Resumo:
The purpose of this study was to evaluate stress distribution in the hybrid layer produced by two adhesive systems using three-dimensional finite element analysis (FEA). Four FEA models (M) were developed: Mc, a representation of a dentin specimen (41 x 41 x 82 mu m) restored with composite resin, exhibiting the adhesive layer, hybrid layer (HL), resin tags, peritubular dentin, and intertubular dentin to simulate the etch-and-rinse adhesive system; Mr, similar to Mc, with lateral branches of the adhesive; Ma, similar to Mc, however without resin tags and obliterated tubule orifice, to simulate the environment for the self-etching adhesive system; Mat, similar to Ma, with tags. A numerical simulation was performed to obtain the maximum principal stress (sigma(max)). The highest sigma(max) in the HL was observed for the etch-and-rinse adhesive system. The lateral branches increased the sigma(max) in the HL. The resin tags had a little influence on stress distribution with the self-etching system. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Several studies have assessed the morphology and thickness of hybrid layer, the dentin bend strengths as well as sealing ability of dentin adhesive systems. However, few in vivo studies have evaluated the biocompatibility of the adhesive systems following application to deep dentin or directly to the pulp of human teeth. Many studies performed in non-human primate teeth or teeth of rats have reported pulp healing and dentin bridging following pulp capping with bonding agents. In addition, a few clinical and radiographical reports of the success of resin pulp capping have been described in the dental literature.Objectives: the aim of this review was to evaluate the literature on pulp responses following total acid etching and application of adhesive resins on deep cavities or pulp exposures. In addition, the clinical/radiographical evidence for the apparent success of vital pulp therapy and results obtained from animal and human studies were compared and discussed.Significance and conclusions: the self-etching adhesive systems may be useful and safe when applied on dentin, In contrast, persistent inflammatory reactions as well as delay in pulpal healing and failure of dentin bridging were seen in human pulps capped with bonding agents. The results observed in animal teeth cannot be directly extrapolated to human clinical conditions. Consequently, vital pulp therapy using acidic agents and adhesive resins seems to be contraindicated. (C) 2000 Academy of Dental Materials. Published by Elsevier B.V. Ltd. All rights reserved.
Resumo:
Objective: The aim of this in vitro study was to analyze the effect of glass-ionomer cement as a liner on the dentin/resin adhesive interface of lateral walls of occlusal restorations after thermocycling.Materials and Methods: Occlusal cavities were prepared in 60 human molars, divided into six groups: no liner (1 and 4); glass-ionomer cement (GIC, Ketac Molar Easymix, 3M ESPE) (2 and 5); and resin-modified glass-ionomer cement (RMGIC, Vitrebond, 3M ESPE) (3 and 6). Resin composite (Filtek Z250, 3M ESPE) was placed after application of an adhesive system (Adper Single Bond 2, 3M ESPE) that was mixed with a fluorescent reagent (Rhodamine B) to allow confocal microscopy analysis. Specimens of groups 4, 5 and 6 were thermocycled (5 degrees C-55 degrees C) with a dwell time of 30 seconds for 5000 cycles. After this period, teeth were sectioned in approximately 0.8-mm slices. One slice of each tooth was randomly selected for confocal microscopy analysis. The other slices were sectioned into 0.8 nun x 0.8 mm beams, which were submitted to microtensile testing (MPa). Data were analyzed using two-way ANOVA and Tukey test (p < 0.05).Results: There was no detectedstatistical difference on bond strength among groups (alpha < 0.05). Confocal microscopy analysis showed a higher mean gap size in group 4(12.5 mu m) and a higher percentage of marginal gaps in the thermocycled groups. The RNIGIC liner groups showed the lowest percentage of marginal gaps.Conclusions: Lining with RMGIC resulted in less gap formation at the dentin/resin adhesive interface after artificial aging. RMGIC or GIC liners did not alter the microtensile bond strength of adhesive system/resin composite to dentin on the lateral walls of Class I restorations.
Resumo:
The aim of this study was to evaluate the persistence of methacrylate-based cement residues on the dentin, after dentin surface cleaning with ethanol or acetone, with or without previous application of a dentin adhesive. Forty bovine crown fragments were obtained and the dentin surface was washed with 1.0 mL of 2.5% sodium hypochlorite (NaOCl), followed by 0.1 mL of 17% ethylenediaminetetraacetic acid application for 3 min, and final irrigation with 2.5% NaOCl. The specimens were air dried and resin-based cement was rubbed onto the dentine surface with a microbrush applicator. In 20 specimens, previously to cement, a dentin adhesive was applied in all surfaces. After 15 min, the surface was scrubbed with a cotton pellet and moistened with ethanol or acetone, compounding the following groups: G199.5% ethanol and G2acetone, without previous use of dentin adhesive; G399.5% ethanol and G4acetone, with previous use of dentin adhesive. The dentin surface was scrubbed until the cement residues could not be visually detected. Sections were then processed for scanning electron microscopy and evaluated at 500x magnification and scores were attributed to each image according to the area covered by residual sealer, and data were subjected to KruskalWallis at 5% significance. The lower residue presence was observed in G3 (P = 0.005). All surface presented cement residues when acetone was used as cleaning solution (P = 0.0005). The cleaning solutions were unable to completely remove the cement residues from both surfaces. The ethanol used after previous application of the dentin adhesive promoted the lower presence of residues.
Resumo:
Many in vivo studies have stated that the response of the dentin/pulp complex does not depend on the dental material used as the liner or pulp-capping agent. However, several in vitro studies have reported the metabolic cytotoxic effects of resin components applied to fibroblast and odontoblast cell lines. The aim of this study was to evaluate the human pulp response following direct pulp capping with current bonding agents and calcium hydroxide (CH). Sound premolars scheduled for orthodontic extraction had their pulp tissue mechanically exposed. After hemorrhage control and total acid conditioning, the experimental bonding agents, including All Bond 2, Scotchbond MP-Plus, Clearfil Liner Bond 2, and Prime & Bond 2.1 were applied on the pulp exposure site. CH saline paste was used as the control pulp-capping agent. All cavities were restored with Z-100 resin composite according to the manufacturer's instructions. Following extractions, the teeth were processed for microscopic evaluation. In the short term, the bonding agents elicited a moderate inflammatory pulp response with associated dilated and congested blood vessels adjacent to the pulp exposure site. A mild inflammatory pulp response was observed when Clearfil Liner Bond 2 or CH was applied on the pulp exposures. With time, macrophages and giant cells engulfing globules and components of all experimental bonding agents displaced into the pulp space were seen. This chronic inflammatory response did not allow complete pulp repair, which interfered with the dentin bridge formation. Pulp exposures capped with CH exhibited an initial organization of elongated pulp cells underneath the coagulation necrosis. CH stimulated early pulp repair and dentin bridging that extended into the longest period. The bonding agents evaluated in the present study cannot be recommended for pulp therapy on sound human teeth.
Resumo:
Objectives: The aim of this study was to analyze the stress distribution on dentin/adhesive interface (d/a) through a 3-D finite element analysis (FEA) varying the number and diameter of the dentin tubules orifice according to dentin depth, keeping hybrid layer (HL) thickness and TAǴs length constant. Materials and Methods: 3 models were built through the SolidWorks software: SD - specimen simulating superficial dentin (41 x 41 x 82 μm), with a 3 μm thick HL, a 17 μm length Tag, and 8 tubules with a 0.9 μm diameter restored with composite resin. MD - similar to M1 with 12 tubules with a 1.2 μm diameter, simulating medium dentin. DD - similar to M1 with 16 tubules with a 2.5 μm diameter, simulating deep dentin. Other two models were built in order to keep the diameter constant in 2.5 μm: MS - similar to SD with 8 tubules; and MM - similar to MD with 12 tubules. The boundary condition was applied to the base surface of each specimen. Tensile load (0.03N) was performed on the composite resin top surface. Stress field (maximum principal stress in tension - σMAX) was performed using Ansys Wokbench 10.0. Results: The peak of σMAX (MPa) were similar between SD (110) and MD (106), and higher for DD (134). The stress distribution pathway was similar for all models, starting from peritubular dentin to adhesive layer, intertubular dentin and hybrid layer. The peak of σMAX (MPa) for those structures was, respectively: 134 (DD), 56.9 (SD), 45.5 (DD), and 36.7 (MD). Conclusions: The number of dentin tubules had no influence in the σMAX at the dentin/adhesive interface. Peritubular and intertubular dentin showed higher stress with the bigger dentin tubules orifice condition. The σMAX in the hybrid layer and adhesive layer were going down from superficial dentin to deeper dentin. In a failure scenario, the hybrid layer in contact with peritubular dentin and adhesive layer is the first region for breaking the adhesion. © 2011 Nova Science Publishers, Inc.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The bond strength of composite resins (CRs) to dentin is influenced by the interfacial microstructure of the hybrid layer (HL) and the resin tags (TAG). The contemporary self-etching primer adhesive systems overcame the inconvenient of the etch-and-rinse protocol. Studies, however, have demonstrated that HL thickness and TAG length vary according to the wetting time and additional use of acid-etching prior to self-etching primers. This study investigated the localized stress distribution in the HL and the dentin/adhesive interface. Two HL thicknesses (3 or 6 mu m), two TAG lengths (13 or 17 mu m) and two loading conditions (perpendicular and oblique-25 degrees) were investigated by the finite element (FE) analysis. Five two-dimensional FE models (M) of a dentin specimen restored with CR (38 x 64 mu m) were constructed: M1 - no HL and no TAG; M2 - 3 mu m of HL and 13 mu m of TAG; M3 - 3 mu m of HL and 17 mu m of TAG; M4 - 6 mu m of HL and 13 mu m of TAG; and M5 - 6 mu m of HL and 17 mu m of TAG. Two distributed loadings (L) (20N) were applied on CR surface: L1 - perpendicular, and L2 - oblique (25 degrees). Fixed interfacial conditions were assigned on the border of the dentin specimen. Ansys 10.0 (Ansys (R), Houston, PA, USA) software was used to calculate the stress fields. The peak of von Mises (sigma(vM)) and maximum principal stress (sigma(max)) was higher in L2 than in L1. Microstructures (HL and TAG) had no effect on local stresses for L1. Decreasing HL decreased sigma(vM) and sigma(max) in all structures for L2, but the TAG length had influence only on the peributular dentin. The thickness of HL had more influence on the sigma(vM) and sigma(max) than TAG length. The peritubular dentin and its adjacent structures showed the highest sigma(vM) and sigma(max), mainly in the oblique loading.
Resumo:
The aim of this study was to evaluate the effect of desensitizing agents on the micro-shear bond strength of adhesive systems to dentin. Forty bovine teeth were divided into 8 groups (n=5): G1--Single Bond (SB); G2--GH.F + SB; G3-- Desensibilize + SB; G4--essensiv + SB; G5 --ingle Bond 2 (SB2); G6--H.E + SB2; G7--esensibilize + SB2; G8--Dessensiv + SB2. In all of the groups, the desensitizing agents were applied after phosphoric acid etching and before the dentin adhesive application. Z250 composite resin tubes were bonded on the treated surface. After 24 hours, the teeth were tested in a universal machine. Data were submitted to ANOVA and Tukey's test (5%). The results showed that the groups where Desensibilize and Dessensiv were applied exhibited smaller bond strength values.
Resumo:
Objective: The aim of this research is to use finite element analysis (FEA) to quantify the effect of the sample shape and the imperfections induced during the manufacturing process of samples on the bond strength and modes of failure of dental adhesive systems through microtensile test. Using the FEA prediction for individual parameters effect, estimation of expected variation and spread of the microtensile bond strength results for different sample geometries is made. Methods: The estimated stress distributions for three different sample shapes, hourglass, stick and dumbbell predicted by FEA are used to predict the strength for different fracture modes. Parameters such as the adhesive thickness, uneven interface of the adhesive and composite and dentin, misalignment of axis of loading, the existence of flaws such as induced cracks during shaping the samples or bubbles created during application of the adhesive are considered. Microtensile experiments are performed simultaneously to measure bond strength and modes of failure. These are compared with the FEA results. Results: The relative bonding strength and its standard deviation for the specimens with different geometries measured through the microtensile tests confirm the findings of the FEA. The hourglass shape samples show lower tensile bond strength and standard deviation compared to the stick and dumbbell shape samples. ANOVA analysis confirms no significant difference between dumbbell and stick geometry results, and major differences of these two geometries compared to hourglass shape measured values. Induced flaws in the adhesive and misalignment of the angle of application of load have significant effect on the microtensile bond strength. Using adhesive with higher modulus the differences between the bond strength of the three sample geometries increase. Significance: The result of the research clarifies the importance of the sample geometry chosen in measuring the bond strength. It quantifies the effect of the imperfections on the bond strength for each of the sample geometries through a systematic and all embracing study. The results explain the reasons of the large spread of the microtensile test results reported by various researchers working in different labs and the need for standardization of the test method and sample shape used in evaluation of the dentin-adhesive bonding system. © 2007 Academy of Dental Materials.
Resumo:
Purpose: To assess in vitro the shear bond strength at the resin/dentin interface in primary teeth after contamination with fresh human blood. Methods: 75 crowns of primary molars were embedded in acrylic resin and mechanically ground to expose a flat dentin surface. The specimens were randomly assigned to five groups (n=15), according to the surface treatment. Group I (control) had no blood contamination. The other groups were blood-contaminated and subjected to different post-contamination protocols: in Group 2, the surfaces were rinsed with water; in Group 3, the surfaces were air-dried; in Group 4, the surfaces were rinsed and air-dried; and in Group 5, no post-contamination treatment was done. In all groups, a 3-mm dentin bonding site was demarcated, Single Bond adhesive system was applied and resin composite cylinders were bonded. After 24 hours in distilled water, shear bond strength was tested at a crosshead speed of 0.5 mm/minute. Results: Means (in MPa) were: Group 1: 7.1 (+/- 4.2); Group 2: 4.0 (+/- 1.8); Group 3: 0.9 (+/- 0.7); Group 4: 3.9 (+/- 2.2) and Group 5: 1.3 (+/- 1.5). Data were analyzed statistically by the Kruskal-Wallis test at 5% significance level. Groups 2 and 4 were similar to each other (P > 0.05) and both ware similar to Group 1 (P > 0.05). These groups (2, 3 and 4) had statistically significantly higher bond strengths than Groups 3 and 5 (P < 0.05). Blood contamination negatively affected the shear bond strength to primary tooth dentin. Among the blood-contaminated groups, water-rinsed specimens had higher bond strengths than those that were exclusively air-dried or not submitted to any post-contamination protocol before adhesive application.
Resumo:
Purpose: The aim of the present paper was to determine the effect of different types of ionizing radiation on the bond strength of three different dentin adhesive systems. Materials and Methods: One hundred twenty specimens of 60 human teeth (protocol number: 032/2007) sectioned mesiodistally were divided into 3 groups according to the adhesives systems used: SB (Adper Single Bond Plus), CB (Clearfil SE Bond) and AP (Adper Prompt Self-Etch). The adhesives were applied on dentin and photo-activated using LED (Lec 1000, MMoptics, 1000 mW/cm(2)). Customized elastomer molds (0.5 mm thickness) with three orifices of 1.2 mm diameter were placed onto the bonding areas and filled with composite resin (Filtek Z-250), which was photo-activated for 20 s. Each group was subdivided into 4 Subgroups for application of the different types of ionizing radiation: ultraviolet radiation (UV), diagnostic x-ray radiation (DX), therapeutic x-ray radiation (TX) and without irradiation (control group, CG). Microshear tests were carried out (Instron, model 4411), and afterwards the modes of failure were evaluated by optical and scanning electron microscope and classified using 5 scores: adhesive failure, mixed failures with 3 significance levels, and cohesive failure. The results of the shear bond strength test were submitted to ANOVA with Tukey`s test and Dunnett`s test, and the data from the failure pattern evaluation were analyzed with the Mann Whitney test (p = 0.05). Results: No change in bond strength of CB and AP was observed after application of the different radiation types, only SB showed increase in bond strength after UV (p = 0.0267) irradiation. The UV also changed the failure patterns of SB (p = 0.0001). Conclusion: The radio-induced changes did not cause degradation of the restorations, which means that they can be exposed to these types of ionizing radiation without weakening the bond strength.