Resumo:

Theoretical calculations of the mode characteristics of an equilateral-triangle resonator (ETR) with a 10 mu m cavity side length show that the fundamental mode, with longitudinal mode index of 25, has a wavelength of 2.185 mu m and a longitudinal mode separation of 100 nm. This mode has a quality factor (similar to 2x10(5)) that is much larger than the first (similar to 5x10(4)) and second (similar to 3x10(4)) order modes, indicating that single fundamental mode lasing should be accessible over a broad wavelength tuning range. An electrically injected ETR based on this design is fabricated from an InGaAsSb/AlGaAsSb/GaSb, graded-index separate-confinement heterostructure, laser diode wafer with a 2.1 mu m emission wavelength. This device achieved single mode, continuous wave operation at 77 K with a threshold current of 0.5 mA and a single mode wavelength tuning range of 3.25 nm, which is accomplished by varying the injection current from 0.5 to 6.0 mA. (C) 2008 American Vacuum Society.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Effect of rapid thermal annealing on photoluminescence (PL) properties of InGaAs, InGaNAs, InGaAsSb, and InGaNAsSb quantum wells (QWs) grown by molecular-beam epitaxy was systematically investigated. Variations of PL intensity and full width at half maximum were recorded from the samples annealed at different conditions. The PL peak intensities of InGaAs and InGaNAs QWs initially increase and then decrease when the annealing temperature increased from 600 to 900 degrees C, but the drawing lines of InGaAsSb and InGaNAsSb take on an "M" shape. The enhancement of the PL intensity and the decrease of the full width at half maximum in our samples are likely due to the removal of defects and dislocations as well as the composition's homogenization. In the 800-900 degrees C high-temperature region, interdiffusion is likely the main factor influencing the PL intensity. In-N is easily formed during annealing which will prevent In out diffusion, so the largest blueshift was observed in InGaAsSb in the high-temperature region. (c) 2006 American Institute of Physics.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Radiant heat conversion performance dominated by the active layer of Ga0.84In0.16As0.14Sb0.86 diode has been systematically investigated based on an analytic absorption spectrum, which is suggested here by numerically fitting the limited experimental data. For the concerned diode configuration, our calculation demonstrates that the optimal base doping is 3-4 x 10(17) cm(-3), which is less sensitive to the variation of the external radiation spectrum. Given the scarcity of the alloy elements, an economical device configuration of the 0.2-0.6 mu m emitter and the 4-6 mu m base would be particularly acceptable because the corresponding conversion efficiency cannot exhibit discouraging degradation in comparison to the one for the optimal structure, the thickness of which may be up to 10 mu m. More importantly, the method we suggested here to calculate alloy absorption can be easily transferred to other composition, thus bringing great convenience for design or optimization of the optoelectronic device formed by these alloys.