Resumo:

We report the synthesis and structural characterization of ferroelectric bismuth vanadate (Bi2VO5.5) (BVO) nanotubes within the nanoporous anodic aluminum oxide (AAO) templates via sol-gel method. The as-prepared BVO nanotubes were characterized by X-ray powder diffraction (XRD), Scanning Electron Microscope (SEM), High-Resolution Transmission Electron Microscope (HRTEM) and the stoichiometry of the nanotubes was established by energy-dispersive X-ray spectroscopy (EDX). Postannealed (675 degrees C for 1 h), BVO nanotubes were a polycrystalline and the XRD studies confirmed the crystal structure to be orthorhombic. The uniformity in diameter and length of the nanotubes as reveled by the TEM and SEM suggested that these were influenced to a guest extent by the thickness and pore diameter of the nanoporous AAO template. EDX analysis demonstrated the formation of stoichiometric Bi2VO5.5 phase. HRTEM confirmed that the obtained BVO nanotubes were made up of nanoparticles of 5-9 nm range. The possible formation mechanism of nanotubes was elucidated.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Tellurite-based glasses in the TeO2-K3Li2Nb5O15, TeO2-Ba5Li2Ti2Nb8O30, and V2Te2O9 were fabricated by the conventional melt-quenching technique. Amorphous and glassy characteristics of the as-quenched samples were established via the X-ray powder diffraction technique and differential thermal analysis, respectively. The as-quenched samples were irradiated by an excimer laser (248 nm). The effect of laser power, duration of irradiation, and the frequency of the laser pulses on the surface features of the above glasses were studied. The optical microscopic studies carried out on the above systems revealed the presence of quasi-periodic and periodic structures on their surfaces. The local compositional variations of these structures were confirmed by back-scattered electron imaging using scanning electron microscope accompanied by energy-dispersive X-ray analysis. These results were convincing enough to state that the glasses in the present investigations had undergone spinodal decomposition on laser irradiation. The incidence of the interconnected texture of two different phases was observed owing to the quenching effect produced by the heating and cooling cycle of the successive laser pulses. Ring- and line-shaped patterns were also observed, respectively, when the pulse frequency of the laser and the duration of irradiation were increased.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, we report the synthesis of barium zirconate, BaZrO3, (BZ) nanotubes fabricated by the modified sol-gel method within the nanochannels of anodic aluminum oxide (AAO) templates. The morphology, structure, and composition of as prepared nanotubes were characterized by means of X-ray diffraction (XRD), field emission scanning electron microscope (FE-SEM), transmission electron microscope (TEM), selected-area electron diffraction ( SAED), high resolution TEM (HRTEM) and energy-dispersive X-ray spectroscopy (EDX). The results of XRD and SAED indicated that postannealed (at 650 degrees C for 1 h) BZ nanotubes (BZNTs) exhibited a polycrystalline cubic perovskite crystal structure. SEM and TEM analysis revealed that BZNTs possessed a uniform length and diameter (similar to 200 nm) and the thickness of the wall of the BZNTs was about 20 nm. Y-junctions, multiple branching and typical T-junctions were also observed in some BZNTs. EDX analysis demonstrated that stoichiometric BaZrO3 was formed. HRTEM image confirmed that the obtained BZNTs were composed of nanoparticles in the range of 5-10 nm. The possible formation mechanism of BZNTs was discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this research fabrication of crystalline PbZrO3 (PZ) nanoparticles and their phase transformation behavior is investigated. A novel sol-gel method was used for the synthesis of air-stable and precipitate-free diol-based sol of PZ, which was dried at 150 degrees C and then calcined at 300-700 degrees C for 1 h. The morphology, crystallinity and phase formation of as synthesized nanoparticles were studied by the selected-area electron diffraction (SAED), X-ray diffraction (XRD), thermal gravimetric analysis/differential scanning calorimetry (TGA-DSC), and high resolution transmission electron microscope (HRTEM). The XRD, SAED, and TGA-DSC analyses confirmed the tetragonal lead rich zirconia phase (t-Z phase) and monoclinic zirconia phase (m-Z phase) as the intermediate phases during the calcinations process followed by crystallization of single orthorhombic PZ phase at about 700 degrees C. The average PZ particle size was observed about 20 nm as confirmed by TEM study. Energy-dispersive X-ray spectroscopy (EDX) analysis demonstrated that stoichiometric PbZrO3 was formed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A direct borohydride-hydrogen peroxide fuel cell employing carbon-supported Prussian Blue (PB) as mediated electron-transfer cathode catalyst is reported. While operating at 30 °C, the direct borohydride-hydrogen peroxide fuel cell employing carbon-supported PB cathode catalyst shows superior performance with the maximum output power density of 68 mW cm−2 at an operating voltage of 1.1 V compared to direct borohydride-hydrogen peroxide fuel cell employing the conventional gold-based cathode with the maximum output power density of 47 mW cm−2 at an operating voltage of 0.7 V. X-ray diffraction (XRD), Scanning Electron Microscopy (SEM), and Energy Dispersive X-ray Analysis (EDAX) suggest that anchoring of Cetyl-Trimethyl Ammonium Bromide (CTAB) as a surfactant moiety on carbon-supported PB affects the catalyst morphology. Polarization studies on direct borohydride-hydrogen peroxide fuel cell with carbon-supported CTAB-anchored PB cathode exhibit better performance with the maximum output power density of 50 mW cm−2 at an operating voltage of 1 V than the direct borohydride-hydrogen peroxide fuel cell with carbon-supported Prussian Blue without CTAB with the maximum output power density of 29 mW cm−2 at an operating voltage of 1 V.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Thin films of Cd1−xMnxS (0<=x<=0.5) were deposited on glass substrates by thermal evaporation. All the films were deposited at 300 K and annealed at 373, 473, and 573 K for 1 h in a high vacuum in the range 10−4 Pa. The as-deposited and the annealed films were characterized for composition, structure, and microstructure by using energy-dispersive X-ray, X-ray diffraction, scanning electron microscopy, and atomic force microscopy (AFM). The electrical properties were studied by Hall effect measurement. Electrical conductivity was studied in the temperature range 190–450 K. AFM studies showed that all the films were in nanocrystalline form with grain size varying in the range between 36 and 82 nm. Grain size studies showed a definite increase with annealing temperature. All the films exhibited wurtzite structure of the host material. The lattice parameter varied linearly with composition, following Vegard's law in the entire composition range. Grain size, electrical conductivity, Hall mobility, carrier concentration, and activation energy varied, exhibiting either maxima or minima at x=0.3.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polymeric outdoor insulators are being increasingly used for electrical power transmission and distribution in the recent years. One of the current topics of interest for the power transmission community is the aging of such outdoor polymeric insulators. A few research groups are carrying out aging studies at room temperature with wet period as an integral part of multistress aging cycle as specified by IEC standards. However, aging effect due to dry conditions alone at elevated temperatures and electric stress in the presence of radiation environment has probably not been explored. It is interesting to study and understand the insulator performance under dry conditions where wet periods are either rare or absent and to estimate the extent of aging caused by multiple stresses. This paper deals with the long-term accelerated multistress aging on full-scale 11 kV distribution class composite silicone rubber insulators. In order to assess the long-term synergistic effect of electric stress, temperature and UV radiation on insulators, they are subjected to accelerated aging in a specially designed multistress-aging chamber for 3800 hours. All the stresses are applied at an accelerated level. Using a data acquisition system developed for the work, leakage current has been monitored in LabVIEW environment. Chemical changes due to degradations have been studied using Energy Dispersive X-Ray analysis, Scanning Electron Microscope and Fourier transform Infrared Spectroscopy. Periodically different parameters like low molecular weight (LMW) molecular content, hydrophobicity, leakage current and surface morphology were monitored. The aging study is under progress and only intermediate results are presented in this paper.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The compositional, structural, microstructural, dc electrical conductivity and optical properties of undoped zinc oxide films prepared by the sol-gel process using a spin-coating technique were investigated. The ZnO films were obtained by 5 cycle spin-coated and dried zinc oxide films followed by annealing in air at 600 A degrees C. The films deposited on the platinum coated silicon substrate were crystallized in a hexagonal wurtzite form. The energy-dispersive X-ray (EDX) spectrometry shows Zn and O elements in the products with an approximate molar ratio. TEM image of ZnO thin film shows that a grain of about 60-80 nm in size is really an aggregate of many small crystallites of around 10-20 nm. Electron diffraction pattern shows that the ZnO films exhibited hexagonal structure. The SEM micrograph showed that the films consist in nanocrystalline grains randomly distributed with voids in different regions. The dc conductivity found in the range of 10(-5)-10(-6) (Omega cm)(-1). The optical study showed that the spectra for all samples give the transparency in the visible range.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Wear of etched near-eutectic aluminium silicon alloy slid against a steel ball under ambient is explored. The sliding velocity is kept low (0.01 m/s) and the nominal contact pressure is varied in a 15-40 MPa range. Four stages of wear are identified; ultra mild wear, mild wear, severe wear and post severe oxidative wear. The first transition is controlled by the protrusions of silicon particles, projecting out of the aluminium alloy matrix. Once these protrusions disappear under pressure and sliding, oxidation and bulk energy dissipation mechanisms take over to institute transitions to other stages of wear. The phenomenological characteristics of wear stages are explored using a variety of techniques including nanoindentation, focused ion beam milling, electron microscopy, X-ray photoelectron spectroscopy (XPS), energy dispersive X-ray spectroscopy (EDS) and optical interferometry. (c) 2010 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This thesis comprises four intercomplementary parts that introduce new approaches to brittle reaction layers and mechanical compatibility of metalloceramic joints created when fusing dental ceramics to titanium. Several different methods including atomic layer deposition (ALD), sessile drop contact angle measurements, scanning acoustic microscopy (SAM), three-point bending (TPB, DIN 13 927 / ISO 9693), cross-section microscopy, scanning electron microscopy (SEM), and energy dispersive X-ray spectroscopy (EDS) were employed. The first part investigates the effects of TiO2 layer structure and thickness on the joint strength of the titanium-metalloceramic system. Samples with all tested TiO2 thicknesses displayed good ceramics adhesion to Ti, and uniform TPB results. The fracture mode was independent of oxide layer thickness and structure. Cracking occurred deeper inside titanium, in the oxygen-rich Ti[O]x solid solution surface layer. During dental ceramics firing TiO2 layers dissociate and joints become brittle with increased dissolution of oxygen into metallic Ti and consequent reduction in the metal plasticity. To accomplish an ideal metalloceramic joint this needs to be resolved. The second part introduces photoinduced superhydrophilicity of TiO2. Test samples with ALD deposited anatase TiO2 films were produced. Samples were irradiated with UV light to induce superhydrophilicity of the surfaces through a cascade leading to increased amount of surface hydroxyl groups. Superhydrophilicity (contact angle ~0˚) was achieved within 2 minutes of UV radiation. Partial recovery of the contact angle was observed during the first 10 minutes after UV exposure. Total recovery was not observed within 24h storage. Photoinduced ultrahydrophilicity can be used to enhance wettability of titanium surfaces, an important factor in dental ceramics veneering processes. The third part addresses interlayers designed to restrain oxygen dissolution into Ti during dental ceramics fusing. The main requirements for an ideal interlayer material are proposed. Based on these criteria and systematic exclusion of possible interlayer materials silver (Ag) interlayers were chosen. TPB results were significantly better in when 5 μm Ag interlayers were used compared to only Al2O3-blasted samples. In samples with these Ag interlayers multiple cracks occurred inside dental ceramics, none inside Ti structure. Ag interlayers of 5 μm on Al2O3-blasted samples can be efficiently used to retard formation of the brittle oxygen-rich Ti[O]x layer, thus enhancing metalloceramic joint integrity. The most brittle component in metalloceramic joints with 5 μm Ag interlayers was bulk dental ceramics instead of Ti[O]x. The fourth part investigates the importance of mechanical interlocking. According to the results, the significance of mechanical interlocking achieved by conventional surface treatments can be questioned as long as the formation of the brittle layers (mainly oxygen-rich Ti[O]x) cannot be sufficiently controlled. In summary in contrast to former impressions of thick titanium oxide layers this thesis clearly demonstrates diffusion of oxygen from sintering atmosphere and SiO2 to Ti structures during dental ceramics firing and the following formation of brittle Ti[O]x solid solution as the most important factors predisposing joints between Ti and SiO2-based dental ceramics to low strength. This among other predisposing factors such as residual stresses created by the coefficient of thermal expansion mismatch between dental ceramics and Ti frameworks can be avoided with Ag interlayers.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The out-diffusion of germanium from the core of a photosensitive fiber under elevated temperature is exploited to form a Fabry-Perot filter within a single fiber Bragg grating, by subjecting the diffused region to a single exposure using the standard phase-mask technique. A key aspect of our work is the measurement of the out-diffusion through energy dispersive X-ray analysis. Furthermore, we demonstrate the use of the above single-grating filter for discrimination and simultaneous measurement of strain and temperature. The proposed technique provides a significant advantage over other existing methods that require at least two gratings.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO (core)/graphitic (shell) nanowires were successfully fabricated by a one-step method. Morphology of the as-grown nanowires was studied in detail by scanning electron microscopy, transmission electron microscopy (TEM), and energy dispersive X-ray analysis (EDS). High resolution TEM micrographs and selected area electron diffraction patterns reveal the core/shell morphology of the nanowires that grew along the c-axis of ZnO. EDS study of the nanowires confirms that there are no impurities within the detectable limit. Superconducting quantum interference device magnetometer measurements show room temperature ferromagnetic ordering in these core/shell nanowires. (C) 2010 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Germanium nanowires were grown on Au coated Si substrates at 380 degrees C in a high vacuum (5 x 10(-5) Torr) by e-beam evaporation of Germanium (Ge). The morphology observation by a field emission scanning electron microscope (FESEM) shows that the grown nanowires are randomly oriented with an average length and diameter of 600 nm and 120 nm respectively for a deposition time of 60 min. The nanowire growth ratewas measured to be similar to 10 nm/min. Transmission electron microscope (TEM) studies revealed that the Ge nanowires were single crystalline in nature and further energy dispersive X-ray analysis(EDAX) has shown that the tip of the grown nanowires was capped with Au nanoparticles, this shows that the growth of the Ge nanowires occurs by the vapour liquid solid (VLS) mechanism. HRTEM studies on the grown Ge nanowire show that they are single crystalline in nature and the growth direction was identified to be along [110]. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Monophasic Na0.5La0.5Bi4Ti4O15 powders were synthesized via the conventional solid-state reaction route. The X-ray powder diffraction (XRD), selected area electron diffraction (SAED) and high resolution transmission electron microscopy (HRTEM) studies carried out on the as synthesized powdered samples confirmed the phase to be a four-layer Aurivillius that crystallizes in an orthorhombic A2(1)am space group. The microstructure and the chemical composition of the sintered sample were examined by scanning electron microscope (SEM) equipped with an energy dispersive X-ray analyzer (EDX). The dielectric properties of the ceramics have been studied in the 27-700 degrees C temperature range at various frequencies (100 Hz to 1 MHz). A sharp dielectric anomaly was observed at 580 degrees C for all the frequencies corresponding to the ferroelectric to paraelectric phase transition. Saturated ferroelectric hysteresis loops were observed at 200 degrees C and the associated remnant polarization (P-r) and coercive field (E-c) were found to be 7.4 mu C/cm(2) and 34.8 kV/cm, respectively. AC conductivity analysis confirmed the existence of two different conduction mechanisms in the ferroelectric region. Activation energies calculated from the Arrhenius plots were similar to 0.24 eV and similar to 0.84 eV in the 300-450 degrees C and 450-580 degrees C temperature ranges, respectively. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In EHV and UHV power transmission lines, corona could occur even on well designed transmission line hardware and insulators especially under wet conditions. Corona if allowed to occur continuously can significantly damage the polymeric insulators used in such lines in the long run. This paper presents the experimental results of corona aging studies conducted on unfilled silicone rubber as well as filled silicone rubber nanocomposites. Corona aging studies were conducted on silicone rubber samples with filler concentrations of 0, 1, 2 and 3 % by wt of nanosilica for 25 h and 50 h. Needle-plane electrode geometry has been used to create the corona on the samples. Different characterization techniques such as Scanning Electron Microscopy, Energy Dispersive X-ray analysis, Hydrophobicity, Fourier Transform Infrared Spectroscopy, and Optical Profilometry have been used to assess the relative performance of the samples with respect to corona aging. Results indicate that at 3 wt %, the performance of the nanocomposite is much better than the unfilled silicon rubber which can be attributed to the modifications in the material caused by the size factor of the filler.