876 resultados para Implant surface treatment


Relevância:

90.00% 90.00%

Publicador:

Resumo:

The aim of this study was to evaluate implants installed with compromised primary stability associated or not with polylactide and polyglycolide copolymer (PLA/PGA). Two 0.4-mm overdrilled defects (3 mm in diameter and 6 mm long) were produced in the right tibia of 25 rabbits. Half of the defects were left untreated, and the other half was filled with PLA/PGA. Implants of 2.6 mm in diameter and 6 mm long were placed into all defects. Animals were killed at 5, 15, 40, and 60 postoperative days, and biomechanical analysis (torque-reverse), histomorphometry, and immunohistochemistry (osteoprotegerin, receptor activator of NFJB ligand [RANKL], osteocalcin, and collagen-1 [ COL- I] staining) were performed. All the implants achieved osseointegration. There were no statistically significant differences in the torque-reverse and in linear contact extension between bone tissue and implant surface and no statistically significant difference in osteoprotegerin, RANKL, osteocalcin, and collagen-1 expression between the studied groups in all studied periods (P > 0.05). We can conclude that osseointegration can occur in compromised primary implant stability situations, and the addition of PLA/PGA did not improve the osseointegration process in this experimental model.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Nanostructures on implant surfaces have been shown to enhance osseointegration; however, commonly used evaluation techniques are probably not sufficiently sensitive to fully determine the effects of this process. This study aimed to observe the osseointegration properties of nanostructured calcium phosphate (CaP)-coated implants, by using a combination of three-dimensional imaging and conventional histology. Titanium implants were coated with stable CaP nanoparticles using an immersion technique followed by heat treatment. Uncoated implants were used as the control. After topographical and chemical characterizations, implants were inserted into the rabbit femur. After 2 and 4 weeks, the samples were retrieved for micro-computed tomography and histomorphometric evaluation. Scanning electron microscopy evaluation indicated that the implant surface was modified at the nanoscale by CaP to obtain surface textured with rod-shaped structures. Relative to the control, the bone-to-implant contact for the CaP-coated implant was significantly higher at 4 weeks after the implant surgery. Further, corresponding 3-D images showed active bone formation surrounding the implant. 3-D quantification and 2-D histology demonstrated statistical correlation; moreover, 3-D quantification indicated a statistical decrease in bone density in the non-coated control implant group between 2 and 4 weeks after the surgery. The application of 3-D evaluation further clarified the temporal characteristics and biological reaction of implants in bone. (C) 2011 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Background: Chemical modification of implant surface is typically associated with surface topographic alterations that may affect early osseointegration. This study investigates the effects of controlled surface alterations in early osseointegration in an animal model.Methods: Five implant surfaces were evaluated: 1) alumina-blasting, 2) biologic blasting, 3) plasma, 4) microblasted resorbable blasting media (microblasted RBM), and 5) alumina-blasting/acid-etched (AB/AE). Surface topography was characterized by scanning electron microscopy and optical interferometry, and chemical assessment by x-ray photoelectron spectroscopy. The implants were placed in the radius of six dogs, remaining 2 and 4 weeks in vivo. After euthanization, specimens were torqued-to-interface failure and non-decalcified - processed for histomorphologic bone-implant contact, and bone area fraction-occupied evaluation. Statistical evaluation was performed by one-way analysis of variance (P < 0.05) and post hoc testing by the Tukey test.Results: The alumina-blasting surface presented the highest average surface roughness and mean root square of the surface values, the biologic blasting the lowest, and AB/AE an intermediate value. The remaining surfaces presented intermediate values between the biologic blasting and AB/AE. The x-ray photoelectron spectroscopy spectra revealed calcium and phosphorus for the biologic blasting and microblasted RBM surfaces, and the highest oxygen levels for the plasma, microblasted RBM, and AB/AE surfaces. Significantly higher torque was observed at 2 weeks for the microblasted RBM surface (P < 0.04), but no differences existed between surfaces at 4 weeks (P > 0.74). No significant differences in bone-implant contact and bone area fraction-occupied values were observed at 2 and 4 weeks.Conclusion: The five surfaces were osteoconductive and resulted in high degrees of osseointegration and biomechanical fixation. J Periodontol 2011;82:742-750.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Statement of problem. Although titanium presents attractive physical and mechanical properties, there is a need for improving the bond at the titanium/luting cement interface for the longevity of metal ceramic restorations.Purpose. The purpose of this study was to evaluate the effect of surface treatments on the shear bond strength (SBS) of resin-modified glass ionomer and resin cements to commercially pure titanium (CP Ti).Material and methods. Two hundred and forty CP Ti cast disks (9.0 x 3.0 mm) were divided into 8 surface treatment groups (n=30): 1) 50 mu m Al2O3 particles; 2) 120 mu m Al2O3 particles; 3) 250 mu m Al2O3 particles; 4) 50 mu m Al2O3 particles + silane (RelyX Ceramic Primer); 5) 120 mu m Al2O3 particles + silane; 6) 250 mu m Al2O3 particles + silane; 7) 30 mu m silica-modified Al2O3 particles (Cojet Sand) + silane; and 8) 120 mu m Al2O3 particles, followed by 110 mu m silica-modified Al2O3 particles (Rocatec). The luting cements 1) RelyX Luting 2; 2) RelyX ARC; or 3) RelyX U100 were applied to the treated CP Ti surfaces (n=10). Shear bond strength (SBS) was tested after thermal cycling (5000 cycles, 5 degrees C to 55 degrees C). Data were analyzed by 2-way analysis of variance (ANOVA) and the Tukey HSD post hoc test (alpha=.05). Failure mode was determined with a stereomicroscope (x20).Results. The surface treatments, cements, and their interaction significantly affected the SBS (P<.001). RelyX Luting 2 and RelyX U100 exhibited similar behavior for all surface treatments. For both cements, only the group abraded with 50 mu m Al2O3 particles had lower SBS than the other groups (P<.05). For RelyX ARC, regardless of silane application, abrasion with 50 mu m Al2O3 particles resulted in significantly lower SBS than abrasion with 120 mu m and 250 mu m particles, which exhibited statistically similar SBS values to each other. Rocatec + silane promoted the highest SBS for RelyX ARC. RelyX U100 presented the highest SBS mean values (P<.001). All groups showed a predominance of adhesive failure mode.Conclusions. The adhesive capability of RelyX Luting 2 and RelyX U100 on the SBS was decisive, while for RelyX ARC, mechanical and chemical factors were more influential. (J Prosthet Dent 2012;108:370-376)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objective: The purpose of this study was to evaluate the flexural strength of repairs made with autopolymerising acrylic resin after different treatments of joint surfaces.Material and Methods: Fifty rectangular specimens were made with heat-polymerised acrylic resin and 40 were repaired with autopolymerising acrylic resin following joint surface treatments: group 1 (intact specimens), group 2 (chemical treatment: wetting with methyl-methacrylate for 180 s), group 3 (abraded with silicon carbide paper), group 4 (abraded and wetting with methyl-methacrylate for 180 s) and group 5 (without surface treatment). The flexural strength was measured by a three-point bending test using a universal testing machine with a 100 Kgf load cell in the centre of repair at 5 mm/min cross-head speed. All data were analysed using one-way ANOVA and Tukey HSD test for multiple comparisons (p < 0.05).Results: Among repaired specimens, groups 2 and 4 had 66.53 +/- 3.4 and 69.38 +/- 1.8 MPa mean values and were similar. These groups had superior flexural strength than groups 3 and 5 that were similar and had 54.11 +/- 3.4 and 51.24 +/- 2.8 MPa mean values, respectively. Group 1 had a mean value of 108.30 +/- 2.8 MPa being the highest result.Conclusion: It can be concluded that the treatment of the joint surfaces with methyl-methacrylate increases the flexural strength of denture base repairs, although the strength is still lower than that observed for the intact denture base resin. Abrasion with sandpaper was not able to influence the flexural strength of repaired denture bases.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Purpose: To evaluate the effect of airborne-particle abrasion and mechanico-thermal cycling on the flexural strength of a ceramic fused to cobalt-chromium alloy or gold alloy.Materials and Methods: Metallic bars (n = 120) were made (25 mm x 3 mm x 0.5 mm): 60 with gold alloy and 60 with Co-Cr. At the central area of the bars (8 mm x 3 mm), a layer of opaque ceramic and then two layers of glass ceramic (Vita VM13, Vita Zahnfabrick) were fired onto it (thickness: 1 mm). Ten specimens from each alloy group were randomly allocated to a surface treatment [(tungsten bur or air-particle abrasion (APA) with Al(2)O(3) at 10 mm or 20 mm away)] and mechanico-thermal cycling (no cycling or mechanically loaded 20,000 cycles; 10 N distilled water at 37 degrees C and then thermocycled 3000 cycles; 5 degrees C to 55 degrees C, dwell time 30 seconds) combination. Those specimens that did not undergo mechanico-thermal cyclingwere stored inwater (37 degrees C) for 24 hours. Bond strength was measured using a three-point bend test, according to ISO 9693. After the flexural strength test, failure types were noted. The data were analyzed using three factor-ANOVA and Tukey's test (alpha = 0.05).Results: There were no significant differences between the flexural bond strength of gold and Co-Cr groups (42.64 +/- 8.25 and 43.39 +/- 10.89 MPa, respectively). APA 10 and 20 mm away surface treatment (45.86 +/- 9.31 and 46.38 +/- 8.89 MPa, respectively) had similar mean flexural strength values, and both had significantly higher bond strength than tungsten bur treatment (36.81 +/- 7.60 MPa). Mechanico-thermal cycling decreased the mean flexural strength values significantly for all six alloy-surface treatment combinations tested when compared to the control groups. The failure type was adhesive in the metal/ceramic interface for specimens surface treated only with the tungsten bur, and mixed for specimens surface treated with APA 10 and 20 mm.Conclusions: Considering the levels adopted in this study, the alloy did not affect the bond strength; APA with Al(2)O(3) at 10 and 20 mm improved the flexural bond strength between ceramics and alloys used, and the mechanico-thermal cycling of metal-ceramic specimens resulted in a decrease of bond strength.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Statement of the Problem: the ceramic composition and surface microstructure of all-ceramic restorations are important components of an effective bonding substrate. Hydrofluoric acid and sandblasting are well-known procedures for surface treatment; however, surface treatment for high alumina-containing and lithium disilicate ceramics have not been fully investigated.Purpose: This in vitro study evaluated the tensile bond strength of resin cement to two types of ceramic systems with different surface treatments.Methods and Materials: Thirty specimens of each ceramic system were made according to the manufacturer's instructions and embedded in polyester resin. Specimens of In-Ceram Alumina [1] and IPS Empress 2 [E] were distributed to three groups with differing surface treatments (n=10): sandblasting with 50 jam aluminum oxide (APA); sandblasting with 110 pm aluminum oxide modified with silica particles (ROCATEC System-RS); a combination of sandblasting with APA and 10% hydrofluoric acid etching (HA) for two minutes on In-Ceram and for 20 seconds for IPS Empress 2. After the respective surface treatments, all the specimens were silanated, and Rely-X resin cement was injected onto the ceramic surface and light polymerized. The specimens were stored in distilled water at 37 degrees C for 24 hours and thermally cycled 1,100 times (5 degrees C/55 degrees C). The tensile bond strength test was performed in a universal testing machine at a 0.5 mm/minute crosshead speed.Results: the mean bond strength values (AWa) for IPS Empress 2 were 12.01 +/- 5.93 (EAPA), 10.34 +/- 1.77 (ERS) and 14.49 +/- 3.04 (EHA). The mean bond strength values for In-Ceram Alumina were 9.87 +/- 2.40 JAPA) and 20.40 +/- 6.27 (IRS). All In-Ceram specimens treated with 10% hydrofluoric acid failed during thermal cycling.Conclusion: the Rocatec system was the most effective surface treatment for In-Ceram Alumina ceramics; whereas, the combination of aluminum oxide sandblasting and hydrofluoric acid etching for 20 seconds worked more effectively for Empress 2 ceramics.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objectives. Alterations in the commercially pure titanium (cpTi) surface may be undertaken to improve its biological properties. The aim of this study is to investigate the biocompatibility of cpTi submitted to different surface treatments.Methods. The cpTi surfaces were prepared so that machined and blasted surfaces, either acid etched or not, were compared using rat bone marrow cells cultured to differentiated into osteoblast. For attachment evaluation, cells were cultured for 4 and 24 h. Cell morphology was evaluated after 3 days. After 7, 14, and 21 days cell proliferation was evaluated. Total protein content and alkaline phosphatase (ALP) activity were evaluated after 14 and 21 days. For bone-like nodule formation, cells were cultured for 21 days. Data were compared by analysis of variance.Results. Cell attachment, cell morphology, cell proliferation, and ALP activity were not affected by surface treatments. Total. protein content was reduced by blasted and acid etched surface. Bone-Like nodule formation was significantly reduced by blasted, acid etched, and a combination of both blasted and acid etched surfaces.Conclusions. Based on these results, it can be suggested that cpTi surfaces that were submitted only to machining treatment favor the final event of osteoblastic differentiation of the rat bone marrow cells, evidenced by increased bone-Like nodule formation. (C) 2003 Elsevier B.V. Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Aim: To study the influence on the healing of soft and hard peri-implant tissues when implants of different sizes and configurations were installed into sockets immediately after tooth extraction.Material and methods: Transmucosal cylindrical implants, 3.3 mm in diameter in the control sites, and conical 5 mm in diameter in the test sites, were installed into the distal socket of the fourth mandibular premolars in dogs immediately after tooth extraction. After 4 months, the hard and soft tissue healing was evaluated histologically. Results: All implants were integrated in mineralized mature bone. Both at the test and control sites, the alveolar crest underwent resorption. The buccal bony surface at the implant test sites (conical; 3.8 mm) was more resorbed compared with the control sites (cylindrical; 1.6 mm). The soft tissue dimensions were similar in both groups. However, in relation to the implant shoulder, the peri-implant mucosa was located more apically at the test compared with the control sites.Conclusion: The present study confirmed that the distance between the implant surface and the outer contour of the buccal alveolar bony crest influenced the degree of resorption of the buccal bone plate. Consequently, in relation to the implant shoulder, the peri-implant mucosa will be established at a more apical level, if the distance between the implant surface and the outer contour of the alveolar crest is small.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

AimTo evaluate the influence (i) of various implant platform configurations and (ii) of implant surface characteristics on peri-implant tissue dimensions in a dog model.Material and methodsMandibular premolars and first molars were extracted bilaterally in six Labrador dogs. After 3 months of healing, two implants, one with a turned and a second with a moderately rough surface, were installed on each side of the mandible in the premolar region. on the right side of the mandible, implants with a tapered and enlarged platform were used, while standard cylindrical implants were installed in the left side of the mandible. Abutments with the diameter of the cylindrical implants were used resulting in a mismatch of 0.25 mm at the tapered implant sites. The flaps were sutured to allow a non-submerged healing. After 4 months, the animals were sacrificed and ground sections were obtained for histometric assessment.ResultsAll implants were completely osseointegrated. A minimal buccal bone resorption was observed for both implant configurations and surface topographies. Considering the animals as the statistical unit, no significant differences were found at the buccal aspect in relation to bone levels and soft tissue dimensions. The surface topographies did not influence the outcomes either.ConclusionsThe present study failed to show differences in peri-implant tissue dimensions when a mismatch of 0.25 mm from a tapered platform to an abutment was applied. The surface topographies influence a neither marginal bone resorption or peri-implant soft tissue dimension.To cite this article:Baffone GM, Botticelli D, Pantani F, Cardoso LC, Schweikert MT, Lang NP. Influence of various implant platform configurations on peri-implant tissue dimensions: an experimental study in dog.Clin. Oral Impl. Res. 22, 2011; 438-444.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Purpose: This investigation studied the effects of 3 surface treatments on the shear bond strength of a light-activated composite resin bonded to acrylic resin denture teeth. Materials and Methods: The occlusal surfaces of 30 acrylic resin denture teeth were ground flat with up to 400-grit silicon carbide paper. Three different surface treatments were evaluated: (1) the flat ground surfaces were primed with methyl methacrylate (MMA) monomer for 180 seconds; (2) light-cured adhesive resin was applied and light polymerized according to the manufacturer's instructions; and (3) treatment 1 followed by treatment 2. The composite resin was packed on the prepared surfaces using a split mold. The interface between tooth and composite was loaded at a cross-head speed of 0.5 mm/min until failure. Results: Analysis of variance indicated significant differences between the surface treatments. Results of mean comparisons using Tukey's test showed that significantly higher shear bond strengths were developed by bonding composite resin to the surfaces that were previously treated with MMA and then with the bonding agent when compared to the other treatments. Conclusion: Combined surface treatment of MMA monomer followed by application of light-cured adhesive resin provided the highest shear bond strength between composite resin and acrylic resin denture teeth.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The aim of this investigation was to evaluate the cleaning effect of CO 2 on surface topography and composition of failed dental implant surfaces. Ten failed dental implants were retrieved from nine patients (mean age, 46.33 ± 5.81 years) as a result of early or late failure. The implants were divided into two parts: one side of the implant was irradiated with a CO 2 laser (test side), while the other side did not receive irradiation (control side). The CO 2 laser was operated at 1.2 W in a continuous wave for 40 seconds (40 J energy). The handpiece of the CO 2 laser was kept at a distance of 30 mm from the implant surface, resulting in a spot area of 0.031415 cm 2 (38.20 W/cm 2; 1559 J/cm 2) in scanning mode (cervical-apical). One unused dental implant was used as a negative control for both groups. All implant surfaces were examined by scanning electron mi croscopy (SEM) and energy-dispersive spectrometer x-ray (EDS) for element analysis. SEM showed that the surface of the test sides consisted of different degrees of organic residues, appearing mainly as dark stains similar to those observed on the control sides. None of the test surfaces presented alterations such as crater-like alterations, lava-like layers, or melting compared with the nonirradiated surfaces. Foreign elements such as carbon, oxygen, sodium, calcium, and aluminum were detected on both sides. These results suggest that CO 2 laser irradiation does not modify the implant surface, although the cleaning effect was not satisfactory.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

This work aims at finding out the threshold to burning in surface grinding process. Acoustic emission and electric power signals are acquired from an analog-digital converter and processed through algorithms in order to generate a control signal to inform the operator or interrupt the process in the case of burning occurrence. The thresholds that dictate the situation of burn and non-burn were studied as well as a comparison between the two parameters was carried out. In the experimental work one type of steel (ABNT-1045 annealed) and one type of grinding wheel referred to as TARGA model 3TG80.3-NV were employed. Copyright © 2005 by ABCM.