Resumo:

Based on experimental results and theoretical analysis effects of the crystal structure on the optical and electrical properties of pyrite FeS2 films produced by thermally sulfurizing iron films at various temperatures have been systematically studied. The results indicate that the crystal structure and some related factors, such as the crystallization and the stoichiometry, remarkably influence the optical and electrical performances of the pyrite films. It is also shown that the preferred orientation of the crystal grain plays a major role in determining the crystal structure and the optical and electrical properties of the pyrite FeS2 films. Also we find that it is the crystal grains, rather than the particles that exercise a decisive influence on the electrical performance of pyrite films. (C) 2003 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A new compound Ce(6-x)Ln(x)MoO(15-delta) has been synthesized by wet-chemistry method. Their crystal structure and oxide ionic conductivity were characterized by powder X-ray diffraction, Raman, IR spectrum and A.C. impedance technique. The XRD results showed that Ce6MO15-delta, Ce(5)LnMoO(15-delta) have cubic symmetry with Fm3m space group. The refined lattice parameters showed that their lattice constants decrease with the decrease of the ionic radius of Ln(3+). The electrochemical measurements showed that the ionic conductivity of resulting oxides Ce(6-x)Ln(x)MoO(15-delta) have an enhance, which may be a kind of promising material for SOFCs.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Colloidal crystals formed by two types of polystyrene particles of different sizes (94 and 141 nm) at various number ratios (94:141 nm) are studied. Experiments showed that the formation time of crystals lengthens as the number ratio of the two components approaches 1:1. The dependence of the mean interparticle distance (D-0), crystal structure and alloy structure on the number ratio of the two types of particles was Studied by means of Kossel diffraction technique and reflection spectra. The results showed that as the number ratio decreased, the mean interparticle distance (D-0) became larger. And the colloidal crystal in binary mixtures is more preferably to form the bcc structure. This study found that binary systems form the substitutional solid solution (sss)-type alloy structure in all cases except when the number ratio of two types of particles is 5:1, which results instead in the superlattice structure. (C) 2008 Elsevier Inc. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Gd1.99-xYxCe0.01SiO5 (Ce:GYSO) crystals (x = 0, 0.0995, 0.199) have been grown by the Czochralski (Cz) method. Crystal structure and the distribution coefficients of Ce have been determined for all three crystals. Spectroscopic measurements indicate that optical transmittance and luminescence intensity of Gd1.99-xYxCe0.01SiO5 (x = 0.0995, 0.199) crystals are Substantially higher than those of Ce:Gd2SiO5 (Ce:GSO), especially at x = 0.0995, which makes them good candidate materials for scintillation applications. The particularly important result is that the alloyed Ce:GYSO crystals can be grown easily by the Cz method and, unlike Ce:GSO, they do not undergo cleavage during the growth process or subsequent mechanical treatment. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The crystal structure and liquid crystalline properties of a biphenyl-containing acetylene, [5-[(4'-heptoxy-4- biphenylyl) carbonyloxy]-1-pentyne (A3EO7) were investigated by electron crystallography, X-ray diffraction, polarizing optical microscopy, differential scanning calorimetry, transmission electron microscopy, and atomic force microscopy. A3EO7 crystals obtained from a toluene solution adopts a monoclinic P112/m space group with unit cell parameters of a = 6.25 Angstrom, b = 7.82 Angstrom, c = 46.70 Angstrom and gamma = 96.7degrees, as determined using electron diffraction. Upon cooling from the isotropic phase, A3EO7 exhibits a smectic A phase in the temperature range 72.4 - 53.6degreesC. Further lowering of the temperature results in the formation of a smectic C phase which exhibits a strong tendency towards crystallization.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A new tetrakis praseodymium(tu) complex Pr(TFNB)(3)Phen has been synthesized, in which TFNB is 4,4,4-trifluoro-1-(2-naphthyl)-1,3-butanedione and Phen is 1,10-phenanthroline. Its crystal structure and luminescent spectra were successfully determined and investigated. The typical antenna effect existing in the luminescence of Pr(TFNB)(3)Phen was revealed by the study of the UV-Vis absorption spectra of ligands and the excitation spectrum of Pr(TFNB)(3)Phen.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Gallium-doped zinc oxide (ZnO:Ga 1, 2 3, 4 and 5 at%) samples were prepared in powder form by modifying the Pechini method. The formation of zinc gallate (ZnGa2O4) With the spinel crystal structure was observed even in ZnO:Ga 1 at% by X-ray diffraction. The presence of ZnGa2O4 in ZnO:Ga samples was also evidenced by luminescence spectroscopy through its blue emission at 430 nm, assigned to charge transfer between Ga3+ at regular octahedral symmetry and its surrounding O2- ions. The amount of ZnGa2O4 increases as the dopant concentration increases, as observed by the quantitative phase analysis by the Rietveld method. (C) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Bi4Ti3O12 powder was synthesized from bismuth oxide and titanium oxide. Mixture of oxides was milled in zirconium oxide jar in the planetary ball-mill during 1, 3 and 6 h. Extended time of milling directed to formation of higher amount of titanates perovskite phase. Bi4Ti3O12 was formed between 1 and 3 h of milling time. The phase formation of Bi4Ti3O12, crystal structure and powder particle size were followed by XRD, Raman spectroscopy and SEM analysis. After milling for various times the powders were compacted by pressing and isothermal sintering. Sample milled for 3 h and subsequently sintered at 1000C for 24 h exhibit a hysteresis loop, confirming that the synthesized material possesses ferroelectric properties. All results affect that the structure Bi4Ti3O12 is strongly dependent on the milling time.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Magnesium borate hydroxide (MBH) nanowhiskers were synthesized using a one step hydrothermal process with different surfactants. The effect surfactants have on the structure and morphology of the MBH nanowhiskers has been investigated. The X-ray diffraction profile confirms that the as-synthesized material is of single phase, monoclinic MgBO2(OH). The variations in the size and shape of the different MBH nanowhiskers have been discussed based on the surface morphology analysis. The annealing of MBH nanowhiskers at 500 °C for 4 h has significant effect on the crystal structure and surface morphology. The UV–vis absorption spectra of the MBH nanowhiskers synthesized with and without surfactants show enhanced absorption in the low-wavelength region, and their optical band gaps were estimated from the optical band edge plots. The photoluminescence spectra of the MBH nanowhiskers produced with and without surfactants show broad emission band with the peak maximum at around 400 nm, which confirms the dominant contribution from the surface defect states.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Phonon modes in spherical GaAs quantum dots (QDs) with up to 11,855 atoms (8 nm in size) are calculated by using an empirical microscopic model. The group theory is employed to reduce the computational intensity, which further allows us to investigate the quantum confinement of phonon modes with different symmetries and reveals a phenomenon that phonon modes with different symmetries have different quantum confinement effect. For zinc-blende structure, the modes with the A(1) symmetry has the strongest quantum confinement effect and the T-1 modes the weakest. This could cause a crossover of symmetries of the highest frequency from A(1) to T-2 when the size of QDs decreases. (C) 1999 Elsevier Science Ltd, All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of binary diphenylphosphinates with Eu3+ and Gd3+ were prepared. The compounds have the general formula Gd1-xEux(DPP)(3), where x ranges from 0 to 1. The spectroscopic measurements show interesting behavior. The intensity of the D-5(0) --> F-7(2) transitions decreases relative to D-5(0) --> F-7(1) With an increase in europium dispersion. Inside the temporal domain, the same decrease is observed with increasing delay after excitation. The lifetimes are also affected, which can be seen in the x = 1 compound, where the decay is a first-order process and lifetime values are 4.81 ms. In the binary compound, as an effect of dispersion, the lifetime of the D-5(0) level measured at the D-5(0) --> F-7(1) transition increases with europium dispersion, and the average along the series is 6.25 ms. The decay measured at the D-5(0) --> F-7(2) transitions reveals a second-order process with lifetimes ranging from 1.90 to 6.00 ms. (C) 2001 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A new ruthenium(II) complex of the type [Ru(O2CMe)(MeCN)2(PPh3)2](CiO4) (1) has been isolated from a reaction between Ru2Cl(O2CMe), and PPh3 in MeCN followed by the addition of NaClO4. The structure of 1 is determined by single crystal X-ray studies. The crystal belongs to the monoclinic space group C2/m with the following unit cell dimensions for the C42H39N2O6P2ClRu(M = 866.15): a = 23.295(1)angstrom, b = 23.080(1)angstrom, c = 9.159(1)angstrom, beta = 107.32(1)-degrees, V = 4701(1)angstrom3, Z = 4, D(c) = 1.224 gcm-3, lambda(Mo - K-alpha) = 0.7107 angstrom, mu(Mo - K-alpha) = 4.09 cm-1, T = 293K, R = 0.081 (R(w) = 0.094) for 2860 reflections with I greater-than-or-equal-to 3-sigma(I) and g = 0.015853. In the complex cation, the symmetry about the metal centre is essentially octahedral showing the presence of a chelating acetato, two cis-oriented MeCN and two trans-disposed PPh3 ligands. The mechanistic aspects of the core cleavage reaction are discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Cerium-doped lutetium pyrosilicate crystal, Ce:Lu2Si2O7 (Ce:LPS), was grown by the Czochralski method. The segregation coefficient of Ce3+ ion was studied by the ICP-AES method. X-ray diffraction analysis showed that the structure of Ce:LPS crystal was monoclinic symmetry with space group of C2/m. Perfect cleavage planes (110) and imperfect cleavage planes (001) were observed by optical microscope. The reasons why it is difficult to grow crack-free crystals were studied. After optimized growth parameters, a Ce:LPS crystal with dimension of Phi 25 x 30 mm was grown, which is colorless, high optical quality, cracking-free and no inclusions. The transmittance of Ce:LPS crystal from 380 to 800 nm is over 82% and there is no observable absorption. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The title complex [(VB1)(2)DMFHPMo12O40.5DMF, VB1 = vitamin B-1 (thiamine chloride), DMF = N,N-dimethylformamide] has been synthesized and characterized by elemental analysis, IR, UV-Vis, electron spin resonance, X-ray photoelectron spectroscopy and cyclic voltammetry methods. The X-ray crystal structure revealed that there is one independent molecule in the unit cell of the title complex that contains one mixed-valence heteropolyanion, two VB1+ cations and six DMF molecules. The title complex possesses a centrosymmetrical arrangement in the unit cell, with the P atom at the symmetry center of the heteropolyanion and with eight O atoms surrounding the central P atom, such that two sets of PO4 tetrahedra are formed. The PO4 tetrahedra and MoO66-(7-) octahedra are disordered in the heteropolyanion. The bond distances of P-O-a and Mo=O-d are in the ranges 1.57 (4)-1.70 (4) Angstrom and 1.61 (2)-1.67 (2) Angstrom, respectively.