968 resultados para Dielectric ceramics
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Complex dielectric permittivity measurements in Pb Nb2 O6 ceramics were performed in a frequency and temperature range of 1 kHz-1 MHz and from 15 to 900 K, respectively. The results revealed two dielectric anomalies showing typical characteristics of relaxor ferroelectric materials at cryogenic temperatures. Comparison with other tetragonal tungsten bronze (TTB) structure-type materials suggests the existence of successive phase transitions, which until now were not reported. The observed low temperature dielectric behaviors seem to be due to intrinsic physical characteristics related to the TTB structure. © 2007 American Institute of Physics.
Resumo:
The dielectric properties of the 0.65[Pb(Mg 1/3Nb 2/3)O 3]-0.35PbTiO 3 ferroelectric ceramic composition were investigated viewing the capability to be used for tunable microwave applications. The dielectric response has been studied for three selected temperatures (300 K, 370 K and 400 K), below the paraelectric- ferroelectric phase transition temperature, as a function of the applied 'bias' electric field. The obtained dielectric tunability was found to be around 60 %, under an electric field of 19 kV/cm, which makes the studied ceramic composition an excellent candidate for application in the electro-electronic industry, as tunable devices. © 2010 IEEE.
Resumo:
Dielectric spectroscopy was used in this study to examine polycrystalline vanadium and tungstendoped BaZr 0.1Ti 0.90O 3 (BZT10:2V and BZT10:2W) ceramics obtained by the mixed oxide method. According to X-ray diffraction analyses, addition of vanadium and tungsten lead to ceramics free of secondary phases. SEM analyses reveal that both dopants result in slower oxygen ion motion and consequently lower grain growth rate. Temperature dependence dielectric study showed normal ferroelectric to paraelectric transition well above the room temperature for the BZT10 and BZT10:2V ceramics. However, BZT10:2W ceramic showed a relaxor-like behavior near phase transition characterized by the empirical parameter γ. Piezoelectric force microscopy images reveals that the piezoelectric coefficient is strongly influenced by type of donor dopant suggesting promising applications for dynamic random access memories and data-storage media. Copyright © 2010 American Scientific Publishers All rights reserved.
Resumo:
This paper reports the influence of Sr- and Ca-substitution on the structural and ferroelectric properties of Pb1-xSrxZr0.40Ti0.60O3 (PSZT) and Pb1-xCaxZr0.40Ti0.60O3 (PCZT) ceramic systems. The dielectric measurements show that these substitutions cause a diffuse behavior in the dielectric permittivity curves for all samples. According to the X-ray absorption near-edge structure (XANES) spectra collected at Ti K- and LIII-edge, when Pb was replaced by Sr or Ca, a decrease in the local distortion around Ti atoms in the TiO6 octahedron could be observed. The O K-edge XANES spectra also revealed that the hybridization between O 2p and Pb 6sp states decreased as the amount of Sr or Ca atoms increased. Based on these results, it was possible to ascertain that the ferroelectric behavior in PSZT and PCZT samples bears a close correlation to the hybridization weakening between O 2p and Pb 6 sp states. © 2013 by American Scientific Publishers.
Resumo:
Ca-1 -xSmxCu3Ti4O12 (x = 0.0, 0.2, 03) electronic ceramics were fabricated via the chemical route using metal nitrate solutions in order to improve the dielectric properties of this ceramic. X-ray diffraction (XRD) analysis indicated the formation of a single CaCu3Ti4O12 (CCTO). Grain size of the samples doped with Sm3+ was in the range of 1-2 mu m, as opposed to 50-100 mu m in the pure samples of CCTO. The cutoff frequency with the doping was remarkably shifted, from 1 MHz (pure CCTO) to 10 MHz (doped CCTO). Meanwhile, the real dielectric (epsilon(r)) and imaginary dielectric (epsilon '') constants showed a decrease as the doping was increased. (C) 2013 Elsevier B.V. All rights reserved.
Resumo:
The electrical response of Ba(Ti0.90Zr0.10)O3 (BZT) ceramics obtained by the mixed oxide method as a functionof tungsten content was investigated. According to X-ray diffraction analysis the single phase BZT1W (1wt.% W doped BZT) and BZT2W (2 wt.% W doped BZT) ceramics, crystallized in a perovskite structure, wereobtained. It is also shown that tungsten substituted ceramics can be sintered at a reduced temperature whencompared to the undoped BZT. Electron paramagnetic resonance (EPR) analyses reveals that substitution ofTi4+ by W6+ causes distortion in the crystal structure changing lattice parameter. Substitution of W6+ on B-siteof ABO3 perovskite BZT ceramics shifted the phase transition to lower temperatures up to a tungsten contentof 2 wt.% leading to a relaxor-like behaviour.Keywords: donor dopant; ceramics; dielectric response; mixed oxide method
Resumo:
Bi3.25La0.75-xErxTi3O12 and Bi3.25La0.75Ti3-xErxO12-delta ceramics were prepared and studied in this work in terms of dopant-induced phase and microstructure development as well as dielectric response. The results show that introduction of Er3+ tends to reduce the materials' sintering temperature and average grain size. Moreover, it was noted that in these systems the substitution site of this dopant is controlled by valence state and ionic radii mismatch effects. In particular, even when a nominal substitution of Ti4+ is conceived, here it is found that Er3+ also incorporates at the (Bi,La)(3+) sites. These and other interesting concluding remarks from this work, including Er3+ tolerance, were possible only after comparing, especially, the X-ray diffraction results and the intrinsic ferroelectric characteristics extracted from the dielectric measurements. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Ba0.77Ca0.23TiO3 ceramics were produced in this work starting from nanopowders synthesized via a polymeric precursor method. By adjusting the pH values of the precursor solutions above 7, it was possible to prepare powders weakly aggregated and with a smaller particle size, both facts which traduced into an enhanced nanopowders' sintering process at comparatively lower temperatures. Irrespective of the initial pH value, highly-dense and second phase-free ceramics were obtained following optimal sintering parameters (temperature and time) extracted from dilatometric and density measurements. By considering these and other sintering conditions, moreover, polycrystalline materials with an average grain size varying from 0.35 to 8 mm were produced, the grain growth process involving liquid phase-assisted sintering for heat treatments achieved at 1320 °C. The study of grain size effects on the ferroelectric properties of these materials was conducted, the results being discussed in the light of previous debates, including grain size-dependent degree of tetragonal distortion in such materials, as verified in this work.
Resumo:
CaCu3Ti4O12 (CCTO) was prepared by a conventional synthesis (CS) and through reaction sintering, in which synthesis and sintering of the material take place in one single step. The microstructure and the dielectric properties of CCTO have been studied by XRD, FE-SEM, EDS, AFM, and impedance spectroscopy to correlate structure, microstructure, and electrical properties. Samples prepared by reactive sintering show very similar dielectric behavior to those prepared by CS. Therefore, it is possible to prepare CCTO by means of a single-step processing method.
Resumo:
CaCu3(Ti4xHfx)O12 ceramics (JC = 0.04, 0.1 and 0.2) were prepared by conventional synthesis (CS) and through reactive sintering (RS), in which synthesis and sintering of the material take place in one single step. The microstructure and the dielectric properties of Hf-doped CCTO (CCTOHf) have been studied by XRD, FE-SEM, AFM, Raman and impedance spectroscopy (IS) in order to correlate the structure, microstructure and the electrical properties. Samples prepared by reactive sintering show slightly higher dielectric constant than those prepared by conventional synthesis in the same way than the pure CCTO. Dielectric constant and dielectric losses decrease slightly increasing Hf content. For CCTOHf ceramics with x> 0.04 for CS and x> 0.1 for RS, a secondary phase HfTi04 appears. As expected, the reactive sintering processing method allows a higher incorporation of Hf in the CCTO lattice than the conventional synthesis one.
Resumo:
Single-phase Ba(Cd1/3Ta2/3)O-3 powder was produced using conventional solid state reaction methods. Ba(Cd1/3Ta2/3)O-3 ceramics with 2 wt % ZnO as sintering additive sintered at 1550 degreesC exhibited a dielectric constant of similar to32 and loss tangent of 5x10(-5) at 2 GHz. X-ray diffraction and thermogravimetric measurements were used to characterize the structural and thermodynamic properties of the material. Ab initio electronic structure calculations were used to give insight into the unusual properties of Ba(Cd1/3Ta2/3)O-3, as well as a similar and more widely used material Ba(Zn1/3Ta2/3)O-3. While both compounds have a hexagonal Bravais lattice, the P321 space group of Ba(Cd1/3Ta2/3)O-3 is reduced from P (3) under bar m1 of Ba(Zn1/3Ta2/3)O-3 as a result of a distortion of oxygen away from the symmetric position between the Ta and Cd ions. Both of the compounds have a conduction band minimum and valence band maximum composed of mostly weakly itinerant Ta 5d and Zn 3d/Cd 4d levels, respectively. The covalent nature of the directional d-electron bonding in these high-Z oxides plays an important role in producing a more rigid lattice with higher melting points and enhanced phonon energies, and is suggested to play an important role in producing materials with a high dielectric constant and low microwave loss. (C) 2005 American Institute of Physics.
Resumo:
The ferroelectric and dielectric properties of cerium (Ce) substituted La2Ti2O7 (LTO) have been investigated. Single phase, dense La2-xCexTi2O7 (x=0.15, 0.25, 0.35) ceramics were prepared by spark plasma sintering. The solubility limit of Ce in La2-xCexTi2O7 was found to be between 0.35 and 0.5. The a-, b- and c-axes of the unit cell decrease with increasing Ce substitution. The Curie point (Tc) of La2-xCexTi2O7 (x=0, 0.15, 0.25, 0.35) decreases and dielectric constant and loss increase with increasing Ce substitution. Cerium can increase the d33 of La2Ti2O7. The highest d33 was 3.9±0.1pC/N for La1.85Ce0.15Ti2O7 textured ceramic. © 2012 Elsevier Ltd.
Resumo:
The solid solution system Nd2−xCexTi2O7 has been investigated. The solubility limit of Ce in Nd2−xCexTi2O7 was found to be 0·5–0·75 according to X-ray diffraction and X-ray photoelectron spectroscopy results. Ce substitution increases the b and c axes and the volume of the unit cell due to its larger ionic radius. Nd2−xCexTi2O7 (x = 0·05, 0·25, 0·5, 0·75) textured ceramics were fabricated using spark plasma sintering. The ferroelectric and dielectric properties of the ceramics were studied. Ce substitution decreases the Curie point Tc of Nd2−xCexTi2O7 compounds. The results suggest that the Tc of Ce2Ti2O7 is <1445°C.