999 resultados para Hydrological stability
Resumo:
用密度泛含方法研究了LaC5n(n=-1,0,+1)分子簇的结构和稳定性及振动光谱,对这个六原子体系提出了三种可能构型,点群结构为C2v对称性.第一个构型为La接在弯曲的C5链上,第二个是La通过二个键与C5环相连第三个是La通过一个键与C5环相连;结果表明,第一个构型即当La接在弯曲的C5链上时能量最低.振动光谱分析指出,当n=-1时,第二个构型为局域极小值;当n=+1时,第一个和第二个构型为局域极小值;对n=0,局域极小值没有找到.
Resumo:
Polytetrafluoroethylene (PTFE) has never been reported to form a network structure when subjected to high energy radiation. Results obtained in this work indicates that when irradiation is performed under 330-340-degrees-C in vacuo PTFE can be crosslinked
Resumo:
The spectrochemistry of Eu2+-doped perovskite KMgF3 was examined and discussed. Eu2+ can replace some of the K+ in the KMgF3 crystal, and simultaneously the corresponding cation hole can be compensated with the F- or O2- in the matrix. The emission intensity of Eu2+ due to the f --> f transition increased when Na+, Rb+ or F- was doped in KMgF3:Eu2+. Two mechanisms of charge compensation were proposed. No obvious valence change of Eu2+ occurred in KMgF3:Eu2+ after calcinating at high temperature, e.g. 900-degrees-C. It was found that the valence stability of Eu2+ improved after incorporation into the matrix.
Resumo:
In this work, the effects of radiation on polytetrafluoroethylene (PTFE) samples with different crystallinity were studied. Using Suwa's equation for calculating the number-average molecular weight of PTFE, the radiation-induced reduction in molecular weight was followed and the G values for scission of PTFE were also obtained on the basis of the changes in molecular weight. The G(scission) for as-polymerized PTFE was 2.15 +/- 0.01, whereas for sintered sample, which has a relative low crystallinity, G(scission) = 6.0 +/- 0.14.
Resumo:
By examining the changes in melting temperature, heat of fusion, tensile strength and ultimate elongation at 150-degrees-C, and weight loss, radiation effects on perfluoroalkoxy resins (PFA) were investigated. The results show that at the temperatures used here the predominant effect caused by radiation on PFA is degradation of the molecular weight. The radiation stability is much better than that of polytetrafluoroethylene, however.
Resumo:
As a typical example of a polymer degraded by radiation, the radiation stability of PTFE was observed to depend upon irradiation conditions. Increases in irradiation temperature and crystallinity were found to increase its radiation stability whereas increase in the concentration of oxygen in the system over a certain range was observed to have little effect on radiation-induced reactions of PTFE as measured by changes in number-average molecular weight, melting temperature and crystallinity.
Resumo:
The melt flow behaviour of LDPE/HDPE blends with various compositions have been determined by melt flow index (MFI) measurement. The effects of stabilizers, photo-sensitizers, multiple extrusions and short-term photooxidation have been studied. The results show that there is no marked thermal stability difference between homopolymers and blends without multiple extrusions, no matter whether stabilizers or photo-sensitizers are added. Multiple extrusions or photo-sensitizers reduce their thermal stability, shown by the decrease in MFI. The decrease in MFI of photooxidized samples does not imply serious structural change and shows that the active species formed during photooxidation induce a crosslinking reaction in the melt indexer. Multiple extrusions increase the number of active species formed in LDPE or blends and lead to an obvious decrease in MFI. It is suggested that LDPE and LDPE-rich blends after short-term photooxidation can be characterized by MFI measurement. In contrast, HDPE cannot be characterized by this method due to its linear structure.
Resumo:
The gel content of crosslinked perfluoroethylene-propylene copolymer was obtained by extraction with fluoro-chloro oil. It was then treated by the Charlesby-Pinner equation. The results obtained revealed that both the gelation dose and the ratio of fracture to crosslinking density decreased with increasing irradiation temperature.