928 resultados para colloidal, crystalization, vitrification, dynamic light scattering, static light scattering, soft matter
Resumo:
5,6-Bis(benzylideneamino)-2-mercaptopyrimidin-4-ol (SCR7) is a new anti cancer molecule having capability to selectively inhibit non-homologous end joining (NHEJ), one of the DNA double strand break (DSB) repair pathways inside the cells. In spite of the promising potential as an anticancer agent, hydrophobicity of SCR7 decreases its bioavailability. Herein the entrapment of SCR7 in Pluronic copolymer is reported. The size of the aggregates was determined by transmission electron microscopy (TEM) and dynamic light scattering (DLS) which yields an average diameter of 23 nm. SCR7 encapsulated micelles (ES) were also characterized by small-angle neutron scattering (SANS). Evaluation of its biological properties by using a variety of techniques, including Trypan blue, MTT and Live-dead cell assays, reveal that encapsulated SCR7 can induce cytotoxicity in cancer cell lines, being more effective in breast cancer cell line. Encapsulated SCR7 treatment resulted in accumulation of DNA breaks within the cells, resulting in cell cycle arrest at G1 phase and activation of apoptosis. More importantly, we found approximate to 5 fold increase in cell death, when encapsulated SCR7 was used in comparison with SCR7 alone.
Resumo:
Small heat shock proteins (sHSPs) are a family of ATP-independent molecular chaperones which prevent cellular protein aggregation by binding to misfolded proteins. sHSPs form large oligomers that undergo drastic rearrangement/dissociation in order to execute their chaperone activity in protecting substrates from stress. Substrate-binding sites on sHSPs have been predominantly mapped on their intrinsically disordered N-terminal arms. This region is highly variable in sequence and length across species, and has been implicated in both oligomer formation and in mediating chaperone activity. Here, we present our results on the functional and structural characterization of five sHSPs in rice, each differing in their subcellular localisation, viz., cytoplasm, nucleus, chloroplast, mitochondria and peroxisome. We performed activity assays and dynamic light scattering studies to highlight differences in the chaperone activity and quaternary assembly of sHSPs targeted to various organelles. By cloning constructs that differ in the length and sequence of the tag in the N-terminal region, we have probed the sensitivity of sHSP oligomer assembly and chaperone activity to the length and amino acid composition of the N-terminus. In particular, we have shown that the incorporation of an N-terminal tag has significant consequences on sHSP quaternary structure.
Resumo:
采用配液结晶法制取了溶菌酶蛋白质晶体,使用动态光散射测量了溶液中聚集体的颗粒度几率分布;使用Zeiss显微镜测定了溶菌酶(110)晶面的生长速度.实验表明:随着蛋白质和NaCl浓度的增加,溶液中聚集体的颗粒尺寸也相应增加.随着反应时间的增加,溶菌酶分子在溶液中的聚集反应,逐渐达到平衡;在蛋白质和NaCl浓度较高时,溶菌酶晶体的(110)面生长较快,而在蛋白质和NaCl浓度较低时,该晶面生长较慢.基于二维成核生长机理,从晶体生长动力学理论方程出发,计算了二维成核的形成能a=4.01×10-8J?cm-2.
Resumo:
用动态光散射法研究了不同浓度NaCl对液—液扩散法生长溶菌酶晶体的影响,并测量了晶体生长前后体系的Zeta电势.结果表明,NaCl浓度较高时,在溶菌酶溶液—凝胶界面处会发生液液分层现象,溶液中一直存在较大的聚集体,生长出的晶体质量较差.而在合适的NaCl浓度下,随着溶液Zeta电势降低,溶液中溶菌酶的大的聚集体发生解聚集,生长出的晶体质量较高.
Resumo:
The lysozyme crystals were made by batch crystallization method and the distribution of aggregate in solution were measured by dynamic light scattering. The results showed that the dimension of aggregate increased with the increase of the concentration of lysozyme and NaCl, lysozyme molecules aggregated gradually in solution and finally arrived at balance each other. The higher the concentrations of lysozyme and NaCl were, the faster the growth rate of (I 10) face was. The growth rates of lysozyme crystal were obtained by a Zeiss microscope, and the effective surface energy (a) of growing steps were calculated about 4.01 X 10(-8) J.cm(-2) according to the model of multiple two-dimensional nucleation mechanism.
Resumo:
The interactions between poly(vinylpyrrolidone) (PVP) and the reversed micelles composed of water, AOT, and n-heptane are investigated with the aid of phase diagram, measurements of conductivity and viscosity, Fourier transform infrared (FTIR) spectrum, and dynamic light scattering (DLS). The phase diagrams of water/AOT/heptane in the presence of and absence of PVP are given. The conductivity of the water/AOT/heptane reversed micelle without PVP initially increases and then decreases with the increase of water content, ω0 (the molar ratio of water to AOT), while the plots of conductivity (K) versus ω0 of the reversed micelle in the presence of PVP depend on the PVP concentrations. The plot of K versus ω0 with 2.0%wt PVP is similar to that without PVP. Only the ω0,max (the water content that the maximum conductivity corresponds to) is larger than that without PVP. Nevertheless, the conductivity of the reversed micelle containing more than 4%wt PVP always rises with the increase of the water content in the measured range. The DLS results indicate that the hydrodynamic radius (Rh) in the presence and absence of PVP rises with the increase of ω0. The plots with PVP and without PVP have almost the same value when ω0<17; and after that, it quickly increases with the increase of ω0. It is interesting to find that there is almost no effect of the PVP concentration on the viscosity and Rh of the reversed micelle at ω0 = 15. The FTIR results suggest that the contents of SO3--bound water and Na+-bound water both decrease with PVP added, while the content of the bulky-like water increases. However, the trapped water in the hydrophobic chain of the surfactant is nearly unaffected by PVP. It is also found from the FTIR that the carbonyl group stretching vibration of AOT is fitted into two sub-peaks, which center at 1740 and 1729 cm-1, corresponding to the trans and cis conformations of AOT, respectively.
Resumo:
Our previous studies have shown that the determination of coagulation rate constants by turbidity measurement becomes impossible for a certain operating wavelength (that is, its blind point) because at this wavelength the change in the turbidity of a dispersion completely loses its response to the coagulation process. Therefore, performing the turbidity measurement in the wavelength range near the blind point should be avoided. In this article, we demonstrate that the turbidity measurement of the rate constant for coagulation of a binary dispersion containing particles of two different sizes (heterocoagulation) presents special difficulties because the blind point shifts with not only particle size but also with the component fraction. Some important aspects of the turbidity measurement for the heterocoagulation rate constant are discussed and experimentally tested. It is emphasized that the T-matrix method can be used to correctly evaluate extinction cross sections of doublets formed during the heterocoagulation process, which is the key data determining the rate constant from the turbidity measurement, and choosing the appropriate operating wavelength and component fraction are important to achieving a more accurate rate constant. Finally, a simple scheme in experimentally determining the sensitivity of the turbidity changes with coagulation over a wavelength range is proposed.
Resumo:
采用原子力显微镜对溶菌酶和刀豆蛋白A的分子间相互作用力的情况进行了研究,并用动态光散射研究了此二种分子间相互作用力有较大差异的蛋白质在晶体生长条件和非生长条件下,溶液中的聚集体的状态(大小和分散度)随浓度和温度的变化情况.实验结果表明,范德华力强的刀豆蛋白A在成核前,溶液中的聚集体不能很快转变为生长基元,导致晶体生长时间长;而范德华力弱的溶菌酶,溶液中的聚集体可以很快转变成生长基元,晶体生长时间也较短.
Resumo:
首次采用动态光散射研究了气相扩散法生长溶菌酶晶体 .实验中采用了两种溶解溶菌酶的方法,所得实验结果是有区别的 .这种区别表明了 NaCl对溶菌酶分子间相互作用产生十分重要的影响 .实验结果表明,晶体生长过程中,溶液中溶菌酶始终保持单分子与两分子聚集体的状态,这种状态是生长晶体的基础 .
Resumo:
为研究气相扩散速率对溶菌酶晶体生长的影响,特设计了一种可方便调节气相扩散速率的晶体生长样品池,并用动态光散射法对不同气相扩散速率下晶体生长过程进行了研究.实验结果表明,随着气相扩散速率的增加,晶体生长过程中的成核阶段缩短.气相扩散速率通过影响溶菌酶溶液形成过饱和的速率来影响生长出的晶体的数量和大小.
Resumo:
"Click" chemistry has become an efficient avenue to unimolecular polymeric nanoparticles through the self-crosslinking of individual polymer chains containing appropriate functional groups. Herein we report the synthesis of ultra-small (7 nm in size) polymethyl methacrylate (PMMA) nanoparticles (NPs) by the "metal-free" cross-linking of PMMA-precursor chains prepared by reversible addition-fragmentation chain transfer (RAFT) polymerization containing beta-ketoester functional groups. Intramolecular collapse was performed by the one-pot reaction of beta-ketoester moieties with alkyl diamines in tetrahydrofurane at r.t. (i.e., by enamine formation). The collapsing process was followed by size exclusion chromatography and by nuclear magnetic resonance spectroscopy. The size of the resulting PMMA-NPs was determined by dynamic light scattering. Enamine "click" chemistry increases the synthetic toolbox for the efficient synthesis of metal-free, ultra-small polymeric NPs.
Resumo:
Copolímeros casca-núcleo de poli(acrilato de butila) (núcleo) e poliestireno (casca) foram sintetizados por meio de polimerização em emulsão, conduzida em duas etapas. A adição de ácido itacônico como monômero funcional na polimerização do núcleo foi realizada para verificar seu efeito sobre suas propriedades mecânicas e de processamento. Os copolímeros foram caracterizados por espalhamento dinâmico de luz (DLS), microscopia eletrônica de transmissão (MET), cromatografia de exclusão por tamanho (SEC), espectrometria na região do infravermelho (FTIR) e calorimetria diferencial por varredura (DSC). A incorporação do monômero funcional foi confirmada por DSC e quantificada por titulação. A proporção de poli(acrilato de butila) e poliestireno influenciou diretamente o processamento e as propriedades mecânicas do polímero. Os copolímeros com teores de poliestireno acima de 50% foram processados por compressão e extrusão a temperatura ambiente, apresentando comportamento baroplástico. A presença do monômero funcional não alterou o processamento do polímero e melhorou significativamente sua resistência à tração, aumentando sua tenacidade
Resumo:
Huntington’s disease (HD) is a fatal autosomal dominant neurodegenerative disease. HD has no cure, and patients pass away 10-20 years after the onset of symptoms. The causal mutation for HD is a trinucleotide repeat expansion in exon 1 of the huntingtin gene that leads to a polyglutamine (polyQ) repeat expansion in the N-terminal region of the huntingtin protein. Interestingly, there is a threshold of 37 polyQ repeats under which little or no disease exists; and above which, patients invariably show symptoms of HD. The huntingtin protein is a 350 kDa protein with unclear function. As the polyQ stretch expands, its propensity to aggregate increases with polyQ length. Models for polyQ toxicity include formation of aggregates that recruit and sequester essential cellular proteins, or altered function producing improper interactions between mutant huntingtin and other proteins. In both models, soluble expanded polyQ may be an intermediate state that can be targeted by potential therapeutics.
In the first study described herein, the conformation of soluble, expanded polyQ was determined to be linear and extended using equilibrium gel filtration and small-angle X-ray scattering. While attempts to purify and crystallize domains of the huntingtin protein were unsuccessful, the aggregation of huntingtin exon 1 was investigated using other biochemical techniques including dynamic light scattering, turbidity analysis, Congo red staining, and thioflavin T fluorescence. Chapter 4 describes crystallization experiments sent to the International Space Station and determination of the X-ray crystal structure of the anti-polyQ Fab MW1. In the final study, multimeric fibronectin type III (FN3) domain proteins were engineered to bind with high avidity to expanded polyQ tracts in mutant huntingtin exon 1. Surface plasmon resonance was used to observe binding of monomeric and multimeric FN3 proteins with huntingtin.
Resumo:
Neste trabalho foi feito um estudo sobre a preparação e caracterização de microesferas poliméricas à base de poli(ácido metacrílico-co-divinilbenzeno) por polimerização por precipitação. As partículas foram sintetizadas e analisadas em diferentes condições de reação. Partículas esféricas políméricas foram sintetizadas na faixa de 1,66 - 8,41 m, assim como partículas no estado de microgel. As partículas foram caracterizadas pelas técnicas de espalhamento de luz dinâmica (DLS), análise termogravimétrica (TGA), espectroscopia na região do infravermelho (FTIR), adsorção de nitrogênio pelos métodos BET (Brunauer, Emmett e Teller) e BJH (Barret, Joyner e Halenda), microscopia ótica, microscopia eletrônica de varredura, e testes de razão de inchamento. A análise das partículas foi feita para verificar a influência da mudança na composição de comonômeros, grau de reticulação, relação de monômeros totais/diluentes em massa/volume (g/100 mL), e quanto à relação volumétrica de diluentes. Verificou-se que houve um aumento no tamanho das partículas e da resistência térmica com a diminuição da fração molar de MAA (ácido metacrílico). Na preparação de partículas com fração molar de 50% de MAA, e relação volumétrica acetonitrila/tolueno de 75/25, quanto maior a relação de monômeros totais/diluentes (g/100 mL), maior o tamanho e o rendimento das partículas. Com a mudança da relação volumétrica de diluentes, houve mudança nas características de porosidade, tamanho das partículas, e grau de inchamento das partículas, sendo que na relação volumétrica acetonitrila/tolueno de 50/50, houve formação de microgel
Resumo:
Single-chain technology (SCT) allows the transformation of individual polymer chains to folded/collapsed unimolecular soft nanoparticles. In this work we contribute to the enlargement of the SCT toolbox by demonstrating the efficient synthesis of single-chain polymer nanoparticles (SCNPs) via intrachain amide formation. In particular, we exploit cross-linking between active methylene groups and isocyanate moieties as powerful "click" chemistry driving force for SCNP construction. By employing poly(methyl methacrylate)- (PMMA-) based copolymers bearing beta-ketoester units distributed randomly along the copolymer chains and bifunctional isocyanate cross-linkers, SCNPs were successfully synthesized at r.t. under appropriate reaction conditions. Characterization of the resulting SCNPs was carried out by means of a combination of techniques including size exclusion chromatography (SEC), infrared (IR) spectroscopy, proton nuclear magnetic resonance (H-1 NMR) spectroscopy, dynamic light scattering (DLS), and elemental analysis (EA).