uniform magnetic field or completely actuating the sample mechanically. These methods have produced significant results in characterizing the MSM effect, the properties of Ni-Mn-Ga and have pioneered the development of applications from this material. Twin boundaries and their configuration within a Ni-Mn-Ga sample are a key component in the magnetic shape memory effect. Applications that are developed require an understanding of twin boundary characteristics and, more importantly, the ability to predictably control them. Twins have such a critical role that the twinning stress of a Ni-Mn-Ga crystal is the defining characteristic that indicates its quality and significant research has been conducted to minimize this property. This dissertation reports a decrease in the twinning stress, predictably controlling the twin configuration and characterizing the dynamics of twin boundaries. A reduction of the twinning stress is demonstrated by the discovery of Type II twins within Ni-Mn-Ga which have as little as 10% of the twinning stress of traditional Type I twins. Furthermore, new methods of actuating a Ni-Mn-Ga element using localized unidirectional or bidirectional magnetic fields were developed that can predictably control the twin configuration in a localized area of a Ni-Mn-Ga element. This method of controlling the local twin configuration was used in the characterization of twin boundary dynamics. Using a localized magnetic pulse, the velocity and acceleration of a single twin boundary were measured to be 82.5 m/s and 2.9 × 107 m/s2, and the time needed for the twin boundary to nucleate and begin moving was less than 2.8 μs. Using a bidirectional magnetic field from a diametrically magnetized cylindrical magnet, a highly reproducible and controllable local twin configuration was created in a Ni-Mn-Ga element which is the fundamental pumping mechanism in the MSM micropump that has been co-invented and extensively characterized by the author.
Resumo:
The TA2 phonon dispersion curves of Ni-Mn-Ga alloys with different compositions which transform to different martensitic structures have been measured over a broad temperature range covering both paramagnetic and ferromagnetic phases. The branches show an anomaly (dip) at a wave number that depends on the particular martensitic structure, and there is softening of these anomalous phonons with decreasing temperature. This softening is enhanced below the Curie point, as a consequence of spin-phonon coupling. This effect is stronger for systems with higher electronic concentration.
Resumo:
The magnetocaloric effect that originates from the martensitic transition in the ferromagnetic Ni-Mn-Ga shape-memory alloy is studied. We show that this effect is controlled by the magnetostructural coupling at both the martensitic variant and magnetic domain length scales. A large entropy change induced by moderate magnetic fields is obtained for alloys in which the magnetic moment of the two structural phases is not very different. We also show that this entropy change is not associated with the entropy difference between the martensitic and the parent phase arising from the change in the crystallographic structure which has been found to be independent of the magnetic field within this range of fields.
Resumo:
We have measured the adiabatic second order elastic constants of two Ni-Mn-Ga magnetic shape memory crystals with different martensitic transition temperatures, using ultrasonic methods. The temperature dependence of the elastic constants has been followed across the ferromagnetic transition and down to the martensitic transition temperature. Within experimental errors no noticeable change in any of the elastic constants has been observed at the Curie point. The temperature dependence of the shear elastic constant C' has been found to be very different for the two alloys. Such a different behavior is in agreement with recent theoretical predictions for systems undergoing multi-stage structural transitions.
Resumo:
A set of stacked ribbon samples with the compositions Fe(85)Ga(15), Fe(78)Ni(7)Ga(15) and Fe(78)Co(7)Ga(15) were prepared. XRD on these ribbons show that the binary Fe(85)Ga(15) ribbon exhibits the disordered A2 structure where as the addition of Co and Ni leads to the appearance of an additional ordered DO(3) structure. A comparison of the ratio of the XRD-line intensities gave strong evidence of a (100) texture perpendicular to the ribbon surface. The optical studied microstructure supports these results because it shows a columnar grain growth parallel to the solidification direction-which is parallel to ribbon thickness. The highest magnetostriction was found for Fe(78)Ni(7)Ga(15) (370 ppm), while the Fe(78)Co(7)Ga(15) a smaller magnetostriction of 270 ppm was found. The enhancement of the magnetostriction is attributed to the (100) texture in these ribbons. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Os resíduos gerados em domicílios incluem diversos produtos, como pesticidas, produtos farmacêuticos, detergentes, óleos de cozinha, metais pesados contidos em baterias e outros utensílios. Esses resíduos são lançados continuamente em aterro sanitário ou lixões em cidades como Manaus. O chorume produzido nesses aterros, quando não tratados, contamina recursos hídricos superficiais e subterrâneos. Neste estudo foi feita uma avaliação das conseqüências da liberação do chorume no sistema hídrico da bacia do Tarumã-Açu. Amostras de água e sedimento foram coletadas nos igarapés Matrinxã, Acará, Bolívia, bacia do Tarumã-Açu e dentro do aterro sanitário (Manaus - Amazonas - Brasil) em março 2001. As amostras de água foram filtradas em filtro Milipore (0,45 mm de poro) e, em seguida, tratadas com HNO3 concentrado. As amostras de sedimento foram peneiradas em malha de 0,053 mm e digeridas com HCl:HNO3 (1:3) a 150ºC. As concentrações de alguns metais pesados (Co, Cu, Fe, Cr, Ni, Mn, Pb e Zn) foram determinadas nas amostras de água e sedimento por espectrometria de absorção atômica de chama. Os resultados revelaram que a concentração dos metais pesados é muito acima dos permitidos pela resolução 357/2005 do CONAMA em praticamente todos os locais amostrados, mostrando que o Aterro Sanitário é um dos principais responsáveis pelo impacto ambiental observado nos corpos hídricos estudados. As análises dos componentes principais (PCA) e hierárquica de cluster (HCA), revelam que os pontos de coleta localizados dentro do aterro sanitário apresentam características diferentes dos outros locais amostrados. Além disso, o HCA e PCA mostraram que existe uma similaridade entre os pontos de coleta localizados fora do aterro o que permite afirmar que o chorume do aterro se dissolve por todo corpo hídrico estudado.
Resumo:
Structural and magnetic transformations in the Heusler-based system Ni0.50Mn0.50¿xSnx are studied by x-ray diffraction, optical microscopy, differential scanning calorimetry, and magnetization. The structural transformations are of austenitic-martensitic character. The austenite state has an L21 structure, whereas the structures of the martensite can be 10M , 14M , or L10 depending on the Sn composition. For samples that undergo martensitic transformations below and around room temperature, it is observed that the magnetic exchange in both parent and product phases is ferromagnetic, but the ferromagnetic exchange, characteristic of each phase, is found to be of different strength. This gives rise to different Curie temperatures for the austenitic and martensitic states.